ISO 630-5 S355W Steel Plate | ISO 630-5 Weathering Steel - SHH STEEL

ISO 630-5 S355W Steel Plate | ISO↔EN 10025-5 Map

ISO 630-5 S355W is a hot-rolled structural weathering steel designation under ISO 630-5 (technical delivery conditions for steels with improved atmospheric corrosion resistance). It overlaps the EN 10025-5 W purchasing family; many projects dual-certify or accept EN product pages as the working specification. This page maps ISO 630-5 S355W to the live EN 10025-5 grades and links those product pages rather than duplicating SEO content. SHH STEEL supplies ISO 630-5 / EN 10025-5 weathering plate with EN 10204 3.1 (or 3.2) mill test certificates.
Equivalent Grades:
Primary map: EN 10025-5 S355J0W, EN 10025-5 S355J2W, EN 10025-5 S355K2W. Also compared with ASTM A588 / A242, Corten, GB/T 4171 NH/GNH, JIS SPA-H depending on W vs WP. Confirm against project specs; prefer the EN product page when the PO cites EN 10025-5.
Heat Treatment
S235 / S295 / S355 families: as-rolled, normalized/normalized rolled, TMCP or Q&T as ordered. Higher S420-S550: TMCP or Q&T.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
S355W vs EN / sibling ISO
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 630-5 S355W steel plate?

ISO 630-5 S355W belongs to ISO 630-5 Annex A structural weathering steels. Class: W (standard phosphorus weathering). ISO 630-5 Annex A grade designations (S235W, S295W, S355W, S355WP, S420W, …) overlap heavily with EN 10025-5 W/WP purchasing. These pages map ISO ↔ EN and link to existing EN product pages. They are not an SEO grade farm that duplicates every EN URL.

ISO designation uses a grade name plus a quality letter (Qualities A (no impact), B (+20 °C), C (0 °C), D and D1 (-20 °C; D1 higher energy), E (-40 °C).). It does not embed EN-style J0 / J2 tokens inside the ISO grade string. ISO qualities C / D / D1 / E roughly align with EN J0 / J2 / K2-style Charpy packages (C ≈ 0 °C; D/D1 ≈ -20 °C; E ≈ -40 °C). Order the ISO quality letter explicitly.

For day-to-day purchasing, start from the matching EN pages: EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W. Category hubs: ISO 630-5 · EN 10025-5 · Weathering Steel Plates.

Sibling ISO pages: ISO 630-5 S355WP · ISO 630-5 S235W. Related: Corten B · Q355NH · ASTM A242 Type 1 · JIS G3125 SPA-H.

Material Specification for ISO 630-5 S355W

Parameter Specification
Standard ISO 630-5 (Primary reference ISO 630-5:2023; confirm ordered edition on the MTC)
Grade S355W + quality letter (A-E / D1 as ordered)
Class W (standard phosphorus weathering)
EN map (primary) S355J0W / S355J2W / S355K2W
Product form Plate (reversing mill), wide flats, hot-rolled sections and bars (not sheet/strip; not tubular)
Thickness window Plates / wide flats / sections / bars: maximum nominal thickness 150 mm for S355W under ISO 630-5:2023
Delivery condition S235 / S295 / S355 families: as-rolled, normalized/normalized rolled, TMCP or Q&T as ordered. Higher S420-S550: TMCP or Q&T.
Certification EN 10204 3.1 / 3.2; ISO 10474 inspection documents as ordered; dual EN 10025-5 marking when agreed
Density 7.85 g/cm³

Chemical Composition guidance for ISO 630-5 S355W (EN dual-cert talk)

Important: ISO 630-5 heat and product analysis shall meet Tables A.1 / A.2 of the ordered edition. Public preview copies of ISO 630-5 often omit the full annex tables, so this page does not invent ISO cell values. When mills dual-certify to EN 10025-5, the EN chemistry below is the practical purchasing reference. Always verify every element on the MTC against the ordered ISO (and EN, if dual-certified) edition.

EN heat-analysis talk commonly used when mills dual-certify ISO 630-5 S355W with EN 10025-5 W grades. ISO Table A.1 / A.2 for the ordered edition still rule the ISO certificate.

Element EN 10025-5 S355J0W / S355J2W / S355K2W (dual-cert talk)
C ≤0.16
Si ≤0.50
Mn 0.50-1.50
P ≤0.035 (J0) / ≤0.030 (J2/K2)
S ≤0.035 (J0) / ≤0.030 (J2/K2)
Cr 0.40-0.80
Cu 0.25-0.55
Ni ≤0.65

Optional micro-alloying / nitrogen-binding practice follows the ordered standard (Al, Nb, V, Ti as applicable). Mo and Zr may appear within EN / ISO limits.

Mechanical Properties guidance for ISO 630-5 S355W

Mechanical properties for ISO 630-5 S355W shall meet Table A.3 (tensile) and Table A.4 (Charpy) of the ordered edition. Common dual-cert talk with EN 10025-5 uses the values below as a purchasing guide. Confirm every figure on the MTC.

Item Purchasing guide
Yield class ≥355 MPa (≤16 mm class; thickness steps per ISO Table A.3)
Tensile class About 470-630 MPa class (confirm ISO Table A.3 / dual-cert EN package)
Impact ISO qualities C / D / D1 / E roughly align with EN J0 / J2 / K2-style Charpy packages (C ≈ 0 °C; D/D1 ≈ -20 °C; E ≈ -40 °C). Order the ISO quality letter explicitly.

Prefer ordering against the live EN product page when the contract accepts EN 10025-5: EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W.

Density is approximately 7.85 g/cm³.

Delivery Conditions for ISO 630-5 S355W

S235 / S295 / S355 families: as-rolled, normalized/normalized rolled, TMCP or Q&T as ordered. Higher S420-S550: TMCP or Q&T.

The delivery condition shall be indicated in the inspection document. SHH STEEL supplies the condition named on the order and can dual-mark ISO 630-5 + EN 10025-5 when the mill package supports it.

Weldability of ISO 630-5 S355W

S355W is intended for welded or bolted structures. See ISO 630-5 Annex C for weldability notes and follow a qualified WPS based on composition, thickness and service temperature. W grades are generally the more fabrication-friendly track versus WP.

Related EN fabrication pages: EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W. Also: Q355NH · A588 Grade A.

Dimensional Tolerances for ISO 630-5 S355W

Dimensions, tolerances and mass follow ISO 630-1 as referenced by ISO 630-5, unless the order cites another dimensional agreement (for dual-cert EN packages, EN 10029 / EN 10051 etc. may apply as ordered).

Plates / wide flats / sections / bars: maximum nominal thickness 150 mm for S355W under ISO 630-5:2023

Applications and service limits for ISO 630-5 S355W

Typical applications for S355W (ISO / EN dual-cert talk):

  • Bridges and outdoor structural frames
  • Building facades and architectural weathering structures
  • Vehicles, containers and industrial outdoor fabrications
  • RFQs that cite ISO 630-5 S355W or the matching EN 10025-5 grade

Prefer the EN product pages for detailed fabrication content: EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W.

Related: ISO 630-5 S355WP · ISO 630-5 S235W · Corten A · Corten B · A242 Type 1 · SPA-H · Weathering Steel Plates.

Atmospheric exposure guidance for ISO 630-5 S355W

Bare S355W is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.

Environment Typical fit for bare ISO / EN weathering plate Note
Rural / mild industrial Usually suitable Needs wet/dry cycles for patina
Urban / general industrial Often suitable Check local pollution and design details
Coastal / marine splash with moderate chloride Use with caution May need coating, WSE talk, or another grade
Sheltered pockets that stay wet Not preferred bare Design out traps or coat locally
Continuous immersion / aggressive chloride Not recommended bare Select coated carbon steel or another material

ISO 630-5 also defines S355WSE (saline-environment weathering) as a separate class; it is not covered on this page.

ISO 630-5 S355W ↔ EN 10025-5 map and related grades

These grades are commonly compared with ISO 630-5 S355W. They are approximate, not automatic substitutes. Prefer the EN product page when the purchase order cites EN 10025-5.

Standard / family Grade Relation Product page
ISO 630-5 S355W This page –
ISO 630-5 S355WP Sibling ISO designation S355WP
ISO 630-5 S235W Sibling ISO designation S235W
EN 10025-5 S355J0W Primary overlap / dual-cert map S355J0W
EN 10025-5 S355J2W Primary overlap / dual-cert map S355J2W
EN 10025-5 S355K2W Primary overlap / dual-cert map S355K2W
Commercial / ASTM Corten B / A588 W-family talk Corten B · A588 Gr.A
GB/T 4171 Q355NH / Q235NH NH talk by strength class Q355NH · Q235NH
Category ISO / EN hubs Navigation ISO 630-5 · EN 10025-5 · Weathering Steel Plates

ISO 630-5 S355W vs sibling ISO vs EN 10025-5 (selection aid)

Selection aid for ISO ↔ EN purchasing. Not automatic substitutes.

Item S355W S355WP EN S355J2W
Standard home ISO 630-5 ISO 630-5 EN 10025-5 (live product pages)
Phosphorus track W (standard P) WP (high P) W
When buyers ask PO cites ISO 630-5 S355W PO cites ISO 630-5 S355WP PO cites EN 10025-5
Pages This page S355WP EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W

Why choose SHH STEEL for ISO 630-5 S355W

Supply, cutting and inspection for ISO 630-5 S355W

Item SHH STEEL supply note
Thickness Within ISO 630-5 window for S355W; confirm against ordered form
Size Width / length per order; cut-to-size on request
Delivery condition As ordered (AR / N / TMCP / Q&T per ISO rules for the grade family)
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request; dual ISO+EN marking when agreed
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs ISO 630-5 S355W + quality letter (and/or EN grade), thickness × width × length, quantity, delivery condition, inspection level

FAQ

Is ISO 630-5 S355W the same as EN 10025-5?
Not identical as a document, but purchasing overlap is strong. Prefer the EN product pages when the contract cites EN 10025-5: EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W. Dual-certification is common when mill practice supports both.
How do ISO qualities map to EN J0 / J2?
ISO qualities C / D / D1 / E roughly align with EN J0 / J2 / K2-style Charpy packages (C ≈ 0 °C; D/D1 ≈ -20 °C; E ≈ -40 °C). Order the ISO quality letter explicitly.
Why does this page avoid inventing ISO chemistry cells?
ISO Annex tables are normative and edition-specific. This page gives EN dual-cert chemistry as a practical reference and requires MTC verification against ISO 630-5 Tables A.1 / A.2.
Should I order ISO or EN on the PO?
Order the document the project specification cites. If both are acceptable, naming the EN grade often matches existing steelspecs product pages and mill dual-cert practice.
Are S295W / S420W / S460W covered here?
Not in this tight set. See INDEX.md for the overlap note and future-page list. S355W / S355WP / S235W are the priority ISO↔EN maps.

Request a quotation

Send ISO 630-5 S355W + quality letter (and/or the matching EN 10025-5 grade), thickness × width × length, quantity, delivery condition and any inspection requirement. SHH STEEL will return mill availability, dual-cert options and a quotation.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: ISO 630-5 · EN 10025-5 · EN 10025-5 S355J0W · EN 10025-5 S355J2W · EN 10025-5 S355K2W · Weathering Steel Plates · Structural Steel Plates

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X