GB/T 11263 Q235B H-Beam | GB/T 11263 H-Beams - SHH STEEL

GB/T 11263 Q235B H-Beam

GB/T 11263 Q235B H-beam is a hot-rolled Chinese H-section in carbon structural steel Q235B (GB/T 700), with 235 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Sizes follow the HW, HM and HN series under GB/T 11263. SHH STEEL reviews grade, size series, standard edition and certificate requirements before quoting.
Keywords
GB/T 11263 Q235B H-Beam, Q235B HW, Q235B HM, Q235B HN, Q235B structural H-beam
Equivalent Grades:
Near-equivalents only, not automatic substitutes: Q235C/D; S235JR; ASTM A36; JIS SS400.
Share:
General Description
Material Specification
Available Sizes of Q235B H-Beam
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source Q235B H-Beams from SHH STEEL
FAQ
Conclusion

What is GB/T 11263 Q235B H-Beam?

GB/T 11263 Q235B H-beam is a hot-rolled H-section whose material grade is Q235B under GB/T 700 and whose shape, tolerances and theoretical mass are ordered to GB/T 11263. Q stands for yield strength, 235 is the minimum upper yield strength in MPa for the thinnest tabulated thickness band, and B is the quality grade, which carries a longitudinal Charpy V-notch requirement of 27 J at +20 °C when impact testing applies.

This page covers the rolled H-section, not plate. The same grade in plate form is listed separately as GB/T 700 Q235B steel plate. For plates, tensile specimens are taken transverse to the rolling direction and elongation may be two percentage points lower than the Table 2 values used for sections and bars. The plate page is not a substitute data sheet for H-beams.

These beams are filed under GB/T 11263 in the steel beam profiles category of steel structural profiles. The Chinese commercial size families are HW, HM and HN — wide, medium and narrow flange — and those names belong only to this dimensional system. They are not interchangeable with European HEA/HEB/IPE or with American W-shapes of a similar nominal depth.

Q235B is a general carbon structural steel for building frames, workshops and ordinary fabrication where a +20 °C impact quality is accepted. It is not a 355 MPa grade, not a weathering steel, and not a pressure-vessel or nuclear safety material. If an enquiry only says “Q235 H-beam,” the quality letter and the dimensional standard still need to be confirmed before rolling or allocation.

Material, Dimensions and Tolerances for Q235B Sections

Three documents should appear, separately, on the purchase order and on the inspection certificate:

  • GB/T 700 is the material standard for carbon structural steels. This article uses ladle-analysis limits and tensile values from GB/T 700-2006, which remains the current edition. The edition named on the order governs acceptance.
  • GB/T 11263 is the product standard for hot-rolled H-sections and split T-sections. It sets the size series, dimensional and shape tolerances, theoretical mass and section surface rules. The 2017 edition classified sections as HW, HM, HN (and HT for split tees). GB/T 11263-2024, implemented on 2025-05-01, reclassified sections as H and HK and revised appendix dimensions and masses. Export orders still often call sizes as HW, HM or HN. The tables below use the established HW/HM/HN series with 2017 theoretical masses. Masses in the 1998, 2017 and 2024 editions are not identical for every size, so the edition used for settlement must be written on the order.
  • Tolerances on depth, width, thickness, out-of-square, web off-centre, straightness and mass are those of the ordered GB/T 11263 edition, not of GB/T 700.

A mill may certify Q235B on a Japanese or European shape, or roll an HW section to a different material standard, if that combination is in its programme and is fully documented. Do not treat “Q235B H-beam” as if it automatically meant an HW 300×300, and do not substitute EN 10025-2 S355JR H-beam sizes or ASTM A36 W-shapes by matching a nominal 300 mm or 12 in depth.

