GB/T 14976 06Cr17Ni12Mo2N Seamless Stainless Steel Pipe

GB/T 14976 06Cr17Ni12Mo2N seamless stainless steel pipe (316N / UNS S31658, S31658), austenitic, Table 2 cast analysis, Rm min 550 MPa / Rp0.2 min 275 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr17Ni12Mo2N (S31658 / 316N / UNS S31658 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr17Ni12Mo2N Seamless Stainless Steel Pipe

Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 06Cr17Ni12Mo2N is the Table 2/3 Chinese grade name for this austenitic chemistry (S31658). When the stress calc outgrew 06Cr17Ni12Mo2 but the medium still fits Mo austenitic practice, GB/T 14976 06Cr17Ni12Mo2N is the governed Chinese choice.

Mill path for 06Cr17Ni12Mo2N: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr17Ni12Mo2N before production starts. Size practice for 06Cr17Ni12Mo2N remains W-H or W-C by wall; PA/PC tolerance class named on the order.

Body text may mention 316N / UNS S31658 (unified S31658) for cross-reference, but the H1 and order line stay on 06Cr17Ni12Mo2N. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints.

Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N, 06Cr19Ni13Mo3 before stretching surface finish or wall alone. Duty thread: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. Document the medium, design temperature, and weld map beside the 06Cr17Ni12Mo2N line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to 06Cr17Ni12Mo2N: 316/316L fillers; LN-aware heat input when N is specified on the base metal.

Inside this GB/T 14976 series, compare GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 022Cr17Ni12Mo2N, GB/T 14976 06Cr19Ni10N, GB/T 14976 06Cr19Ni13Mo3. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP316.

When 06Cr17Ni12Mo2N pipe sits beside plate on the same BOM, the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 06Cr17Ni12Mo2N. See also the GB/T 4237 hub for related plate designations. Confirm 06Cr17Ni12Mo2N OD × wall and plate thickness on separate drawings.

Chemical Composition of GB/T 14976 06Cr17Ni12Mo2N

Table 2 sets the melt limits for 06Cr17Ni12Mo2N. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 10.00–13.00, Cr 16.00–18.00, Mo 2.00–3.00. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 316N / UNS S31658. Every ladle analysis for 06Cr17Ni12Mo2N is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Corrosion framing beside 06Cr17Ni12Mo2N: tracks 06Cr17Ni12Mo2 aqueous ranking; N is a mechanical lever.

The composition table below is the cast window SHH STEEL quotes against for 06Cr17Ni12Mo2N. Edition framing is GB/T 14976-2025. Use thread: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr17Ni12Mo2N before the order is acknowledged. Size practice for 06Cr17Ni12Mo2N remains W-H or W-C by wall; PA/PC tolerance class named on the order.

Grade C Si Mn P S Ni Cr Mo N
06Cr17Ni12Mo2N ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 10.00–13.00 16.00–18.00 2.00–3.00 0.10–0.16

Mechanical Properties of GB/T 14976 06Cr17Ni12Mo2N

Table 3 mechanical acceptance for 06Cr17Ni12Mo2N: Rm min 550 MPa, Rp0.2 min 275 MPa, elongation longitudinal min 35% / transverse min 30%. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 06Cr17Ni12Mo2N. Tensile sampling follows the batch rules for the ordered test unit of 06Cr17Ni12Mo2N, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Corrosion framing beside 06Cr17Ni12Mo2N: tracks 06Cr17Ni12Mo2 aqueous ranking; N is a mechanical lever.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr17Ni12Mo2N 550 275 35 30

Ambient values from GB/T 14976-2025 Table 3 for 06Cr17Ni12Mo2N. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr17Ni12Mo2N

For 06Cr17Ni12Mo2N, the mill path is pierce/extrude/draw — never ERW or automatic-arc under GB/T 14976. Delivery is heat-treated and pickled unless overall ground/bored or bright protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Seamless W-C and W-H options remain available for 06Cr17Ni12Mo2N; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

After forming, 06Cr17Ni12Mo2N receives Table 1 treatment — 1010–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless.

