GB/T 706 Q355B Equal and Unequal Steel Angles | GB/T 706 Steel Angles - SHH STEEL

GB/T 706 Q355B Equal and Unequal Steel Angles

GB/T 706 Q355B steel angle is a Chinese L-section in as-rolled low-alloy steel Q355B (GB/T 1591-2018), with 355 MPa minimum yield up to 16 mm and 34 J longitudinal impact at +20 °C. Sizes use GB/T 706-2016 as the numeric basis. The ordered edition governs. SHH STEEL reviews grade, condition, designation and certificate requirements before quoting.
Keywords
GB/T 706 Q355B Steel Angle, Q355B equal angle, Q355B unequal angle, as-rolled Q355B angle, GB/T 706 angle
Equivalent Grades:
Near-equivalents only, not automatic substitutes: former Q345B; Q355C/D; S355JR; ASTM A572 Grade 50.
Share:
General Description
Material Specification
Available Sizes of GB/T 706 Q355B Equal Leg Steel Angles
Available Sizes of GB/T 706 Q355B Unequal Leg Steel Angles
Chemical Composition
Carbon Equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source Q355B Steel Angles from SHH STEEL
FAQ
Conclusion

What is GB/T 706 Q355B Steel Angle?

GB/T 706 Q355B steel angle is a hot-rolled Chinese L-section whose material grade is as-rolled Q355B under GB/T 1591 and whose shape, tolerances and theoretical mass are ordered to GB/T 706. Q stands for yield strength, 355 is the minimum upper yield strength in MPa for the thinnest tabulated thickness band, and B is the quality grade. For quality B the Charpy V-notch requirement is 34 J on a longitudinal specimen, or 27 J on a transverse specimen, at +20 °C. Longitudinal specimens are the default; transverse testing is by agreement.

This page covers the rolled angle, not plate, not a channel and not an H-section. The same grade in plate form is listed separately as Q355B steel plate (GB/T 1591). Sampling direction, elongation and some thickness-band footnotes differ between plates and sections, so the plate page is not a substitute data sheet for angles, and neither is GB/T 11263 Q355B H-beam. GB/T 1591 itself refers the dimensions, shape, mass and tolerances of hot-rolled section steel to GB/T 706.

These bars are filed under steel angle profiles in the steel structural profiles category. They are Chinese equal-leg and unequal-leg angles. They are not European EN 10056 L-sections, American L-shapes, or Japanese angles of a similar millimetre leg, and they are not channels, I-beams or GB/T 11263 H-sections. A Q355B channel to GB/T 706 is a different product, with its own designation and its own page when that page is published.

Q355B is the current as-rolled 355 MPa quality-B grade in GB/T 1591-2018, which replaced the former Q345 designation. It is a high-strength low-alloy structural steel for building frames, plant structures and general fabrication where a +20 °C impact quality is accepted. It is not Q355N or Q355M, not a weathering grade, and not a pressure-vessel or nuclear safety material. An enquiry that still says only “Q345B angle” should be confirmed against the 2018 designation, the as-rolled condition and the dimensional standard before rolling.

This page covers Equal and Unequal Steel Angles whose grade is Q355B (GB/T 1591) and whose sizes follow GB/T 706. The Equal Leg Steel Angles and Unequal Leg Steel Angles are Table A.3 and Table A.4 series; the material standard does not by itself define the dimensions.

Material, Dimensions and Tolerances for Q355B Angles

Three documents should appear, separately, on the purchase order and on the inspection certificate:

  • GB/T 1591 is the material standard for high-strength low-alloy structural steels. This article uses the as-rolled Q355B chemistry, carbon equivalent, tensile and impact values published in GB/T 1591-2018. Normalized (N) and thermomechanical (M) Q355 grades have their own tables and are a different order. The edition named on the order governs acceptance.
  • GB/T 706 is the product standard for hot-rolled section steel, including these equal-leg and unequal-leg angles. It sets the size series, dimensional and shape tolerances, theoretical mass and section surface rules, and it points chemistry and mechanical properties to GB/T 700 or GB/T 1591. It is not itself the material certificate. The size tables below are the complete standard series in GB/T 706-2016 Table A.3 (equal-leg) and Table A.4 (unequal-leg). GB/T 706-2016 is used as the numeric basis. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition of GB/T 706 named on the order governs dimensional acceptance.
  • Tolerances on leg length, thickness, out-of-square, length, straightness and mass are those of the ordered GB/T 706 edition, not of GB/T 1591 and not of GB/T 11263.

