GOST 9941 08Х18Н10 Seamless Stainless Steel Pipe

GOST 9941 08Х18Н10 seamless stainless steel pipe (304 / UNS S30400 (approx)), austenitic 18-8, GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 37%, cold-/warm-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
08Х18Н10 (GOST 5632 / 304 / UNS S30400 (approx) — body alias)
Standard
GOST 9941-81
Product form
Seamless stainless steel pipe (cold-/warm-deformed), delivery heat-treated by default (clause 2.3); without HT only by purchaser request
Size
OD × wall per Table 1; mark cap cold/warm Table 1 practice; random length typically 1.5–12.5 m by wall band
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9941 08Х18Н10 Seamless Stainless Steel Pipe

GOST 9941-81 is the Soviet / CIS product standard for seamless cold-/warm-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 08Х18Н10 sits in the austenitic 18-8 set under Table 3. The everyday 18-8 cold-/warm-deformed seamless mark — not a silent ASTM A312 certificate.

SHH STEEL can produce and supply GOST 9941 08Х18Н10 as cold-/warm-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated by default (without HT only when the PO waives it), descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: standard 18-8 austenitic seamless pipe for general CIS fluid service.

Shop language may still say “304 pipe,” yet that commercial alias does not select GOST 5632 cast limits, cold-/warm-deformed tensile floors, or GOST 9941 marking. The purchase order has to name GOST 9941 and 08Х18Н10 so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Scope discipline: 08Х18Н10 is cold-/warm-deformed seamless pipe under GOST 9941, not hot-deformed GOST 9940 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Role reminder: standard 18-8 austenitic seamless pipe for general CIS fluid service. Diameter note: cold/warm Table 1 practice.

Inside this GOST 9941 series, compare GOST 9941 04Х18Н10, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н9. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 08Х18Н10 (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304.

For 08Х18Н10, vertical navigation stays form-specific — keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with ASTM A240 Type 304. Keep 08Х18Н10 acceptance text on the governing pipe/tube standard.

Chemical Composition of GOST 9941 08Х18Н10

Cast analysis for GOST 9941 08Х18Н10 is not printed inside 9941 itself — clause 2.2 points to GOST 5632. Key windows on a typical certificate include C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 9.00–11.00, Cr 17.00–19.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 304 / UNS S30400 (approx). Corrosion thread: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life.

Chemical limits for 08Х18Н10 appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: standard 18-8 austenitic seamless pipe for general CIS fluid service. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х18Н10 before the order is acknowledged. Size practice for 08Х18Н10 remains common cold-/warm 18-8 OD×wall band under Table 1.

Grade C Si Mn P S Ni Cr
08Х18Н10 ≤0.08 ≤0.80 ≤2.00 ≤0.035 ≤0.020 9.00–11.00 17.00–19.00

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9941 08Х18Н10

Ambient tensile floors for 08Х18Н10 come from GOST 9941-81 Table 3: Rm min 529 N/mm², elongation δ5 min 37% (yield not normalised in Table 3). Note: Yield not normalised in Table 3. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic 18-8. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Yield strength is numerically normalised in GOST 9941 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 08Х18Н10, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 7.9 g/cm³. Role: standard 18-8 austenitic seamless pipe for general CIS fluid service.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
08Х18Н10 529 — (not normalised) 37 7.9 cold/warm Table 1 practice

Ambient values from GOST 9941-81 Table 3 for 08Х18Н10. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.

Seamless Pipe Manufacture of GOST 9941 08Х18Н10

For 08Х18Н10, the mill path is cold or warm deformation of a seamless hollow — never ERW under GOST 9941. Heat treatment is mandatory by default under clause 2.3; without HT only when the purchaser explicitly orders it (then mech and curvature by agreement). Order ordinary, high, or elevated precision class with the size.

Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception. Heat-treatment note for 08Х18Н10: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: standard 18-8 austenitic seamless pipe for general CIS fluid service.

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 08Х18Н10: common cold-/warm 18-8 OD×wall band under Table 1. Diameter cap: cold/warm Table 1 practice.

Dimensions and Tolerances for GOST 9941 08Х18Н10

SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 08Х18Н10 before the mill slot is locked. Table 1 lists the cold-/warm OD×wall grid (smaller OD and thinner walls than GOST 9940), with measured length limits per size cell. Size hint: common cold-/warm 18-8 OD×wall band under Table 1. Mark cap: cold/warm Table 1 practice.

OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: standard 18-8 austenitic seamless pipe for general CIS fluid service. Fixed lengths and multiple cut lengths for 08Х18Н10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 08Х18Н10: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life.

Equivalent Grades for GOST 9941 08Х18Н10

Do not treat 304 / UNS S30400 (approx) as interchangeable paperwork for GOST 9941 08Х18Н10. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (08Х18Н10).

System Designation Notes
GOST 9941 08Х18Н10 Governing pipe grade for this page
Commercial / UNS (body only) 304 / UNS S30400 (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related 304 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other EN 1.4301 Starting point for comparison only; no automatic dual-cert

Order discipline for 08Х18Н10 still points at GOST 9941, not the brochure alias. Neighbours GOST 9941 04Х18Н10, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н9 each carry their own mechanical table. Category hub: GOST 9941. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (08Х18Н10). Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (08Х18Н10).

