GB/T 14976 06Cr23Ni13 Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 06Cr23Ni13 Seamless Stainless Steel Pipe

GB/T 14976 06Cr23Ni13 seamless stainless steel pipe (309S / UNS S30908, S30908), austenitic, Table 2 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr23Ni13 (S30908 / 309S / UNS S30908 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr23Ni13 Seamless Stainless Steel Pipe

GB/T 14976-2025 is the Chinese national standard for seamless stainless steel pipes for fluid transport — replacing the 2012 edition and folding in prior LNG and oxygen-line tube GBs. Grade 06Cr23Ni13 (unified number S30908) sits in the austenitic set of Table 1. GB/T 14976 06Cr23Ni13 is the heat-facing step up from 06Cr19Ni10 when chromium alone — not molybdenum — is the missing alloying lever.

SHH STEEL can produce and supply GB/T 14976 06Cr23Ni13 as seamless W-C or W-H pipe across the enquiry OD×wall band, heat-treated per Table 1, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and Table 3 tensile results. Duty focus: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Shop language may still say “309S pipe,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 14976 and 06Cr23Ni13 so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters.

Scope discipline: 06Cr23Ni13 is seamless fluid-transport pipe under GB/T 14976, not a boiler tube under GB/T 13296 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti, 07Cr19Ni10. Role reminder: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Inside this GB/T 14976 series, compare GB/T 14976 06Cr25Ni20, GB/T 14976 06Cr19Ni10, GB/T 14976 06Cr18Ni11Ti, GB/T 14976 07Cr19Ni10. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP309S.

Chemical Composition of GB/T 14976 06Cr23Ni13

Cast analysis for GB/T 14976 06Cr23Ni13 follows Table 2. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 12.00–15.00, Cr 22.00–24.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 309S / UNS S30908; unified number S30908. Corrosion thread: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy this mark.

Chemical limits for 06Cr23Ni13 under GB/T 14976-2025 appear in the table underneath. Source priority is the 2025 Table 2 extract. If your client specification cites a 2012 footnote, send it before the heat is melted — phosphorus and several grade rows changed. Duty thread: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Grade C Si Mn P S Ni Cr
06Cr23Ni13 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 12.00–15.00 22.00–24.00

Mechanical Properties of GB/T 14976 06Cr23Ni13

Ambient tensile floors for 06Cr23Ni13 come from GB/T 14976 Table 3: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr23Ni13 520 205 35 30

Ambient values from GB/T 14976-2025 Table 3 for 06Cr23Ni13. Heat treatment (Table 1): 1030–1150 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr23Ni13

SHH STEEL can produce 06Cr23Ni13 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 06Cr23Ni13; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Corrosion framing beside 06Cr23Ni13: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy this mark.

Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Heat-treatment reference for 06Cr23Ni13: 1030–1150 °C, water or rapid cool. Pickling follows unless bright heat treatment or overall machining leaves a scale-free surface. Duty thread: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 06Cr23Ni13: hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs.

Dimensions and Tolerances for GB/T 14976 06Cr23Ni13

SHH STEEL aligns nominal OD (or ID), wall, length tolerance, and precision class (PA ordinary / PC higher) for 06Cr23Ni13 before the mill slot is locked. Dimensions follow GB/T 17395 unless otherwise agreed. Size hint: hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs. Tolerance class (PA/PC) follows the precision ordered for 06Cr23Ni13, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 06Cr23Ni13: 309/309L-class fillers; manage dilution when buttering carbon steel.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against GB/T 2102 so pickled finishes are not iron-stained in transit. Duty thread: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. Fixed lengths and multiple cut lengths for 06Cr23Ni13 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 06Cr23Ni13: 309/309L-class fillers; manage dilution when buttering carbon steel.

Equivalent Grades for GB/T 14976 06Cr23Ni13

For 06Cr23Ni13, start with identity under GB/T 14976 and only then walk commercial / UNS aliases. 309S / UNS S30908 is useful in body text; it is not the PO grade by itself. ASTM A312 related counterparts share a chemistry family at best — wall basis and NDT do not transfer by default.

System Designation Notes
GB/T 14976 06Cr23Ni13 Governing pipe grade for this page
Commercial / UNS (body only) 309S / UNS S30908 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related related chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Sister pages worth reading beside 06Cr23Ni13: GB/T 14976 06Cr25Ni20, GB/T 14976 06Cr19Ni10, GB/T 14976 06Cr18Ni11Ti, GB/T 14976 07Cr19Ni10. Duty locked here: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. Any EN or ASTM designation above is a starting point for comparison, not a substitute grade on the GB/T 14976 certificate. Series hub: GB/T 14976.

Heat Treatment and Delivery Condition for GB/T 14976 06Cr23Ni13

06Cr23Ni13 is delivered solution annealed under GB/T 14976. Table 1 reference: 1030–1150 °C, water or rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 309/309L-class fillers; manage dilution when buttering carbon steel. Recorded furnace charts for 06Cr23Ni13 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for 06Cr23Ni13 stays furnace exhaust stubs, thermal oxidiser interconnects, kiln transfer lines, and hot flue-gas fluid piping on Chinese specs.

Cooling type matters — austenitics need rapid cool after solution treatment; ferritic/martensitic anneal practice follows the air or slow-cool notes in Table 1. Duty thread: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. Density 7.98 kg/dm³ for weight calcs. Field heat treatment of 06Cr23Ni13 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr23Ni13: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy this mark.

Corrosion Resistance of GB/T 14976 06Cr23Ni13

Corrosion behaviour of GB/T 14976 06Cr23Ni13 tracks its austenitic balance: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy this mark. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr23Ni13 unless the mark is one of the four carbon-floor exemptions. Design caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 06Cr23Ni13 is filed as austenitic. Caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr23Ni13 rather than relying on wall thickness alone. Size practice for 06Cr23Ni13 remains hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs.

