GB/T 14976 06Cr19Ni13Mo3 Seamless Stainless Steel Pipe
What is GB/T 14976 06Cr19Ni13Mo3 Seamless Stainless Steel Pipe
When the approved vendor list and isometric notes say GB/T 14976, the grade mark has to be the Chinese designation. 06Cr19Ni13Mo3 is the full product grade for this austenitic seamless pipe. GB/T 14976 06Cr19Ni13Mo3 locks 317-class Mo under seamless fluid-transport acceptance — not an ASTM A312 certificate by default. Buyers working Chinese fluid-transport packages should treat 06Cr19Ni13Mo3 as a governed product grade under GB/T 14976-2025, with Table 2 chemistry and Table 3 tensile floors enforced on the same heat. Keep the 06Cr19Ni13Mo3 caution visible here: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty.
SHH STEEL can supply 06Cr19Ni13Mo3 seamless pipe in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the line: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr19Ni13Mo3 before production starts. This paragraph is locked to 06Cr19Ni13Mo3 duty: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum.
Equivalence talk to 317 / UNS S31708 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 14976 06Cr19Ni13Mo3, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 06Cr19Ni13Mo3 so informal alias language cannot reopen the carbon or molybdenum window after melt. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; heat-input control on non-L heats.
Related ASTM pipe pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 06Cr18Ni12Mo2Cu2. Use thread: chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. Document the medium, design temperature, and weld map beside the 06Cr19Ni13Mo3 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the 06Cr19Ni13Mo3 caution visible here: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty.
Inside this GB/T 14976 series, compare GB/T 14976 022Cr19Ni13Mo3, GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 015Cr20Ni18Mo6CuN, GB/T 14976 06Cr18Ni12Mo2Cu2. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP317L.
On 06Cr19Ni13Mo3 packages that also list flats, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 4237 06Cr19Ni13Mo3. Confirm 06Cr19Ni13Mo3 OD × wall and plate thickness on separate drawings.
Chemical Composition of GB/T 14976 06Cr19Ni13Mo3
Chemistry control on 06Cr19Ni13Mo3 starts at the ladle. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 11.00–15.00, Cr 18.00–20.00, Mo 3.00–4.00 within Table 2, reported on the inspection document against the heat. Body alias 317 / UNS S31708 does not widen those windows. Every ladle analysis for 06Cr19Ni13Mo3 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Corrosion framing beside 06Cr19Ni13Mo3: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review.
Read the table with the family in mind — austenitic — and with caution 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. Numbers without the matching Table 1 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr19Ni13Mo3 before the order is acknowledged. This paragraph is locked to 06Cr19Ni13Mo3 duty: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 06Cr19Ni13Mo3 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 11.00–15.00 | 18.00–20.00 | 3.00–4.00 |
Mechanical Properties of GB/T 14976 06Cr19Ni13Mo3
Proof stress and tensile minima for 06Cr19Ni13Mo3 sit at Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Flattening or bend testing backs ductility when ordered. Watch-out: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. Tensile sampling follows the batch rules for the ordered test unit of 06Cr19Ni13Mo3, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Application context for 06Cr19Ni13Mo3 stays chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 06Cr19Ni13Mo3 | 520 | 205 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 06Cr19Ni13Mo3. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 06Cr19Ni13Mo3
SHH STEEL can produce 06Cr19Ni13Mo3 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 06Cr19Ni13Mo3; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. This paragraph is locked to 06Cr19Ni13Mo3 duty: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum.
Process control for 06Cr19Ni13Mo3 ends with verified heat treatment (1010–1150 °C, water or rapid cool) and surface conditioning. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.
Bevel geometry is by agreement when ordered without a drawing. Size practice: broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement. Density for theoretical weight of 06Cr19Ni13Mo3: 7.98 kg/dm³ per Table 1. Hydrostatic pressure or NDT class for 06Cr19Ni13Mo3 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Corrosion framing beside 06Cr19Ni13Mo3: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review.
Dimensions and Tolerances for GB/T 14976 06Cr19Ni13Mo3
Usual length for GB/T 14976 pipe is 4000–12000 mm; fixed and multiple lengths sit inside that band with stated plus tolerances. For 06Cr19Ni13Mo3, confirm whether your project uses OD or ID ordering. Context: broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement. Tolerance class (PA/PC) follows the precision ordered for 06Cr19Ni13Mo3, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 06Cr19Ni13Mo3 remains broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement.
