GB/T 14976 022Cr19Ni10N Seamless Stainless Steel Pipe

GB/T 14976 022Cr19Ni10N seamless stainless steel pipe (304LN / UNS S30453, S30453), austenitic, Table 2 cast analysis, Rm min 550 MPa / Rp0.2 min 245 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
022Cr19Ni10N (S30453 / 304LN / UNS S30453 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 022Cr19Ni10N Seamless Stainless Steel Pipe

Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 022Cr19Ni10N is the Table 2/3 Chinese grade name for this austenitic chemistry (S30453). GB/T 14976 022Cr19Ni10N is the Chinese mark for buyers who need 304LN-class strength without inventing a non-standard nitrogen add on plain 022Cr19Ni10.

Mill path for 022Cr19Ni10N: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour.

Body text may mention 304LN / UNS S30453 (unified S30453) for cross-reference, but the H1 and order line stay on 022Cr19Ni10N. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric.

Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N, 06Cr19Ni9NbN before stretching surface finish or wall alone. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. Document the medium, design temperature, and weld map beside the 022Cr19Ni10N line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for 022Cr19Ni10N remains cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing.

Inside this GB/T 14976 series, compare 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N, 06Cr19Ni9NbN. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): A312 TP304L.

Chemical Composition of GB/T 14976 022Cr19Ni10N

Table 2 sets the melt limits for 022Cr19Ni10N. Highlight band: C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00, N 0.10–0.16. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 304LN / UNS S30453. Every ladle analysis for 022Cr19Ni10N is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Weld-shop note tied to 022Cr19Ni10N: 308L fillers; watch nitrogen pickup/loss in the weld pool and keep procedures matched to LN base metal.

The composition table below is the cast window SHH STEEL quotes against for 022Cr19Ni10N. Edition framing is GB/T 14976-2025. Use thread: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 022Cr19Ni10N before the order is acknowledged. Weld-shop note tied to 022Cr19Ni10N: 308L fillers; watch nitrogen pickup/loss in the weld pool and keep procedures matched to LN base metal.

Grade C Si Mn P S Ni Cr N
022Cr19Ni10N ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.030 8.00–11.00 18.00–20.00 0.10–0.16

Mechanical Properties of GB/T 14976 022Cr19Ni10N

Table 3 mechanical acceptance for 022Cr19Ni10N: Rm min 550 MPa, Rp0.2 min 245 MPa, elongation longitudinal min 35% / transverse min 30%. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 022Cr19Ni10N. Tensile sampling follows the batch rules for the ordered test unit of 022Cr19Ni10N, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Keep the 022Cr19Ni10N caution visible here: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
022Cr19Ni10N 550 245 35 30

Ambient values from GB/T 14976-2025 Table 3 for 022Cr19Ni10N. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.93 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 022Cr19Ni10N

GB/T 14976 manufactures 022Cr19Ni10N as seamless pipe only — cold-rolled or cold-drawn (symbol W-C) or hot-rolled, extruded, forged or expanded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded pipe is outside this standard. Seamless W-C and W-H options remain available for 022Cr19Ni10N; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. This paragraph is locked to 022Cr19Ni10N duty: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades.

After forming, 022Cr19Ni10N receives Table 1 treatment — 1010–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour.

Marking carries the grade 022Cr19Ni10N, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing. Weld thread for fabricator joints: 308L fillers; watch nitrogen pickup/loss in the weld pool and keep procedures matched to LN base metal. Hydrostatic pressure or NDT class for 022Cr19Ni10N is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 022Cr19Ni10N caution visible here: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric.

Dimensions and Tolerances for GB/T 14976 022Cr19Ni10N

Dimensional order lines for 022Cr19Ni10N should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour. Tolerance class (PA/PC) follows the precision ordered for 022Cr19Ni10N, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for 022Cr19Ni10N stays higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour.

OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric. Fixed lengths and multiple cut lengths for 022Cr19Ni10N are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 022Cr19Ni10N duty: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades.

Equivalent Grades for GB/T 14976 022Cr19Ni10N

Identity first: GB/T 14976 022Cr19Ni10N is the HX/pipe grade for this page. 304LN / UNS S30453 helps buyers who think in AISI/UNS labels. Role: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. Foreign product standards remain separate documents.

System Designation Notes
GB/T 14976 022Cr19Ni10N Governing pipe grade for this page
Commercial / UNS (body only) 304LN / UNS S30453 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Inside this series compare 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N, 06Cr19Ni9NbN before swapping marks for medium or temperature. Confirm chemistry windows on the 022Cr19Ni10N MTC before dual-cert claims. Hub: GB/T 14976. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (022Cr19Ni10N).

Heat Treatment and Delivery Condition for GB/T 14976 022Cr19Ni10N

Mill heat treatment for 022Cr19Ni10N: 1010–1150 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 022Cr19Ni10N should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 022Cr19Ni10N: corrosion ranking stays Mo-free 18-8; the N addition is a strength lever, not a chloride fix.

Certificate wording for 022Cr19Ni10N should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour. Field heat treatment of 022Cr19Ni10N after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 022Cr19Ni10N remains cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing.

Corrosion Resistance of GB/T 14976 022Cr19Ni10N

corrosion ranking stays Mo-free 18-8; the N addition is a strength lever, not a chloride fix Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 022Cr19Ni10N unless the mark is one of the four carbon-floor exemptions.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 022Cr19Ni10N honestly against 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N, 06Cr19Ni9NbN. Role: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr19Ni10N rather than relying on wall thickness alone. Size practice for 022Cr19Ni10N remains cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing.

