GOST 9941 04Х18Н10 Seamless Stainless Steel Pipe
What is GOST 9941 04Х18Н10 Seamless Stainless Steel Pipe
When the approved vendor list and isometric say GOST 9941, the grade mark has to be the GOST 5632 designation. 04Х18Н10 is the full product grade for this austenitic low-carbon 18-8 seamless pipe. Mill brand ЭИ842 / ЭП550. The low-carbon 18-8 mark when the Russian PO wants welded corrosion duty without titanium.
SHH STEEL can supply 04Х18Н10 seamless pipe in the cold-/warm-deformed route, with plain or bevelled ends, random or cut lengths, and GOST 10692 / EN 10204 3.1 style inspection documents when specified. Role on the line: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941.
Equivalence talk to 304L / UNS S30403 (approx) belongs in engineering notes, not as a substitute for the GOST mark. Lock GOST 9941 04Х18Н10, OD × wall, precision class, and HT yes/no before melt. Watch-out: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Related ASTM A312 pipe pages share chemistry families but not GOST acceptance text — confirm before dual-cert claims. Sisters on this hub: 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Use thread: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9.
Inside this GOST 9941 series, compare GOST 9941 08Х18Н10, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н10Т. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 04Х18Н10 (different Rm/δ5 and HT default — not interchangeable by certificate). ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304L.
On 04Х18Н10 packages that also list flats, keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with ASTM A240 Type 304L. Quote 04Х18Н10 pipe and plate under separate line items.
Chemical Composition of GOST 9941 04Х18Н10
Chemistry control on 04Х18Н10 starts at the ladle under GOST 5632. Expect C ≤0.04, Si ≤0.80, Mn ≤2.00, P ≤0.030, S ≤0.020, Ni 9.00–11.00, Cr 17.00–19.00 within the mark’s windows, reported on the inspection document against the heat. Body alias 304L / UNS S30403 (approx) does not widen those windows.
Read the table with the family in mind — austenitic low-carbon 18-8 — and with caution low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Numbers without the matching Table 3 tensile row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 04Х18Н10 before the order is acknowledged. Size practice for 04Х18Н10 remains cold-/warm-deformed OD×wall across Table 1 precision classes.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 04Х18Н10 | ≤0.04 | ≤0.80 | ≤2.00 | ≤0.030 | ≤0.020 | 9.00–11.00 | 17.00–19.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9941 04Х18Н10
Tensile minima for 04Х18Н10 sit at Rm min 490 N/mm², elongation δ5 min 45% (yield not normalised in Table 3). Note: Yield not normalised in Table 3. Flattening or drift expanding backs ductility when ordered. Watch-out: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Elongation δ5 floors and Rm floors travel together on the MTC for 04Х18Н10. Do not accept a certificate that quotes only hardness. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 04Х18Н10 certificate without a written dual-product plan. Corrosion framing beside 04Х18Н10: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 04Х18Н10 | 490 | — (not normalised) | 45 | 7.9 | cold/warm Table 1 practice |
Ambient values from GOST 9941-81 Table 3 for 04Х18Н10. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement.
Seamless Pipe Manufacture of GOST 9941 04Х18Н10
Seamless is not optional wording for 04Х18Н10: GOST 9941 covers cold- and warm-deformed seamless corrosion-resistant pipe. Hot-deformed sisters of related marks live under GOST 9940-81 with different tensile floors. SHH STEEL will not quietly substitute a welded or hot-pierced-only route under a 9941 PO.
Process control for 04Х18Н10 ends with verified dimensions, surface, and any ordered HT (Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement). Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception.
Bevel geometry on walls over 5 mm is by agreement when ordered without a drawing. Size practice: cold-/warm-deformed OD×wall across Table 1 precision classes. Density for theoretical weight of 04Х18Н10: 7.9 g/cm³. Hydrostatic pressure or UT class for 04Х18Н10 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. This paragraph is locked to 04Х18Н10 duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941.
Dimensions and Tolerances for GOST 9941 04Х18Н10
Random length is typically 0.75–12.5 m by wall band (longer by agreement; up to 16 m for OD ≤25 mm); exact lengths take +15 mm; multiple lengths add 5 mm per cut. For 04Х18Н10, confirm whether your project hits the mark-specific OD ceiling. Context: cold-/warm-deformed OD×wall across Table 1 precision classes.
Mass of 1 m uses M = π/1000 · (D − s) · s · ρ with ρ = 7.9 g/cm³ for 04Х18Н10. Size reminder: cold-/warm-deformed OD×wall across Table 1 precision classes. Fixed lengths and multiple cut lengths for 04Х18Н10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 04Х18Н10 stays chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9.
Equivalent Grades for GOST 9941 04Х18Н10
Under GOST 9941, 04Х18Н10 is the governing seamless stainless steel pipe (cold-/warm-deformed) designation on this page. Commercial shorthand such as 304L / UNS S30403 (approx) helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GOST 9941 04Х18Н10 line. ASTM A312 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.
| System | Designation | Notes |
|---|---|---|
| GOST 9941 | 04Х18Н10 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 304L / UNS S30403 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 304L chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 04Х18Н10 still points at GOST 9941, not the brochure alias. Neighbours GOST 9941 08Х18Н10, GOST 9941 08Х18Н10Т, GOST 9941 12Х18Н10Т each carry their own mechanical table. Category hub: GOST 9941. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (04Х18Н10).
Heat Treatment and Delivery Condition for GOST 9941 04Х18Н10
Other heat-treatment schedules are allowed only by written agreement — silence does not invent a mandatory anneal. For 04Х18Н10: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Recorded furnace charts for 04Х18Н10 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 04Х18Н10: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb.
After local hot work in the field, restore ordered HT practice when the corrosion file demands it. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Field heat treatment of 04Х18Н10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 04Х18Н10 duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941.