Full-length bend ≤0.15% of length; per-metre bend ≤1.5 mm (S≤15 mm) or ≤2.0 mm (S>15 mm). 06Cr19Ni13Mo3 must meet those geometry floors unless a written waiver exists. Fixed lengths and multiple cut lengths for 06Cr19Ni13Mo3 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; heat-input control on non-L heats.
Equivalent Grades for GB/T 14976 06Cr19Ni13Mo3
GB/T 14976 does not make 317 / UNS S31708 a drop-in certificate for 06Cr19Ni13Mo3. Use the commercial name in dual-cert talk, then verify every Table limit that matters for this pipe. Sisters in the series are comparison pages, not interchangeable stock codes. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr19Ni13Mo3).
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 06Cr19Ni13Mo3 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 317 / UNS S31708 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 317 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
When the service outgrows 06Cr19Ni13Mo3, move to a sister rather than stretching the alias: GB/T 14976 022Cr19Ni13Mo3, GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 015Cr20Ni18Mo6CuN, GB/T 14976 06Cr18Ni12Mo2Cu2. Apps context: 317/317L fillers; heat-input control on non-L heats. Full list under GB/T 14976. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (06Cr19Ni13Mo3).
Heat Treatment and Delivery Condition for GB/T 14976 06Cr19Ni13Mo3
Other heat-treatment schedules are allowed only by written agreement (6.3.4) — silence means Table 1 defaults. For 06Cr19Ni13Mo3: 1010–1150 °C, water or rapid cool. Recorded furnace charts for 06Cr19Ni13Mo3 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 06Cr19Ni13Mo3 caution visible here: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty.
After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. Field heat treatment of 06Cr19Ni13Mo3 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 06Cr19Ni13Mo3 remains broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement.
Corrosion Resistance of GB/T 14976 06Cr19Ni13Mo3
Pick tests that match how 06Cr19Ni13Mo3 is filed — austenitic. Corrosion thread: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review. Caution: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. Coupon orientation, weld condition, and surface finish for 06Cr19Ni13Mo3 belong in the corrosion test order so annex results can be compared to the installed spool honestly. Corrosion framing beside 06Cr19Ni13Mo3: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review.
Oxygen-line Annex B and cryogenic Annex A add impact, UT, and cleanliness rules — they do not change the alloy selection logic. Use thread: chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr19Ni13Mo3 rather than relying on wall thickness alone. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; heat-input control on non-L heats.
Applications of GB/T 14976 06Cr19Ni13Mo3 Seamless Pipe
Project types that repeatedly call 06Cr19Ni13Mo3: chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. Duty: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. Caution still applies: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. Spool fabricators should copy 06Cr19Ni13Mo3 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 06Cr19Ni13Mo3: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review.
Cryogenic, oxygen, and corrosive process lines all appear in 14976’s scope options — alloy choice still follows the medium. For this mark: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. Commissioning teams benefit when the as-built dossier repeats 06Cr19Ni13Mo3 beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; heat-input control on non-L heats.
Weldability of GB/T 14976 06Cr19Ni13Mo3
Even seamless W-C/W-H pipe of 06Cr19Ni13Mo3 will see field welds. Use: 317/317L fillers; heat-input control on non-L heats. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 06Cr19Ni13Mo3 should use the same product form and wall class as production, including the seamless finish that will ship. Application context for 06Cr19Ni13Mo3 stays chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”.
Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. Consumable lot control and shielding-gas notes for 06Cr19Ni13Mo3 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 06Cr19Ni13Mo3 caution visible here: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty.
Surface Finishes for GB/T 14976 06Cr19Ni13Mo3
Welded or heavily formed 06Cr19Ni13Mo3 may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 14976 seamless stainless fluid-transport pipe. State OD/ID scope for 06Cr19Ni13Mo3 before booking grind or polish.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
OD stencil ink on 06Cr19Ni13Mo3 should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows. Close bundles only after free-iron and burn marks are cleared. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06Cr19Ni13Mo3.
Inspection and Testing for GB/T 14976 06Cr19Ni13Mo3
Batching rules limit pieces per heat/size/heat-treat lot. For 06Cr19Ni13Mo3, keep the heat identity unbroken from melt to bundle tag. Duty: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. Sampling plans for 06Cr19Ni13Mo3 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 06Cr19Ni13Mo3: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review.