A mill may certify Q355B on a European or Japanese angle, or roll a Chinese angle to a different material standard, if that combination is in its programme and is fully documented. Matching a nominal 50 mm or 2 in leg is not a substitution.

GB/T 706 Q355B Equal Leg Steel Angles

The tables list the complete standard angle series in GB/T 706-2016: Table A.3 equal-leg angles, 115 sizes from 20×20×3 to 250×250×35, and Table A.4 unequal-leg angles, 71 sizes from 25×16×3 to 200×125×18. The usual designation is the leg and thickness string, written ∠b×b×d for equal legs (for example ∠200×200×24, often abbreviated ∠200×24) and ∠B×b×d for unequal legs (for example ∠160×100×16). Theoretical mass uses a density of 7.85 g/cm³. The root radii in GB/T 706 are for roll-pass design and are not delivery conditions, so they are not listed in the size tables. Use the tables to identify and estimate, not as a rolling programme for Q355B. Mid-range equal legs such as 50×50×5 and 75×75×8 are the usual enquiry core; the 20×20 families, the 200×200 and 250×250 rows, and the larger unequal legs should be confirmed size by size.

GB/T 706-2016 is used as the numeric basis. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition of GB/T 706 named on the order governs dimensional acceptance. This page does not invent rows that Tables A.3 and A.4 do not list, and it does not treat a Chinese 50×50×5 as interchangeable with a European, American or Japanese 50 mm equal angle.

The governing thickness is ordinarily the leg thickness d, not the leg length. Several of the larger tabulated equal-leg angles, and 200×125×18 among the unequal-leg rows, have a leg thickness over 16 mm and therefore fall into the 345 MPa band. The two thickest equal-leg rows, 250×250×32 and 250×250×35, also sit above 30 mm, so the tighter 0.22% carbon footnote and the 0.47% CEV band apply when the leg is the test location.

Equal-leg angles — Table A.3, Models 2 to 6.3 equal (36 sizes)

Swipe horizontally to view all dimensions.

Model Designation (b×b×d) b (mm) d (mm) A (cm²) Mass (kg/m)
2 20×20×3 20 3 1.132 0.89
2 20×20×4 20 4 1.459 1.15
2.5 25×25×3 25 3 1.432 1.12
2.5 25×25×4 25 4 1.859 1.46
3 30×30×3 30 3 1.749 1.37
3 30×30×4 30 4 2.276 1.79
3.6 36×36×3 36 3 2.109 1.66
3.6 36×36×4 36 4 2.756 2.16
3.6 36×36×5 36 5 3.382 2.65
4 40×40×3 40 3 2.359 1.85
4 40×40×4 40 4 3.086 2.42
4 40×40×5 40 5 3.792 2.98
4.5 45×45×3 45 3 2.659 2.09
4.5 45×45×4 45 4 3.486 2.74
4.5 45×45×5 45 5 4.292 3.37
4.5 45×45×6 45 6 5.077 3.99
5 50×50×3 50 3 2.971 2.33
5 50×50×4 50 4 3.897 3.06
5 50×50×5 50 5 4.803 3.77
5 50×50×6 50 6 5.688 4.46
5.6 56×56×3 56 3 3.343 2.62
5.6 56×56×4 56 4 4.39 3.45
5.6 56×56×5 56 5 5.415 4.25
5.6 56×56×6 56 6 6.42 5.04
5.6 56×56×7 56 7 7.404 5.81
5.6 56×56×8 56 8 8.367 6.57
6 60×60×5 60 5 5.829 4.58
6 60×60×6 60 6 6.914 5.43
6 60×60×7 60 7 7.977 6.26
6 60×60×8 60 8 9.02 7.08
6.3 63×63×4 63 4 4.978 3.91
6.3 63×63×5 63 5 6.143 4.82
6.3 63×63×6 63 6 7.288 5.72
6.3 63×63×7 63 7 8.412 6.60
6.3 63×63×8 63 8 9.515 7.47
6.3 63×63×10 63 10 11.66 9.15

Equal-leg angles — Table A.3, Models 7 to 12.5 equal (41 sizes)

Swipe horizontally to view all dimensions.

