ISO 5832-2 Grade 4A Titanium Plate | Annealed Implant Grade 4
What is ISO 5832-2 Grade 4A titanium plate?
ISO 5832-2 Grade 4A titanium plate is made to ISO 5832-2, the international standard for unalloyed titanium used to manufacture surgical implants. Grade 4A is the annealed condition of the highest-oxygen grade, with 550 MPa minimum tensile strength. It is the usual Grade 4 condition for plate and sheet.
Unalloyed titanium for implants is commercially pure titanium with tightly controlled interstitials. Strength rises with oxygen and iron content, and the material cannot be hardened by heat treatment, so higher strength grades rely on higher interstitials or, for Grade 4B, cold work. Biocompatibility rests on the stable oxide film formed on the surface.
Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.
The ISO 5832 series covers metallic materials for surgical implants; Part 2 covers unalloyed titanium and Part 3 covers Ti-6Al-4V. Grades are defined by oxygen and iron limits and the resulting tensile strength, with Grade 4 available annealed (4A) or cold worked (4B).
SHH STEEL handles Grade 4A plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ISO 5832-2 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 4, ASME SB-265 Grade 4, JIS H4600 Class 4 TP550.
Material specification for ISO 5832-2 Grade 4A
ISO 5832-2 specifies the characteristics of, and test methods for, unalloyed titanium for use in the manufacture of surgical implants. It is a raw-material standard: it covers chemistry, microstructure and mechanical properties, not the finished device. The 2025 edition lists six grades defined by tensile strength.
| Ordering item | ISO 5832-2 basis |
|---|---|
| Standard | ISO 5832-2; state the edition (2018 or 2025) required by the device file |
| Grade | Grade 4A |
| Condition | Annealed |
| Product form | Plate or sheet cut to the device maker’s size; bar and wire are also covered by the standard |
| Microstructure | Uniform, grain size not coarser than the specified limit, free of continuous alpha case |
| Certificate | Inspection certificate with chemistry, hydrogen after final processing and mechanical results |
Except for hydrogen, chemical requirements may be met by the ingot analysis; hydrogen is determined on the product after the final heat treatment and pickling. Device makers normally add their own requirements for surface condition, traceability and cleanliness on the purchase order.
Device files often cite both ISO 5832-2 and ASTM F67, the ASTM specification for unalloyed titanium for surgical implants. The two are close but not identical in grade limits and test details, so material certified to one standard is not automatically acceptable under the other. If both are named, the certificate must show compliance with each, and the edition of each standard should be fixed in the device technical file.
Chemical composition of ISO 5832-2 Grade 4A
Single values are maximums. Titanium is the balance, and no other elements are intentionally added.
| Element | Limit, % (mass fraction) |
|---|---|
| Nitrogen (N) | 0.05 max |
| Carbon (C) | 0.08 max |
| Hydrogen (H) | 0.0125 max |
| Iron (Fe) | 0.50 max |
| Oxygen (O) | 0.40 max |
| Titanium (Ti) | Balance |
Except for hydrogen, chemical requirements may be met by the ingot analysis. Hydrogen is determined on the product after the final heat treatment and pickling, because surface treatments can raise it.
Mechanical properties of ISO 5832-2 Grade 4A
The values below are the requirements for Grade 4A plate in the annealed condition.
| Property | Requirement |
|---|---|
| Condition | Annealed |
| Tensile strength Rm, min | 550 MPa |
| 0.2% proof strength Rp0.2, min | 483 MPa |
| Elongation after fracture A, min | 15% |
| Reduction of area Z, min | 25% |
Tensile tests follow ISO 6892-1 at room temperature. Values are for the annealed condition. The microstructure must be uniform, with a grain size not coarser than the limit in the standard and no continuous alpha case.
Fatigue and device-level properties are not set by the material standard and must be validated by the device manufacturer.
Delivery condition, finish and marking
Implant-grade plate is supplied in the condition stated for the grade, with a surface agreed with the device manufacturer. Surface contamination, embedded particles and alpha case are not acceptable.
- Condition: Annealed
- Surface: pickled, ground or machined, as agreed
- Traceability: heat and lot identification on every piece and on the certificate
- Packing: clean, protected packing that prevents contamination and damage
Material is supplied annealed, except Grade 4B, which is supplied cold worked. Device makers often specify extra cleanliness, inclusion or ultrasonic requirements; include them on the order.
Welding and fabrication of Grade 4A titanium plate
Implant manufacturers rarely weld Grade 4A plate, but where joining is used the same rules as for industrial CP titanium apply: full inert-gas shielding until the metal is below about 400 °C, and no contamination of the surface.
- Cut and machine with clean, sharp tools and controlled heat
- Avoid iron pick-up and embedded abrasive; agree pickling or passivation after machining
- Keep material traceability to heat and lot through every processing step
- Qualify any welding or forming route as part of the device validation
Forming of plate for craniofacial and trauma parts is normally done on annealed material, with bend radii and springback set by the device maker’s process qualification.
Machining for implants uses sharp tools, controlled speeds and clean coolant that is compatible with the later cleaning process. Surface layers affected by machining or grinding are removed or controlled by the device maker’s validated finishing route.
These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.
