GB/T 706 Q235B I-Beam

GB/T 706 Q235B I-beam is a Chinese taper-flange I-section with 235 MPa minimum yield in the first thickness band and a 27 J longitudinal impact requirement at +20 °C when testing applies. This page lists the complete GB/T 706-2016 Table A.1 series, chemistry and mechanicals, and how the web thickness governs the test location.
Keywords
GB/T 706 Q235B I-Beam, Q235B I-beam, GB/T 706 I-beam, Q235B taper-flange I-beam, Chinese I-beam
Equivalent Grades:
Q355B I-beam (GB/T 1591, same Table A.1 shape); Q235B H-beam (GB/T 11263); S235JR; SS400; ASTM A36 — comparisons only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of Q235B I-Beam
Chemical Composition of Q235B I-Beam
Mechanical Properties of Q235B I-Beam
Delivery Conditions, Inspection and Identification
Weldability and Surface Condition of Q235B I-Beams
Shape Tolerances and Theoretical Mass
Applications and Service Limits
Q235B I-Beam Compared with Q355B, S235JR and A36
Near-Equivalents: Not Automatic Substitutes
Sourcing Q235B I-Beams from SHH STEEL
FAQ
Conclusion

What is GB/T 706 Q235B I-Beam?

GB/T 706 Q235B I-beam is a hot-rolled Chinese taper-flange I-section whose material grade is Q235B under GB/T 700 and whose shape, tolerances and theoretical mass are ordered to GB/T 706. Q stands for yield strength, 235 is the minimum upper yield strength in MPa for the thinnest tabulated thickness band, and B is the quality grade, which carries a longitudinal Charpy V-notch requirement of 27 J at +20 °C when impact testing applies.

This page covers the rolled taper-flange I-beam, not plate and not a parallel-flange H-section. The same grade in plate form is listed separately as GB/T 700 Q235B steel plate. For plates, tensile specimens are taken transverse to the rolling direction and elongation may be two percentage points lower than the Table 2 values used for sections and bars. The plate page is not a substitute data sheet for I-beams, and neither is GB/T 11263 Q235B H-beam.

These bars are filed under steel beam profiles in the steel structural profiles category. They are Chinese taper-flange I-beams (the inner face of the flange is sloped). They are not European IPE or HE sections, American W or S shapes, Japanese I-beams of a similar millimetre depth, or GB/T 11263 H-sections. A Q235B channel or angle to GB/T 706 is a different product: see GB/T 706 Q235B steel channel and GB/T 706 Q235B steel angle.

Q235B is a general carbon structural steel for building frames, workshops and ordinary fabrication where a +20 °C impact quality is accepted. It is not a 355 MPa grade, not a weathering steel, and not a pressure-vessel or nuclear safety material. If an enquiry only says “Q235 I-beam” or “I16,” the quality letter and the dimensional standard still have to be named.

Material, Dimensions and Tolerances for Q235B I-Beams

Three documents should appear, separately, on the purchase order and on the inspection certificate:

  • the material standard and edition, GB/T 700-2006 unless the order names another edition, and the grade Q235B;
  • the dimensional standard and edition, GB/T 706, with the I-beam designation (the model number, or the h × b × d size);
  • the delivery condition, inspection document type, and any agreed options such as a relocated test specimen or a raised carbon limit.

GB/T 706 is the shape, tolerance and mass standard. It is not the material certificate. Chemistry and mechanical properties come from GB/T 700. Size tables on this page use GB/T 706-2016 as the numeric basis. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition named on the order governs.

These I-beams have a sloped inner flange face. Parallel-flange H-sections belong to GB/T 11263 and are a different product, even when both are supplied in Q235B.

Q235B I-Beam Sizes: GB/T 706 Standard I-Beam Series

The table below is the complete GB/T 706-2016 Table A.1 standard I-beam series: 45 sizes, models 10 through 63c. A section may be designated by its model (16a, 20b, 63c) or by the dimensions h × b × d, for example 100×68×4.5 for model 10 and 630×180×17 for model 63c. Theoretical mass uses a density of 7.85 g/cm³. Root and flange-toe radii in Table A.1 are for roll-pass design; they are not delivery conditions and are omitted here.

Not every mill rolls every model in Q235B. The order should name the models actually required rather than assuming the whole series is a single production run.

Models 10 to 36c (27 sizes)

Swipe horizontally to view all dimensions.

Model Designation (h×b×d) h (mm) b (mm) d (mm) t (mm) A (cm²) Mass (kg/m)
10 100×68×4.5 100 68.0 4.5 7.6 14.33 11.3
12 120×74×5 120 74.0 5.0 8.4 17.8 14.0
12.6 126×74×5 126 74.0 5.0 8.4 18.1 14.2
14 140×80×5.5 140 80.0 5.5 9.1 21.5 16.9
16 160×88×6 160 88.0 6.0 9.9 26.11 20.5
18 180×94×6.5 180 94.0 6.5 10.7 30.74 24.1
20a 200×100×7 200 100.0 7.0 11.4 35.55 27.9
20b 200×102×9 200 102.0 9.0 11.4 39.55 31.1
22a 220×110×7.5 220 110.0 7.5 12.3 42.1 33.1
22b 220×112×9.5 220 112.0 9.5 12.3 46.5 36.5
24a 240×116×8 240 116.0 8.0 13.0 47.71 37.5
24b 240×118×10 240 118.0 10.0 13.0 52.51 41.2
25a 250×116×8 250 116.0 8.0 13.0 48.51 38.1
25b 250×118×10 250 118.0 10.0 13.0 53.51 42.0
27a 270×122×8.5 270 122.0 8.5 13.7 54.52 42.8
27b 270×124×10.5 270 124.0 10.5 13.7 59.92 47.0
28a 280×122×8.5 280 122.0 8.5 13.7 55.37 43.5
28b 280×124×10.5 280 124.0 10.5 13.7 60.97 47.9
30a 300×126×9 300 126.0 9.0 14.4 61.22 48.1
30b 300×128×11 300 128.0 11.0 14.4 67.22 52.8
30c 300×130×13 300 130.0 13.0 14.4 73.22 57.5
32a 320×130×9.5 320 130.0 9.5 15.0 67.12 52.7
32b 320×132×11.5 320 132.0 11.5 15.0 73.52 57.7
32c 320×134×13.5 320 134.0 13.5 15.0 79.92 62.7
36a 360×136×10 360 136.0 10.0 15.8 76.44 60.0
36b 360×138×12 360 138.0 12.0 15.8 83.64 65.7
36c 360×140×14 360 140.0 14.0 15.8 90.84 71.3

Models 40a to 63c (18 sizes)

Swipe horizontally to view all dimensions.

Model Designation (h×b×d) h (mm) b (mm) d (mm) t (mm) A (cm²) Mass (kg/m)
40a 400×142×10.5 400 142.0 10.5 16.5 86.07 67.6
40b 400×144×12.5 400 144.0 12.5 16.5 94.07 73.8
40c 400×146×14.5 400 146.0 14.5 16.5 102.1 80.1
45a 450×150×11.5 450 150.0 11.5 18.0 102.4 80.4
45b 450×152×13.5 450 152.0 13.5 18.0 111.4 87.4
45c 450×154×15.5 450 154.0 15.5 18.0 120.4 94.5
50a 500×158×12 500 158.0 12.0 20.0 119.2 93.6
50b 500×160×14 500 160.0 14.0 20.0 129.2 101.0
50c 500×162×16 500 162.0 16.0 20.0 139.2 109.0
55a 550×166×12.5 550 166.0 12.5 21.0 134.1 105.0
55b 550×168×14.5 550 168.0 14.5 21.0 145.1 114.0
55c 550×170×16.5 550 170.0 16.5 21.0 156.1 123.0
56a 560×166×12.5 560 166.0 12.5 21.0 135.4 106.0
56b 560×168×14.5 560 168.0 14.5 21.0 146.6 115.0
56c 560×170×16.5 560 170.0 16.5 21.0 157.8 124.0
63a 630×176×13 630 176.0 13.0 22.0 154.6 121.0
63b 630×178×15 630 178.0 15.0 22.0 167.2 131.0
63c 630×180×17 630 180.0 17.0 22.0 179.8 141.0

Q235B Chemical Composition for I-Beams (GB/T 700 Ladle Analysis)

The figures below are ladle-analysis maxima from GB/T 700-2006 for Q235B. Product analysis, where required, follows the standard’s permitted deviations; those deviations are not retabulated here. There is no published carbon-equivalent cap for Q235B.

Element Maximum, ladle analysis (mass %) Notes for Q235B I-beams
C 0.20 May be raised to 0.22% only with the purchaser’s agreement. The 2006 edition sets no carbon minimum.
Si 0.35 —
Mn 1.40 Maximum only. The 1988 range 0.30–0.70% was withdrawn; do not treat that older range as the current default.
P 0.045 —
S 0.045 —
Cr, Ni, Cu (each, residual) 0.30 Need not be analysed if the supplier guarantees the limit.
N 0.008 May be higher under the standard’s nitrogen/phosphorus and nitrogen-binding rules; those cases belong on the certificate.
As 0.080 General maximum; arsenic-bearing ore routes are a matter for agreement.

For these I-beams the tensile and bend specimens are taken from the web, so the relevant thickness is ordinarily the web d, not the flange t and not the overall depth. The same chemistry applies to Q235B plate, but the plate page is not this data sheet.

Q235B I-Beam Mechanical Properties: Yield, Tensile and +20 °C Impact

Table 2 of GB/T 700-2006 gives the following values for sections and bars, with tensile and bend specimens taken longitudinally. For these I-beams the tensile and bend specimens are taken from the web, so the relevant thickness is ordinarily the web d, not the flange t and not the overall depth.

Nominal thickness or diameter t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 235 370–500 26
16 < t ≤ 40 225 370–500 26
40 < t ≤ 60 215 370–500 25
60 < t ≤ 100 215 370–500 24
100 < t ≤ 150 195 370–500 22
150 < t ≤ 200 185 370–500 21

Of the 45 tabulated Table A.1 webs, model 50c has a web of 16.0 mm and remains in the first band (235 MPa, 26% elongation) when the web is the test location. Models 55c and 56c have webs of 16.5 mm, and model 63c has a web of 17.0 mm; those three sit in the second band (225 MPa, 26% elongation). Flange thickness on the larger models can exceed 16 mm (it reaches 22 mm on model 63) and must not be used as the default thickness basis unless the order relocates the specimen.

Later thickness bands are shown because a special section or a relocated specimen can take the test location out of the first two bands. For t > 100 mm the standard allows the lower tensile limit to be reduced by 20 N/mm²; no Table A.1 web reaches that thickness.

When impact testing applies, Q235B requires a longitudinal Charpy V-notch result of 27 J at +20 °C. The obligation is written for thickness of 12 mm or more (or diameter of 16 mm or more). Twenty of the tabulated webs meet or exceed 12 mm; the other twenty-five, including the lighter a-series models, are thinner than 12 mm and sit outside that obligation as written. For Q235B thinner than 25 mm the test may be omitted if the supplier guarantees conformity and the purchaser agrees — a waiver of inspection, not a deletion of the requirement. All tabulated webs are 17 mm or thinner, so that option can still be discussed for this series.

Delivery Conditions, Inspection and Identification

Q235B I-beams are commonly delivered as-rolled. The inspection document should identify GB/T 700 and its edition, the grade Q235B, the GB/T 706 designation and edition, the delivery condition, ladle analysis, and mechanical results against the thickness at the test location, ordinarily the web. Packaging, marks and certificates follow GB/T 2101 in the ordered edition.

A plate certificate or an H-beam certificate does not, by itself, identify a taper-flange I-beam. Heat identity, model and the two standards should be traceable from the bar marks to the document.

Weldability and Surface Condition of Q235B I-Beams

Q235B is a weldable carbon structural steel. It has no published CEV cap, so preheat and consumable choice should be based on the actual ladle analysis, thickness and joint design rather than on a single assumed carbon equivalent. Taper-flange fillets and the web-to-flange junction need the usual care on fit-up and heat input; they are not a reason to treat the grade as a non-weldable steel.

Surface quality, depth of imperfections and repair practice belong to the ordered edition of GB/T 706. This page does not reproduce those millimetre limits.

GB/T 706 Shape Tolerances and Theoretical Mass

Shape, straightness, length and theoretical mass belong to the ordered edition of GB/T 706. Mass in the size table is calculated at 7.85 g/cm³ from the published section area. Permitted mass deviation and the millimetre tolerance tables are not reproduced here; they should be read from the edition named on the order.

GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. Until an order names that edition, the 2016 numeric table on this page is the reference used for the listed models.

Applications and Service Limits

Q235B I-beams are used in building frames, workshops, platforms and ordinary welded or bolted fabrication where a +20 °C impact quality is accepted and a 235 MPa yield class in the first thickness band is sufficient. They are not specified here for pressure equipment, nuclear safety, low-temperature service that needs a 0 °C or sub-zero quality, or weathering exposure that needs a dedicated atmospheric-corrosion grade.

A taper-flange I-beam is not a drop-in substitute for a GB/T 11263 H-section of similar depth, nor for an IPE or W shape of similar mass. Connection design, stability checks and rolling-programme availability all have to be reviewed against the actual designation.

Q235B I-Beam Compared with Q355B, S235JR and A36

Buyers often compare this product with a higher-strength Chinese I-beam, with the same grade as an H-section, or with European and American 235–250 MPa carbon steels. The comparisons below are an orientation only; they are not automatic substitutes.

