GOST 9941 15Х25Т Seamless Stainless Steel Pipe
What is GOST 9941 15Х25Т Seamless Stainless Steel Pipe
Russian and CIS piping packages that print GOST 9941 expect cold-/warm-deformed seamless stainless pipe, not a welded substitute and not an automatic ASTM A312 certificate. 15Х25Т is the Cyrillic mark on Table 3 for this ferritic high-chromium (Ti-stabilised) chemistry. Mill brand ЭИ439. The Ti-bearing high-Cr ferritic that CIS furnace BOMs still print.
Mill path for 15Х25Т: cold-/warm-deformed seamless route, clause 2.3 heat-treatment (mandatory by default), GOST 5632 chemistry, Table 3 Rm and elongation, optional hydro / UT / IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name.
Body text may mention 446Ti / UNS S44600 family (approx) for cross-reference, but the H1 and order line stay on Cyrillic 15Х25Т. Silent alias swaps are how wrong carbon ceilings and wrong Table 3 numbers enter the MTC. Keep this caution in view: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
Order the standard the drawing and regulatory file actually require. Inside this 9941 series, compare 08Х17Т, 12Х17, 08Х13 before stretching surface finish or wall alone. Duty thread: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes. Document the medium, design temperature, and weld map beside the 15Х25Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for 15Х25Т stays thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name.
Inside this GOST 9941 series, compare GOST 9941 08Х17Т, GOST 9941 12Х17, GOST 9941 08Х13. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 15Х25Т (different Rm/δ5 and HT default — not interchangeable by certificate).
Chemical Composition of GOST 9941 15Х25Т
GOST 5632 sets the melt limits for 15Х25Т. Highlight band: C ≤0.15, Si ≤1.00, Mn ≤0.80, P ≤0.035, S ≤0.025, Cr 24.00–27.00, Ti 5×C–0.90. For pipe intended for welding, GOST 9941 can tighten sulphur to ≤0.020% when the order states that duty. Alias note: 446Ti / UNS S44600 family (approx).
The composition table below is the cast window SHH STEEL quotes against for 15Х25Т. Edition framing is GOST 5632 for chemistry and GOST 9941-81 for the pipe product. Use thread: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 15Х25Т before the order is acknowledged. This paragraph is locked to 15Х25Т duty: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes.
| Grade | C | Si | Mn | P | S | Cr | Ti |
|---|---|---|---|---|---|---|---|
| 15Х25Т | ≤0.15 | ≤1.00 | ≤0.80 | ≤0.035 | ≤0.025 | 24.00–27.00 | 5×C–0.90 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9941 15Х25Т
Table 3 mechanical acceptance for 15Х25Т: Rm min 461 N/mm², elongation δ5 min 17% (yield not normalised in Table 3). Note: Yield not normalised in Table 3. Delivery framing: heat-treated by default (clause 2.3); without HT only by purchaser request. Density for mass calc: 7.6 g/cm³. Sampling follows GOST 9941 batch rules (party ≤300 pcs).
Elevated-temperature tensile at 623 K (350 °C) and yield determination are purchaser options, not defaults. For 15Х25Т, state them on the PO if the stress calculation needs them. Use: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 15Х25Т certificate without a written dual-product plan. Application context for 15Х25Т stays thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 15Х25Т | 461 | — (not normalised) | 17 | 7.6 | OD typically ≥21 mm for this mark (Table 1 note) |
Ambient values from GOST 9941-81 Table 3 for 15Х25Т. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Ferritic soften/anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech.
Seamless Pipe Manufacture of GOST 9941 15Х25Т
GOST 9941-81 manufactures 15Х25Т as seamless cold- and warm-deformed stainless pipe only — cold draw, cold roll, or warm reduce to Table 1 sizes after a hollow is prepared. SHH STEEL confirms the cold-/warm-deformed seamless route on the acknowledgement before finishing starts; welded pipe and hot-deformed GOST 9940 product are outside this line item.
After hot deformation, 15Х25Т receives heat treatment by default — without HT only if the order waives it — Ferritic soften/anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech. Ferritic heats follow softening / anneal practice as the default HT path — not austenitic solution charts. Grain growth after overheating remains a shop risk. Use thread: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name.
Marking carries the grade 15Х25Т, size, precision cue when high class, manufacturer ID, and GOST 9941 reference. Size hint: OD typically ≥21 mm; cold/warm thin-wall practice. Weld thread for fabricator joints: Ti already present; keep heat input modest and match ferritic filler practice. Hydrostatic pressure or UT class for 15Х25Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 15Х25Т caution visible here: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
Dimensions and Tolerances for GOST 9941 15Х25Т
Dimensional order lines for 15Х25Т should state OD × wall, length type (random, exact, multiple, or limited), end finish, and precision class. Use: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. Max OD for this mark: None mm. Precision class follows the tolerance ordered for 15Х25Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 15Х25Т duty: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes.
