GB/T 14976 06Cr25Ni20 Seamless Stainless Steel Pipe
What is GB/T 14976 06Cr25Ni20 Seamless Stainless Steel Pipe
Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 06Cr25Ni20 is the Table 2/3 Chinese grade name for this austenitic chemistry (S31008). GB/T 14976 06Cr25Ni20 is what Chinese heat-equipment fluid specs reach for when 06Cr23Ni13 still looks thin on chromium and nickel.
Mill path for 06Cr25Ni20: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs.
Body text may mention 310S / UNS S31008 (unified S31008) for cross-reference, but the H1 and order line stay on 06Cr25Ni20. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10, 07Cr19Ni10 before stretching surface finish or wall alone. Duty thread: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. Document the medium, design temperature, and weld map beside the 06Cr25Ni20 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for 06Cr25Ni20 stays radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs.
Inside this GB/T 14976 series, compare GB/T 14976 06Cr23Ni13, GB/T 14976 015Cr21Ni26Mo5Cu2, GB/T 14976 06Cr19Ni10, GB/T 14976 07Cr19Ni10. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP310S.
Buyers comparing 06Cr25Ni20 tubulars with sheet/plate can the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 3280 06Cr25Ni20. See also the GB/T 4237 hub for related plate designations. Do not stretch a 06Cr25Ni20 pipe certificate onto plate.
Chemical Composition of GB/T 14976 06Cr25Ni20
Table 2 sets the melt limits for 06Cr25Ni20. Highlight band: C ≤0.08, Si ≤1.50, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 19.00–22.00, Cr 24.00–26.00. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 310S / UNS S31008. Every ladle analysis for 06Cr25Ni20 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Corrosion framing beside 06Cr25Ni20: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is secondary.
The composition table below is the cast window SHH STEEL quotes against for 06Cr25Ni20. Edition framing is GB/T 14976-2025. Use thread: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr25Ni20 before the order is acknowledged. Size practice for 06Cr25Ni20 remains heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 06Cr25Ni20 | ≤0.08 | ≤1.50 | ≤2.00 | ≤0.035 | ≤0.030 | 19.00–22.00 | 24.00–26.00 |
Mechanical Properties of GB/T 14976 06Cr25Ni20
Table 3 mechanical acceptance for 06Cr25Ni20: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 06Cr25Ni20. Tensile sampling follows the batch rules for the ordered test unit of 06Cr25Ni20, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Size practice for 06Cr25Ni20 remains heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 06Cr25Ni20 | 520 | 205 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 06Cr25Ni20. Heat treatment (Table 1): 1030–1180 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 06Cr25Ni20
GB/T 14976 manufactures 06Cr25Ni20 as seamless pipe only — cold-rolled or cold-drawn (symbol W-C) or hot-rolled, extruded, forged or expanded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded pipe is outside this standard. Seamless W-C and W-H options remain available for 06Cr25Ni20; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Size practice for 06Cr25Ni20 remains heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD.
After forming, 06Cr25Ni20 receives Table 1 treatment — 1030–1180 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs.
Marking carries the grade 06Cr25Ni20, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD. Weld thread for fabricator joints: 310/310L fillers; control heat input on thick walls to limit hot cracking risk. Hydrostatic pressure or NDT class for 06Cr25Ni20 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for 06Cr25Ni20 remains heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD.
Dimensions and Tolerances for GB/T 14976 06Cr25Ni20
Dimensional order lines for 06Cr25Ni20 should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. Tolerance class (PA/PC) follows the precision ordered for 06Cr25Ni20, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 06Cr25Ni20: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is secondary.
OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. Fixed lengths and multiple cut lengths for 06Cr25Ni20 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 06Cr25Ni20 caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Equivalent Grades for GB/T 14976 06Cr25Ni20
Under GB/T 14976, 06Cr25Ni20 is the governing seamless stainless fluid-transport pipe designation on this page. Commercial shorthand such as 310S / UNS S31008 helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GB/T 14976 06Cr25Ni20 line. ASTM A312 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 06Cr25Ni20 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 310S / UNS S31008 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | related chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 06Cr25Ni20 still points at GB/T 14976, not the brochure alias. Neighbours GB/T 14976 06Cr23Ni13, GB/T 14976 015Cr21Ni26Mo5Cu2, GB/T 14976 06Cr19Ni10, GB/T 14976 07Cr19Ni10 each carry their own mechanical table. Category hub: GB/T 14976. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr25Ni20).
Heat Treatment and Delivery Condition for GB/T 14976 06Cr25Ni20
Mill heat treatment for 06Cr25Ni20: 1030–1180 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 06Cr25Ni20 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for 06Cr25Ni20 stays radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs.
Certificate wording for 06Cr25Ni20 should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. Field heat treatment of 06Cr25Ni20 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 06Cr25Ni20 stays radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs.