Dimensional tolerances and flatness
ISO 5832-2 does not set plate dimensional tolerances; these are agreed between the device manufacturer and the supplier, often by drawing or by reference to an industrial plate standard.
State thickness, width, length, flatness, surface roughness and any cut-to-size drawing on the order. No stock sizes are implied by this page.
Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.
Applications and service limits of Grade 4A titanium plate
Typical uses of Grade 4A plate include:
- Craniomaxillofacial and trauma plates
- Bone plates, mesh and reconstruction plates
- Dental implant and abutment blanks
- Instrument and device components to the device maker’s drawing
ISO 5832-2 covers the raw material only. Fitness for a medical device depends on the design, processing, cleaning, sterilisation and regulatory approval, which are the device manufacturer’s responsibility. The material should not be bought to this standard for industrial process equipment, where ASTM B265 or similar industrial specifications apply.
When selecting Grade 4A, compare it with Grade 1 ELI, Grade 1, Grade 2. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.
Compare Grade 4A with other ISO 5832-2 grades
The grades below are the closest neighbours of Grade 4A in ISO 5832-2. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.
| Grade | Tensile strength | Yield / proof strength | Elongation, min | Typical role |
|---|---|---|---|---|
| Grade 1 ELI | 200 MPa | 140 MPa min | 30% | Lowest-interstitial implant grade |
| Grade 1 | 240 MPa | 170 MPa min | 24% | Most ductile standard implant grade |
| Grade 2 | 345 MPa | 275 MPa min | 20% | Common orthopaedic CP grade |
| Grade 3 | 450 MPa | 380 MPa min | 18% | Higher-strength implant CP grade |
| Grade 4A | 550 MPa | 483 MPa min | 15% | Annealed Grade 4 |
| Grade 4B | 680 MPa | 520 MPa min | 10% | Cold-worked Grade 4 |
Higher-oxygen grades give more strength but less ductility. Grade 4A and Grade 4B differ in condition, not in chemistry, and must not be interchanged without device-level review.
ISO 5832-2 Grade 4A equivalent grades
The designations below are commonly compared with ISO 5832-2 Grade 4A. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.
| Standard / system | Designation | Relationship to ISO 5832-2 Grade 4A |
|---|---|---|
| ASTM B265 | Grade 4 | Close equivalent; ASTM limits and tests apply |
| ASME SB-265 | Grade 4 | ASME Code version of the ASTM grade; ordered for pressure equipment |
| JIS H4600 | Class 4 (TP550) | Close equivalent; JIS strength range and tests differ |
| GB/T 3621 | TA4G | Close equivalent; confirm grade name and limits in the ordered edition |
| ISO 5832-2 | Grade 4B | Implant-grade counterpart; medical scope and tighter controls |
| UNS | R50700 | Same unified number as ASTM Grade 4 |
| DIN / EN material number | 3.7065 (Ti 4) | Close CP equivalent |
Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.
Why choose SHH STEEL for Grade 4A titanium plate
SHH STEEL supports specification-led purchasing of titanium plate and sheet.
- We quote to the ISO 5832-2 edition required by your device file
- Certificates are checked against the Grade 4A chemistry, hydrogen, tensile and microstructure requirements
- Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
- Finish, marking and packing are agreed before production
Questions on equivalents, dual certification or edition changes are answered before an order is placed.
How to enquire for ISO 5832-2 Grade 4A plate
Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.
| Enquiry item | Information required |
|---|---|
| Material | ISO 5832-2 Grade 4A, edition |
| Product form | Plate or sheet; device drawing if cut to size |
| Dimensions | Thickness, width, length, quantity and any cutting drawing |
| Finish | Descaled, sandblasted, ground or other agreed surface |
| Testing | Hydrogen after final processing, microstructure and any device-specific tests |
| Documents | Certificate type and any third-party inspection |
| Destination | Delivery place and packing requirements |
FAQ
-
Can ISO 5832-2 Grade 4A be used for industrial equipment?
- It can be supplied, but ISO 5832-2 is a raw-material standard for surgical implants and costs more to certify. Industrial process equipment is normally ordered to ASTM B265 or a similar industrial plate standard.
-
What is the tensile strength of ISO 5832-2 Grade 4A titanium plate?
- The requirement is 550 MPa minimum. The 0.2% proof or yield strength is 483 MPa minimum. Minimum elongation is 15%. Values apply to the condition and thickness range stated in the standard.
-
What is Grade 4A mainly used for?
- Typical uses include craniomaxillofacial and trauma plates, bone plates, mesh and reconstruction plates and dental implant and abutment blanks. The design engineer should confirm the grade for the actual service.
-
Does ISO 5832-2 set plate dimensions?
- No. It sets chemistry, microstructure and mechanical properties. Dimensions, tolerances and surface condition are agreed between the device maker and the supplier, usually by drawing.
-
What should I send for a quotation?
- Send ISO 5832-2 Grade 4A, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.
Request a quotation for ISO 5832-2 Grade 4A titanium plate
ISO 5832-2 Grade 4A is annealed implant Grade 4 specified for 550 MPa minimum tensile strength, 483 MPa minimum yield or proof strength and 15% minimum elongation in the annealed condition. Typical uses include craniomaxillofacial and trauma plates and bone plates, mesh and reconstruction plates.
Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ISO 5832-2 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.
Contact: admin@steelspecs.com