Ovality has no separate number — it must not push OD outside the diameter tolerance. Caution: still ferritic — do not expect 18-8 toughness or chloride pitting resistance. Fixed lengths and multiple cut lengths for 15Х25Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 15Х25Т caution visible here: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
Equivalent Grades for GOST 9941 15Х25Т
Under GOST 9941, 15Х25Т is the governing seamless stainless steel pipe (cold-/warm-deformed) designation on this page. Commercial shorthand such as 446Ti / UNS S44600 family (approx) helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GOST 9941 15Х25Т line. ASTM A312 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.
| System | Designation | Notes |
|---|---|---|
| GOST 9941 | 15Х25Т | Governing pipe grade for this page |
| Commercial / UNS (body only) | 446Ti / UNS S44600 family (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Read the notes column literally for 15Х25Т: related chemistry is not automatic dual-cert. Cross-check GOST 9941 08Х17Т, GOST 9941 12Х17, GOST 9941 08Х13 when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9941. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (15Х25Т). Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (15Х25Т).
15Х25Т sourcing notes should keep forms separate: keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with ASTM A240 UNS S44600. Keep 15Х25Т acceptance text on the governing pipe/tube standard.
Heat Treatment and Delivery Condition for GOST 9941 15Х25Т
Mill heat treatment for 15Х25Т is mandatory by default per clause 2.3 — Ferritic soften/anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech. Bright or descaled finishes are separate order items. Delivery label: heat-treated by default (clause 2.3); without HT only by purchaser request.
Certificate wording for 15Х25Т should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature — or explicitly “without heat treatment” when that was ordered. Use: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. Field heat treatment of 15Х25Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 15Х25Т stays thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name.
Corrosion Resistance of GOST 9941 15Х25Т
oxidation and many nitric-family media; Ti improves welded IGC behaviour versus plain 15Х28 Ordering IGC does not create a blanket corrosion warranty for every medium. Family filing: ferritic high-chromium (Ti-stabilised). Coupon orientation, weld condition, and surface finish for 15Х25Т belong in the corrosion test order so results can be compared to the installed spool honestly. Keep the 15Х25Т caution visible here: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 15Х25Т honestly against 08Х17Т, 12Х17, 08Х13. Role: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 15Х25Т rather than relying on wall thickness alone. Corrosion framing beside 15Х25Т: oxidation and many nitric-family media; Ti improves welded IGC behaviour versus plain 15Х28.
Applications of GOST 9941 15Х25Т Seamless Pipe
Typical BOM language pairs GOST 9941 15Х25Т with OD × wall, precision class, and heat-treatment yes/no. Primary sketch: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. Spool fabricators should copy 15Х25Т onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to 15Х25Т: Ti already present; keep heat input modest and match ferritic filler practice.
Spell 15Х25Т on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 08Х17Т, 12Х17, 08Х13. Commissioning teams benefit when the as-built dossier repeats 15Х25Т beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 15Х25Т remains OD typically ≥21 mm; cold/warm thin-wall practice.
Weldability of GOST 9941 15Х25Т
Weldability of 15Х25Т follows ferritic high-chromium (Ti-stabilised) practice. Filler/shop note: Ti already present; keep heat input modest and match ferritic filler practice. Caution: still ferritic — do not expect 18-8 toughness or chloride pitting resistance. Procedure qualification for 15Х25Т should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Keep the 15Х25Т caution visible here: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
For corrosive as-welded duty on 15Х25Т, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: Ti already present; keep heat input modest and match ferritic filler practice. Order sulphur ≤0.020% when the pipe is intended for welding. Consumable lot control and shielding-gas notes for 15Х25Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 15Х25Т: oxidation and many nitric-family media; Ti improves welded IGC behaviour versus plain 15Х28.
Surface Finishes for GOST 9941 15Х25Т
Welded or heavily formed 15Х25Т may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GOST 9941 seamless stainless steel pipe (cold-/warm-deformed). Caution: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
| Finish | Typical supply | Order note |
|---|---|---|
| Annealed and pickled | Standard pipe mill finish after anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; inspect before polish on ferritic stock |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Reject grinding burns, embedded free iron, and unrepaired undercut on 15Х25Т before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GOST 9941 for this ferritic high-chromium (Ti-stabilised) mark. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 15Х25Т.
