GB/T 14976 06Cr19Ni10 Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 06Cr19Ni10 Seamless Stainless Steel Pipe

GB/T 14976 06Cr19Ni10 seamless stainless steel pipe (304 / UNS S30408, S30408), austenitic, Table 2 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr19Ni10 (S30408 / 304 / UNS S30408 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr19Ni10 Seamless Stainless Steel Pipe

Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 06Cr19Ni10 is the Table 2/3 Chinese grade name for this austenitic chemistry (S30408). When a Chinese project specification names GB/T 14976 and “06Cr19Ni10” rather than a vague “304 pipe”, the purchase order finally locks cast chemistry, heat treatment, and hydrostatic/NDT acceptance under one seamless product standard.

Mill path for 06Cr19Ni10: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

Body text may mention 304 / UNS S30408 (unified S30408) for cross-reference, but the H1 and order line stay on 06Cr19Ni10. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints.

Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 07Cr19Ni10 before stretching surface finish or wall alone. Duty thread: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified. Document the medium, design temperature, and weld map beside the 06Cr19Ni10 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the 06Cr19Ni10 caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints.

Inside this GB/T 14976 series, compare 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 07Cr19Ni10. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): A312 TP304.

Chemical Composition of GB/T 14976 06Cr19Ni10

Table 2 sets the melt limits for 06Cr19Ni10. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 304 / UNS S30408. Every ladle analysis for 06Cr19Ni10 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Application context for 06Cr19Ni10 stays plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

The composition table below is the cast window SHH STEEL quotes against for 06Cr19Ni10. Edition framing is GB/T 14976-2025. Use thread: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr19Ni10 before the order is acknowledged. Size practice for 06Cr19Ni10 remains common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules.

Grade C Si Mn P S Ni Cr
06Cr19Ni10 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 8.00–11.00 18.00–20.00

Mechanical Properties of GB/T 14976 06Cr19Ni10

Table 3 mechanical acceptance for 06Cr19Ni10: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 06Cr19Ni10. Tensile sampling follows the batch rules for the ordered test unit of 06Cr19Ni10, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Weld-shop note tied to 06Cr19Ni10: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr19Ni10 520 205 35 30

Ambient values from GB/T 14976-2025 Table 3 for 06Cr19Ni10. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.93 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr19Ni10

For 06Cr19Ni10, the mill path is pierce/extrude/draw — never ERW or automatic-arc under GB/T 14976. Delivery is heat-treated and pickled unless overall ground/bored or bright protective-atmosphere treatment allows omitting pickle. Order W-C or W-H explicitly when the purchaser cares which route ships. Seamless W-C and W-H options remain available for 06Cr19Ni10; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Corrosion framing beside 06Cr19Ni10: chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter.

After forming, 06Cr19Ni10 receives Table 1 treatment — 1010–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

Marking carries the grade 06Cr19Ni10, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules. Weld thread for fabricator joints: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Dimensions and Tolerances for GB/T 14976 06Cr19Ni10

Dimensional order lines for 06Cr19Ni10 should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”. Tolerance class (PA/PC) follows the precision ordered for 06Cr19Ni10, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for 06Cr19Ni10 stays plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints. Fixed lengths and multiple cut lengths for 06Cr19Ni10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 06Cr19Ni10 stays plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

Equivalent Grades for GB/T 14976 06Cr19Ni10

Lock 06Cr19Ni10 on the PO when the datasheet owner wants GB/T 14976 seamless stainless fluid-transport pipe. Commercial talk as 304 / UNS S30408 is fine in emails; mill paperwork must still show GB/T 14976 06Cr19Ni10. Application framing: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

System Designation Notes
GB/T 14976 06Cr19Ni10 Governing pipe grade for this page
Commercial / UNS (body only) 304 / UNS S30408 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related 304 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Inside this series compare 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 07Cr19Ni10 before swapping marks for medium or temperature. Keep this caution visible for 06Cr19Ni10: as-welded intergranular attack risk rises when cast carbon sits near the 0. Hub: GB/T 14976. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr19Ni10).

Heat Treatment and Delivery Condition for GB/T 14976 06Cr19Ni10

Mill heat treatment for 06Cr19Ni10: 1010–1150 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 06Cr19Ni10 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 06Cr19Ni10: chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter.

Certificate wording for 06Cr19Ni10 should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”. Field heat treatment of 06Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 06Cr19Ni10 remains common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules.

