GOST 9941 08Х17Н15М3Т Seamless Stainless Steel Pipe
What is GOST 9941 08Х17Н15М3Т Seamless Stainless Steel Pipe
GOST 9941-81 is the Soviet / CIS product standard for seamless cold-/warm-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 08Х17Н15М3Т sits in the austenitic Mo + Ti (317Ti class) set under Table 3. Mill brand ЭИ580. The Mo-rich Ti austenitic when 316Ti chemistry is not enough on a GOST 9941 pipe BOM.
SHH STEEL can produce and supply GOST 9941 08Х17Н15М3Т as cold-/warm-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated by default (without HT only when the PO waives it), descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Shop language may still say “317Ti pipe,” yet that commercial alias does not select GOST 5632 cast limits, cold-/warm-deformed tensile floors, or GOST 9941 marking. The purchase order has to name GOST 9941 and 08Х17Н15М3Т so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard.
Scope discipline: 08Х17Н15М3Т is cold-/warm-deformed seamless pipe under GOST 9941, not hot-deformed GOST 9940 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т. Role reminder: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. Diameter note: cold/warm Table 1 practice.
Inside this GOST 9941 series, compare GOST 9941 10Х17Н13М2Т, GOST 9941 06ХН28МДТ, GOST 9941 08Х18Н10Т. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 08Х17Н15М3Т (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP317L, ASTM A312 TP316Ti.
Chemical Composition of GOST 9941 08Х17Н15М3Т
Cast analysis for GOST 9941 08Х17Н15М3Т is not printed inside 9941 itself — clause 2.2 points to GOST 5632. Key windows on a typical certificate include C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 14.00–16.00, Cr 16.00–18.00, Mo 3.00–4.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 317Ti / UNS S31726 family (approx). Mill brand ЭИ580. Corrosion thread: Mo ~3–4% plus Ti — above 316Ti for many reducing/chloride mixes.
Chemical limits for 08Х17Н15М3Т appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | Ti |
|---|---|---|---|---|---|---|---|---|---|
| 08Х17Н15М3Т | ≤0.08 | ≤0.80 | ≤2.00 | ≤0.035 | ≤0.020 | 14.00–16.00 | 16.00–18.00 | 3.00–4.00 | 0.30–0.60 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9941 08Х17Н15М3Т
Ambient tensile floors for 08Х17Н15М3Т come from GOST 9941-81 Table 3: Rm min 549 N/mm², elongation δ5 min 35% (yield not normalised in Table 3). Note: Yield not normalised in Table 3. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic Mo + Ti (317Ti class). Caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard.
Yield strength is numerically normalised in GOST 9941 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 08Х17Н15М3Т, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 8.1 g/cm³. Role: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х17Н15М3Т | 549 | — (not normalised) | 35 | 8.1 | cold/warm Table 1 practice |
Ambient values from GOST 9941-81 Table 3 for 08Х17Н15М3Т. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.
Seamless Pipe Manufacture of GOST 9941 08Х17Н15М3Т
Seamless is not optional wording for 08Х17Н15М3Т: GOST 9941 covers cold- and warm-deformed seamless corrosion-resistant pipe. Hot-deformed sisters of related marks live under GOST 9940-81 with different tensile floors. SHH STEEL will not quietly substitute a welded or hot-pierced-only route under a 9941 PO.
Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception. Heat-treatment note for 08Х17Н15М3Т: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 08Х17Н15М3Т: cold-/warm Mo-rich sizes; confirm OD×wall against Table 1 cells. Diameter cap: cold/warm Table 1 practice.
Dimensions and Tolerances for GOST 9941 08Х17Н15М3Т
SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 08Х17Н15М3Т before the mill slot is locked. Table 1 lists the cold-/warm OD×wall grid (smaller OD and thinner walls than GOST 9940), with measured length limits per size cell. Size hint: cold-/warm Mo-rich sizes; confirm OD×wall against Table 1 cells. Mark cap: cold/warm Table 1 practice.
OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Equivalent Grades for GOST 9941 08Х17Н15М3Т
Equivalence language around 08Х17Н15М3Т is often looser than a pipe purchase order can afford. GOST 9941 08Х17Н15М3Т governs this article; 317Ti / UNS S31726 family (approx) is body-only framing for catalogues and dual-cert talk, not a substitute mark on the MTC. Keep the GOST 9941 symbol unless a written dual-cert plan lists both standards with separate test scopes.
| System | Designation | Notes |
|---|---|---|
| GOST 9941 | 08Х17Н15М3Т | Governing pipe grade for this page |
| Commercial / UNS (body only) | 317Ti / UNS S31726 family (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 08Х17Н15М3Т still points at GOST 9941, not the brochure alias. Neighbours GOST 9941 10Х17Н13М2Т, GOST 9941 06ХН28МДТ, GOST 9941 08Х18Н10Т each carry their own mechanical table. Category hub: GOST 9941. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х17Н15М3Т).
On 08Х17Н15М3Т packages that also list flats, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 UNS S31726. Quote 08Х17Н15М3Т pipe and plate under separate line items.
Heat Treatment and Delivery Condition for GOST 9941 08Х17Н15М3Т
08Х17Н15М3Т is delivered heat-treated by default (clause 2.3); without HT only by purchaser request under GOST 9941. Guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 317L/Mo-bearing fillers; Ti on the heat already; control heat input.
Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. Density 8.1 g/cm³ for weight calcs. Field heat treatment of 08Х17Н15М3Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 08Х17Н15М3Т: 317L/Mo-bearing fillers; Ti on the heat already; control heat input.
