GOST 9941 08Х20Н14С2 Seamless Stainless Steel Pipe
What is GOST 9941 08Х20Н14С2 Seamless Stainless Steel Pipe
GOST 9941 covers seamless cold-/warm-deformed stainless pipe across the cold-/warm Table 1 OD×wall grid in ordinary, high, and elevated precision classes. Inside that standard, 08Х20Н14С2 is filed as austenitic heat-resisting Si-bearing. Mill brand ЭИ732. Silicon is intentional — this mark fights carburising gases under cold-/warm-deformed GOST 9941.
From pierce through marking and crate protection, SHH STEEL can produce GOST 9941 08Х20Н14С2 for the sizes and tests on your RFQ. Application sketch: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Size and test clarity on the RFQ lets SHH STEEL lock the correct cold-/warm-deformed seamless scope for 08Х20Н14С2 before production starts. Application context for 08Х20Н14С2 stays carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732.
On the floor people latinise marks; in QA they must not. 08Х20Н14С2 under GOST 9941 carries specific Table 3 floors that a loose “309Si” note will not enforce. Caution: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 08Х20Н14С2 so informal alias language cannot reopen the carbon or molybdenum window after melt. Application context for 08Х20Н14С2 stays carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732.
Pair standard GOST 9940 uses many of the same marks with hot deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 10Х23Н18, 08Х22Н6Т. Use thread: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Document the medium, design temperature, and weld map beside the 08Х20Н14С2 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the 08Х20Н14С2 caution visible here: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1.
Inside this GOST 9941 series, compare GOST 9941 10Х23Н18, GOST 9941 08Х22Н6Т. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 08Х20Н14С2 (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP309S.
Project teams specifying 08Х20Н14С2 should form hubs stay Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates — no verified plate product page is attached for this chemistry yet. Do not stretch a 08Х20Н14С2 pipe certificate onto plate.
Chemical Composition of GOST 9941 08Х20Н14С2
For 08Х20Н14С2, the melt ticket has to show GOST 5632 compliance — C ≤0.08, Si 2.00–3.00, Mn ≤1.50, P ≤0.035, S ≤0.025, Ni 12.00–15.00, Cr 19.00–22.00. Optional residual limits still forbid blurring grade identity. Corrosion framing: designed for carburisation / oxidation — not a chloride aqueous champion.
Where Mo, Ti or Nb appear, they are intentional levers for 08Х20Н14С2, not optional marketing. Confirm them on the MTC line-by-line. Role: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х20Н14С2 before the order is acknowledged. Corrosion framing beside 08Х20Н14С2: designed for carburisation / oxidation — not a chloride aqueous champion.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 08Х20Н14С2 | ≤0.08 | 2.00–3.00 | ≤1.50 | ≤0.035 | ≤0.025 | 12.00–15.00 | 19.00–22.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9941 08Х20Н14С2
Do not confuse Table 3 cold-/warm-deformed floors with GOST 9940 hot-deformed numbers that share the 309Si / heat-resisting Si grade (approx) alias. For 08Х20Н14С2 under 9941 expect Rm min 510 N/mm², elongation δ5 min 35% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised in Table 3.
When comparing 08Х20Н14С2 to a hot-deformed GOST 9940 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 08Х20Н14С2 certificate without a written dual-product plan. Size practice for 08Х20Н14С2 remains cold-/warm Si heat-resisting sizes under Table 1.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х20Н14С2 | 510 | — (not normalised) | 35 | 7.7 | cold/warm Table 1 practice |
Ambient values from GOST 9941-81 Table 3 for 08Х20Н14С2. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.
Seamless Pipe Manufacture of GOST 9941 08Х20Н14С2
For 08Х20Н14С2, the mill path is cold or warm deformation of a seamless hollow — never ERW under GOST 9941. Heat treatment is mandatory by default under clause 2.3; without HT only when the purchaser explicitly orders it (then mech and curvature by agreement). Order ordinary, high, or elevated precision class with the size.