Heat Treatment and Delivery Condition for GOST 9941 08Х18Н10

08Х18Н10 is delivered heat-treated by default (clause 2.3); without HT only by purchaser request under GOST 9941. Guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty.

Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: standard 18-8 austenitic seamless pipe for general CIS fluid service. Density 7.9 g/cm³ for weight calcs. Field heat treatment of 08Х18Н10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 08Х18Н10: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty.

Corrosion Resistance of GOST 9941 08Х18Н10

Corrosion behaviour of GOST 9941 08Х18Н10 tracks its austenitic 18-8 balance: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life. Intergranular corrosion testing is a purchaser option under GOST 9941, not an automatic coupon on every lot. Design caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 08Х18Н10 is filed as austenitic 18-8. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Applications of GOST 9941 08Х18Н10 Seamless Pipe

Applications of GOST 9941 08Х18Н10 seamless pipe centre on water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9941. Role summary: standard 18-8 austenitic seamless pipe for general CIS fluid service. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9941. Duty thread: standard 18-8 austenitic seamless pipe for general CIS fluid service. Commissioning teams benefit when the as-built dossier repeats 08Х18Н10 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 08Х18Н10 remains common cold-/warm 18-8 OD×wall band under Table 1.

Weldability of GOST 9941 08Х18Н10

08Х18Н10 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 08Х18Н10 should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Size practice for 08Х18Н10 remains common cold-/warm 18-8 OD×wall band under Table 1.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic 18-8 — not a single shop habit. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Surface Finishes for GOST 9941 08Х18Н10

Surface condition for 08Х18Н10 is part of the pipe identity under GOST 9941. Order annealed/pickled as default HX or process supply, then add bright anneal or polish only with OD/ID scope named. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 08Х18Н10.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

For 08Х18Н10, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (08Х18Н10).

Inspection and Testing for GOST 9941 08Х18Н10

Inspection for GOST 9941 08Х18Н10 covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.

Marking includes 08Х18Н10, manufacturer, size, and GOST 9941. Traceability from stencil to MTC is part of supply, not an upgrade. Use: water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9941. Non-conforming 08Х18Н10 lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.

Packaging and Shipping for GOST 9941 08Х18Н10

Packaging for 08Х18Н10 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 08Х18Н10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed. Desiccant and wrap choices for 08Х18Н10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Shipping documents list GOST 9941, 08Х18Н10, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: standard 18-8 austenitic seamless pipe for general CIS fluid service. Claims handling for 08Х18Н10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.

Why Choose SHH STEEL

SHH STEEL can produce and supply GOST 9941 08Х18Н10 with the cold-/warm-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: standard 18-8 austenitic seamless pipe for general CIS fluid service.

Technical sales can map 08Х18Н10 against sisters 04Х18Н10, 08Х18Н10Т, 12Х18Н9 and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 08Х18Н10, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х18Н10 to that written scope.

Supply Capability

SHH STEEL can produce and supply GOST 9941 08Х18Н10 across enquiry-oriented OD × wall bands (within cold/warm Table 1 practice), in the cold-/warm-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.

Item Capability
Standard GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes
Grade 08Х18Н10 (GOST 5632 chemistry; alias 304 / UNS S30400 (approx))
Product form Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940)
Delivery condition heat-treated by default (clause 2.3); without HT only by purchaser request
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice
Precision Ordinary, high, or elevated (indices per marking examples)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

SHH STEEL can produce and supply GOST 9941 08Х18Н10. Stock / Available sizes: enquiry band typically aligns with GOST 9941 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 08Х18Н10, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: common cold-/warm 18-8 OD×wall band under Table 1. Cap: cold/warm Table 1 practice.

Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Email the size list to start. SHH STEEL can produce trial lengths of 08Х18Н10 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9941 08Х18Н10 seamless stainless steel pipe used for?
GOST 9941 08Х18Н10 is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9941. Role summary: standard 18-8 austenitic seamless pipe for general CIS fluid service. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9941 08Х18Н10 seamless only, or does it cover welded pipe?
Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 08Х18Н10 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 08Х18Н10 under GOST 9941?
By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
How does 08Х18Н10 compare with sister grades 04Х18Н10, 08Х18Н10Т, 12Х18Н9?
08Х18Н10 is filed as austenitic 18-8. Typical sisters on the same RFQ are 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Design caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 08Х18Н10?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
Is 304 / UNS S30400 (approx) the same as ordering 08Х18Н10?
No. 304 / UNS S30400 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 08Х18Н10 so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9941 08Х18Н10?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х18Н10 within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: common cold-/warm 18-8 OD×wall band under Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
How should 08Х18Н10 be welded on site?
Shop guidance: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed
When should I choose a Mo-bearing or duplex grade instead of 08Х18Н10?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic 18-8 practice can defend for the temperature and stress state. Caution for this mark: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed Sister pointers: 04Х18Н10, 08Х18Н10Т, 12Х18Н9. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9941 08Х18Н10 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 08Х18Н10 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9941 08Х18Н10 differ from GOST 9940 of the same mark?
GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х18Н10.

Conclusion

GOST 9941 08Х18Н10 is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — standard 18-8 austenitic seamless pipe for general CIS fluid service. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X