Model Designation (b×b×d) b (mm) d (mm) A (cm²) Mass (kg/m)
7 70×70×4 70 4 5.570 4.37
7 70×70×5 70 5 6.876 5.40
7 70×70×6 70 6 8.160 6.41
7 70×70×7 70 7 9.424 7.40
7 70×70×8 70 8 10.67 8.37
7.5 75×75×5 75 5 7.412 5.82
7.5 75×75×6 75 6 8.797 6.91
7.5 75×75×7 75 7 10.16 7.98
7.5 75×75×8 75 8 11.50 9.03
7.5 75×75×9 75 9 12.83 10.1
7.5 75×75×10 75 10 14.13 11.1
8 80×80×5 80 5 7.912 6.21
8 80×80×6 80 6 9.397 7.38
8 80×80×7 80 7 10.86 8.53
8 80×80×8 80 8 12.30 9.66
8 80×80×9 80 9 13.73 10.8
8 80×80×10 80 10 15.13 11.9
9 90×90×6 90 6 10.64 8.35
9 90×90×7 90 7 12.30 9.66
9 90×90×8 90 8 13.94 10.9
9 90×90×9 90 9 15.57 12.2
9 90×90×10 90 10 17.17 13.5
9 90×90×12 90 12 20.31 15.9
10 100×100×6 100 6 11.93 9.37
10 100×100×7 100 7 13.80 10.8
10 100×100×8 100 8 15.64 12.3
10 100×100×9 100 9 17.46 13.7
10 100×100×10 100 10 19.26 15.1
10 100×100×12 100 12 22.80 17.9
10 100×100×14 100 14 26.26 20.6
10 100×100×16 100 16 29.63 23.3
11 110×110×7 110 7 15.20 11.9
11 110×110×8 110 8 17.24 13.5
11 110×110×10 110 10 21.26 16.7
11 110×110×12 110 12 25.20 19.8
11 110×110×14 110 14 29.06 22.8
12.5 125×125×8 125 8 19.75 15.5
12.5 125×125×10 125 10 24.37 19.1
12.5 125×125×12 125 12 28.91 22.7
12.5 125×125×14 125 14 33.37 26.2
12.5 125×125×16 125 16 37.74 29.6

Equal-leg angles — Table A.3, Models 14 to 25 equal (38 sizes)

Swipe horizontally to view all dimensions.

Model Designation (b×b×d) b (mm) d (mm) A (cm²) Mass (kg/m)
14 140×140×10 140 10 27.37 21.5
14 140×140×12 140 12 32.51 25.5
14 140×140×14 140 14 37.57 29.5
14 140×140×16 140 16 42.54 33.4
15 150×150×8 150 8 23.75 18.6
15 150×150×10 150 10 29.37 23.1
15 150×150×12 150 12 34.91 27.4
15 150×150×14 150 14 40.37 31.7
15 150×150×15 150 15 43.06 33.8
15 150×150×16 150 16 45.74 35.9
16 160×160×10 160 10 31.50 24.7
16 160×160×12 160 12 37.44 29.4
16 160×160×14 160 14 43.30 34.0
16 160×160×16 160 16 49.07 38.5
18 180×180×12 180 12 42.24 33.2
18 180×180×14 180 14 48.90 38.4
18 180×180×16 180 16 55.47 43.5
18 180×180×18 180 18 61.96 48.6
20 200×200×14 200 14 54.64 42.9
20 200×200×16 200 16 62.01 48.7
20 200×200×18 200 18 69.30 54.4
20 200×200×20 200 20 76.51 60.1
20 200×200×24 200 24 90.66 71.2
22 220×220×16 220 16 68.67 53.9
22 220×220×18 220 18 76.75 60.3
22 220×220×20 220 20 84.76 66.5
22 220×220×22 220 22 92.68 72.8
22 220×220×24 220 24 100.5 78.9
22 220×220×26 220 26 108.3 85.0
25 250×250×18 250 18 87.84 69.0
25 250×250×20 250 20 97.05 76.2
25 250×250×22 250 22 106.2 83.3
25 250×250×24 250 24 115.2 90.4
25 250×250×26 250 26 124.2 97.5
25 250×250×28 250 28 133.0 104
25 250×250×30 250 30 141.8 111
25 250×250×32 250 32 150.5 118
25 250×250×35 250 35 163.4 128