Precision class (ordinary or high) is an order item for 08Х20Н14С2; unmarked class means ordinary. Heat treatment: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception.
Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless cold-/warm-deformed. Size: cold-/warm Si heat-resisting sizes under Table 1. Hydrostatic pressure or UT class for 08Х20Н14С2 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for 08Х20Н14С2 remains cold-/warm Si heat-resisting sizes under Table 1.
Dimensions and Tolerances for GOST 9941 08Х20Н14С2
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 08Х20Н14С2. Duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Cap: cold/warm Table 1 practice. Precision class follows the tolerance ordered for 08Х20Н14С2, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 08Х20Н14С2: designed for carburisation / oxidation — not a chloride aqueous champion.
High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 08Х20Н14С2. Fixed lengths and multiple cut lengths for 08Х20Н14С2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 08Х20Н14С2 remains cold-/warm Si heat-resisting sizes under Table 1.
Equivalent Grades for GOST 9941 08Х20Н14С2
Buyers searching under 309Si / heat-resisting Si grade (approx) still need the GOST 9941 08Х20Н14С2 row locked on the acknowledgement. Inside austenitic heat-resisting Si-bearing practice the mechanical table and inspection clauses of GOST 9941 control acceptance, not a brochure equivalent. Duty context: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.
| System | Designation | Notes |
|---|---|---|
| GOST 9941 | 08Х20Н14С2 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 309Si / heat-resisting Si grade (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
When the service outgrows 08Х20Н14С2, move to a sister rather than stretching the alias: GOST 9941 10Х23Н18, GOST 9941 08Х22Н6Т. Apps context: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Full list under GOST 9941. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (08Х20Н14С2).
Heat Treatment and Delivery Condition for GOST 9941 08Х20Н14С2
Unlike GOST 9940, GOST 9941 forces heat treatment on every pipe by default. Confirm for 08Х20Н14С2. Band note: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Recorded furnace charts for 08Х20Н14С2 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Size practice for 08Х20Н14С2 remains cold-/warm Si heat-resisting sizes under Table 1.
Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 08Х20Н14С2. Field heat treatment of 08Х20Н14С2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 08Х20Н14С2 duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.
Corrosion Resistance of GOST 9941 08Х20Н14С2
Medium, temperature, crevice geometry and weld condition decide whether 08Х20Н14С2 is enough. Summary: designed for carburisation / oxidation — not a chloride aqueous champion. Escalate via sisters 10Х23Н18, 08Х22Н6Т when coupons fail. Coupon orientation, weld condition, and surface finish for 08Х20Н14С2 belong in the corrosion test order so results can be compared to the installed spool honestly. Keep the 08Х20Н14С2 caution visible here: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 08Х20Н14С2. Corrosion framing: designed for carburisation / oxidation — not a chloride aqueous champion. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х20Н14С2 rather than relying on wall thickness alone. This paragraph is locked to 08Х20Н14С2 duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.
Applications of GOST 9941 08Х20Н14С2 Seamless Pipe
From utility rooms to process racks, 08Х20Н14С2 shows up wherever CIS fluid specs want austenitic heat-resisting Si-bearing cold-/warm-deformed seamless behaviour. Use list: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Spool fabricators should copy 08Х20Н14С2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for 08Х20Н14С2 stays carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732.
If the only reason for 08Х20Н14С2 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1. Commissioning teams benefit when the as-built dossier repeats 08Х20Н14С2 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 08Х20Н14С2 remains cold-/warm Si heat-resisting sizes under Table 1.
Weldability of GOST 9941 08Х20Н14С2
Automatic mill welding is outside GOST 9941; manual and automatic field welds must still respect 08Х20Н14С2 chemistry. Guidance: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal. Procedure qualification for 08Х20Н14С2 should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. This paragraph is locked to 08Х20Н14С2 duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 08Х20Н14С2 are procedure items, not afterthoughts. Guidance: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal. Consumable lot control and shielding-gas notes for 08Х20Н14С2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 08Х20Н14С2: designed for carburisation / oxidation — not a chloride aqueous champion.
