GOST 9941 08Х22Н6Т Seamless Stainless Steel Pipe

GOST 9941 08Х22Н6Т seamless stainless steel pipe (lean duplex / 22Cr-6Ni Ti (approx)), austenitic-ferritic (duplex-lean) Ti-stabilised, GOST 5632 cast analysis, Rm min 588 N/mm² / δ5 min 20%, cold-/warm-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
08Х22Н6Т (GOST 5632 / lean duplex / 22Cr-6Ni Ti (approx) — body alias)
Standard
GOST 9941-81
Product form
Seamless stainless steel pipe (cold-/warm-deformed), delivery heat-treated by default (clause 2.3); without HT only by purchaser request
Size
OD × wall per Table 1; mark cap cold/warm Table 1 practice; random length typically 1.5–12.5 m by wall band
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9941 08Х22Н6Т Seamless Stainless Steel Pipe

GOST 9941 covers seamless cold-/warm-deformed stainless pipe across the cold-/warm Table 1 OD×wall grid in ordinary, high, and elevated precision classes. Inside that standard, 08Х22Н6Т is filed as austenitic-ferritic (duplex-lean) Ti-stabilised. Mill brand ЭП53. The duplex-lean Russian mark that tops Table 3 tensile strength under GOST 9941.

From pierce through marking and crate protection, SHH STEEL can produce GOST 9941 08Х22Н6Т for the sizes and tests on your RFQ. Application sketch: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Size and test clarity on the RFQ lets SHH STEEL lock the correct cold-/warm-deformed seamless scope for 08Х22Н6Т before production starts. Size practice for 08Х22Н6Т remains cold-/warm lean-duplex sizes under Table 1.

On the floor people latinise marks; in QA they must not. 08Х22Н6Т under GOST 9941 carries specific Table 3 floors that a loose “lean duplex” note will not enforce. Caution: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 08Х22Н6Т so informal alias language cannot reopen the carbon or molybdenum window after melt. Size practice for 08Х22Н6Т remains cold-/warm lean-duplex sizes under Table 1.

Pair standard GOST 9940 uses many of the same marks with hot deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Use thread: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Document the medium, design temperature, and weld map beside the 08Х22Н6Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Inside this GOST 9941 series, compare GOST 9941 08Х18Н10Т, GOST 9941 10Х17Н13М2Т, GOST 9941 08Х20Н14С2. Hub: GOST 9941. Related hot-deformed product page: GOST 9940 08Х22Н6Т (different Rm/δ5 and HT default — not interchangeable by certificate).

Chemical Composition of GOST 9941 08Х22Н6Т

For 08Х22Н6Т, the melt ticket has to show GOST 5632 compliance — C ≤0.08, Si ≤0.80, Mn ≤0.80, P ≤0.035, S ≤0.025, Ni 5.30–6.30, Cr 21.00–23.00, Ti 5×C–0.65. Optional residual limits still forbid blurring grade identity. Corrosion framing: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Where Mo, Ti or Nb appear, they are intentional levers for 08Х22Н6Т, not optional marketing. Confirm them on the MTC line-by-line. Role: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х22Н6Т before the order is acknowledged. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3.

Grade C Si Mn P S Ni Cr Ti
08Х22Н6Т ≤0.08 ≤0.80 ≤0.80 ≤0.035 ≤0.025 5.30–6.30 21.00–23.00 5×C–0.65

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9941-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9941 08Х22Н6Т

Do not confuse Table 3 cold-/warm-deformed floors with GOST 9940 hot-deformed numbers that share the lean duplex / 22Cr-6Ni Ti (approx) alias. For 08Х22Н6Т under 9941 expect Rm min 588 N/mm², elongation δ5 min 20% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised in Table 3.

When comparing 08Х22Н6Т to a hot-deformed GOST 9940 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. Do not substitute GOST 9940 hot-deformed tensile numbers onto a cold-/warm-deformed 08Х22Н6Т certificate without a written dual-product plan. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
08Х22Н6Т 588 — (not normalised) 20 7.6 cold/warm Table 1 practice

Ambient values from GOST 9941-81 Table 3 for 08Х22Н6Т. Yield not normalised in Table 3. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request. Heat-treatment guidance: Phase-balance-aware anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech.

Seamless Pipe Manufacture of GOST 9941 08Х22Н6Т

For 08Х22Н6Т, the mill path is cold or warm deformation of a seamless hollow — never ERW under GOST 9941. Heat treatment is mandatory by default under clause 2.3; without HT only when the purchaser explicitly orders it (then mech and curvature by agreement). Order ordinary, high, or elevated precision class with the size.

