GB/T 14976 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Pipe

GB/T 14976 06Cr18Ni12Mo2Cu2 seamless stainless steel pipe (316Cu-class / UNS S31688, S31688), austenitic, Table 2 cast analysis, Rm min 520 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr18Ni12Mo2Cu2 (S31688 / 316Cu-class / UNS S31688 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr18Ni12Mo2Cu2 Seamless Stainless Steel Pipe

GB/T 14976-2025 is the Chinese national standard for seamless stainless steel pipes for fluid transport — replacing the 2012 edition and folding in prior LNG and oxygen-line tube GBs. Grade 06Cr18Ni12Mo2Cu2 (unified number S31688) sits in the austenitic set of Table 1. If the process medium needs copper and molybdenum together under a Chinese seamless fluid standard, GB/T 14976 06Cr18Ni12Mo2Cu2 is the governed mark.

SHH STEEL can produce and supply GB/T 14976 06Cr18Ni12Mo2Cu2 as seamless W-C or W-H pipe across the enquiry OD×wall band, heat-treated per Table 1, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and Table 3 tensile results. Duty focus: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

Shop language may still say “316Cu-class pipe,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 14976 and 06Cr18Ni12Mo2Cu2 so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate.

Scope discipline: 06Cr18Ni12Mo2Cu2 is seamless fluid-transport pipe under GB/T 14976, not a boiler tube under GB/T 13296 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3, 015Cr21Ni26Mo5Cu2. Role reminder: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

Inside this GB/T 14976 series, compare GB/T 14976 022Cr18Ni14Mo2Cu2, GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 06Cr19Ni13Mo3, GB/T 14976 015Cr21Ni26Mo5Cu2. Hub: GB/T 14976.

Project teams specifying 06Cr18Ni12Mo2Cu2 should the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 06Cr18Ni12Mo2Cu2. Confirm 06Cr18Ni12Mo2Cu2 OD × wall and plate thickness on separate drawings.

Chemical Composition of GB/T 14976 06Cr18Ni12Mo2Cu2

Cast analysis for GB/T 14976 06Cr18Ni12Mo2Cu2 follows Table 2. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 10.00–14.00, Cr 16.00–18.00, Mo 1.20–2.75. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 316Cu-class / UNS S31688; unified number S31688. Corrosion thread: Cu + Mo target reducing acids; do not market as a universal chloride upgrade over 317L.

Chemical limits for 06Cr18Ni12Mo2Cu2 under GB/T 14976-2025 appear in the table underneath. Source priority is the 2025 Table 2 extract. If your client specification cites a 2012 footnote, send it before the heat is melted — phosphorus and several grade rows changed. Duty thread: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

Grade C Si Mn P S Ni Cr Mo Cu
06Cr18Ni12Mo2Cu2 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 10.00–14.00 16.00–18.00 1.20–2.75 1.00–2.50

Mechanical Properties of GB/T 14976 06Cr18Ni12Mo2Cu2

Ambient tensile floors for 06Cr18Ni12Mo2Cu2 come from GB/T 14976 Table 3: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr18Ni12Mo2Cu2 520 205 35 30

Ambient values from GB/T 14976-2025 Table 3 for 06Cr18Ni12Mo2Cu2. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr18Ni12Mo2Cu2

Seamless is not optional wording for 06Cr18Ni12Mo2Cu2: clause 6.2 limits manufacture to W-C or W-H seamless routes. Pick W-C when OD precision and surface finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 14976 line item. Seamless W-C and W-H options remain available for 06Cr18Ni12Mo2Cu2; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Weld-shop note tied to 06Cr18Ni12Mo2Cu2: Cu-bearing austenitic fillers; heat-input discipline on standard-carbon heats.

Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Heat-treatment reference for 06Cr18Ni12Mo2Cu2: 1010–1150 °C, water or rapid cool. Pickling follows unless bright heat treatment or overall machining leaves a scale-free surface. Duty thread: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 06Cr18Ni12Mo2Cu2: W-H for heavier acid-line walls; W-C when ID finish matters.

