GB/T 14976 10Cr15 Seamless Stainless Steel Pipe

GB/T 14976 10Cr15 seamless stainless steel pipe (429-class / UNS S11510, S11510), ferritic, Table 2 cast analysis, Rm min 415 MPa / Rp0.2 min 240 MPa, annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
10Cr15 (S11510 / 429-class / UNS S11510 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 10Cr15 Seamless Stainless Steel Pipe

When the approved vendor list and isometric notes say GB/T 14976, the grade mark has to be the Chinese designation. 10Cr15 is the full product grade for this ferritic seamless pipe. GB/T 14976 10Cr15 fills the Chinese ferritic gap between 12Cr and 17Cr seamless fluid pipe without pretending it is an austenitic.

SHH STEEL can supply 10Cr15 seamless pipe in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the line: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks.

Equivalence talk to 429-class / UNS S11510 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 14976 10Cr15, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10.

Related ASTM pipe pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 10Cr17, 06Cr13, 06Cr13Al, 022Cr17NbTi. Use thread: mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. Document the medium, design temperature, and weld map beside the 10Cr15 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 10Cr15: higher Cr than 12Cr grades improves aqueous film stability in mild media; chlorides still constrain use.

Inside this GB/T 14976 series, compare GB/T 14976 10Cr17, GB/T 14976 06Cr13, GB/T 14976 06Cr13Al, GB/T 14976 022Cr17NbTi. Hub: GB/T 14976.

When 10Cr15 pipe sits beside plate on the same BOM, form hubs stay Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates — no verified plate product page is attached for this chemistry yet. Quote 10Cr15 pipe and plate under separate line items.

Chemical Composition of GB/T 14976 10Cr15

Chemistry control on 10Cr15 starts at the ladle. Expect C ≤0.12, Si ≤1.00, Mn ≤1.00, P ≤0.035, S ≤0.030, Ni ≤0.60, Cr 14.00–16.00 within Table 2, reported on the inspection document against the heat. Body alias 429-class / UNS S11510 does not widen those windows. Every ladle analysis for 10Cr15 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Corrosion framing beside 10Cr15: higher Cr than 12Cr grades improves aqueous film stability in mild media; chlorides still constrain use.

Read the table with the family in mind — ferritic — and with caution ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10. Numbers without the matching Table 1 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 10Cr15 before the order is acknowledged. Corrosion framing beside 10Cr15: higher Cr than 12Cr grades improves aqueous film stability in mild media; chlorides still constrain use.

Grade C Si Mn P S Ni Cr
10Cr15 ≤0.12 ≤1.00 ≤1.00 ≤0.035 ≤0.030 ≤0.60 14.00–16.00

Mechanical Properties of GB/T 14976 10Cr15

Proof stress and tensile minima for 10Cr15 sit at Rm min 415 MPa, Rp0.2 min 240 MPa, elongation longitudinal min 20% / transverse min 18%. Flattening or bend testing backs ductility when ordered. Watch-out: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10. Tensile sampling follows the batch rules for the ordered test unit of 10Cr15, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Weld-shop note tied to 10Cr15: 430-class lean practice; low heat input; PWHT when specified.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
10Cr15 415 240 20 18

Ambient values from GB/T 14976-2025 Table 3 for 10Cr15. Heat treatment (Table 1): 780–850 °C air or slow cool. Density 7.7 kg/dm³. Delivery: annealed.

Seamless Pipe Manufacture of GB/T 14976 10Cr15

SHH STEEL can produce 10Cr15 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 10Cr15; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Application context for 10Cr15 stays mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13.

Process control for 10Cr15 ends with verified heat treatment (780–850 °C air or slow cool) and surface conditioning. Ferritic heats follow Table 1 anneal bands with air or slow cool as listed — not austenitic solution practice. Do not copy 06Cr19Ni10 furnace charts onto ferritic marks. Pickling or bright-anneal decisions for 10Cr15 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Application context for 10Cr15 stays mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13.

Bevel geometry is by agreement when ordered without a drawing. Size practice: anneal 780–850 °C; W-C for thinner walls. Density for theoretical weight of 10Cr15: 7.7 kg/dm³ per Table 1. Hydrostatic pressure or NDT class for 10Cr15 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for 10Cr15 remains anneal 780–850 °C; W-C for thinner walls.

