GOST 9941 08Х18Н12Б Seamless Stainless Steel Pipe

GOST 9941 08Х18Н12Б seamless stainless steel pipe (347 / UNS S34700 (approx)), austenitic Nb-stabilised 18-12, GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 37%, cold-/warm-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
08Х18Н12Б (GOST 5632 / 347 / UNS S34700 (approx) — body alias)
Standard
GOST 9941-81
Product form
Seamless stainless steel pipe (cold-/warm-deformed), delivery heat-treated by default (clause 2.3); without HT only by purchaser request
Size
OD × wall per Table 1; mark cap cold/warm Table 1 practice; random length typically 1.5–12.5 m by wall band
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9941 08Х18Н12Б Seamless Stainless Steel Pipe

GOST 9941 covers seamless cold-/warm-deformed stainless pipe across the cold-/warm Table 1 OD×wall grid in ordinary, high, and elevated precision classes. Inside that standard, 08Х18Н12Б is filed as austenitic Nb-stabilised 18-12. Mill brand ЭИ402. Niobium-stabilised sister of the Ti 18-8 marks under cold-/warm-deformed GOST 9941.

From pierce through marking and crate protection, SHH STEEL can produce GOST 9941 08Х18Н12Б for the sizes and tests on your RFQ. Application sketch: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Size and test clarity on the RFQ lets SHH STEEL lock the correct cold-/warm-deformed seamless scope for 08Х18Н12Б before production starts. Weld-shop note tied to 08Х18Н12Б: Nb-bearing 347-class fillers; match Nb:C intent on the WPS.

On the floor people latinise marks; in QA they must not. 08Х18Н12Б under GOST 9941 carries specific Table 3 floors that a loose “347” note will not enforce. Caution: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 08Х18Н12Б so informal alias language cannot reopen the carbon or molybdenum window after melt. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

Pair standard GOST 9940 uses many of the same marks with hot deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Use thread: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Document the medium, design temperature, and weld map beside the 08Х18Н12Б line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 08Х18Н12Б: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Inside this GOST 9941 series, compare GOST 9941 08Х18Н12Т, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н10Т. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 08Х18Н12Б (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP347.

Chemical Composition of GOST 9941 08Х18Н12Б

For 08Х18Н12Б, the melt ticket has to show GOST 5632 compliance — C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 11.00–13.00, Cr 17.00–19.00, Nb 10×C–1.10. Optional residual limits still forbid blurring grade identity. Corrosion framing: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Where Mo, Ti or Nb appear, they are intentional levers for 08Х18Н12Б, not optional marketing. Confirm them on the MTC line-by-line. Role: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х18Н12Б before the order is acknowledged. Corrosion framing beside 08Х18Н12Б: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Grade C Si Mn P S Ni Cr Nb
08Х18Н12Б ≤0.08 ≤0.80 ≤2.00 ≤0.035 ≤0.020 11.00–13.00 17.00–19.00 10×C–1.10

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9941 08Х18Н12Б

Do not confuse Table 3 cold-/warm-deformed floors with GOST 9940 hot-deformed numbers that share the 347 / UNS S34700 (approx) alias. For 08Х18Н12Б under 9941 expect Rm min 529 N/mm², elongation δ5 min 37% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised in Table 3.

When comparing 08Х18Н12Б to a hot-deformed GOST 9940 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 08Х18Н12Б certificate without a written dual-product plan. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
08Х18Н12Б 529 — (not normalised) 37 7.9 cold/warm Table 1 practice

Ambient values from GOST 9941-81 Table 3 for 08Х18Н12Б. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.

Seamless Pipe Manufacture of GOST 9941 08Х18Н12Б

GOST 9941-81 manufactures 08Х18Н12Б as seamless cold- and warm-deformed stainless pipe only — cold draw, cold roll, or warm reduce to Table 1 sizes after a hollow is prepared. SHH STEEL confirms the cold-/warm-deformed seamless route on the acknowledgement before finishing starts; welded pipe and hot-deformed GOST 9940 product are outside this line item.

