GOST 9941 06ХН28МДТ Seamless Stainless Steel Pipe

GOST 9941 06ХН28МДТ seamless stainless steel pipe (Alloy 28 / UNS N08028 family (approx)), austenitic high-Ni Mo-Cu Ti (Hastelloy-class CIS alloy), GOST 5632 cast analysis, Rm min 490 N/mm² / δ5 min 30%, cold-/warm-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
06ХН28МДТ (GOST 5632 / Alloy 28 / UNS N08028 family (approx) — body alias)
Standard
GOST 9941-81
Product form
Seamless stainless steel pipe (cold-/warm-deformed), delivery heat-treated by default (clause 2.3); without HT only by purchaser request
Size
OD × wall per Table 1; mark cap OD 14–85 mm × wall 1–5 mm (Table 1 note for this alloy); random length typically 1.5–12.5 m by wall band
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9941 06ХН28МДТ Seamless Stainless Steel Pipe

When the approved vendor list and isometric say GOST 9941, the grade mark has to be the GOST 5632 designation. 06ХН28МДТ is the full product grade for this austenitic high-Ni Mo-Cu Ti (Hastelloy-class CIS alloy) seamless pipe. Mill brand ЭИ943. The alloy mark unique to GOST 9941 Table 3 among the Jack title set — 06ХН28МДТ (ЭИ943), absent from GOST 9940.

SHH STEEL can supply 06ХН28МДТ seamless pipe in the cold-/warm-deformed route, with plain or bevelled ends, random or cut lengths, and GOST 10692 / EN 10204 3.1 style inspection documents when specified. Role on the line: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941.

Equivalence talk to Alloy 28 / UNS N08028 family (approx) belongs in engineering notes, not as a substitute for the GOST mark. Lock GOST 9941 06ХН28МДТ, OD × wall, precision class, and HT yes/no before melt. Watch-out: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

Related ASTM A312 pipe pages share chemistry families but not GOST acceptance text — confirm before dual-cert claims. Sisters on this hub: 08Х17Н15М3Т, 10Х17Н13М2Т, 10Х23Н18. Use thread: sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory.

Inside this GOST 9941 series, compare GOST 9941 08Х17Н15М3Т, GOST 9941 10Х17Н13М2Т, GOST 9941 10Х23Н18. Hub: GOST 9941. Note: 06ХН28МДТ appears in GOST 9941 Table 3 and is absent from GOST 9940 Table 3.

Project teams specifying 06ХН28МДТ should form hubs stay Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates — no verified plate product page is attached for this chemistry yet. Quote 06ХН28МДТ pipe and plate under separate line items.

Chemical Composition of GOST 9941 06ХН28МДТ

Chemistry control on 06ХН28МДТ starts at the ladle under GOST 5632. Expect C ≤0.06, Si ≤0.80, Mn ≤0.80, P ≤0.035, S ≤0.020, Ni 26.00–29.00, Cr 22.00–25.00, Mo 2.50–3.50 within the mark’s windows, reported on the inspection document against the heat. Body alias Alloy 28 / UNS N08028 family (approx) does not widen those windows.

Read the table with the family in mind — austenitic high-Ni Mo-Cu Ti (Hastelloy-class CIS alloy) — and with caution OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap. Numbers without the matching Table 3 tensile row are incomplete purchase data.

Grade C Si Mn P S Ni Cr Mo Cu Ti
06ХН28МДТ ≤0.06 ≤0.80 ≤0.80 ≤0.035 ≤0.020 26.00–29.00 22.00–25.00 2.50–3.50 2.50–3.50 0.40–0.90

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9941 06ХН28МДТ

Tensile minima for 06ХН28МДТ sit at Rm min 490 N/mm², elongation δ5 min 30% (yield not normalised in Table 3). Note: Yield not normalised in Table 3. Flattening or drift expanding backs ductility when ordered. Watch-out: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

Elongation δ5 floors and Rm floors travel together on the MTC for 06ХН28МДТ. Do not accept a certificate that quotes only hardness. Caution: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 06ХН28МДТ certificate without a written dual-product plan. This paragraph is locked to 06ХН28МДТ duty: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
06ХН28МДТ 490 — (not normalised) 30 7.96 OD 14–85 mm × wall 1–5 mm (Table 1 note for this alloy)

Ambient values from GOST 9941-81 Table 3 for 06ХН28МДТ. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Solution anneal mandatory by default under GOST 9941 clause 2.3; without HT only by agreement.

Seamless Pipe Manufacture of GOST 9941 06ХН28МДТ

SHH STEEL can produce 06ХН28МДТ as cold-/warm-deformed seamless pipe to GOST 9941-81, then apply the mandatory heat treatment (unless the PO waives HT), lighten or pickle the surface, and finish ends. Plain square-cut ends are default; weld bevels on walls over 5 mm only when the purchaser asks.