Q235B H-Beam Sizes: HW, HM and HN Reference Tables

The tables give designation, actual depth h, width b, web thickness tw, flange thickness tf and theoretical mass per metre for the HW, HM and HN series as published against GB/T 11263-2017. They are reference dimensions for identification and estimating, not a rolling list for any one mill and not a claim that every size is produced in Q235B. Availability depends on the mill programme and on certification of the ordered grade. Mid-range HW and HN sizes are the usual enquiry core; the lightest HN rows, the heavier HN 700–1000 sizes, and less common variants should be confirmed size by size.

HW sections are the wide-flange, essentially square family (for example HW 200×200×8×12). HM sits between square and narrow (HM 300×200 has an actual depth of 294 mm). HN is the narrow-flange family used as beams rather than columns. A model name such as HM 150×100 is a series call; the actual depth may be slightly less, just as a European HEA 300 is 290 mm deep. Root radius and cross-sectional area are omitted because they were not printed in the 2017 mass table used here.

Theoretical mass is the 2017 figure. Settlement on 1998 masses (which are higher for many of the same designations) or on 2024 appendix masses will give a different kilogram total. State the edition, and whether theoretical or weighed mass applies, on the order.

HW series

Wide-flange H-sections, 11 sizes in the 2017 table, from HW 100×100×6×8 to HW 400×400×13×21, including the heavier 250×255 and 300×305 variants.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) Mass (kg/m)
HW 100×100×6×8 100 100 6 8 16.9
HW 125×125×6.5×9 125 125 6.5 9 23.6
HW 150×150×7×10 150 150 7 10 31.1
HW 175×175×7.5×11 175 175 7.5 11 40.4
HW 200×200×8×12 200 200 8 12 49.9
HW 250×250×9×14 250 250 9 14 71.8
HW 250×255×14×14 250 255 14 14 81.6
HW 300×300×10×15 300 300 10 15 93
HW 300×305×15×15 300 305 15 15 105
HW 350×350×12×19 350 350 12 19 135
HW 400×400×13×21 400 400 13 21 172

HM series

Medium-flange H-sections, 11 sizes, from HM 148×100×6×9 to the 600 mm-class 588×300×12×20.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) Mass (kg/m)
HM 148×100×6×9 148 100 6 9 20.7
HM 194×150×6×9 194 150 6 9 29.9
HM 244×175×7×11 244 175 7 11 43.6
HM 294×200×8×12 294 200 8 12 55.8
HM 340×250×9×14 340 250 9 14 78.1
HM 390×300×10×16 390 300 10 16 105
HM 440×300×11×18 440 300 11 18 121
HM 482×300×11×15 482 300 11 15 111
HM 488×300×11×18 488 300 11 18 125
HM 582×300×12×17 582 300 12 17 133
HM 588×300×12×20 588 300 12 20 147

HN series

Narrow-flange H-sections, 30 sizes, from HN 100×50×5×7 to HN 1000×300×19×36. Several 2017 rows (including 550, 625, 630 and 1000) do not appear in the older 1998 column and should be called by their actual 2017 dimensions.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) Mass (kg/m)
HN 100×50×5×7 100 50 5 7 9.3
HN 125×60×6×8 125 60 6 8 13.1
HN 150×75×5×7 150 75 5 7 14
HN 175×90×5×8 175 90 5 8 18
HN 198×99×4.5×7 198 99 4.5 7 17.8
HN 200×100×5.5×8 200 100 5.5 8 20.9
HN 248×124×5×8 248 124 5 8 25.1
HN 250×125×6×9 250 125 6 9 29
HN 298×149×5.5×8 298 149 5.5 8 32
HN 300×150×6.5×9 300 150 6.5 9 36.7
HN 346×174×6×9 346 174 6 9 41.2
HN 350×175×7×11 350 175 7 11 49.4
HN 400×150×8×13 400 150 8 13 55.2
HN 396×199×7×11 396 199 7 11 56.1
HN 400×200×8×13 400 200 8 13 65.4
HN 446×199×8×12 446 199 8 12 65.1
HN 450×200×9×14 450 200 9 14 74.9
HN 496×199×9×14 496 199 9 14 77.9
HN 500×200×10×16 500 200 10 16 88.1
HN 546×199×9×14 546 199 9 14 81.5
HN 550×200×10×16 550 200 10 16 92
HN 596×199×10×15 596 199 10 15 92.4
HN 600×200×11×17 600 200 11 17 103
HN 625×198.5×13.5×17.5 625 198.5 13.5 17.5 118
HN 630×200×15×20 630 200 15 20 133
HN 700×300×13×24 700 300 13 24 182
HN 800×300×14×26 800 300 14 26 207
HN 890×299×15×23 890 299 15 23 210
HN 900×300×16×28 900 300 16 28 240
HN 1000×300×19×36 1000 300 19 36 310