Precision class (ordinary or high) is an order item for 08Х18Н12Б; unmarked class means ordinary. Heat treatment: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception.

Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless cold-/warm-deformed. Size: cold-/warm Nb-stabilised sizes under Table 1 practice. Hydrostatic pressure or UT class for 08Х18Н12Б is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Corrosion framing beside 08Х18Н12Б: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Dimensions and Tolerances for GOST 9941 08Х18Н12Б

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 08Х18Н12Б. Duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. Cap: cold/warm Table 1 practice. Precision class follows the tolerance ordered for 08Х18Н12Б, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 08Х18Н12Б: Nb-bearing 347-class fillers; match Nb:C intent on the WPS.

High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 08Х18Н12Б. Fixed lengths and multiple cut lengths for 08Х18Н12Б are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

Equivalent Grades for GOST 9941 08Х18Н12Б

European and ASTM marks may sit near 347 / UNS S34700 (approx), yet GOST 9941 hydrostatic and heat-treatment text for 08Х18Н12Б still diverge. Keep 08Х18Н12Б as the governing symbol. Caution retained from pack notes: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т.

System Designation Notes
GOST 9941 08Х18Н12Б Governing pipe grade for this page
Commercial / UNS (body only) 347 / UNS S34700 (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related 347 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other EN 1.4550 Starting point for comparison only; no automatic dual-cert

Read the notes column literally for 08Х18Н12Б: related chemistry is not automatic dual-cert. Cross-check GOST 9941 08Х18Н12Т, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н10Т when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9941. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х18Н12Б).

Project teams specifying 08Х18Н12Б should link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and ASTM A240 Type 347 so purchasing does not treat one product form as the other. Confirm 08Х18Н12Б OD × wall and plate thickness on separate drawings.

Heat Treatment and Delivery Condition for GOST 9941 08Х18Н12Б

Unlike GOST 9940, GOST 9941 forces heat treatment on every pipe by default. Confirm for 08Х18Н12Б. Band note: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Recorded furnace charts for 08Х18Н12Б should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 08Х18Н12Б: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 08Х18Н12Б. Field heat treatment of 08Х18Н12Б after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 08Х18Н12Б: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Corrosion Resistance of GOST 9941 08Х18Н12Б

Medium, temperature, crevice geometry and weld condition decide whether 08Х18Н12Б is enough. Summary: Nb stabilisation for IGC after welding; hot strength similar to 347 practice. Escalate via sisters 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т when coupons fail. Coupon orientation, weld condition, and surface finish for 08Х18Н12Б belong in the corrosion test order so results can be compared to the installed spool honestly. Corrosion framing beside 08Х18Н12Б: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 08Х18Н12Б. Corrosion framing: Nb stabilisation for IGC after welding; hot strength similar to 347 practice. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х18Н12Б rather than relying on wall thickness alone. Application context for 08Х18Н12Б stays furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium.

Applications of GOST 9941 08Х18Н12Б Seamless Pipe

From utility rooms to process racks, 08Х18Н12Б shows up wherever CIS fluid specs want austenitic Nb-stabilised 18-12 cold-/warm-deformed seamless behaviour. Use list: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Spool fabricators should copy 08Х18Н12Б onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

If the only reason for 08Х18Н12Б is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т. Commissioning teams benefit when the as-built dossier repeats 08Х18Н12Б beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

Weldability of GOST 9941 08Х18Н12Б

Automatic mill welding is outside GOST 9941; manual and automatic field welds must still respect 08Х18Н12Б chemistry. Guidance: Nb-bearing 347-class fillers; match Nb:C intent on the WPS. Procedure qualification for 08Х18Н12Б should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Application context for 08Х18Н12Б stays furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium.