Corrosion Resistance of GB/T 14976 06Cr25Ni20
excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is secondary Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr25Ni20 unless the mark is one of the four carbon-floor exemptions.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 06Cr25Ni20 honestly against 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10, 07Cr19Ni10. Role: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr25Ni20 rather than relying on wall thickness alone. Keep the 06Cr25Ni20 caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Applications of GB/T 14976 06Cr25Ni20 Seamless Pipe
Typical BOM language pairs GB/T 14976 06Cr25Ni20 with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. Spool fabricators should copy 06Cr25Ni20 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 06Cr25Ni20 caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Spell 06Cr25Ni20 on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10, 07Cr19Ni10. Commissioning teams benefit when the as-built dossier repeats 06Cr25Ni20 beside heat numbers, linking isometric revisions to the same mill certificates. Keep the 06Cr25Ni20 caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Weldability of GB/T 14976 06Cr25Ni20
Weldability of 06Cr25Ni20 follows austenitic practice. Filler/shop note: 310/310L fillers; control heat input on thick walls to limit hot cracking risk. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. Procedure qualification for 06Cr25Ni20 should use the same product form and wall class as production, including the seamless finish that will ship. Corrosion framing beside 06Cr25Ni20: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is secondary.
For corrosive as-welded duty on 06Cr25Ni20, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 310/310L fillers; control heat input on thick walls to limit hot cracking risk. Consumable lot control and shielding-gas notes for 06Cr25Ni20 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 06Cr25Ni20 caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Surface Finishes for GB/T 14976 06Cr25Ni20
06Cr25Ni20 under GB/T 14976 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06Cr25Ni20.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
For 06Cr25Ni20, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (06Cr25Ni20).
Inspection and Testing for GB/T 14976 06Cr25Ni20
SHH STEEL reports the tests actually performed for 06Cr25Ni20 — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade. Sampling plans for 06Cr25Ni20 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 06Cr25Ni20 duty: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service.
NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD. Non-conforming 06Cr25Ni20 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Keep the 06Cr25Ni20 caution visible here: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade.
Packaging and Shipping for GB/T 14976 06Cr25Ni20
Export packing for GB/T 14976 06Cr25Ni20 is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. Bundle tickets for 06Cr25Ni20 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 06Cr25Ni20 stays radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 06Cr25Ni20. Desiccant and wrap choices for 06Cr25Ni20 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 06Cr25Ni20: 310/310L fillers; control heat input on thick walls to limit hot cracking risk.
Photographic packing records are available on request for project QA files on 06Cr25Ni20. Claims handling for 06Cr25Ni20 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 06Cr25Ni20: excellent high-temperature oxidation resistance from the high Cr-Ni balance; aqueous pitting is secondary.
Why Choose SHH STEEL
Buyers choose SHH STEEL for 06Cr25Ni20 because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. SHH STEEL can produce and supply 06Cr25Ni20 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 06Cr25Ni20 cleanly. Ask for a written acknowledgement that names 06Cr25Ni20, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr25Ni20 to that written scope.
Supply Capability
Supply capability for 06Cr25Ni20 covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr25Ni20 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 06Cr25Ni20 (S31008) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes for 06Cr25Ni20: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD. SHH STEEL can supply alternate walls and precision classes for 06Cr25Ni20 once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 06Cr25Ni20 supply scope when the PO says so. Use: radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. SHH STEEL can produce trial lengths of 06Cr25Ni20 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GB/T 14976 06Cr25Ni20 seamless stainless steel pipe used for?
- GB/T 14976 06Cr25Ni20 is seamless stainless pipe for fluid transport — radiant-adjacent hot gas lines, sulphur-bearing hot fluid transfer, cement kiln ducts, and high-temperature process heaters under Chinese fluid specs. Role summary: 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. It is a Chinese product standard grade (S31008), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 06Cr25Ni20 seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr25Ni20 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 06Cr25Ni20?
- 06Cr25Ni20 is delivered solution annealed under GB/T 14976. Table 1 reference: 1030–1180 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr25Ni20 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr25Ni20 compare with sister grades 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10?
- 06Cr25Ni20 is filed as austenitic. Typical sisters on the same RFQ are 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10. Design caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr25Ni20?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 310S / UNS S31008 the same as ordering 06Cr25Ni20?
- No. 310S / UNS S31008 is a commercial / UNS cross-walk for body text (unified S31008). The purchase order should lock GB/T 14976 and 06Cr25Ni20 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 06Cr25Ni20?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr25Ni20 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: heavy-wall W-H dominates furnace RFQs; W-C for smaller precision hot-service OD. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 06Cr25Ni20 be welded on site?
- Shop guidance: 310/310L fillers; control heat input on thick walls to limit hot cracking risk. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr25Ni20?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: sigma-phase risk on long isothermal holds still needs design attention; not a seawater process grade Sister pointers: 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 06Cr25Ni20 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr25Ni20 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr25Ni20 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 06Cr25Ni20?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr25Ni20 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 06Cr25Ni20 is seamless stainless steel pipe for fluid transport — 25Cr-20Ni austenitic seamless pipe for severe oxidation and carburising-lean hot fluid service. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr23Ni13, 015Cr21Ni26Mo5Cu2, 06Cr19Ni10. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.