GB/T 706 Q355B Unequal Leg Steel Angles

Unequal-leg angles — Table A.4, Models 2.5/1.6 to 10/8 unequal (41 sizes)

Swipe horizontally to view all dimensions.

Model Designation (B×b×d) B (mm) b (mm) d (mm) A (cm²) Mass (kg/m)
2.5/1.6 25×16×3 25 16 3 1.152 0.91
2.5/1.6 25×16×4 25 16 4 1.499 1.18
3.2/2 32×20×3 32 20 3 1.492 1.17
3.2/2 32×20×4 32 20 4 1.939 1.52
4/2.5 40×25×3 40 25 3 1.890 1.48
4/2.5 40×25×4 40 25 4 2.467 1.94
4.5/2.8 45×28×3 45 28 3 2.149 1.69
4.5/2.8 45×28×4 45 28 4 2.806 2.20
5/3.2 50×32×3 50 32 3 2.431 1.91
5/3.2 50×32×4 50 32 4 3.177 2.49
5.6/3.6 56×36×3 56 36 3 2.743 2.15
5.6/3.6 56×36×4 56 36 4 3.590 2.82
5.6/3.6 56×36×5 56 36 5 4.415 3.47
6.3/4 65×40×4 65 40 4 4.058 3.19
6.3/4 65×40×5 65 40 5 4.993 3.92
6.3/4 65×40×6 65 40 6 5.908 4.64
6.3/4 65×40×7 65 40 7 6.802 5.34
7/4.5 70×45×4 70 45 4 4.553 3.57
7/4.5 70×45×5 70 45 5 5.609 4.40
7/4.5 70×45×6 70 45 6 6.644 5.22
7/4.5 70×45×7 70 45 7 7.658 6.01
7.5/5 75×50×5 75 50 5 6.136 4.81
7.5/5 75×50×6 75 50 6 7.260 5.70
7.5/5 75×50×8 75 50 8 9.467 7.43
7.5/5 75×50×10 75 50 10 11.59 9.10
8/5 80×50×5 80 50 5 6.376 5.00
8/5 80×50×6 80 50 6 7.560 5.93
8/5 80×50×7 80 50 7 8.724 6.85
8/5 80×50×8 80 50 8 9.867 7.75
9/5.6 90×56×5 90 56 5 7.212 5.66
9/5.6 90×56×6 90 56 6 8.557 6.72
9/5.6 90×56×7 90 56 7 9.880 7.76
9/5.6 90×56×8 90 56 8 11.18 8.78
10/6.3 100×63×6 100 63 6 9.618 7.55
10/6.3 100×63×7 100 63 7 11.11 8.72
10/6.3 100×63×8 100 63 8 12.58 9.88
10/6.3 100×63×10 100 63 10 15.47 12.1
10/8 100×80×6 100 80 6 10.64 8.35
10/8 100×80×7 100 80 7 12.30 9.66
10/8 100×80×8 100 80 8 13.94 10.9
10/8 100×80×10 100 80 10 17.17 13.5

Unequal-leg angles — Table A.4, Models 11/7 to 20/12.5 unequal (30 sizes)

Swipe horizontally to view all dimensions.