Intergranular corrosion testing is mandatory for most austenitics — see the IGC note for 06Cr19Ni13Mo3. Order extras (grain size, inclusions, elevated tensile) under 7.8.3 when needed. Non-conforming 06Cr19Ni13Mo3 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 06Cr19Ni13Mo3 remains broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement.
Packaging and Shipping for GB/T 14976 06Cr19Ni13Mo3
Small-OD 06Cr19Ni13Mo3 often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. Bundle tickets for 06Cr19Ni13Mo3 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 06Cr19Ni13Mo3: Mo window 3–4% lifts pitting resistance versus 316; crevice and hot chloride SCC still need review.
Bevelled ends get protectors so landing edges survive trucking. Size hint: broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement. Desiccant and wrap choices for 06Cr19Ni13Mo3 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; heat-input control on non-L heats.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. Claims handling for 06Cr19Ni13Mo3 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr19Ni13Mo3 remains broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement.
Why Choose SHH STEEL
Project teams working to Chinese fluid-transport specs need a supplier that reads Chinese grade names correctly. SHH STEEL can make 06Cr19Ni13Mo3 to that discipline. Caution we keep visible: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. SHH STEEL can produce and supply 06Cr19Ni13Mo3 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (GB/T + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN, 06Cr18Ni12Mo2Cu2. Ask for a written acknowledgement that names 06Cr19Ni13Mo3, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr19Ni13Mo3 to that written scope.
Supply Capability
Whether you need prototype spools or project tonnage of 06Cr19Ni13Mo3, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr19Ni13Mo3 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 06Cr19Ni13Mo3 (S31708) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes piercing/drawing slots for 06Cr19Ni13Mo3 rather than promising anonymous warehouse tons. Typical conversation starts around broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement. SHH STEEL can supply alternate walls and precision classes for 06Cr19Ni13Mo3 once the design pressure and corrosion allowance are clear.
If the project needs dual GB/T 14976 + ASTM documentation, say so before melt. Caution: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty. SHH STEEL can produce trial lengths of 06Cr19Ni13Mo3 for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of 06Cr19Ni13Mo3 for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to 06Cr19Ni13Mo3: 317/317L fillers; heat-input control on non-L heats.
FAQ
-
What is GB/T 14976 06Cr19Ni13Mo3 seamless stainless steel pipe used for?
- GB/T 14976 06Cr19Ni13Mo3 is seamless stainless pipe for fluid transport — chemical process transfer, higher-chloride utilities, and Chinese BOMs that still say “317 seamless”. Role summary: standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. It is a Chinese product standard grade (S31708), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 06Cr19Ni13Mo3 seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr19Ni13Mo3 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 06Cr19Ni13Mo3?
- 06Cr19Ni13Mo3 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr19Ni13Mo3 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr19Ni13Mo3 compare with sister grades 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN?
- 06Cr19Ni13Mo3 is filed as austenitic. Typical sisters on the same RFQ are 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. Design caution: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr19Ni13Mo3?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 317 / UNS S31708 the same as ordering 06Cr19Ni13Mo3?
- No. 317 / UNS S31708 is a commercial / UNS cross-walk for body text (unified S31708). The purchase order should lock GB/T 14976 and 06Cr19Ni13Mo3 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 06Cr19Ni13Mo3?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr19Ni13Mo3 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: broad OD×wall; name W-C or W-H and PA/PC on the acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 06Cr19Ni13Mo3 be welded on site?
- Shop guidance: 317/317L fillers; heat-input control on non-L heats. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr19Ni13Mo3?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: 0.08% carbon — prefer 022Cr19Ni13Mo3 for corrosive as-welded duty Sister pointers: 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 06Cr19Ni13Mo3 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr19Ni13Mo3 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr19Ni13Mo3 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 06Cr19Ni13Mo3?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr19Ni13Mo3 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 06Cr19Ni13Mo3 is seamless stainless steel pipe for fluid transport — standard higher-Mo austenitic seamless pipe for chloride fluid lines that need 317-class molybdenum. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr19Ni13Mo3, 06Cr17Ni12Mo2, 015Cr20Ni18Mo6CuN. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.