Precision class (ordinary or high) is an order item for 08Х22Н6Т; unmarked class means ordinary. Heat treatment: Phase-balance-aware anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech. Duplex-lean heats need phase-balance-aware anneal as the default HT path; austenitic-only quench charts are the wrong default.

Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless cold-/warm-deformed. Size: cold-/warm lean-duplex sizes under Table 1. Hydrostatic pressure or UT class for 08Х22Н6Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3.

Dimensions and Tolerances for GOST 9941 08Х22Н6Т

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 08Х22Н6Т. Duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. Cap: cold/warm Table 1 practice. Precision class follows the tolerance ordered for 08Х22Н6Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3.

High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 08Х22Н6Т. Fixed lengths and multiple cut lengths for 08Х22Н6Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Equivalent Grades for GOST 9941 08Х22Н6Т

Lock 08Х22Н6Т on the PO when the datasheet owner wants GOST 9941 seamless stainless steel pipe (cold-/warm-deformed). Commercial talk as lean duplex / 22Cr-6Ni Ti (approx) is fine in emails; mill paperwork must still show GOST 9941 08Х22Н6Т. Application framing: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8.

System Designation Notes
GOST 9941 08Х22Н6Т Governing pipe grade for this page
Commercial / UNS (body only) lean duplex / 22Cr-6Ni Ti (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 08Х22Н6Т, move to a sister rather than stretching the alias: GOST 9941 08Х18Н10Т, GOST 9941 10Х17Н13М2Т, GOST 9941 08Х20Н14С2. Apps context: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Full list under GOST 9941. Dual marking is a purchase-order option that still requires every limit that matters for 08Х22Н6Т to be verified on the heat.

08Х22Н6Т sourcing notes should keep forms separate: start from Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; add a plate product link later once the slug returns 200. Do not stretch a 08Х22Н6Т pipe certificate onto plate.

Heat Treatment and Delivery Condition for GOST 9941 08Х22Н6Т

Unlike GOST 9940, GOST 9941 forces heat treatment on every pipe by default. Confirm for 08Х22Н6Т. Band note: Phase-balance-aware anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech. Recorded furnace charts for 08Х22Н6Т should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Keep the 08Х22Н6Т caution visible here: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice.

Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 08Х22Н6Т. Field heat treatment of 08Х22Н6Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 08Х22Н6Т caution visible here: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice.

Corrosion Resistance of GOST 9941 08Х22Н6Т

Medium, temperature, crevice geometry and weld condition decide whether 08Х22Н6Т is enough. Summary: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr. Escalate via sisters 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2 when coupons fail. Coupon orientation, weld condition, and surface finish for 08Х22Н6Т belong in the corrosion test order so results can be compared to the installed spool honestly. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 08Х22Н6Т. Corrosion framing: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х22Н6Т rather than relying on wall thickness alone. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Applications of GOST 9941 08Х22Н6Т Seamless Pipe

From utility rooms to process racks, 08Х22Н6Т shows up wherever CIS fluid specs want austenitic-ferritic (duplex-lean) Ti-stabilised cold-/warm-deformed seamless behaviour. Use list: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Spool fabricators should copy 08Х22Н6Т onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

If the only reason for 08Х22Н6Т is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice. Commissioning teams benefit when the as-built dossier repeats 08Х22Н6Т beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 08Х22Н6Т stays chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8.

Weldability of GOST 9941 08Х22Н6Т

Automatic mill welding is outside GOST 9941; manual and automatic field welds must still respect 08Х22Н6Т chemistry. Guidance: duplex WPS — control heat input and ferrite; Ti present on cast. Procedure qualification for 08Х22Н6Т should use the same product form and wall class as production, including the cold-/warm-deformed seamless finish that will ship. Keep the 08Х22Н6Т caution visible here: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice.

Ferrite control on high-Ni austenitics and hydrogen management on martensitic 08Х22Н6Т are procedure items, not afterthoughts. Guidance: duplex WPS — control heat input and ferrite; Ti present on cast. Consumable lot control and shielding-gas notes for 08Х22Н6Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 08Х22Н6Т caution visible here: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice.

Surface Finishes for GOST 9941 08Х22Н6Т

Surface supply for 08Х22Н6Т should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless pipe, so finish is part of performance, not only appearance. Application framing: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Ambiguous “bright pipe” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Annealed and pickled Standard pipe mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; inspect before polish on ferritic stock
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Do not polish over unresolved defects on 08Х22Н6Т; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GOST 9941 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (08Х22Н6Т).