Marking carries the grade 06Cr17Ni12Mo2N, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: W-H or W-C by wall; PA/PC tolerance class named on the order. Weld thread for fabricator joints: 316/316L fillers; LN-aware heat input when N is specified on the base metal. Hydrostatic pressure or NDT class for 06Cr17Ni12Mo2N is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 06Cr17Ni12Mo2N stays elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless.

Dimensions and Tolerances for GB/T 14976 06Cr17Ni12Mo2N

Dimensional order lines for 06Cr17Ni12Mo2N should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. Tolerance class (PA/PC) follows the precision ordered for 06Cr17Ni12Mo2N, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 06Cr17Ni12Mo2N: 316/316L fillers; LN-aware heat input when N is specified on the base metal.

OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints. Fixed lengths and multiple cut lengths for 06Cr17Ni12Mo2N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

Equivalent Grades for GB/T 14976 06Cr17Ni12Mo2N

Buyers searching under 316N / UNS S31658 still need the GB/T 14976 06Cr17Ni12Mo2N row locked on the acknowledgement. Inside austenitic practice the mechanical table and inspection clauses of GB/T 14976 control acceptance, not a brochure equivalent. Duty context: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

System Designation Notes
GB/T 14976 06Cr17Ni12Mo2N Governing pipe grade for this page
Commercial / UNS (body only) 316N / UNS S31658 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

We deliberately avoid inventing a false one-to-one for every foreign system on 06Cr17Ni12Mo2N. Use GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 022Cr17Ni12Mo2N, GB/T 14976 06Cr19Ni10N, GB/T 14976 06Cr19Ni13Mo3 for in-series alternatives, and keep GB/T 14976 as the category landing page. Dual marking is a purchase-order option that still requires every limit that matters for 06Cr17Ni12Mo2N to be verified on the heat.

Heat Treatment and Delivery Condition for GB/T 14976 06Cr17Ni12Mo2N

Mill heat treatment for 06Cr17Ni12Mo2N: 1010–1150 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 06Cr17Ni12Mo2N should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

Certificate wording for 06Cr17Ni12Mo2N should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. Field heat treatment of 06Cr17Ni12Mo2N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 06Cr17Ni12Mo2N stays elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless.

Corrosion Resistance of GB/T 14976 06Cr17Ni12Mo2N

tracks 06Cr17Ni12Mo2 aqueous ranking; N is a mechanical lever Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr17Ni12Mo2N unless the mark is one of the four carbon-floor exemptions. Coupon orientation, weld condition, and surface finish for 06Cr17Ni12Mo2N belong in the corrosion test order so annex results can be compared to the installed spool honestly. Keep the 06Cr17Ni12Mo2N caution visible here: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 06Cr17Ni12Mo2N honestly against 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N, 06Cr19Ni13Mo3. Role: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr17Ni12Mo2N rather than relying on wall thickness alone. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

Applications of GB/T 14976 06Cr17Ni12Mo2N Seamless Pipe

Typical BOM language pairs GB/T 14976 06Cr17Ni12Mo2N with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. Spool fabricators should copy 06Cr17Ni12Mo2N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

Spell 06Cr17Ni12Mo2N on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N, 06Cr19Ni13Mo3. Commissioning teams benefit when the as-built dossier repeats 06Cr17Ni12Mo2N beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 06Cr17Ni12Mo2N stays elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless.

Weldability of GB/T 14976 06Cr17Ni12Mo2N

Weldability of 06Cr17Ni12Mo2N follows austenitic practice. Filler/shop note: 316/316L fillers; LN-aware heat input when N is specified on the base metal. Caution: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints. Procedure qualification for 06Cr17Ni12Mo2N should use the same product form and wall class as production, including the seamless finish that will ship. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

For corrosive as-welded duty on 06Cr17Ni12Mo2N, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 316/316L fillers; LN-aware heat input when N is specified on the base metal. Consumable lot control and shielding-gas notes for 06Cr17Ni12Mo2N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 06Cr17Ni12Mo2N: 316/316L fillers; LN-aware heat input when N is specified on the base metal.

Surface Finishes for GB/T 14976 06Cr17Ni12Mo2N

06Cr17Ni12Mo2N under GB/T 14976 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (06Cr17Ni12Mo2N).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

When 06Cr17Ni12Mo2N ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless.