Surface Finishes for GOST 9941 08Х20Н14С2
Surface supply for 08Х20Н14С2 should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless pipe, so finish is part of performance, not only appearance. Application framing: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Ambiguous “bright pipe” language is clarified before finishing slots are booked.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Do not polish over unresolved defects on 08Х20Н14С2; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GOST 9941 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (08Х20Н14С2).
Inspection and Testing for GOST 9941 08Х20Н14С2
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9941 for 08Х20Н14С2. Sampling plans for 08Х20Н14С2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 08Х20Н14С2: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal.
Dimensional inspection against Table 2 tolerances closes the lot. Role: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Non-conforming 08Х20Н14С2 lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Corrosion framing beside 08Х20Н14С2: designed for carburisation / oxidation — not a chloride aqueous champion.
Packaging and Shipping for GOST 9941 08Х20Н14С2
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 08Х20Н14С2 stays visible on outer tags. Bundle tickets for 08Х20Н14С2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 08Х20Н14С2 caution visible here: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1.
Container loading plans should keep heavy walls from crushing thin-wall 08Х20Н14С2 layers. Desiccant and wrap choices for 08Х20Н14С2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 08Х20Н14С2 duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 08Х20Н14С2. Claims handling for 08Х20Н14С2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 08Х20Н14С2: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 08Х20Н14С2 as a governed product grade, not a marketing synonym for 309Si / heat-resisting Si grade (approx). Role: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. SHH STEEL can produce and supply 08Х20Н14С2 against the OD × wall, cold-/warm-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 08Х20Н14С2 enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Ask for a written acknowledgement that names 08Х20Н14С2, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х20Н14С2 to that written scope.
Supply Capability
Capability framing for 08Х20Н14С2: GOST-spec seamless cold-/warm-deformed pipe, documented heats. Caution remains: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х20Н14С2 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes |
| Grade | 08Х20Н14С2 (GOST 5632 chemistry; alias 309Si / heat-resisting Si grade (approx)) |
| Product form | Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940) |
| Delivery condition | heat-treated by default (clause 2.3); without HT only by purchaser request |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice |
| Precision | Ordinary, high, or elevated (indices per marking examples) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 08Х20Н14С2 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. SHH STEEL can supply alternate walls and precision classes for 08Х20Н14С2 once the design pressure and corrosion allowance are clear.
Repeat orders for 08Х20Н14С2 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. SHH STEEL can produce trial lengths of 08Х20Н14С2 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9941 08Х20Н14С2 seamless stainless steel pipe used for?
- GOST 9941 08Х20Н14С2 is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Role summary: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9941 08Х20Н14С2 seamless only, or does it cover welded pipe?
- Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 08Х20Н14С2 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х20Н14С2 under GOST 9941?
- By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
-
How does 08Х20Н14С2 compare with sister grades 10Х23Н18, 08Х22Н6Т?
- 08Х20Н14С2 is filed as austenitic heat-resisting Si-bearing. Typical sisters on the same RFQ are 10Х23Н18, 08Х22Н6Т. Design caution: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1 Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х20Н14С2?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
-
Is 309Si / heat-resisting Si grade (approx) the same as ordering 08Х20Н14С2?
- No. 309Si / heat-resisting Si grade (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 08Х20Н14С2 so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9941 08Х20Н14С2?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х20Н14С2 within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm Si heat-resisting sizes under Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
-
How should 08Х20Н14С2 be welded on site?
- Shop guidance: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1
-
When should I choose a Mo-bearing or duplex grade instead of 08Х20Н14С2?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic heat-resisting Si-bearing practice can defend for the temperature and stress state. Caution for this mark: Si 2–3% changes weld pool fluidity versus plain 18-8; confirm size against Table 1 Sister pointers: 10Х23Н18, 08Х22Н6Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9941 08Х20Н14С2 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 08Х20Н14С2 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9941 08Х20Н14С2 differ from GOST 9940 of the same mark?
- GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х20Н14С2.
Conclusion
GOST 9941 08Х20Н14С2 is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Х23Н18, 08Х22Н6Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.