Model Designation (B×b×d) B (mm) b (mm) d (mm) A (cm²) Mass (kg/m)
11/7 110×70×6 110 70 6 10.64 8.35
11/7 110×70×7 110 70 7 12.30 9.66
11/7 110×70×8 110 70 8 13.94 10.9
11/7 110×70×10 110 70 10 17.17 13.5
12.5/8 125×80×7 125 80 7 14.10 11.1
12.5/8 125×80×8 125 80 8 15.99 12.6
12.5/8 125×80×10 125 80 10 19.71 15.5
12.5/8 125×80×12 125 80 12 23.35 18.3
14/9 140×90×8 140 90 8 18.04 14.2
14/9 140×90×10 140 90 10 22.26 17.5
14/9 140×90×12 140 90 12 26.40 20.7
14/9 140×90×14 140 90 14 30.46 23.9
15/9 150×90×8 150 90 8 18.84 14.8
15/9 150×90×10 150 90 10 23.26 18.3
15/9 150×90×12 150 90 12 27.60 21.7
15/9 150×90×14 150 90 14 31.86 25.0
15/9 150×90×15 150 90 15 33.95 26.7
15/9 150×90×16 150 90 16 36.03 28.3
16/10 160×100×10 160 100 10 25.32 19.9
16/10 160×100×12 160 100 12 30.05 23.6
16/10 160×100×14 160 100 14 34.71 27.2
16/10 160×100×16 160 100 16 39.28 30.8
18/11 180×110×10 180 110 10 28.37 22.3
18/11 180×110×12 180 110 12 33.71 26.5
18/11 180×110×14 180 110 14 38.97 30.6
18/11 180×110×16 180 110 16 44.14 34.6
20/12.5 200×125×12 200 125 12 37.91 29.8
20/12.5 200×125×14 200 125 14 43.87 34.4
20/12.5 200×125×16 200 125 16 49.74 39.0
20/12.5 200×125×18 200 125 18 55.53 43.6

Q355B Chemical Composition for Angles (GB/T 1591 As-Rolled Ladle Analysis)

The figures below are ladle-analysis maxima for as-rolled Q355B in GB/T 1591-2018 Table 1. They are limits, not typical heat results. Product analysis, when required, follows the deviations in GB/T 222. These values are not the Table 3 or Table 5 limits used for Q355N or Q355M, and they should not be taken from unofficial trader sheets that still quote a 0.20% carbon cap or a 0.030% phosphorus cap as if those were the quality-B as-rolled defaults. Quality C and D of the same steel grade use a thickness-split carbon table and tighter phosphorus and sulphur; those are different quality letters, not a silent tightening of Q355B. The certificate still has to identify the angle, not a plate or H-beam heat that happens to share the name.

Element Maximum, ladle analysis (mass %) Notes for as-rolled Q355B angles
C 0.24 Tabulated maximum. For nominal thickness or diameter greater than 30 mm, carbon shall not exceed 0.22%. For sections thicker than 100 mm, carbon may be agreed by both parties.
Si 0.55 If silicon is deliberately held down for galvanizing, see the CEV footnotes in the next table.
Mn 1.60 —
P 0.035 For sections and bars the standard allows this maximum to be raised by 0.005% (to 0.040%).
S 0.035 For sections and bars the standard allows this maximum to be raised by 0.005% (to 0.040%).
Nb, V, Ti — Not required additions in Table 1 for Q355. Other alloying elements may be added by agreement and shall be reported on the certificate.
Cr 0.30 —
Ni 0.30 —
Cu 0.40 —
Mo — —
N 0.012 If the supplier guarantees nitrogen, analysis may be omitted. If acid-soluble aluminium is at least 0.015% or total aluminium is at least 0.020%, or other nitrogen-binding elements are added, nitrogen is not restricted and shall be stated on the certificate.
B — —

Most tabulated standard angles have a leg of 30 mm or less, so the 0.24% carbon maximum applies when the leg is the test location. The two 250×250 rows at 32 mm and 35 mm fall under the footnote that carbon shall not exceed 0.22% above 30 mm. The agreement option for sections thicker than 100 mm remains in the table because a special heavier bar could be agreed.

Q355B Carbon Equivalent for As-Rolled Angles

The carbon equivalent is calculated from the ladle analysis by the standard IIW formula given in GB/T 1591: CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. Table 2 maxima for as-rolled Q355 (qualities B, C and D share these cells) are shown below. Legs of 30 mm and under sit in the first (0.45%) band. The 250×250×32 and 250×250×35 rows sit in the second (0.47%) band when the leg is the test location.