Japanese metric H sizes follow JIS G 3192 and are not selected from these HW/HM/HN tables. European HEA/HEB/IPE sizes belong to that material system, as shown on the S355JR H-beam page, not as Q235B dimensions.

Q235B Chemical Composition (GB/T 700 Ladle Analysis)

The figures below are ladle-analysis maxima for Q235B in GB/T 700-2006. They are limits, not typical heat results. Product analysis may differ by the deviations in GB/T 222. Do not mix these values with unofficial tables that still quote the withdrawn 1988 manganese range of 0.30–0.70%.

Element Maximum, ladle analysis (mass %) Notes
C 0.20 May be raised to 0.22% only with the purchaser’s agreement. The 2006 edition sets no carbon minimum.
Si 0.35 —
Mn 1.40 Maximum only. The 1988 range 0.30–0.70% was withdrawn; do not treat that older range as the current default.
P 0.045 —
S 0.045 —
Cr, Ni, Cu (each, residual) 0.30 Need not be analysed if the supplier guarantees the limit.
N 0.008 May be higher under the standard’s nitrogen/phosphorus and nitrogen-binding rules; those cases belong on the certificate.
As 0.080 General maximum; arsenic-bearing ore routes are a matter for agreement.

Q235B may be supplied as rimming steel (F) or killed steel (Z); the letter Z is usually omitted from the designation. Hot-rolled H-sections are commonly killed. The concession that carbon, manganese and silicon need not be delivery conditions if mechanical properties are guaranteed applies to grade A, not to grade B. Residual-element and nitrogen rules belong on the certificate when they are invoked.

GB/T 700 does not specify a carbon-equivalent maximum for Q235B. Weldability still depends on the actual carbon, thickness and welding procedure, which is why the certificate values matter.

Q235B Mechanical Properties: Yield, Tensile and +20 °C Impact

Tensile properties of Q235B are thickness-dependent. The values below are from GB/T 700-2006 Table 2. For sections and bars, tensile and bend specimens are longitudinal. The 2006 edition no longer gives a separate elongation column for t ≤ 16 mm; 26% applies through 40 mm. For plates and strip, specimens are transverse and elongation may be two percentage points lower — use Q235B steel plate rather than this table.

Nominal thickness or diameter t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 235 370–500 26
16 < t ≤ 40 225 370–500 26
40 < t ≤ 60 215 370–500 25
60 < t ≤ 100 215 370–500 24
100 < t ≤ 150 195 370–500 22
150 < t ≤ 200 185 370–500 21

For nominal thickness greater than 100 mm, the standard allows the lower tensile-strength limit to be reduced by 20 N/mm². The upper tensile limit is not a delivery condition for wide strip, including plate cut from strip; that concession is about strip, not about these H-sections.

Quality B requires a longitudinal Charpy V-notch absorbed energy of 27 J at +20 °C, reported as the average of three specimens, with the usual single-value allowance (one result may be lower, but not below 70% of the specified value). Impact tests are required for thickness not less than 12 mm (or diameter not less than 16 mm). For Q235B thinner than 25 mm, the test may be omitted if the supplier guarantees conformity and the purchaser agrees; that is a waiver of inspection, not a deletion of the requirement. If the project needs 27 J at 0 °C or at −20 °C, the grade to nominate is Q235C or Q235D, not Q235B.