Inspection and Testing for GOST 9941 08Х22Н6Т

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9941 for 08Х22Н6Т. Sampling plans for 08Х22Н6Т keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Dimensional inspection against Table 2 tolerances closes the lot. Role: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. Non-conforming 08Х22Н6Т lengths are segregated and retested or rejected under GOST 9941 rather than reworked into unmarked stock. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Packaging and Shipping for GOST 9941 08Х22Н6Т

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 08Х22Н6Т stays visible on outer tags. Bundle tickets for 08Х22Н6Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3.

Container loading plans should keep heavy walls from crushing thin-wall 08Х22Н6Т layers. Desiccant and wrap choices for 08Х22Н6Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 08Х22Н6Т. Claims handling for 08Х22Н6Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 08Х22Н6Т caution visible here: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats 08Х22Н6Т as a governed product grade, not a marketing synonym for lean duplex / 22Cr-6Ni Ti (approx). Role: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. SHH STEEL can produce and supply 08Х22Н6Т against the OD × wall, cold-/warm-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common 08Х22Н6Т enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Ask for a written acknowledgement that names 08Х22Н6Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х22Н6Т to that written scope.

Supply Capability

Capability framing for 08Х22Н6Т: GOST-spec seamless cold-/warm-deformed pipe, documented heats. Caution remains: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х22Н6Т when the mill schedule allows.

Item Capability
Standard GOST 9941-81 seamless cold- and warm-deformed corrosion-resistant steel pipes
Grade 08Х22Н6Т (GOST 5632 chemistry; alias lean duplex / 22Cr-6Ni Ti (approx))
Product form Seamless pipe only — cold-/warm-deformed (hot-deformed = GOST 9940)
Delivery condition heat-treated by default (clause 2.3); without HT only by purchaser request
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice Cold-/warm Table 1 OD×wall (smaller/thinner than 9940); mark note: cold/warm Table 1 practice
Precision Ordinary, high, or elevated (indices per marking examples)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 08Х22Н6Т change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. SHH STEEL can supply alternate walls and precision classes for 08Х22Н6Т once the design pressure and corrosion allowance are clear.

Repeat orders for 08Х22Н6Т go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. SHH STEEL can produce trial lengths of 08Х22Н6Т for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9941 08Х22Н6Т seamless stainless steel pipe used for?
GOST 9941 08Х22Н6Т is cold-/warm-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Role summary: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9941 08Х22Н6Т seamless only, or does it cover welded pipe?
Seamless only — and specifically cold- and warm-deformed. Hot-deformed pipe of related marks belongs under GOST 9940-81. SHH STEEL can produce and supply the cold-/warm-deformed seamless route for 08Х22Н6Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 08Х22Н6Т under GOST 9941?
By default yes. Clause 2.3 requires heat treatment; without HT only when the purchaser orders it (mech then by agreement). Guidance for this mark: Phase-balance-aware anneal mandatory by default under 9941; without HT only by purchaser request with agreed mech. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: heat-treated by default (clause 2.3); without HT only by purchaser request.
How does 08Х22Н6Т compare with sister grades 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2?
08Х22Н6Т is filed as austenitic-ferritic (duplex-lean) Ti-stabilised. Typical sisters on the same RFQ are 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Design caution: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 08Х22Н6Т?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 300 pieces.
Is lean duplex / 22Cr-6Ni Ti (approx) the same as ordering 08Х22Н6Т?
No. lean duplex / 22Cr-6Ni Ti (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9941 and Cyrillic 08Х22Н6Т so cast limits, cold-/warm-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9941 08Х22Н6Т?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х22Н6Т within Table 1 practice, respecting the mark’s diameter cap (cold/warm Table 1 practice). Size context: cold-/warm lean-duplex sizes under Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–12.5 m by wall band.
How should 08Х22Н6Т be welded on site?
Shop guidance: duplex WPS — control heat input and ferrite; Ti present on cast. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice
When should I choose a Mo-bearing or duplex grade instead of 08Х22Н6Т?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic-ferritic (duplex-lean) Ti-stabilised practice can defend for the temperature and stress state. Caution for this mark: not ASTM A790 S31803 — phase balance and PREN differ; confirm cold/warm size practice Sister pointers: 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9941 08Х22Н6Т with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9941 08Х22Н6Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9941 08Х22Н6Т differ from GOST 9940 of the same mark?
GOST 9941 is cold-/warm-deformed (smaller OD, thinner wall, HT mandatory by default); GOST 9940 is hot-deformed (larger OD/wall, HT optional) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х22Н6Т.

Conclusion

GOST 9941 08Х22Н6Т is cold-/warm-deformed seamless stainless steel pipe for CIS corrosion-resistant service — lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9941 Table 3. SHH STEEL can produce and supply it in the cold-/warm-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X