Nominal thickness or diameter (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.45
30 < t ≤ 63 0.47
63 < t ≤ 150 0.47
150 < t ≤ 250 0.49 (for sections and bars the standard allows this maximum to be 0.54%)
250 < t ≤ 400 Not specified for quality B (the 0.49 value in this band applies only to quality D plate).

When silicon is controlled, for example for a hot-dip galvanizing route, and carbon or manganese is raised to keep the tensile properties, the standard allows the tabulated CEV maximum to be increased by 0.02% if silicon is not more than 0.030%, or by 0.01% if silicon is not more than 0.25%. Those increments should appear on the order if they are to be used. This page does not quote other raised CEV figures for thinner bands, because the 0.54% allowance is the one the standard attaches to the >150–250 mm cell for sections and bars.

Q355B Angle Mechanical Properties: Yield, Tensile and +20 °C Impact

Tensile properties of as-rolled Q355 are thickness-dependent. The values below are from GB/T 1591-2018 Tables 7 and 8, using the longitudinal elongation column that applies to sections and bars. For these angles the governing thickness is ordinarily the leg thickness d, which is the specimen-preparation thickness under GB/T 2975, not the leg length. Do not read the 355 MPa figure against the leg length, and do not treat a 16 mm plate rule as if it automatically described a 100 mm or 200 mm leg. Several of the larger tabulated angles have a leg thickness over 16 mm and therefore fall into the 345 MPa band; the later bands remain in the table because still heavier special bars can be agreed. For plates, specimens are usually transverse and elongation may be lower — use the Q355B steel plate page for those figures, not this table. When yield is not clearly pronounced, Rp0.2 may be used in place of ReH, as the standard allows.

Nominal thickness or diameter t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A, longitudinal (%)
t ≤ 16 355 470–630 22
16 < t ≤ 40 345 470–630 22
40 < t ≤ 63 335 470–630 21
63 < t ≤ 80 325 470–630 20
80 < t ≤ 100 315 470–630 20
100 < t ≤ 150 295 450–600 18
150 < t ≤ 200 285 450–600 17
200 < t ≤ 250 275 450–600 17

Quality B requires a Charpy V-notch absorbed energy at +20 °C of 34 J on a longitudinal specimen, or 27 J if a transverse specimen is agreed. The default is longitudinal. GB/T 1591 requires the impact test when the nominal thickness is not less than 6 mm (or the nominal diameter is not less than 12 mm); for these angles that thickness is ordinarily the leg thickness d. A number of the lighter tabulated legs are under 6 mm and therefore sit outside that obligation as written; the remainder are inside it. If a standard 10 mm × 10 mm × 55 mm specimen cannot be prepared, the standard allows a 7.5 mm or 5 mm subsidiary specimen at 75% or 50% of the Table 11 value, with the larger size preferred. The specimen size actually used belongs on the certificate. If the project needs 34 J at 0 °C or at −20 °C, the grade to nominate is Q355C or Q355D, not Q355B.

Delivery Conditions, Inspection and Identification

This product is as-rolled Q355B. GB/T 1591 also defines normalized and thermomechanical Q355 grades; those conditions, and their chemistry tables, must be named if they are required. The inspection document should identify Q355B, the GB/T 1591 edition, the as-rolled delivery condition, the carbon equivalent, the GB/T 706 designation and the edition used for dimensions and mass, the heat number, ladle analysis, and the tensile and impact results against the thickness at the test location, which for these angles is ordinarily the leg thickness d. Packaging, marks and certificates follow GB/T 2101 in the edition named on the order. A plate certificate, or an H-beam or channel certificate, does not, by itself, identify an angle.

An EN 10204 type 3.1 document is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification on the product follows the mill’s marking practice and the ordered standards. Length is a matter for the rolling programme and the order.

Weldability and Surface Condition of Q355B Angles

Q355B is a weldable high-strength low-alloy structural steel when thickness, joint design, hydrogen control and the actual carbon equivalent are taken into account. The CEV table above is the starting point; the certificate values and a procedure suited to the thickness are the practical controls. This page does not prescribe a procedure or a preheat chart.