Process control for 06ХН28МДТ ends with verified dimensions, surface, and any ordered HT (Solution anneal mandatory by default under GOST 9941 clause 2.3; without HT only by agreement). Austenitic heats take solution annealing with rapid cool as the default HT path under 9941; skip inventing a without-HT shipment unless the PO freezes that exception.

Bevel geometry on walls over 5 mm is by agreement when ordered without a drawing. Size practice: OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note). Density for theoretical weight of 06ХН28МДТ: 7.96 g/cm³. Hydrostatic pressure or UT class for 06ХН28МДТ is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 06ХН28МДТ stays sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory.

Dimensions and Tolerances for GOST 9941 06ХН28МДТ

Random length is typically 0.75–12.5 m by wall band (longer by agreement; up to 16 m for OD ≤25 mm); exact lengths take +15 mm; multiple lengths add 5 mm per cut. For 06ХН28МДТ, confirm whether your project hits the mark-specific OD ceiling. Context: OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note).

Mass of 1 m uses M = π/1000 · (D − s) · s · ρ with ρ = 7.96 g/cm³ for 06ХН28МДТ. Size reminder: OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note). Fixed lengths and multiple cut lengths for 06ХН28МДТ are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 06ХН28МДТ remains OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note).

Equivalent Grades for GOST 9941 06ХН28МДТ

Lock 06ХН28МДТ on the PO when the datasheet owner wants GOST 9941 seamless stainless steel pipe (cold-/warm-deformed). Commercial talk as Alloy 28 / UNS N08028 family (approx) is fine in emails; mill paperwork must still show GOST 9941 06ХН28МДТ. Application framing: matching high-Ni Mo-Cu fillers; control dilution; Ti already on cast; treat as alloy weld procedure, not 308L habit.

System Designation Notes
GOST 9941 06ХН28МДТ Governing pipe grade for this page
Commercial / UNS (body only) Alloy 28 / UNS N08028 family (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 06ХН28МДТ still points at GOST 9941, not the brochure alias. Neighbours GOST 9941 08Х17Н15М3Т, GOST 9941 10Х17Н13М2Т, GOST 9941 10Х23Н18 each carry their own mechanical table. Category hub: GOST 9941. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (06ХН28МДТ).

Heat Treatment and Delivery Condition for GOST 9941 06ХН28МДТ

Other heat-treatment schedules are allowed only by written agreement — silence does not invent a mandatory anneal. For 06ХН28МДТ: Solution anneal mandatory by default under GOST 9941 clause 2.3; without HT only by agreement. Recorded furnace charts for 06ХН28МДТ should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Keep the 06ХН28МДТ caution visible here: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

After local hot work in the field, restore ordered HT practice when the corrosion file demands it. Caution: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap. Field heat treatment of 06ХН28МДТ after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 06ХН28МДТ caution visible here: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

Corrosion Resistance of GOST 9941 06ХН28МДТ

Pick tests that match how 06ХН28МДТ is filed — austenitic high-Ni Mo-Cu Ti (Hastelloy-class CIS alloy). Corrosion thread: Mo + Cu + high Ni for reducing acids; IGC test method ВУ (WU) per GOST 6032 when ordered — different from AM/AMU used on most stainless marks. Caution: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

Sulphur atmospheres, carburising gases, and chlorides are different failure modes — match the mark to the gas or liquid analysis. Use thread: sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06ХН28МДТ rather than relying on wall thickness alone. This paragraph is locked to 06ХН28МДТ duty: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941.

Applications of GOST 9941 06ХН28МДТ Seamless Pipe

Project types that repeatedly call 06ХН28МДТ: sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory. Duty: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941. Caution still applies: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

Furnace, chemical, and aqueous lines all appear in 9941 RFQs — alloy choice still follows the medium. For this mark: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941. Commissioning teams benefit when the as-built dossier repeats 06ХН28МДТ beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 06ХН28МДТ remains OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note).

Weldability of GOST 9941 06ХН28МДТ

Even cold-/warm-deformed seamless pipe of 06ХН28МДТ will see field welds. Use: matching high-Ni Mo-Cu fillers; control dilution; Ti already on cast; treat as alloy weld procedure, not 308L habit. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 06ХН28МДТ should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Weld-shop note tied to 06ХН28МДТ: matching high-Ni Mo-Cu fillers; control dilution; Ti already on cast; treat as alloy weld procedure, not 308L habit.

Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941. Consumable lot control and shielding-gas notes for 06ХН28МДТ stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 06ХН28МДТ remains OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note).

Surface Finishes for GOST 9941 06ХН28МДТ

06ХН28МДТ under GOST 9941 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (06ХН28МДТ).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

SHH STEEL sequences pickle, optional passivation, and any agreed polish for 06ХН28МДТ after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long pipe life in the field. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06ХН28МДТ.

Inspection and Testing for GOST 9941 06ХН28МДТ

Batching rules limit a party to 300 pieces of one size, one mark, and one heat-treatment kind (and one heat when ordered). For 06ХН28МДТ, keep the heat identity unbroken from melt to bundle tag. Duty: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941.

