GB/T 706 Q355B I-Beam
What is GB/T 706 Q355B I-Beam?
GB/T 706 Q355B I-beam is a hot-rolled Chinese taper-flange I-section whose material grade is as-rolled Q355B under GB/T 1591 and whose shape, tolerances and theoretical mass are ordered to GB/T 706. Q stands for yield strength, 355 is the minimum upper yield strength in MPa for the thinnest tabulated thickness band, and B is the quality grade, which carries a longitudinal Charpy V-notch requirement of 34 J at +20 °C when impact testing applies.
This page covers the rolled taper-flange I-beam, not plate and not a parallel-flange H-section. The same grade in plate form is listed separately as GB/T 1591 Q355B steel plate. For plates, tensile specimens are taken transverse to the rolling direction and the elongation table differs. The plate page is not a substitute data sheet for I-beams, and neither is GB/T 11263 Q355B H-beam.
These bars are filed under steel beam profiles in the steel structural profiles category. They are Chinese taper-flange I-beams (the inner face of the flange is sloped). They are not European IPE or HE sections, American W or S shapes, or GB/T 11263 H-sections. A Q355B channel or angle to GB/T 706 is a different product: see GB/T 706 Q355B steel channel and GB/T 706 Q355B steel angle.
Q355B is a high-strength low-alloy structural steel for building frames, workshops and ordinary fabrication where a +20 °C impact quality is accepted. It is not Q355C or Q355D, not a TMCP or normalized Q355M/Q355N grade, not a weathering steel, and not a pressure-vessel material. GB/T 1591-2018 replaced the older Q345 designation with Q355; an enquiry that only says “Q345 I-beam” still has to name the current grade and quality letter.
Material, Dimensions and Tolerances for Q355B I-Beams
Three documents should appear, separately, on the purchase order and on the inspection certificate:
- the material standard and edition, GB/T 1591-2018 unless the order names another edition, the grade Q355B, and the delivery condition (this page is the as-rolled product);
- the dimensional standard and edition, GB/T 706, with the I-beam designation (the model number, or the h × b × d size);
- the inspection document type and any agreed options such as a relocated test specimen, a raised phosphorus or sulphur limit for sections, or a controlled-silicon CEV increment.
GB/T 706 is the shape, tolerance and mass standard. It is not the material certificate. Chemistry, carbon equivalent and mechanical properties come from GB/T 1591. Size tables on this page use GB/T 706-2016 as the numeric basis. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition named on the order governs.
These I-beams have a sloped inner flange face. Parallel-flange H-sections belong to GB/T 11263 and are a different product, even when both are supplied in as-rolled Q355B.
Q355B I-Beam Sizes: GB/T 706 Standard I-Beam Series
The table below is the complete GB/T 706-2016 Table A.1 standard I-beam series: 45 sizes, models 10 through 63c. A section may be designated by its model (16a, 20b, 63c) or by the dimensions h × b × d, for example 100×68×4.5 for model 10 and 630×180×17 for model 63c. Theoretical mass uses a density of 7.85 g/cm³. Root and flange-toe radii in Table A.1 are for roll-pass design; they are not delivery conditions and are omitted here.
Not every mill rolls every model in Q355B. The order should name the models actually required rather than assuming the whole series is a single production run.
Models 10 to 36c (27 sizes)
Swipe horizontally to view all dimensions.
Models 40a to 63c (18 sizes)
Swipe horizontally to view all dimensions.
Q355B Chemical Composition for I-Beams (GB/T 1591 Ladle Analysis)
The figures below are ladle-analysis maxima from GB/T 1591-2018 Table 1 for as-rolled Q355B. Product analysis, where required, follows the standard’s permitted deviations; those deviations are not retabulated here. Qualities C and D, and the N and M delivery conditions, have their own rules and are not this table.
For these I-beams GB/T 706 directs specimens taken under GB/T 2975 to the web, so the relevant thickness is ordinarily the web d, not the flange t and not the overall depth.