Grade / designation Standard Relationship to Q235B I-beam Caution
Q355B I-beam GB/T 1591; a GB/T 706 I-beam may be certified to Q355B when that is the order A higher-strength Chinese comparison at the 355 MPa yield class, on the same Table A.1 shape family. Q355B is not Q235B. Chemistry, CEV practice and impact quality follow GB/T 1591, not GB/T 700. See GB/T 706 Q355B I-beam.
Q235B H-beam GB/T 700 with dimensions GB/T 11263 The same material grade in a parallel-flange H-section. A GB/T 11263 HW, HM or HN designation is not a Table A.1 I-beam. See GB/T 11263 Q235B H-beam.
S235JR EN 10025-2; dimensions EN 10365 / tolerances EN 10034 for I and H sections A 235 MPa European general-structure comparison, usually as IPE, HEA or HEB when the product is a beam. S235JR has its own carbon, manganese and CEV table and a +20 °C impact test on a different thickness basis. An IPE 200 is not a Chinese 20a.
SS400 JIS G 3101; dimensions JIS G 3192 A Japanese general-structure comparison named for a 400–510 N/mm² tensile range, not a 400 N/mm² yield. SS400 does not publish carbon or manganese maxima and has no Charpy test. The JIS G 3192 designation is not a GB/T 706 model number.
A36 ASTM A36/A36M; dimensions ASTM A6/A6M A common American carbon-steel comparison used in export enquiries. A36 has its own chemistry, yield and tensile table, including footnote B rules that apply to certain W shapes, not to these Chinese I-beams. A W or S designation is not a GB/T 706 20a.

Near-Equivalents: Not Automatic Substitutes

A near-equivalent is a starting point for a discussion, not a licence to swap certificates. EN 10025-2 S235JR steel plate and JIS G 3101 SS400 steel plate use different chemistry and impact rules, and a plate is not an I-beam. ASTM A36 wide-flange beam is an American W shape to ASTM A6, not a GB/T 706 model. GB/T 11263 Q355B H-beam is both a different grade and a different shape system.

If a project specification names one of those grades, the order should keep that name, the matching dimensional standard, and the required impact temperature, rather than treating Q235B I-beam as a silent replacement.

Sourcing Q235B I-Beams from SHH STEEL

SHH STEEL supplies GB/T 706 Q235B I-beams against a named model list, the material edition and the inspection document type. Enquiries should state the designations (for example 16a, 20b or 200 × 102 × 9), cut lengths or mill lengths, any processing, and whether the sister grade GB/T 706 Q355B I-beam is an acceptable alternative on part of the list.

The size table is the standard series, not a claim that every model is rolled in every heat. Once the list is clear, a quotation can be prepared against the stated edition and certificate.

Q235B I-Beam FAQs

Is a GB/T 706 Q235B I-beam the same as a Q235B H-beam?
No. Both may be certified Q235B to GB/T 700, but the I-beam is a taper-flange section to GB/T 706 Table A.1 and the H-beam is a parallel-flange section to GB/T 11263. Designations, tolerances, connection details and rolling programmes are not interchangeable.
Which thickness is used for the yield and impact requirements?
For I-beams, tensile and bend specimens are taken from the web, so the governing thickness is ordinarily the web d. Model 50c stays in the first yield band; models 55c, 56c and 63c move into the second band when the web is the test location. Impact testing, when it applies, is written for thickness of 12 mm or more.
Does the size table use the 2016 or the 2026 edition of GB/T 706?
The numeric table uses GB/T 706-2016. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition named on the order governs; this page does not substitute unverified 2026 dimensions.
Which standards should appear on the inspection document?
At least GB/T 700 and its edition, the grade Q235B, the GB/T 706 designation and the edition used for dimensions and mass, the delivery condition, ladle analysis, and mechanical results against the thickness at the test location, ordinarily the web. Packaging, marks and certificates follow GB/T 2101. A plate or H-beam certificate does not, by itself, identify an I-beam.

Request a Quotation for GB/T 706 Q235B I-Beam

GB/T 706 Q235B I-beam is a taper-flange Chinese I-section with 235 MPa minimum yield in the first thickness band and a 27 J impact requirement at +20 °C when testing applies. Nominate the GB/T 706 designation (for example 16a, 20b or 200 × 102 × 9) and the material to GB/T 700-2006 (or the edition on the order). The size table uses GB/T 706-2016 as the numeric basis; GB/T 706-2026 is the successor edition, with implementation from 1 December 2026; the ordered edition governs. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X