Apply the band that matches the governing thickness of the ordered size, usually the flange on an H-section, not the headline 235 MPa value. An HW 400×400 flange is 21 mm, so the minimum yield is 225 MPa.

Delivery Conditions, Inspection and Identification

GB/T 700 states that steel is generally delivered in the hot-rolled, controlled-rolled or normalized condition. Hot-rolled H-sections are commonly supplied as-rolled unless the order calls for another condition. The delivery condition should appear on the inspection document together with the material edition, the grade Q235B, the GB/T 11263 edition used for dimensions and mass, the size designation, the heat number, ladle analysis and the tensile and impact results.

An EN 10204 type 3.1 document is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification on the product follows the mill’s marking practice and the ordered standards: typically the grade, mill identification and heat or piece reference.

Length is not fixed by the size table. Mills commonly roll these sections in fixed lengths in the region of 6–15 m; other lengths are a matter for the rolling programme and the order.

Weldability and Surface Condition of Q235B H-Beams

Q235B is a weldable carbon structural steel when thickness, joint design and hydrogen control are taken into account. Because GB/T 700 does not set a CEV cap for this grade, the actual ladle carbon and manganese on the certificate, together with a welding procedure suited to the thickness, are the practical controls. This page does not prescribe a procedure or a preheat chart.

The as-rolled surface is mill scale. A blast class, a paint system, or a hot-dip galvanizing chemistry is an order option, not something implied by the grade name. If galvanizing is planned, the silicon and phosphorus on the heat, and the processor’s coating specification, should be reviewed before production. Surface quality also follows the ordered edition of GB/T 11263; special finish requirements belong in the enquiry.

Cutting to length, weld-end preparation, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.

GB/T 11263 Shape Tolerances and Theoretical Mass

Dimensional and mass tolerances for these H-sections are those of GB/T 11263, not of GB/T 700. The ordered edition matters: 2017 and 2024 do not use identical tolerance wording or mass appendices. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.

The size tables above are nominal reference dimensions. A delivered HW 200×200 will measure close to 200 × 200 × 8 × 12 mm within those tolerances, not as a set of exact advertised millimetres. Out-of-square and web off-centre matter for end-plate connections.

The kg/m column is a 2017 theoretical mass. Weighed mass may sit above or below that figure and still be within tolerance. Settlement should follow the contract — 2017 theoretical mass, 2024 theoretical mass, 1998 theoretical mass, or weighed mass — not an informal mix of those bases.

Applications and Service Limits

Q235B H-beams are used where a 235 MPa yield class and a +20 °C impact quality are accepted:

  • Building frames, workshops, platforms and general structural fabrication.
  • Machinery bases, skids and support steelwork that do not require a 355 MPa grade.
  • Secondary members in larger structures, when the specification actually names Q235B rather than Q355B or a European S355 quality.

It is not specified here for pressure equipment, for nuclear safety-related components, or for structures whose specification requires a lower impact-test temperature or a fine-grain weldable grade. Durability comes from the coating or fire-protection system, not from the grade name. Weathering or marine exposure needs an agreed protection system, not bare Q235B.

Q235B Compared with Q355B, S235JR and A36

Q235B and Q355B share the HW/HM/HN shape system under GB/T 11263, but they are different material standards and different yield classes. Q355B is specified to GB/T 1591, with a 355 MPa yield class, tighter phosphorus and sulphur, a published CEV table, and a 34 J longitudinal impact requirement at +20 °C. An enquiry that says only “Chinese H-beam” is incomplete.

S235JR in the EN 10025-2 beam family is a near-equivalent in yield class, but it is rolled as HEA, HEB or IPE (or UB/UC), not as HW/HM/HN, unless a mill has a documented special combination. ASTM A36 wide-flange beams are a 36 ksi (250 MPa) grade on W-shapes to ASTM A6. JIS G 3101 SS400 is the usual Japanese general-structural comparison, with dimensions typically to JIS G 3192.