Q355B Carbon Equivalent for I-Beams
GB/T 1591-2018 Table 2 publishes the following ladle-analysis CEV maxima for as-rolled Q355 qualities B, C and D, using the formula C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15.
When the web is the test location, every Table A.1 web is 17 mm or thinner, so the first band (0.45%) is the one that applies to the standard series. The thicker bands are shown because a special section, a relocated specimen, or a non-standard thickness can leave that band. If silicon is held down for galvanizing, the standard allows a stated CEV increment when carbon or manganese is increased to meet the tensile requirements; that increment should appear on the certificate rather than being assumed.
Q355B I-Beam Mechanical Properties: Yield, Tensile and +20 °C Impact
Tables 7 and 8 of GB/T 1591-2018 give the following values for as-rolled Q355B, with longitudinal elongation for sections and bars. For these I-beams GB/T 706 directs specimens taken under GB/T 2975 to the web, so the relevant thickness is ordinarily the web d, not the flange t and not the overall depth. When the yield point is not clearly pronounced, Rp0.2 may replace ReH.
Of the 45 tabulated Table A.1 webs, model 50c has a web of 16.0 mm and remains in the first band (355 MPa, 22% elongation) when the web is the test location. Models 55c and 56c have webs of 16.5 mm, and model 63c has a web of 17.0 mm; those three sit in the second band (345 MPa, still 22% elongation). Flange thickness on the larger models can exceed 16 mm (it reaches 22 mm on model 63) and must not be used as the default thickness basis unless the order relocates the specimen. No Table A.1 web reaches the 40 mm, 63 mm or 100 mm steps, where yield, elongation and tensile range change again.
When impact testing applies, Q355B requires 34 J longitudinally (27 J transversely, by agreement) at +20 °C. Steels with nominal thickness of 6 mm or more, or nominal diameter of 12 mm or more, shall be impact tested. Four tabulated webs — models 10, 12, 12.6 and 14 — are thinner than 6 mm and sit outside that obligation as written; the other forty-one tabulated webs are inside it. If a standard 10 × 10 × 55 mm specimen cannot be prepared, a larger permitted subsize is preferred, with the Table 11 value reduced to 75% or 50% according to the subsize. The inspection waiver written for Q235B under 25 mm is a GB/T 700 rule and is not applied here.
Delivery Conditions, Inspection and Identification
This page is the as-rolled Q355B product. GB/T 1591 also allows normalized, normalizing-rolled or TMCP delivery; those conditions have their own chemistry and CEV tables and must be named if they are required. The inspection document should identify GB/T 1591 and its edition, the grade Q355B, the delivery condition, the GB/T 706 designation and edition, ladle analysis and CEV, and mechanical results against the thickness at the test location, ordinarily the web. Packaging, marks and certificates follow GB/T 2101 for these sections.
A plate certificate or an H-beam certificate does not, by itself, identify a taper-flange I-beam. Heat identity, model and the two standards should be traceable from the bar marks to the document.
Weldability and Surface Condition of Q355B I-Beams
Q355B is a weldable high-strength low-alloy structural steel. Preheat and consumable choice should use the certified CEV, the actual thickness and the joint design, not a single assumed carbon equivalent. Taper-flange fillets and the web-to-flange junction need the usual care on fit-up and heat input.
Surface quality, depth of imperfections and repair practice belong to the ordered edition of GB/T 706. This page does not reproduce those millimetre limits.
GB/T 706 Shape Tolerances and Theoretical Mass
Shape, straightness, length and theoretical mass belong to the ordered edition of GB/T 706. Mass in the size table is calculated at 7.85 g/cm³ from the published section area. Permitted mass deviation and the millimetre tolerance tables are not reproduced here; they should be read from the edition named on the order.
GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. Until an order names that edition, the 2016 numeric table on this page is the reference used for the listed models.