Inspection and Testing for GB/T 14976 06Cr17Ni12Mo2N

SHH STEEL reports the tests actually performed for 06Cr17Ni12Mo2N — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints. Sampling plans for 06Cr17Ni12Mo2N keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 06Cr17Ni12Mo2N remains W-H or W-C by wall; PA/PC tolerance class named on the order.

NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: W-H or W-C by wall; PA/PC tolerance class named on the order. Non-conforming 06Cr17Ni12Mo2N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 06Cr17Ni12Mo2N duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

Packaging and Shipping for GB/T 14976 06Cr17Ni12Mo2N

Export packing for GB/T 14976 06Cr17Ni12Mo2N is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. Bundle tickets for 06Cr17Ni12Mo2N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 06Cr17Ni12Mo2N stays elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 06Cr17Ni12Mo2N. Desiccant and wrap choices for 06Cr17Ni12Mo2N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 06Cr17Ni12Mo2N: tracks 06Cr17Ni12Mo2 aqueous ranking; N is a mechanical lever.

Photographic packing records are available on request for project QA files on 06Cr17Ni12Mo2N. Claims handling for 06Cr17Ni12Mo2N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 06Cr17Ni12Mo2N: tracks 06Cr17Ni12Mo2 aqueous ranking; N is a mechanical lever Claims handling for 06Cr17Ni12Mo2N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Order-line discipline for 06Cr17Ni12Mo2N still points at role: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines.

Why Choose SHH STEEL

Buyers choose SHH STEEL for 06Cr17Ni12Mo2N because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. SHH STEEL can produce and supply 06Cr17Ni12Mo2N against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 06Cr17Ni12Mo2N cleanly. Ask for a written acknowledgement that names 06Cr17Ni12Mo2N, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr17Ni12Mo2N to that written scope.

Supply Capability

Supply capability for 06Cr17Ni12Mo2N covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr17Ni12Mo2N when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr17Ni12Mo2N (S31658)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes for 06Cr17Ni12Mo2N: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: W-H or W-C by wall; PA/PC tolerance class named on the order. SHH STEEL can supply alternate walls and precision classes for 06Cr17Ni12Mo2N once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the 06Cr17Ni12Mo2N supply scope when the PO says so. Use: elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. SHH STEEL can produce trial lengths of 06Cr17Ni12Mo2N for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr17Ni12Mo2N seamless stainless steel pipe used for?
GB/T 14976 06Cr17Ni12Mo2N is seamless stainless pipe for fluid transport — elevated design-pressure process headers, weight-sensitive rack piping, and Chinese BOMs calling 316N seamless. Role summary: nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. It is a Chinese product standard grade (S31658), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr17Ni12Mo2N seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr17Ni12Mo2N when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr17Ni12Mo2N?
06Cr17Ni12Mo2N is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr17Ni12Mo2N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr17Ni12Mo2N compare with sister grades 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N?
06Cr17Ni12Mo2N is filed as austenitic. Typical sisters on the same RFQ are 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N. Design caution: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr17Ni12Mo2N?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316N / UNS S31658 the same as ordering 06Cr17Ni12Mo2N?
No. 316N / UNS S31658 is a commercial / UNS cross-walk for body text (unified S31658). The purchase order should lock GB/T 14976 and 06Cr17Ni12Mo2N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr17Ni12Mo2N?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr17Ni12Mo2N within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-H or W-C by wall; PA/PC tolerance class named on the order. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr17Ni12Mo2N be welded on site?
Shop guidance: 316/316L fillers; LN-aware heat input when N is specified on the base metal. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr17Ni12Mo2N?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: strength gain does not erase the carbon sensitisation caution — prefer 022Cr17Ni12Mo2N for corrosive as-welded joints Sister pointers: 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr17Ni12Mo2N with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr17Ni12Mo2N does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr17Ni12Mo2N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr17Ni12Mo2N?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr17Ni12Mo2N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr17Ni12Mo2N is seamless stainless steel pipe for fluid transport — nitrogen-strengthened standard-carbon Mo austenitic seamless pipe for higher-strength chloride fluid lines. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr17Ni12Mo2, 022Cr17Ni12Mo2N, 06Cr19Ni10N. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X