Inspection and Testing for GOST 9941 15Х25Т
SHH STEEL reports the tests actually performed for 15Х25Т — no surrogate NDT lines. Hydrostatic versus ultrasonic choice belongs on the PO. Caution: still ferritic — do not expect 18-8 toughness or chloride pitting resistance. Sampling plans for 15Х25Т keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 15Х25Т: Ti already present; keep heat input modest and match ferritic filler practice.
Retests use double sample counts from the same party — failures are not silently shipped. Size context: OD typically ≥21 mm; cold/warm thin-wall practice. Non-conforming 15Х25Т lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Weld-shop note tied to 15Х25Т: Ti already present; keep heat input modest and match ferritic filler practice.
Packaging and Shipping for GOST 9941 15Х25Т
Export packing for GOST 9941 15Х25Т is built around rust prevention and transit abrasion control. Bundle tickets repeat the Cyrillic grade symbol and heat number. Duty: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes. Bundle tickets for 15Х25Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 15Х25Т remains OD typically ≥21 mm; cold/warm thin-wall practice.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 15Х25Т. Desiccant and wrap choices for 15Х25Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 15Х25Т duty: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes.
Photographic packing records are available on request for project QA files on 15Х25Т. Claims handling for 15Х25Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 15Х25Т duty: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes.
Why Choose SHH STEEL
Buyers choose SHH STEEL for 15Х25Т because the paperwork matches the stencil: GOST 5632 chemistry, Table 3 tensile, ordered HT, and honest seamless marking. Application fit: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. SHH STEEL can produce and supply 15Х25Т against the OD × wall, cold-/warm-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 15Х25Т cleanly. Ask for a written acknowledgement that names 15Х25Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 15Х25Т to that written scope.
Supply Capability
Supply capability for 15Х25Т covers cold-/warm-deformed seamless manufacture, ordered heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 15Х25Т when the mill schedule allows. Keep the 15Х25Т caution visible here: still ferritic — do not expect 18-8 toughness or chloride pitting resistance.
| Item | Capability |
|---|---|
| Standard | GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes |
| Grade | 15Х25Т (GOST 5632 chemistry; alias 446Ti / UNS S44600 family (approx)) |
| Product form | Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940) |
| Delivery condition | heat-treated by default (clause 2.3); without HT only by purchaser request |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: OD typically ≥21 mm for this mark (Table 1 note) |
| Precision | Ordinary, high, or elevated (indices per marking examples) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes for 15Х25Т: common OD×wall combinations as the project uses. Cold-/warm-deformed availability varies by diameter — confirm with the RFQ. Hint: OD typically ≥21 mm; cold/warm thin-wall practice. SHH STEEL can supply alternate walls and precision classes for 15Х25Т once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 15Х25Т supply scope when the PO says so. Use: thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. SHH STEEL can produce trial lengths of 15Х25Т for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9941 15Х25Т seamless stainless steel pipe used for?
- GOST 9941 15Х25Т is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — thermocouple wells, furnace tube stubs, and nitric-plant ferritic spools that call 15Х25Т by name. Role summary: Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9941 15Х25Т seamless only, or does it cover welded pipe?
- Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 15Х25Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 15Х25Т under GOST 9941?
- By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Ferritic soften/anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
-
How does 15Х25Т compare with sister grades 08Х17Т, 12Х17, 08Х13?
- 15Х25Т is filed as ferritic high-chromium (Ti-stabilised). Typical sisters on the same RFQ are 08Х17Т, 12Х17, 08Х13. Design caution: still ferritic — do not expect 18-8 toughness or chloride pitting resistance Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 15Х25Т?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
-
Is 446Ti / UNS S44600 family (approx) the same as ordering 15Х25Т?
- No. 446Ti / UNS S44600 family (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 15Х25Т so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9941 15Х25Т?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 15Х25Т within Table 1 practice, respecting the mark’s diameter cap (OD typically ≥21 mm for this mark (Table 1 note)). Size context: OD typically ≥21 mm; cold/warm thin-wall practice. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
-
How should 15Х25Т be welded on site?
- Shop guidance: Ti already present; keep heat input modest and match ferritic filler practice. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: still ferritic — do not expect 18-8 toughness or chloride pitting resistance
-
When should I choose a Mo-bearing or duplex grade instead of 15Х25Т?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what ferritic high-chromium (Ti-stabilised) practice can defend for the temperature and stress state. Caution for this mark: still ferritic — do not expect 18-8 toughness or chloride pitting resistance Sister pointers: 08Х17Т, 12Х17, 08Х13. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9941 15Х25Т with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 15Х25Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9941 15Х25Т differ from GOST 9940 of the same mark?
- GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 15Х25Т.
Conclusion
GOST 9941 15Х25Т is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Ti-stabilised ~25% Cr ferritic seamless pipe for oxidising furnace and heat-resistant aqueous notes. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х17Т, 12Х17, 08Х13. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.