Dimensions and Tolerances for GB/T 14976 10Cr15

Usual length for GB/T 14976 pipe is 4000–12000 mm; fixed and multiple lengths sit inside that band with stated plus tolerances. For 10Cr15, confirm whether your project uses OD or ID ordering. Context: anneal 780–850 °C; W-C for thinner walls. Tolerance class (PA/PC) follows the precision ordered for 10Cr15, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for 10Cr15 stays mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13.

Full-length bend ≤0.15% of length; per-metre bend ≤1.5 mm (S≤15 mm) or ≤2.0 mm (S>15 mm). 10Cr15 must meet those geometry floors unless a written waiver exists. Fixed lengths and multiple cut lengths for 10Cr15 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 10Cr15: higher Cr than 12Cr grades improves aqueous film stability in mild media; chlorides still constrain use.

Equivalent Grades for GB/T 14976 10Cr15

Do not treat 429-class / UNS S11510 as interchangeable paperwork for GB/T 14976 10Cr15. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (10Cr15).

System Designation Notes
GB/T 14976 10Cr15 Governing pipe grade for this page
Commercial / UNS (body only) 429-class / UNS S11510 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

We deliberately avoid inventing a false one-to-one for every foreign system on 10Cr15. Use GB/T 14976 10Cr17, GB/T 14976 06Cr13, GB/T 14976 06Cr13Al, GB/T 14976 022Cr17NbTi for in-series alternatives, and keep GB/T 14976 as the category landing page. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (10Cr15).

Heat Treatment and Delivery Condition for GB/T 14976 10Cr15

Other heat-treatment schedules are allowed only by written agreement (6.3.4) — silence means Table 1 defaults. For 10Cr15: 780–850 °C air or slow cool. Recorded furnace charts for 10Cr15 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 10Cr15 duty: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks.

After local hot work in the field, restore annealed practice when the corrosion file demands it. Caution: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10. Field heat treatment of 10Cr15 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 10Cr15 duty: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks.

Corrosion Resistance of GB/T 14976 10Cr15

Pick tests that match how 10Cr15 is filed — ferritic. Corrosion thread: higher Cr than 12Cr grades improves aqueous film stability in mild media; chlorides still constrain use. Caution: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10. Coupon orientation, weld condition, and surface finish for 10Cr15 belong in the corrosion test order so annex results can be compared to the installed spool honestly. Weld-shop note tied to 10Cr15: 430-class lean practice; low heat input; PWHT when specified.

Oxygen-line Annex B and cryogenic Annex A add impact, UT, and cleanliness rules — they do not change the alloy selection logic. Use thread: mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 10Cr15 rather than relying on wall thickness alone. Size practice for 10Cr15 remains anneal 780–850 °C; W-C for thinner walls.

Applications of GB/T 14976 10Cr15 Seamless Pipe

Project types that repeatedly call 10Cr15: mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. Duty: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks. Caution still applies: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10.

Cryogenic, oxygen, and corrosive process lines all appear in 14976’s scope options — alloy choice still follows the medium. For this mark: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks. Commissioning teams benefit when the as-built dossier repeats 10Cr15 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 10Cr15 stays mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13.

Weldability of GB/T 14976 10Cr15

Even seamless W-C/W-H pipe of 10Cr15 will see field welds. Use: 430-class lean practice; low heat input; PWHT when specified. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 10Cr15 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 10Cr15 remains anneal 780–850 °C; W-C for thinner walls.

Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks. Consumable lot control and shielding-gas notes for 10Cr15 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 10Cr15 caution visible here: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10.

Surface Finishes for GB/T 14976 10Cr15

Pickled mill finish covers most RFQs for 10Cr15. Bright anneal, grind, or polish only when the enquiry writes a measurable target and names OD, ID, or both. Pack caution carried into finish control: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10.

Finish Typical supply Order note
Annealed and pickled Standard pipe mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; inspect before polish on ferritic stock
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

SHH STEEL sequences pickle, optional passivation, and any agreed polish for 10Cr15 after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long pipe life in the field. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (10Cr15).