Dual certification is possible only when the delivered piece meets every requirement of each named standard, including chemistry, tests, dimensions and tolerances.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or a mill certificate. Where a project allows an alternative, the substitution should be written into the order and verified on the inspection document.

Grade / designation Standard Relationship to Q235B H-beam Caution
Q235A / Q235C / Q235D GB/T 700 Same 235 MPa yield class. A has no impact test; C and D are tested at 0 °C and −20 °C. Do not treat “Q235” as if it included the B impact requirement.
S235JR EN 10025-2 Comparable 235 MPa yield class with a +20 °C impact quality. Different chemistry, thickness bands and shape series (HEA/HEB/IPE). Not an automatic substitute.
ASTM A36 ASTM A36/A36M; W-shape dimensions ASTM A6 A common general structural carbon steel in export enquiries. Yield class is 36 ksi (250 MPa), not 235 MPa. Chemistry and the W-shape system differ.
SS400 JIS G 3101; dimensions often JIS G 3192 Similar general-structural carbon steel on Japanese and Taiwanese projects. SS400 has its own tensile window and no Q235-style A–D impact ladder.

Sister beam pages in this series (Q355B, A36, S235JR, SS400) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page when the comparison is with the 355 MPa European grade.

Sourcing Q235B H-Beams from SHH STEEL

SHH STEEL supplies Q235B H-beams as an export trading house, coordinating mill production and project procurement. The useful part of that model is to align the material edition (GB/T 700), the shape edition and mass basis (GB/T 11263-2017 or 2024, and whether HW/HM/HN or the newer H/HK calls are to be used), and the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every HW, HM or HN size in Q235B. Mid-range sizes are the usual core; heavier HN and special 2017-only sizes are confirmed per line. Mixed procurement can be used when a take-off spans more than one rolling programme.

The same enquiry can also cover European, American or Japanese designations, provided each line states its material standard, shape standard and size. If cutting, weld-end preparation, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

Q235B H-Beam FAQs

Can I replace an HW section with an HEA or W-shape of the same depth?
No. HW, HM and HN are the GB/T 11263 families. HEA/HEB/IPE and American W-shapes are different series with different widths, flange thicknesses, masses and tolerance standards. HW 300×300 is not HEB 300, IPE 300 or a W12. Select the section from the standard named on the drawing, or obtain a formal design change.
Is Q235 the same as Q235B?
Q235 is the yield class; A, B, C and D are quality grades. B adds a 27 J impact requirement at +20 °C and a tighter sulphur limit than A. An order that says only “Q235 H-beam” is incomplete. If the specification is silent, confirm the quality letter before production.
Can I use 1998 theoretical masses for a 2017 or 2024 size list?
Not without agreement. For many of the same designations the 1998 mass is higher than the 2017 mass (for example HW 100×100×6×8 is 17.2 kg/m in 1998 and 16.9 kg/m in 2017). The 2024 appendix is different again. Write the edition and the mass basis on the order.
Is Q235B the same as S235JR or ASTM A36?
They are near-equivalents in a general-structural carbon class, not automatic substitutes. S235JR is an EN 10025-2 grade, usually supplied as European I or H series. A36 is a 36 ksi (250 MPa) ASTM grade, usually supplied as W-shapes. Chemistry, tests and dimensions all have to be met if dual certification is requested.
Which standards should appear on the mill certificate?
At least GB/T 700 and its edition, the grade Q235B, the GB/T 11263 edition used for dimensions and theoretical mass, the size designation (HW/HM/HN or the 2024 H/HK call, as ordered), the delivery condition, ladle analysis, tensile results by thickness, and the +20 °C impact result unless a documented inspection waiver applies for thin Q235B.

Request a Quotation for GB/T 11263 Q235B H-Beam

GB/T 11263 Q235B H-beam is a carbon structural H-section with 235 MPa minimum yield up to 16 mm and a 27 J longitudinal impact requirement at +20 °C. Nominate the HW, HM or HN size to the agreed edition of GB/T 11263, and name GB/T 700-2006 (or the edition on the order) as the material standard. The tables are 2017 reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *