GOST 9941 10Х17Н13М2Т Seamless Stainless Steel Pipe
What is GOST 9941 10Х17Н13М2Т Seamless Stainless Steel Pipe
Russian and CIS piping packages that print GOST 9941 expect cold-/warm-deformed seamless stainless pipe, not a welded substitute and not an automatic ASTM A312 certificate. 10Х17Н13М2Т is the Cyrillic mark on Table 3 for this austenitic Mo + Ti (316Ti class) chemistry. Mill brand ЭИ448. Russian 316Ti-class seamless pipe under cold-/warm-deformed GOST 9941.
Mill path for 10Х17Н13М2Т: cold-/warm-deformed seamless route, clause 2.3 heat-treatment (mandatory by default), GOST 5632 chemistry, Table 3 Rm and elongation, optional hydro / UT / IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.
Body text may mention 316Ti / UNS S31635 (approx) for cross-reference, but the H1 and order line stay on Cyrillic 10Х17Н13М2Т. Silent alias swaps are how wrong carbon ceilings and wrong Table 3 numbers enter the MTC. Keep this caution in view: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ.
Order the standard the drawing and regulatory file actually require. Inside this 9941 series, compare 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т before stretching surface finish or wall alone. Duty thread: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. Document the medium, design temperature, and weld map beside the 10Х17Н13М2Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. This paragraph is locked to 10Х17Н13М2Т duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty.
Inside this GOST 9941 series, compare GOST 9941 08Х17Н15М3Т, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н10Т. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 10Х17Н13М2Т (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP316Ti.
On 10Х17Н13М2Т packages that also list flats, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 UNS S31635. Keep 10Х17Н13М2Т acceptance text on the governing pipe/tube standard.
Chemical Composition of GOST 9941 10Х17Н13М2Т
GOST 5632 sets the melt limits for 10Х17Н13М2Т. Highlight band: C ≤0.10, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 12.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00. For pipe intended for welding, GOST 9941 can tighten sulphur to ≤0.020% when the order states that duty. Alias note: 316Ti / UNS S31635 (approx).
The composition table below is the cast window SHH STEEL quotes against for 10Х17Н13М2Т. Edition framing is GOST 5632 for chemistry and GOST 9941-81 for the pipe product. Use thread: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 10Х17Н13М2Т before the order is acknowledged. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | Ti |
|---|---|---|---|---|---|---|---|---|---|
| 10Х17Н13М2Т | ≤0.10 | ≤0.80 | ≤2.00 | ≤0.035 | ≤0.020 | 12.00–14.00 | 16.00–18.00 | 2.00–3.00 | 5×C–0.70 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9941 10Х17Н13М2Т
Table 3 mechanical acceptance for 10Х17Н13М2Т: Rm min 529 N/mm², elongation δ5 min 35% (yield not normalised in Table 3). Note: Yield strength norms by agreement when purchaser orders yield determination. Delivery framing: heat-treated by default (clause 2.3); without HT only by purchaser request. Density for mass calc: 8.0 g/cm³. Sampling follows GOST 9941 batch rules (party ≤300 pcs).
Elevated-temperature tensile at 623 K (350 °C) and yield determination are purchaser options, not defaults. For 10Х17Н13М2Т, state them on the PO if the stress calculation needs them. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 10Х17Н13М2Т certificate without a written dual-product plan. Weld-shop note tied to 10Х17Н13М2Т: 316L/316Ti-class fillers; keep Mo in the weld metal.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 10Х17Н13М2Т | 529 | — (not normalised) | 35 | 8.0 | cold/warm Table 1 practice |
Ambient values from GOST 9941-81 Table 3 for 10Х17Н13М2Т. Yield strength norms by agreement when purchaser orders yield determination. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.
Seamless Pipe Manufacture of GOST 9941 10Х17Н13М2Т
SHH STEEL can produce 10Х17Н13М2Т as cold-/warm-deformed seamless pipe to GOST 9941-81, then apply the mandatory heat treatment (unless the PO waives HT), lighten or pickle the surface, and finish ends. Plain square-cut ends are default; weld bevels on walls over 5 mm only when the purchaser asks.
After hot deformation, 10Х17Н13М2Т receives heat treatment by default — without HT only if the order waives it — Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception. Use thread: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.
Marking carries the grade 10Х17Н13М2Т, size, precision cue when high class, manufacturer ID, and GOST 9941 reference. Size hint: cold-/warm 316Ti-class OD×wall under Table 1. Weld thread for fabricator joints: 316L/316Ti-class fillers; keep Mo in the weld metal. Hydrostatic pressure or UT class for 10Х17Н13М2Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for 10Х17Н13М2Т remains cold-/warm 316Ti-class OD×wall under Table 1.
Dimensions and Tolerances for GOST 9941 10Х17Н13М2Т
Dimensional order lines for 10Х17Н13М2Т should state OD × wall, length type (random, exact, multiple, or limited), end finish, and precision class. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Max OD for this mark: None mm. Precision class follows the tolerance ordered for 10Х17Н13М2Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.
Ovality has no separate number — it must not push OD outside the diameter tolerance. Caution: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ. Fixed lengths and multiple cut lengths for 10Х17Н13М2Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 10Х17Н13М2Т caution visible here: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ.
Equivalent Grades for GOST 9941 10Х17Н13М2Т
Identity first: GOST 9941 10Х17Н13М2Т is the HX/pipe grade for this page. 316Ti / UNS S31635 (approx) helps buyers who think in AISI/UNS labels. Role: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. Foreign product standards remain separate documents. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (10Х17Н13М2Т).
| System | Designation | Notes |
|---|---|---|
| GOST 9941 | 10Х17Н13М2Т | Governing pipe grade for this page |
| Commercial / UNS (body only) | 316Ti / UNS S31635 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4571 | Starting point for comparison only; no automatic dual-cert |
Order discipline for 10Х17Н13М2Т still points at GOST 9941, not the brochure alias. Neighbours GOST 9941 08Х17Н15М3Т, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н10Т each carry their own mechanical table. Category hub: GOST 9941. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (10Х17Н13М2Т). Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (10Х17Н13М2Т).
Heat Treatment and Delivery Condition for GOST 9941 10Х17Н13М2Т
Mill heat treatment for 10Х17Н13М2Т is mandatory by default per clause 2.3 — Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Bright or descaled finishes are separate order items. Delivery label: heat-treated by default (clause 2.3); without HT only by purchaser request.
Certificate wording for 10Х17Н13М2Т should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature — or explicitly “without heat treatment” when that was ordered. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Field heat treatment of 10Х17Н13М2Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 10Х17Н13М2Т duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty.
Corrosion Resistance of GOST 9941 10Х17Н13М2Т
Mo raises PREN versus 18-8; Ti covers as-welded IGC Ordering IGC does not create a blanket corrosion warranty for every medium. Family filing: austenitic Mo + Ti (316Ti class). Coupon orientation, weld condition, and surface finish for 10Х17Н13М2Т belong in the corrosion test order so results can be compared to the installed spool honestly. Application context for 10Х17Н13М2Т stays chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 10Х17Н13М2Т honestly against 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Role: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 10Х17Н13М2Т rather than relying on wall thickness alone. Application context for 10Х17Н13М2Т stays chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.
Applications of GOST 9941 10Х17Н13М2Т Seamless Pipe
Typical BOM language pairs GOST 9941 10Х17Н13М2Т with OD × wall, precision class, and heat-treatment yes/no. Primary sketch: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Spool fabricators should copy 10Х17Н13М2Т onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 10Х17Н13М2Т caution visible here: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ.
Spell 10Х17Н13М2Т on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Commissioning teams benefit when the as-built dossier repeats 10Х17Н13М2Т beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 10Х17Н13М2Т: 316L/316Ti-class fillers; keep Mo in the weld metal.
Weldability of GOST 9941 10Х17Н13М2Т
Weldability of 10Х17Н13М2Т follows austenitic Mo + Ti (316Ti class) practice. Filler/shop note: 316L/316Ti-class fillers; keep Mo in the weld metal. Caution: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ. Procedure qualification for 10Х17Н13М2Т should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.
For corrosive as-welded duty on 10Х17Н13М2Т, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 316L/316Ti-class fillers; keep Mo in the weld metal. Order sulphur ≤0.020% when the pipe is intended for welding. Consumable lot control and shielding-gas notes for 10Х17Н13М2Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 10Х17Н13М2Т remains cold-/warm 316Ti-class OD×wall under Table 1.
Surface Finishes for GOST 9941 10Х17Н13М2Т
Surface supply for 10Х17Н13М2Т should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless pipe, so finish is part of performance, not only appearance. Application framing: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Ambiguous “bright pipe” language is clarified before finishing slots are booked.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Bright or polished callouts for 10Х17Н13М2Т never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GOST 9941 pipe does not leave the yard with free-iron blooms. Caution retained: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ.