Applications of GB/T 14976 06Cr23Ni13 Seamless Pipe

Applications of GB/T 14976 06Cr23Ni13 seamless pipe centre on furnace exhaust stubs, thermal oxidiser interconnects, kiln transfer lines, and hot flue-gas fluid piping on Chinese specs. Role summary: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: furnace exhaust stubs, thermal oxidiser interconnects, kiln transfer lines, and hot flue-gas fluid piping on Chinese specs. Duty thread: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Weldability of GB/T 14976 06Cr23Ni13

06Cr23Ni13 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 309/309L-class fillers; manage dilution when buttering carbon steel. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 06Cr23Ni13 should use the same product form and wall class as production, including the seamless finish that will ship. This paragraph is locked to 06Cr23Ni13 duty: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic — not a single shop habit. Caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters. Consumable lot control and shielding-gas notes for 06Cr23Ni13 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 06Cr23Ni13 remains hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs.

Surface Finishes for GB/T 14976 06Cr23Ni13

For GB/T 14976 06Cr23Ni13, pickled finish after heat treatment is the usual mill supply for seamless stainless fluid-transport pipe: matte, scale-free, and ready for fabrication. Bright anneal or a ground/polished callout is available by agreement, but the order must name whether OD, ID, or both surfaces are in scope. Duty: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Bright or polished callouts for 06Cr23Ni13 never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GB/T 14976 pipe does not leave the yard with free-iron blooms. Caution retained: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters.

Inspection and Testing for GB/T 14976 06Cr23Ni13

Inspection for GB/T 14976 06Cr23Ni13 covers cast analysis, tensile tests, hydrostatic test (or replacing UT/ET), dimensions, appearance, and flattening/bend/flare when ordered. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr23Ni13 unless the mark is one of the four carbon-floor exemptions. Documents follow GB/T 2102 / purchaser-specified EN 10204 styles.

Marking includes 06Cr23Ni13, manufacturer, and other mandatory GB/T 2102 data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: furnace exhaust stubs, thermal oxidiser interconnects, kiln transfer lines, and hot flue-gas fluid piping on Chinese specs. Non-conforming 06Cr23Ni13 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 06Cr23Ni13 remains hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs.

Packaging and Shipping for GB/T 14976 06Cr23Ni13

Packaging for 06Cr23Ni13 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 06Cr23Ni13 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 06Cr23Ni13 stays furnace exhaust stubs, thermal oxidiser interconnects, kiln transfer lines, and hot flue-gas fluid piping on Chinese specs.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters. Desiccant and wrap choices for 06Cr23Ni13 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 06Cr23Ni13: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy this mark.

Shipping documents list GB/T 14976, 06Cr23Ni13, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. Claims handling for 06Cr23Ni13 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 06Cr23Ni13 remains hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 06Cr23Ni13 with the seamless route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless capacity covering W-C and W-H for this mark. Duty focus: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium.

Technical sales can map 06Cr23Ni13 against sisters 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti, 07Cr19Ni10 and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 06Cr23Ni13, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr23Ni13 to that written scope.

Supply Capability

SHH STEEL can produce and supply GB/T 14976 06Cr23Ni13 across enquiry-oriented OD × wall bands, in seamless W-C or W-H routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr23Ni13 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr23Ni13 (S30908)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

SHH STEEL can produce and supply GB/T 14976 06Cr23Ni13. Stock / Available sizes: enquiry band typically aligns with GB/T 17395 OD×wall practice, with PA or PC precision as ordered. For 06Cr23Ni13, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs.

Cut lengths, bevels, special NDT, IGC, and Annex A/B extras add lead time — call them early. Sisters often quoted alongside: 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti, 07Cr19Ni10. Email the size list to start. SHH STEEL can produce trial lengths of 06Cr23Ni13 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr23Ni13 seamless stainless steel pipe used for?
GB/T 14976 06Cr23Ni13 is seamless stainless pipe for fluid transport — furnace exhaust stubs, thermal oxidiser interconnects, kiln transfer lines, and hot flue-gas fluid piping on Chinese specs. Role summary: 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. It is a Chinese product standard grade (S30908), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr23Ni13 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr23Ni13 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr23Ni13?
06Cr23Ni13 is delivered solution annealed under GB/T 14976. Table 1 reference: 1030–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr23Ni13 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr23Ni13 compare with sister grades 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti?
06Cr23Ni13 is filed as austenitic. Typical sisters on the same RFQ are 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti. Design caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr23Ni13?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 309S / UNS S30908 the same as ordering 06Cr23Ni13?
No. 309S / UNS S30908 is a commercial / UNS cross-walk for body text (unified S30908). The purchase order should lock GB/T 14976 and 06Cr23Ni13 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr23Ni13?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr23Ni13 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: hot-finished W-H for thick heat-service walls; cold-drawn W-C for precision hot-gas stubs. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr23Ni13 be welded on site?
Shop guidance: 309/309L-class fillers; manage dilution when buttering carbon steel. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr23Ni13?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: oxidation duty is the mission — aqueous chloride process still wants Mo austenitic or superaustenitic sisters Sister pointers: 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr23Ni13 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr23Ni13 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr23Ni13 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr23Ni13?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr23Ni13 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr23Ni13 is seamless stainless steel pipe for fluid transport — 22Cr-13Ni austenitic seamless pipe for heat-facing and oxidation-lean fluid lines that outgrow 18-8 chromium. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr25Ni20, 06Cr19Ni10, 06Cr18Ni11Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X