Corrosion Resistance of GB/T 14976 06Cr19Ni10

chromium-nickel passive film handles aqueous and mild chemical media; outdoor chloride pitting is usually the first limiter Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr19Ni10 unless the mark is one of the four carbon-floor exemptions.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 06Cr19Ni10 honestly against 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 07Cr19Ni10. Role: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr19Ni10 rather than relying on wall thickness alone. Application context for 06Cr19Ni10 stays plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

Applications of GB/T 14976 06Cr19Ni10 Seamless Pipe

Typical BOM language pairs GB/T 14976 06Cr19Ni10 with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”. Spool fabricators should copy 06Cr19Ni10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 06Cr19Ni10 caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints.

Spell 06Cr19Ni10 on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 07Cr19Ni10. Commissioning teams benefit when the as-built dossier repeats 06Cr19Ni10 beside heat numbers, linking isometric revisions to the same mill certificates. Keep the 06Cr19Ni10 caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints.

Weldability of GB/T 14976 06Cr19Ni10

Weldability of 06Cr19Ni10 follows austenitic practice. Filler/shop note: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints. Procedure qualification for 06Cr19Ni10 should use the same product form and wall class as production, including the seamless finish that will ship. Weld-shop note tied to 06Cr19Ni10: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

For corrosive as-welded duty on 06Cr19Ni10, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium. Consumable lot control and shielding-gas notes for 06Cr19Ni10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 06Cr19Ni10 remains common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules.

Surface Finishes for GB/T 14976 06Cr19Ni10

Welded or heavily formed 06Cr19Ni10 may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 14976 seamless stainless fluid-transport pipe. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

For 06Cr19Ni10, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 06Cr19Ni10.

Inspection and Testing for GB/T 14976 06Cr19Ni10

SHH STEEL reports the tests actually performed for 06Cr19Ni10 — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints. Sampling plans for 06Cr19Ni10 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 06Cr19Ni10 remains common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules.

NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules. Non-conforming 06Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified.

Packaging and Shipping for GB/T 14976 06Cr19Ni10

Export packing for GB/T 14976 06Cr19Ni10 is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified. Bundle tickets for 06Cr19Ni10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 06Cr19Ni10: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 06Cr19Ni10. Desiccant and wrap choices for 06Cr19Ni10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 06Cr19Ni10 duty: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified.

Photographic packing records are available on request for project QA files on 06Cr19Ni10. Claims handling for 06Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 06Cr19Ni10 caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 06Cr19Ni10. Buyers choose SHH STEEL for 06Cr19Ni10 because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 06Cr19Ni10 cleanly. Ask for a written acknowledgement that names 06Cr19Ni10, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr19Ni10 to that written scope.

Supply Capability

Supply capability for 06Cr19Ni10 covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr19Ni10 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr19Ni10 (S30408)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes for 06Cr19Ni10: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules. SHH STEEL can supply alternate walls and precision classes for 06Cr19Ni10 once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the 06Cr19Ni10 supply scope when the PO says so. Use: plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”. SHH STEEL can produce trial lengths of 06Cr19Ni10 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr19Ni10 seamless stainless steel pipe used for?
GB/T 14976 06Cr19Ni10 is seamless stainless pipe for fluid transport — plant utility water, food and beverage transfer, HVAC condensate, fire-water rings, and general process lines that still say “304 seamless”. Role summary: workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified. It is a Chinese product standard grade (S30408), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr19Ni10 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr19Ni10 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr19Ni10?
06Cr19Ni10 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr19Ni10 compare with sister grades 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti?
06Cr19Ni10 is filed as austenitic. Typical sisters on the same RFQ are 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti. Design caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr19Ni10?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 304 / UNS S30408 the same as ordering 06Cr19Ni10?
No. 304 / UNS S30408 is a commercial / UNS cross-walk for body text (unified S30408). The purchase order should lock GB/T 14976 and 06Cr19Ni10 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr19Ni10?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr19Ni10 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: common enquiry band mid-bore OD×wall under GB/T 17395; W-C for tight OD, W-H for heavier schedules. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr19Ni10 be welded on site?
Shop guidance: 308/308L-class fillers; control heat input on non-L heats when the joint stays in a corrosive medium. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr19Ni10?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer 022Cr19Ni10 or a stabilised sister for corrosive welded joints Sister pointers: 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr19Ni10 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr19Ni10 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr19Ni10?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr19Ni10 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr19Ni10 is seamless stainless steel pipe for fluid transport — workhorse 18-8 austenitic seamless pipe for Chinese fluid-transport specs where molybdenum is not justified. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr19Ni10, 06Cr17Ni12Mo2, 06Cr18Ni11Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response