Corrosion Resistance of GOST 9941 04Х18Н10
Pick tests that match how 04Х18Н10 is filed — austenitic low-carbon 18-8. Corrosion thread: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Coupon orientation, weld condition, and surface finish for 04Х18Н10 belong in the corrosion test order so results can be compared to the installed spool honestly. Weld-shop note tied to 04Х18Н10: 308L-class fillers; low-C cast already helps as-welded IGC.
Sulphur atmospheres, carburising gases, and chlorides are different failure modes — match the mark to the gas or liquid analysis. Use thread: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 04Х18Н10 rather than relying on wall thickness alone. Weld-shop note tied to 04Х18Н10: 308L-class fillers; low-C cast already helps as-welded IGC.
Applications of GOST 9941 04Х18Н10 Seamless Pipe
Project types that repeatedly call 04Х18Н10: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941. Caution still applies: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Furnace, chemical, and aqueous lines all appear in 9941 RFQs — alloy choice still follows the medium. For this mark: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941. Commissioning teams benefit when the as-built dossier repeats 04Х18Н10 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 04Х18Н10 remains cold-/warm-deformed OD×wall across Table 1 precision classes.
Weldability of GOST 9941 04Х18Н10
Even cold-/warm-deformed seamless pipe of 04Х18Н10 will see field welds. Use: 308L-class fillers; low-C cast already helps as-welded IGC. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 04Х18Н10 should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Application context for 04Х18Н10 stays chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9.
Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941. Consumable lot control and shielding-gas notes for 04Х18Н10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 04Х18Н10 caution visible here: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Surface Finishes for GOST 9941 04Х18Н10
Finish options for 04Х18Н10 follow the ordered heat-treatment route under GOST 9941. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: heat-treated by default (clause 2.3); without HT only by purchaser request.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Passivation restores the chromium-rich film after pickling or light fabrication on 04Х18Н10; it does not replace the heat treatment that sets mechanical properties under GOST 9941. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.
Inspection and Testing for GOST 9941 04Х18Н10
Batching rules limit a party to 300 pieces of one size, one mark, and one heat-treatment kind (and one heat when ordered). For 04Х18Н10, keep the heat identity unbroken from melt to bundle tag. Duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941.
Intergranular corrosion, elevated tensile, and yield checks are extras — see the mechanical note for 04Х18Н10. Order them under the PO when the stress or corrosion file needs them. Non-conforming 04Х18Н10 lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Keep the 04Х18Н10 caution visible here: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Packaging and Shipping for GOST 9941 04Х18Н10
Small-OD 04Х18Н10 often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Bundle tickets for 04Х18Н10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 04Х18Н10 stays chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9.
Bevelled ends get protectors so landing edges survive trucking. Size hint: cold-/warm-deformed OD×wall across Table 1 precision classes. Desiccant and wrap choices for 04Х18Н10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 04Х18Н10: 308L-class fillers; low-C cast already helps as-welded IGC.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Claims handling for 04Х18Н10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 04Х18Н10: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb.
Why Choose SHH STEEL
Project teams working to CIS pipe specs need a supplier that reads Cyrillic grade names correctly. SHH STEEL can make 04Х18Н10 to that discipline. Caution we keep visible: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. SHH STEEL can produce and supply 04Х18Н10 against the OD × wall, cold-/warm-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (GOST + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Ask for a written acknowledgement that names 04Х18Н10, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 04Х18Н10 to that written scope.
Supply Capability
Whether you need prototype spools or project tonnage of 04Х18Н10, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 04Х18Н10 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes |
| Grade | 04Х18Н10 (GOST 5632 chemistry; alias 304L / UNS S30403 (approx)) |
| Product form | Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940) |
| Delivery condition | heat-treated by default (clause 2.3); without HT only by purchaser request |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice |
| Precision | Ordinary, high, or elevated (indices per marking examples) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes piercing slots for 04Х18Н10 rather than promising anonymous warehouse tons. Typical conversation starts around cold-/warm-deformed OD×wall across Table 1 precision classes. SHH STEEL can supply alternate walls and precision classes for 04Х18Н10 once the design pressure and corrosion allowance are clear.
If the project needs dual GOST 9941 + ASTM documentation, say so before melt. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. SHH STEEL can produce trial lengths of 04Х18Н10 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9941 04Х18Н10 seamless stainless steel pipe used for?
- GOST 9941 04Х18Н10 is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Role summary: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9941 04Х18Н10 seamless only, or does it cover welded pipe?
- Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 04Х18Н10 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 04Х18Н10 under GOST 9941?
- By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal / family HT mandatory by default (GOST 9941 clause 2.3); without HT only when purchaser orders it — then mech by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
-
How does 04Х18Н10 compare with sister grades 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т?
- 04Х18Н10 is filed as austenitic low-carbon 18-8. Typical sisters on the same RFQ are 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Design caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 04Х18Н10?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
-
Is 304L / UNS S30403 (approx) the same as ordering 04Х18Н10?
- No. 304L / UNS S30403 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 04Х18Н10 so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9941 04Х18Н10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 04Х18Н10 within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm-deformed OD×wall across Table 1 precision classes. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
-
How should 04Х18Н10 be welded on site?
- Shop guidance: 308L-class fillers; low-C cast already helps as-welded IGC. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades
-
When should I choose a Mo-bearing or duplex grade instead of 04Х18Н10?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic low-carbon 18-8 practice can defend for the temperature and stress state. Caution for this mark: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades Sister pointers: 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9941 04Х18Н10 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 04Х18Н10 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9941 04Х18Н10 differ from GOST 9940 of the same mark?
- GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 04Х18Н10.
Conclusion
GOST 9941 04Х18Н10 is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9941. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.