Inspection and Testing for GB/T 14976 10Cr15

Batching rules limit pieces per heat/size/heat-treat lot. For 10Cr15, keep the heat identity unbroken from melt to bundle tag. Duty: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks. Sampling plans for 10Cr15 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 10Cr15 remains anneal 780–850 °C; W-C for thinner walls.

Intergranular corrosion testing is mandatory for most austenitics — see the IGC note for 10Cr15. Order extras (grain size, inclusions, elevated tensile) under 7.8.3 when needed. Non-conforming 10Cr15 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 10Cr15 remains anneal 780–850 °C; W-C for thinner walls.

Packaging and Shipping for GB/T 14976 10Cr15

Small-OD 10Cr15 often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. Bundle tickets for 10Cr15 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 10Cr15 caution visible here: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10.

Bevelled ends get protectors so landing edges survive trucking. Size hint: anneal 780–850 °C; W-C for thinner walls. Desiccant and wrap choices for 10Cr15 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 10Cr15: 430-class lean practice; low heat input; PWHT when specified.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. Claims handling for 10Cr15 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 10Cr15 stays mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13.

Why Choose SHH STEEL

Project teams working to Chinese fluid-transport specs need a supplier that reads Chinese grade names correctly. SHH STEEL can make 10Cr15 to that discipline. Caution we keep visible: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10. SHH STEEL can produce and supply 10Cr15 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (GB/T + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 10Cr17, 06Cr13, 06Cr13Al, 022Cr17NbTi. Ask for a written acknowledgement that names 10Cr15, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 10Cr15 to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of 10Cr15, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 10Cr15 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 10Cr15 (S11510)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes piercing/drawing slots for 10Cr15 rather than promising anonymous warehouse tons. Typical conversation starts around anneal 780–850 °C; W-C for thinner walls. SHH STEEL can supply alternate walls and precision classes for 10Cr15 once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate walls and PA/PC classes for 10Cr15 once design pressure and corrosion allowance are clear. Keep the 10Cr15 caution visible here: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10.

If the project needs dual GB/T 14976 + ASTM documentation, say so before melt. Caution: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10. SHH STEEL can produce trial lengths of 10Cr15 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 10Cr15 seamless stainless steel pipe used for?
GB/T 14976 10Cr15 is seamless stainless pipe for fluid transport — mild chemical drains, warm water lines, and Chinese ferritic fluid piping that needs more chromium than 06Cr13. Role summary: 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks. It is a Chinese product standard grade (S11510), not an automatic ASTM A312 certificate.
Is GB/T 14976 10Cr15 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 10Cr15 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 10Cr15?
10Cr15 is delivered annealed under GB/T 14976. Table 1 reference: 780–850 °C air or slow cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 10Cr15 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 10Cr15 compare with sister grades 10Cr17, 06Cr13, 06Cr13Al?
10Cr15 is filed as ferritic. Typical sisters on the same RFQ are 10Cr17, 06Cr13, 06Cr13Al. Design caution: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10 Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 10Cr15?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 429-class / UNS S11510 the same as ordering 10Cr15?
No. 429-class / UNS S11510 is a commercial / UNS cross-walk for body text (unified S11510). The purchase order should lock GB/T 14976 and 10Cr15 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 10Cr15?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 10Cr15 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: anneal 780–850 °C; W-C for thinner walls. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 10Cr15 be welded on site?
Shop guidance: 430-class lean practice; low heat input; PWHT when specified. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10
When should I choose a higher-Mo or superaustenitic grade instead of 10Cr15?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: ferritic toughness and weld grain growth limit wall and temperature — not a drop-in for austenitic 06Cr19Ni10 Sister pointers: 10Cr17, 06Cr13, 06Cr13Al. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 10Cr15 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 10Cr15 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 10Cr15 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 10Cr15?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 10Cr15 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 10Cr15 is seamless stainless steel pipe for fluid transport — 15% Cr ferritic seamless pipe for intermediate aqueous fluid service between 12Cr and 17Cr marks. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Cr17, 06Cr13, 06Cr13Al. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X