Applications of GB/T 14976 022Cr19Ni10N Seamless Pipe

Typical BOM language pairs GB/T 14976 022Cr19Ni10N with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour. Spool fabricators should copy 022Cr19Ni10N onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 022Cr19Ni10N: corrosion ranking stays Mo-free 18-8; the N addition is a strength lever, not a chloride fix.

Spell 022Cr19Ni10N on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N, 06Cr19Ni9NbN. Commissioning teams benefit when the as-built dossier repeats 022Cr19Ni10N beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 022Cr19Ni10N remains cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing.

Weldability of GB/T 14976 022Cr19Ni10N

Weldability of 022Cr19Ni10N follows austenitic practice. Filler/shop note: 308L fillers; watch nitrogen pickup/loss in the weld pool and keep procedures matched to LN base metal. Caution: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric. Procedure qualification for 022Cr19Ni10N should use the same product form and wall class as production, including the seamless finish that will ship. This paragraph is locked to 022Cr19Ni10N duty: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades.

For corrosive as-welded duty on 022Cr19Ni10N, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 308L fillers; watch nitrogen pickup/loss in the weld pool and keep procedures matched to LN base metal. Consumable lot control and shielding-gas notes for 022Cr19Ni10N stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for 022Cr19Ni10N stays higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour.

Surface Finishes for GB/T 14976 022Cr19Ni10N

Finish options for 022Cr19Ni10N follow the ordered heat-treatment route under GB/T 14976. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution annealed. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 022Cr19Ni10N.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

For 022Cr19Ni10N, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 022Cr19Ni10N.

Inspection and Testing for GB/T 14976 022Cr19Ni10N

SHH STEEL reports the tests actually performed for 022Cr19Ni10N — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric. Sampling plans for 022Cr19Ni10N keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 022Cr19Ni10N caution visible here: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric.

NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing. Non-conforming 022Cr19Ni10N lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Keep the 022Cr19Ni10N caution visible here: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric.

Packaging and Shipping for GB/T 14976 022Cr19Ni10N

Export packing for GB/T 14976 022Cr19Ni10N is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. Bundle tickets for 022Cr19Ni10N repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 022Cr19Ni10N: corrosion ranking stays Mo-free 18-8; the N addition is a strength lever, not a chloride fix.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 022Cr19Ni10N. Desiccant and wrap choices for 022Cr19Ni10N follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 022Cr19Ni10N: corrosion ranking stays Mo-free 18-8; the N addition is a strength lever, not a chloride fix.

Photographic packing records are available on request for project QA files on 022Cr19Ni10N. Claims handling for 022Cr19Ni10N starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 022Cr19Ni10N: corrosion ranking stays Mo-free 18-8; the N addition is a strength lever, not a chloride fix.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 022Cr19Ni10N. Buyers choose SHH STEEL for 022Cr19Ni10N because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 022Cr19Ni10N cleanly. Ask for a written acknowledgement that names 022Cr19Ni10N, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 022Cr19Ni10N to that written scope.

Supply Capability

Supply capability for 022Cr19Ni10N covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 022Cr19Ni10N when the mill schedule allows. Size practice for 022Cr19Ni10N remains cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 022Cr19Ni10N (S30453)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes for 022Cr19Ni10N: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing. SHH STEEL can supply alternate walls and precision classes for 022Cr19Ni10N once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the 022Cr19Ni10N supply scope when the PO says so. Use: higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour. SHH STEEL can produce trial lengths of 022Cr19Ni10N for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 022Cr19Ni10N seamless stainless steel pipe used for?
GB/T 14976 022Cr19Ni10N is seamless stainless pipe for fluid transport — higher-pressure utility headers, structural-lean fluid racks, cryogenic-adjacent transfer under Annex A options, and welded lines that still want 304L corrosion behaviour. Role summary: nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. It is a Chinese product standard grade (S30453), not an automatic ASTM A312 certificate.
Is GB/T 14976 022Cr19Ni10N seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr19Ni10N when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 022Cr19Ni10N?
022Cr19Ni10N is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 022Cr19Ni10N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 022Cr19Ni10N compare with sister grades 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N?
022Cr19Ni10N is filed as austenitic. Typical sisters on the same RFQ are 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N. Design caution: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 022Cr19Ni10N?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 304LN / UNS S30453 the same as ordering 022Cr19Ni10N?
No. 304LN / UNS S30453 is a commercial / UNS cross-walk for body text (unified S30453). The purchase order should lock GB/T 14976 and 022Cr19Ni10N so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 022Cr19Ni10N?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr19Ni10N within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: cold-drawn W-C for pressure-critical mid-bore; W-H when wall and tonnage favour hot finishing. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 022Cr19Ni10N be welded on site?
Shop guidance: 308L fillers; watch nitrogen pickup/loss in the weld pool and keep procedures matched to LN base metal. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr19Ni10N?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: nitrogen 0.10–0.16% raises strength — confirm the Table 3 floors before swapping plain 022Cr19Ni10 into the same isometric Sister pointers: 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 022Cr19Ni10N with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 022Cr19Ni10N does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 022Cr19Ni10N so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 022Cr19Ni10N?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr19Ni10N when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 022Cr19Ni10N is seamless stainless steel pipe for fluid transport — nitrogen-strengthened low-carbon 18-8 seamless pipe when design needs higher proof stress without jumping to Mo grades. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr19Ni10, 06Cr19Ni10N, 022Cr17Ni12Mo2N. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response