The as-rolled surface is mill scale. A blast class, a paint system, or a hot-dip galvanizing chemistry is an order option, not something implied by the grade name. If galvanizing is planned, the silicon and phosphorus on the heat, the CEV footnotes for controlled silicon, and the processor’s coating specification should be reviewed before production. Surface quality also follows the ordered edition of GB/T 706; special finish requirements belong in the enquiry. Cutting to length, punching, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.

GB/T 706 Shape Tolerances and Theoretical Mass

Dimensional and mass tolerances for these angles are those of GB/T 706, not of GB/T 1591 and not of the GB/T 11263 envelope written for H-sections. This article uses GB/T 706-2016 as the numeric size basis and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026.

A delivered ∠50×50×5 will measure close to 50 × 50 × 5 mm within those tolerances, not as a set of exact advertised millimetres. Out-of-square and leg tilt matter for connections. Settlement on theoretical or weighed mass should follow the contract. Theoretical masses in the size tables use a density of 7.85 g/cm³; they are not a substitute for a weighed-mass agreement if the order requires one.

Applications and Service Limits

Q355B steel angles are used where a 355 MPa yield class, a +20 °C impact quality and a GB/T 706 L-section are accepted:

  • Building frames, bracing, lintels, truss work, plant structures and general structural fabrication.
  • Machinery bases, skids and support steelwork that actually specify a 355 MPa as-rolled grade rather than Q235B.
  • Export packages that compare the grade with S355JR H-beam or with A572 Grade 50 plate, provided each line keeps its own material standard and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for structures whose specification requires a lower impact-test temperature or a normalized or thermomechanical delivery condition. Durability comes from the coating or fire-protection system, not from the grade name. Weathering or marine exposure needs an agreed protection system, not bare Q355B.

Q355B Angle Compared with Q235B, S355JR and A572 Grade 50

Q355B and Q235B can share the GB/T 706 angle series, but they are different material standards and different yield classes. Q235B is specified to GB/T 700, with a 235 MPa yield class, a looser phosphorus and sulphur table, no published CEV maximum, and a 27 J longitudinal impact requirement at +20 °C. An enquiry that says only “Chinese angle” is incomplete.

S355JR H-beam is a near-equivalent in yield class, but a European angle in that grade would be an EN 10056 L, not a Chinese ∠50×50×5, unless a mill has a documented special combination, and its impact requirement is 27 J rather than 34 J longitudinal. ASTM A572 Grade 50 is a 50 ksi (345 MPa) grade on a different shape system. Dual certification is possible only when the delivered piece meets every requirement of each named standard, including chemistry, tests, dimensions and tolerances. Q355B H-beam and Q355B plate share the material grade, not the section.

A Q355B channel to GB/T 706, and a Q235B angle to the same dimensional standard, will be linked here once those pages are published; those product URLs are not pre-linked.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to Q355B angle Caution
Q345B (former designation) Earlier editions of GB/T 1591 GB/T 1591-2018 replaced the Q345 steel grade with Q355. Appendix A maps as-rolled Q355B to the former Q345B. Do not treat a historical Q345B certificate as automatically meeting the 2018 Q355B table. Name the 2018 grade and edition on new orders.
Q355C / Q355D (as-rolled) GB/T 1591-2018 Same 355 MPa yield class. C is tested at 0 °C (34 J longitudinal) and D at −20 °C. Tighter phosphorus and sulphur, and a thickness-split carbon table. Not interchangeable with B on a +20 °C specification.
Q355N / Q355M GB/T 1591-2018 Same yield class in the normalized or thermomechanical conditions, with their own chemistry and CEV tables. Do not certify as-rolled Q355B as Q355N or Q355M unless the actual delivery condition and tables are met.
Q235B GB/T 700; a GB/T 706 angle may be certified to Q235B when that is the order A lower-strength Chinese carbon-steel comparison on the same GB/T 706 angle series. Q235B is not Q355B. It has no published CEV cap and a 27 J, not 34 J longitudinal, impact requirement at +20 °C.
S355JR EN 10025-2; dimensions EN 10056 for angles A comparable 355 MPa European grade with a +20 °C impact quality, usually as an equal-leg or unequal-leg L when the product is an angle. S355JR impact is 27 J, not 34 J longitudinal. Chemistry, CEV rules and the EN 10056 shape system all differ. An EN 10056 L 50×50 is not a Chinese ∠50×50×5.
ASTM A572 Grade 50 ASTM A572/A572M; American angle dimensions ASTM A6/A6M A common 50 ksi (345 MPa) high-strength low-alloy comparison in export enquiries. Yield class, chemistry and the American L shape system differ. Not an automatic substitute.