Intergranular corrosion, elevated tensile, and yield checks are extras — see the mechanical note for 06ХН28МДТ. Order them under the PO when the stress or corrosion file needs them. Non-conforming 06ХН28МДТ lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Corrosion framing beside 06ХН28МДТ: Mo + Cu + high Ni for reducing acids; IGC test method ВУ (WU) per GOST 6032 when ordered — different from AM/AMU used on most stainless marks.

Packaging and Shipping for GOST 9941 06ХН28МДТ

Small-OD 06ХН28МДТ often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory. Bundle tickets for 06ХН28МДТ repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 06ХН28МДТ: Mo + Cu + high Ni for reducing acids; IGC test method ВУ (WU) per GOST 6032 when ordered — different from AM/AMU used on most stainless marks.

Bevelled ends get protectors so landing edges survive trucking. Size hint: OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note). Desiccant and wrap choices for 06ХН28МДТ follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 06ХН28МДТ stays sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory. Claims handling for 06ХН28МДТ starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 06ХН28МДТ: Mo + Cu + high Ni for reducing acids; IGC test method ВУ (WU) per GOST 6032 when ordered — different from AM/AMU used on most stainless marks.

Why Choose SHH STEEL

Project teams working to CIS pipe specs need a supplier that reads Cyrillic grade names correctly. SHH STEEL can make 06ХН28МДТ to that discipline. Caution we keep visible: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap.

Dual-cert discussions (GOST + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 08Х17Н15М3Т, 10Х17Н13М2Т, 10Х23Н18. Ask for a written acknowledgement that names 06ХН28МДТ, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 06ХН28МДТ to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of 06ХН28МДТ, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 06ХН28МДТ when the mill schedule allows.

Item Capability
Standard GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes
Grade 06ХН28МДТ (GOST 5632 chemistry; alias Alloy 28 / UNS N08028 family (approx))
Product form Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940)
Delivery condition heat-treated by default (clause 2.3); without HT only by purchaser request
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: OD 14–85 mm × wall 1–5 mm (Table 1 note for this alloy)
Precision Ordinary, high, or elevated (indices per marking examples)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes piercing slots for 06ХН28МДТ rather than promising anonymous warehouse tons. Typical conversation starts around OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note). SHH STEEL can supply alternate walls and precision classes for 06ХН28МДТ once the design pressure and corrosion allowance are clear.

If the project needs dual GOST 9941 + ASTM documentation, say so before melt. Caution: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap. SHH STEEL can produce trial lengths of 06ХН28МДТ for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9941 06ХН28МДТ seamless stainless steel pipe used for?
GOST 9941 06ХН28МДТ is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — sulphuric/phosphoric acid plant lines, organic acid condensers, and CIS packages that outgrow Mo austenitics into ЭИ943 territory. Role summary: high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9941 06ХН28МДТ seamless only, or does it cover welded pipe?
Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 06ХН28МДТ when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 06ХН28МДТ under GOST 9941?
By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Solution anneal mandatory by default under GOST 9941 clause 2.3; without HT only by agreement. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
How does 06ХН28МДТ compare with sister grades 08Х17Н15М3Т, 10Х17Н13М2Т, 10Х23Н18?
06ХН28МДТ is filed as austenitic high-Ni Mo-Cu Ti (Hastelloy-class CIS alloy). Typical sisters on the same RFQ are 08Х17Н15М3Т, 10Х17Н13М2Т, 10Х23Н18. Design caution: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06ХН28МДТ?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
Is Alloy 28 / UNS N08028 family (approx) the same as ordering 06ХН28МДТ?
No. Alloy 28 / UNS N08028 family (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 06ХН28МДТ so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9941 06ХН28МДТ?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06ХН28МДТ within Table 1 practice, respecting the mark’s diameter cap (OD 14–85 mm × wall 1–5 mm (Table 1 note for this alloy)). Size context: OD 14–85 mm × wall 1–5 mm only (Table 1 alloy note). Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
How should 06ХН28МДТ be welded on site?
Shop guidance: matching high-Ni Mo-Cu fillers; control dilution; Ti already on cast; treat as alloy weld procedure, not 308L habit. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap
When should I choose a Mo-bearing or duplex grade instead of 06ХН28МДТ?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic high-Ni Mo-Cu Ti (Hastelloy-class CIS alloy) practice can defend for the temperature and stress state. Caution for this mark: OD 14–85 mm × wall 1–5 mm only — large bore is outside this alloy’s Table 1 note; not a 316Ti swap Sister pointers: 08Х17Н15М3Т, 10Х17Н13М2Т, 10Х23Н18. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9941 06ХН28МДТ with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 06ХН28МДТ does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9941 06ХН28МДТ differ from GOST 9940 of the same mark?
GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 06ХН28МДТ.

Conclusion

GOST 9941 06ХН28МДТ is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — high-Ni Mo-Cu Ti alloy seamless pipe for reducing acids and severe chemical service on GOST 9941. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х17Н15М3Т, 10Х17Н13М2Т, 10Х23Н18. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X