Corrosion Resistance of GOST 9941 08Х17Н15М3Т
Corrosion behaviour of GOST 9941 08Х17Н15М3Т tracks its austenitic Mo + Ti (317Ti class) balance: Mo ~3–4% plus Ti — above 316Ti for many reducing/chloride mixes. Intergranular corrosion testing is a purchaser option under GOST 9941, not an automatic coupon on every lot. Design caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 08Х17Н15М3Т is filed as austenitic Mo + Ti (317Ti class). Caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard.
Applications of GOST 9941 08Х17Н15М3Т Seamless Pipe
Applications of GOST 9941 08Х17Н15М3Т seamless pipe centre on urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Role summary: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Duty thread: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Weldability of GOST 9941 08Х17Н15М3Т
08Х17Н15М3Т ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 317L/Mo-bearing fillers; Ti on the heat already; control heat input. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 08Х17Н15М3Т should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Application context for 08Х17Н15М3Т stays urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic Mo + Ti (317Ti class) — not a single shop habit. Caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard. Consumable lot control and shielding-gas notes for 08Х17Н15М3Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 08Х17Н15М3Т duty: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Surface Finishes for GOST 9941 08Х17Н15М3Т
Typical GOST 9941 supply for 08Х17Н15М3Т is a clean pickle after the required heat treatment, with bright anneal reserved for scale-free OD/ID appearance and ground/polished finishes reserved for written roughness targets. Use case colour: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Free-iron control starts at the finishing bay, not at commissioning.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Passivation restores the chromium-rich film after pickling or light fabrication on 08Х17Н15М3Т; it does not replace the heat treatment that sets mechanical properties under GOST 9941. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.
Inspection and Testing for GOST 9941 08Х17Н15М3Т
Inspection for GOST 9941 08Х17Н15М3Т covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.
Marking includes 08Х17Н15М3Т, manufacturer, size, and GOST 9941. Traceability from stencil to MTC is part of supply, not an upgrade. Use: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Non-conforming 08Х17Н15М3Т lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Size practice for 08Х17Н15М3Т remains cold-/warm Mo-rich sizes; confirm OD×wall against Table 1 cells.
Packaging and Shipping for GOST 9941 08Х17Н15М3Т
Packaging for 08Х17Н15М3Т uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 08Х17Н15М3Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 08Х17Н15М3Т caution visible here: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard. Desiccant and wrap choices for 08Х17Н15М3Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 08Х17Н15М3Т: Mo ~3–4% plus Ti — above 316Ti for many reducing/chloride mixes.
Shipping documents list GOST 9941, 08Х17Н15М3Т, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. Claims handling for 08Х17Н15М3Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 08Х17Н15М3Т: 317L/Mo-bearing fillers; Ti on the heat already; control heat input.
Why Choose SHH STEEL
SHH STEEL can produce and supply GOST 9941 08Х17Н15М3Т with the cold-/warm-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Technical sales can map 08Х17Н15М3Т against sisters 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 08Х17Н15М3Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х17Н15М3Т to that written scope.
Supply Capability
SHH STEEL can produce and supply GOST 9941 08Х17Н15М3Т across enquiry-oriented OD × wall bands (within cold/warm Table 1 practice), in the cold-/warm-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.
| Item | Capability |
|---|---|
| Standard | GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes |
| Grade | 08Х17Н15М3Т (GOST 5632 chemistry; alias 317Ti / UNS S31726 family (approx)) |
| Product form | Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940) |
| Delivery condition | heat-treated by default (clause 2.3); without HT only by purchaser request |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice |
| Precision | Ordinary, high, or elevated (indices per marking examples) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
SHH STEEL can produce and supply GOST 9941 08Х17Н15М3Т. Stock / Available sizes: enquiry band typically aligns with GOST 9941 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 08Х17Н15М3Т, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: cold-/warm Mo-rich sizes; confirm OD×wall against Table 1 cells. Cap: cold/warm Table 1 practice.
Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т. Email the size list to start. SHH STEEL can produce trial lengths of 08Х17Н15М3Т for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9941 08Х17Н15М3Т seamless stainless steel pipe used for?
- GOST 9941 08Х17Н15М3Т is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Role summary: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9941 08Х17Н15М3Т seamless only, or does it cover welded pipe?
- Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 08Х17Н15М3Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х17Н15М3Т under GOST 9941?
- By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
-
How does 08Х17Н15М3Т compare with sister grades 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т?
- 08Х17Н15М3Т is filed as austenitic Mo + Ti (317Ti class). Typical sisters on the same RFQ are 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т. Design caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х17Н15М3Т?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
-
Is 317Ti / UNS S31726 family (approx) the same as ordering 08Х17Н15М3Т?
- No. 317Ti / UNS S31726 family (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 08Х17Н15М3Т so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9941 08Х17Н15М3Т?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х17Н15М3Т within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm Mo-rich sizes; confirm OD×wall against Table 1 cells. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
-
How should 08Х17Н15М3Т be welded on site?
- Shop guidance: 317L/Mo-bearing fillers; Ti on the heat already; control heat input. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard
-
When should I choose a Mo-bearing or duplex grade instead of 08Х17Н15М3Т?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Mo + Ti (317Ti class) practice can defend for the temperature and stress state. Caution for this mark: confirm OD×wall against Table 1; large-bore RFQs may need hot-deformed 9940 or another standard Sister pointers: 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9941 08Х17Н15М3Т with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 08Х17Н15М3Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9941 08Х17Н15М3Т differ from GOST 9940 of the same mark?
- GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х17Н15М3Т.
Conclusion
GOST 9941 08Х17Н15М3Т is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Х17Н13М2Т, 06ХН28МДТ, 08Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.