Sourcing Q355B Steel Angles from SHH STEEL

SHH STEEL supplies Q355B steel angles as an export trading house, coordinating mill production and project procurement. The useful part of that model is to keep the material edition and the as-rolled Q355B condition (GB/T 1591-2018, rather than a former Q345B call or an N/M condition) distinct from the shape edition (GB/T 706-2016 as the numeric basis here, or the successor edition when that is what the order names), to apply the yield and CEV bands to the leg thickness rather than the leg length, and to align the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every Table A.3 or A.4 size in Q355B. Mid-range equal legs such as 50×50×5 and 75×75×8 are the usual core; the 20×20 families, the 200×200 and 250×250 rows, and the larger unequal legs are confirmed per line.

The same enquiry can also cover channels, H-sections, or European, American or Japanese designations, provided each line states its material standard, shape standard, delivery condition and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

Q355B Steel Angle FAQs

Is Q355B the same as Q345B?
Q355B is the current as-rolled quality-B grade in GB/T 1591-2018; that edition replaced the Q345 designation with Q355. Appendix A maps Q355B to the former Q345B, but a historical Q345B certificate should not be treated as automatically meeting the 2018 tables. New orders should name Q355B, the as-rolled condition, and the 2018 edition or the edition on the contract.
Does the 355 MPa yield apply to every Q355B angle in the tables?
No. The governing thickness is ordinarily the leg thickness d, not the leg length. Angles with d ≤ 16 mm sit in the 355 MPa band. Several larger equal-leg sizes, and 200×125×18 among the unequal-leg rows, have a leg thicker than 16 mm and therefore fall into the 345 MPa band. The later bands remain in the mechanical table for still heavier special bars.
Is the impact requirement 27 J, like S355JR, and does it apply to every size?
No. As-rolled Q355B requires 34 J on a longitudinal specimen at +20 °C, or 27 J if a transverse specimen is agreed. S355JR uses 27 J at +20 °C under EN 10025-2. GB/T 1591 requires the impact test when the nominal thickness is not less than 6 mm; for these angles that thickness is ordinarily the leg. A number of the lighter tabulated legs are under 6 mm and therefore sit outside that obligation as written.
Which edition of GB/T 706 is used for the size tables?
The size tables use GB/T 706-2016 as the numeric basis and are the complete Table A.3 equal-leg series (115 sizes, 20×20×3 to 250×250×35) and Table A.4 unequal-leg series (71 sizes, 25×16×3 to 200×125×18). GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition of GB/T 706 named on the order governs dimensional acceptance.
Which standards should appear on the inspection document?
At least GB/T 1591 and its edition, the grade Q355B, the as-rolled delivery condition, the carbon equivalent, the GB/T 706 designation and the edition used for dimensions and mass, ladle analysis, and tensile and impact results against the thickness at the test location, ordinarily the leg thickness d. Packaging, marks and certificates follow GB/T 2101. A plate, H-beam or channel certificate does not, by itself, identify an angle.

Request a Quotation for GB/T 706 Q355B Steel Angle

GB/T 706 Q355B steel angle is a Chinese equal-leg or unequal-leg L-section in as-rolled Q355B, with 355 MPa minimum yield in the first thickness band and a 34 J longitudinal impact requirement at +20 °C. Nominate the GB/T 706 designation (for example ∠50×50×5, ∠200×200×20 or ∠160×100×16), the material to GB/T 1591-2018 as-rolled Q355B (or the edition on the order), and the carbon equivalent basis. The size tables use GB/T 706-2016 as the numeric basis; GB/T 706-2026 is the successor edition, with implementation from 1 December 2026; the ordered edition governs. Send the size list, edition, condition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X