Inspection and Testing for GOST 9941 10Х17Н13М2Т
SHH STEEL reports the tests actually performed for 10Х17Н13М2Т — no surrogate NDT lines. Hydrostatic versus ultrasonic choice belongs on the PO. Caution: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ. Sampling plans for 10Х17Н13М2Т keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.
Retests use double sample counts from the same party — failures are not silently shipped. Size context: cold-/warm 316Ti-class OD×wall under Table 1. Non-conforming 10Х17Н13М2Т lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Application context for 10Х17Н13М2Т stays chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.
Packaging and Shipping for GOST 9941 10Х17Н13М2Т
Export packing for GOST 9941 10Х17Н13М2Т is built around rust prevention and transit abrasion control. Bundle tickets repeat the Cyrillic grade symbol and heat number. Duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. Bundle tickets for 10Х17Н13М2Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 10Х17Н13М2Т stays chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 10Х17Н13М2Т. Desiccant and wrap choices for 10Х17Н13М2Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 10Х17Н13М2Т: 316L/316Ti-class fillers; keep Mo in the weld metal.
Photographic packing records are available on request for project QA files on 10Х17Н13М2Т. Claims handling for 10Х17Н13М2Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 10Х17Н13М2Т: 316L/316Ti-class fillers; keep Mo in the weld metal.
Why Choose SHH STEEL
Buyers choose SHH STEEL for 10Х17Н13М2Т because the paperwork matches the stencil: GOST 5632 chemistry, Table 3 tensile, ordered HT, and honest seamless marking. Application fit: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. SHH STEEL can produce and supply 10Х17Н13М2Т against the OD × wall, cold-/warm-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 10Х17Н13М2Т cleanly. Ask for a written acknowledgement that names 10Х17Н13М2Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 10Х17Н13М2Т to that written scope.
Supply Capability
Supply capability for 10Х17Н13М2Т covers cold-/warm-deformed seamless manufacture, ordered heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 10Х17Н13М2Т when the mill schedule allows. Weld-shop note tied to 10Х17Н13М2Т: 316L/316Ti-class fillers; keep Mo in the weld metal.
| Item | Capability |
|---|---|
| Standard | GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes |
| Grade | 10Х17Н13М2Т (GOST 5632 chemistry; alias 316Ti / UNS S31635 (approx)) |
| Product form | Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940) |
| Delivery condition | heat-treated by default (clause 2.3); without HT only by purchaser request |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice |
| Precision | Ordinary, high, or elevated (indices per marking examples) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes for 10Х17Н13М2Т: common OD×wall combinations as the project uses. Cold-/warm-deformed availability varies by diameter — confirm with the RFQ. Hint: cold-/warm 316Ti-class OD×wall under Table 1. SHH STEEL can supply alternate walls and precision classes for 10Х17Н13М2Т once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 10Х17Н13М2Т supply scope when the PO says so. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. SHH STEEL can produce trial lengths of 10Х17Н13М2Т for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9941 10Х17Н13М2Т seamless stainless steel pipe used for?
- GOST 9941 10Х17Н13М2Т is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Role summary: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9941 10Х17Н13М2Т seamless only, or does it cover welded pipe?
- Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 10Х17Н13М2Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 10Х17Н13М2Т under GOST 9941?
- By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
-
How does 10Х17Н13М2Т compare with sister grades 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т?
- 10Х17Н13М2Т is filed as austenitic Mo + Ti (316Ti class). Typical sisters on the same RFQ are 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Design caution: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 10Х17Н13М2Т?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
-
Is 316Ti / UNS S31635 (approx) the same as ordering 10Х17Н13М2Т?
- No. 316Ti / UNS S31635 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 10Х17Н13М2Т so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9941 10Х17Н13М2Т?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 10Х17Н13М2Т within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm 316Ti-class OD×wall under Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
-
How should 10Х17Н13М2Т be welded on site?
- Shop guidance: 316L/316Ti-class fillers; keep Mo in the weld metal. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ
-
When should I choose a Mo-bearing or duplex grade instead of 10Х17Н13М2Т?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Mo + Ti (316Ti class) practice can defend for the temperature and stress state. Caution for this mark: Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo / 06ХН28МДТ Sister pointers: 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9941 10Х17Н13М2Т with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 10Х17Н13М2Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9941 10Х17Н13М2Т differ from GOST 9940 of the same mark?
- GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 10Х17Н13М2Т.
Conclusion
GOST 9941 10Х17Н13М2Т is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.