Applications and Service Limits
Q355B I-beams are used in building frames, workshops, platforms and ordinary welded or bolted fabrication where a 355 MPa yield class in the first thickness band and a +20 °C impact quality are accepted. They are not specified here for pressure equipment, nuclear safety, or service that needs a 0 °C (Q355C) or −20 °C (Q355D) quality. Those qualities are not this product.
A taper-flange I-beam is not a drop-in substitute for a GB/T 11263 H-section of similar depth, nor for an IPE or W shape of similar mass. Connection design, stability checks and rolling-programme availability all have to be reviewed against the actual designation.
Q355B I-Beam Compared with Q235B, S355JR and A572 Grade 50
Buyers often compare this product with a lower-strength Chinese I-beam, with the same grade as an H-section, with the former Q345B name, or with European and American 345–355 MPa steels. The comparisons below are an orientation only; they are not automatic substitutes.
Near-Equivalents: Not Automatic Substitutes
A near-equivalent is a starting point for a discussion, not a licence to swap certificates. EN 10025-2 S355JR steel plate and EN 10025-2 S355JR H-beam use different chemistry, CEV and impact rules, and an IPE or HE section is not a GB/T 706 I-beam. ASTM A572 Grade 50 plate is a plate product with its own thickness limits. GB/T 11263 Q235B H-beam is both a different grade and a different shape system.
If a project specification names one of those grades, the order should keep that name, the matching dimensional standard, and the required impact temperature, rather than treating Q355B I-beam as a silent replacement.
Sourcing Q355B I-Beams from SHH STEEL
SHH STEEL supplies GB/T 706 Q355B I-beams against a named model list, the material edition, the delivery condition and the inspection document type. Enquiries should state the designations (for example 16a, 20b or 200 × 102 × 9), cut lengths or mill lengths, any processing, and whether the sister grade GB/T 706 Q235B I-beam is an acceptable alternative on part of the list.
The size table is the standard series, not a claim that every model is rolled in every heat. Once the list is clear, a quotation can be prepared against the stated edition and certificate.
Q355B I-Beam FAQs
-
Is Q355B the same as the older Q345B I-beam?
- GB/T 1591-2018 replaced the Q345 designation with Q355. Appendix A maps as-rolled Q355B to the former Q345B name, but the current grade to order is Q355B, with the 2018 (or otherwise ordered) edition, the quality letter and the GB/T 706 designation all stated on the certificate.
-
Which thickness is used for yield, CEV and impact?
- For I-beams, specimens are taken from the web, so the governing thickness is ordinarily the web d. Model 50c stays in the first yield and CEV bands; models 55c, 56c and 63c move into the second yield band when the web is the test location, but they remain in the first CEV band. Impact testing, when it applies, is written for thickness of 6 mm or more; models 10, 12, 12.6 and 14 sit outside that obligation as written.
-
Does the size table use the 2016 or the 2026 edition of GB/T 706?
- The numeric table uses GB/T 706-2016. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition named on the order governs; this page does not substitute unverified 2026 dimensions.
-
Which standards should appear on the inspection document?
- At least GB/T 1591 and its edition, the grade Q355B, the delivery condition (as-rolled unless otherwise agreed), the GB/T 706 designation and edition, ladle analysis and CEV, and mechanical results against the thickness at the test location, ordinarily the web. Packaging, marks and certificates follow GB/T 2101. A plate or H-beam certificate does not, by itself, identify an I-beam.
Request a Quotation for GB/T 706 Q355B I-Beam
GB/T 706 Q355B I-beam is a taper-flange Chinese I-section in as-rolled Q355B, with 355 MPa minimum yield in the first thickness band and a 34 J longitudinal impact requirement at +20 °C when testing applies. Nominate the GB/T 706 designation (for example 16a, 20b or 200 × 102 × 9) and the material to GB/T 1591-2018 (or the edition on the order). The size table uses GB/T 706-2016 as the numeric basis; GB/T 706-2026 is the successor edition, with implementation from 1 December 2026; the ordered edition governs. Send the size list, edition, delivery condition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.