Ferrite control on high-Ni austenitics and hydrogen management on martensitic 08Х18Н12Б are procedure items, not afterthoughts. Guidance: Nb-bearing 347-class fillers; match Nb:C intent on the WPS. Consumable lot control and shielding-gas notes for 08Х18Н12Б stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

Surface Finishes for GOST 9941 08Х18Н12Б

Welded or heavily formed 08Х18Н12Б may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GOST 9941 seamless stainless steel pipe (cold-/warm-deformed). Caution: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

When 08Х18Н12Б ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium.

Inspection and Testing for GOST 9941 08Х18Н12Б

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9941 for 08Х18Н12Б. Sampling plans for 08Х18Н12Б keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 08Х18Н12Б caution visible here: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т.

Dimensional inspection against Table 2 tolerances closes the lot. Role: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. Non-conforming 08Х18Н12Б lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Size practice for 08Х18Н12Б remains cold-/warm Nb-stabilised sizes under Table 1 practice.

Packaging and Shipping for GOST 9941 08Х18Н12Б

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 08Х18Н12Б stays visible on outer tags. Bundle tickets for 08Х18Н12Б repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.

Container loading plans should keep heavy walls from crushing thin-wall 08Х18Н12Б layers. Desiccant and wrap choices for 08Х18Н12Б follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 08Х18Н12Б caution visible here: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 08Х18Н12Б. Claims handling for 08Х18Н12Б starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 08Х18Н12Б caution visible here: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats 08Х18Н12Б as a governed product grade, not a marketing synonym for 347 / UNS S34700 (approx). Role: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. SHH STEEL can produce and supply 08Х18Н12Б against the OD × wall, cold-/warm-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common 08Х18Н12Б enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Ask for a written acknowledgement that names 08Х18Н12Б, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х18Н12Б to that written scope.

Supply Capability

Capability framing for 08Х18Н12Б: GOST-spec seamless cold-/warm-deformed pipe, documented heats. Caution remains: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х18Н12Б when the mill schedule allows.

Item Capability
Standard GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes
Grade 08Х18Н12Б (GOST 5632 chemistry; alias 347 / UNS S34700 (approx))
Product form Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940)
Delivery condition heat-treated by default (clause 2.3); without HT only by purchaser request
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice
Precision Ordinary, high, or elevated (indices per marking examples)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 08Х18Н12Б change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. SHH STEEL can supply alternate walls and precision classes for 08Х18Н12Б once the design pressure and corrosion allowance are clear.

Repeat orders for 08Х18Н12Б go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. SHH STEEL can produce trial lengths of 08Х18Н12Б for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9941 08Х18Н12Б seamless stainless steel pipe used for?
GOST 9941 08Х18Н12Б is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Role summary: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9941 08Х18Н12Б seamless only, or does it cover welded pipe?
Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 08Х18Н12Б when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 08Х18Н12Б under GOST 9941?
By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
How does 08Х18Н12Б compare with sister grades 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т?
08Х18Н12Б is filed as austenitic Nb-stabilised 18-12. Typical sisters on the same RFQ are 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Design caution: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 08Х18Н12Б?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
Is 347 / UNS S34700 (approx) the same as ordering 08Х18Н12Б?
No. 347 / UNS S34700 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 08Х18Н12Б so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9941 08Х18Н12Б?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х18Н12Б within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm Nb-stabilised sizes under Table 1 practice. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
How should 08Х18Н12Б be welded on site?
Shop guidance: Nb-bearing 347-class fillers; match Nb:C intent on the WPS. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т
When should I choose a Mo-bearing or duplex grade instead of 08Х18Н12Б?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Nb-stabilised 18-12 practice can defend for the temperature and stress state. Caution for this mark: Nb-stabilised mark — confirm OD×wall against 9941 Table 1; do not confuse with Ti-stabilised 08Х18Н12Т Sister pointers: 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9941 08Х18Н12Б with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 08Х18Н12Б does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9941 08Х18Н12Б differ from GOST 9940 of the same mark?
GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х18Н12Б.

Conclusion

GOST 9941 08Х18Н12Б is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X