Dimensions and Tolerances for GB/T 14976 06Cr18Ni12Mo2Cu2

SHH STEEL aligns nominal OD (or ID), wall, length tolerance, and precision class (PA ordinary / PC higher) for 06Cr18Ni12Mo2Cu2 before the mill slot is locked. Dimensions follow GB/T 17395 unless otherwise agreed. Size hint: W-H for heavier acid-line walls; W-C when ID finish matters. Tolerance class (PA/PC) follows the precision ordered for 06Cr18Ni12Mo2Cu2, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 06Cr18Ni12Mo2Cu2 caution visible here: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against GB/T 2102 so pickled finishes are not iron-stained in transit. Duty thread: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy. Fixed lengths and multiple cut lengths for 06Cr18Ni12Mo2Cu2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 06Cr18Ni12Mo2Cu2 caution visible here: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate.

Equivalent Grades for GB/T 14976 06Cr18Ni12Mo2Cu2

06Cr18Ni12Mo2Cu2 is the GB/T 14976 designation for this seamless stainless fluid-transport pipe. Alias 316Cu-class / UNS S31688 appears only as a cross-walk. When a dual-cert path is required, list both GB/T 14976 06Cr18Ni12Mo2Cu2 and the foreign mark with separate scopes instead of assuming one chemistry line clears both files.

System Designation Notes
GB/T 14976 06Cr18Ni12Mo2Cu2 Governing pipe grade for this page
Commercial / UNS (body only) 316Cu-class / UNS S31688 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

We deliberately avoid inventing a false one-to-one for every foreign system on 06Cr18Ni12Mo2Cu2. Use GB/T 14976 022Cr18Ni14Mo2Cu2, GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 06Cr19Ni13Mo3, GB/T 14976 015Cr21Ni26Mo5Cu2 for in-series alternatives, and keep GB/T 14976 as the category landing page. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr18Ni12Mo2Cu2).

Heat Treatment and Delivery Condition for GB/T 14976 06Cr18Ni12Mo2Cu2

06Cr18Ni12Mo2Cu2 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: Cu-bearing austenitic fillers; heat-input discipline on standard-carbon heats. Recorded furnace charts for 06Cr18Ni12Mo2Cu2 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 06Cr18Ni12Mo2Cu2 duty: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

Cooling type matters — austenitics need rapid cool after solution treatment; ferritic/martensitic anneal practice follows the air or slow-cool notes in Table 1. Duty thread: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy. Density 7.98 kg/dm³ for weight calcs. Field heat treatment of 06Cr18Ni12Mo2Cu2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 06Cr18Ni12Mo2Cu2: Cu + Mo target reducing acids; do not market as a universal chloride upgrade over 317L.

Corrosion Resistance of GB/T 14976 06Cr18Ni12Mo2Cu2

Corrosion behaviour of GB/T 14976 06Cr18Ni12Mo2Cu2 tracks its austenitic balance: Cu + Mo target reducing acids; do not market as a universal chloride upgrade over 317L. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni12Mo2Cu2 unless the mark is one of the four carbon-floor exemptions. Design caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 06Cr18Ni12Mo2Cu2 is filed as austenitic. Caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr18Ni12Mo2Cu2 rather than relying on wall thickness alone. Size practice for 06Cr18Ni12Mo2Cu2 remains W-H for heavier acid-line walls; W-C when ID finish matters.

Applications of GB/T 14976 06Cr18Ni12Mo2Cu2 Seamless Pipe

Applications of GB/T 14976 06Cr18Ni12Mo2Cu2 seamless pipe centre on sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry. Role summary: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry. Duty thread: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

Weldability of GB/T 14976 06Cr18Ni12Mo2Cu2

06Cr18Ni12Mo2Cu2 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: Cu-bearing austenitic fillers; heat-input discipline on standard-carbon heats. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 06Cr18Ni12Mo2Cu2 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr18Ni12Mo2Cu2 caution visible here: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic — not a single shop habit. Caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate. Consumable lot control and shielding-gas notes for 06Cr18Ni12Mo2Cu2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 06Cr18Ni12Mo2Cu2: Cu + Mo target reducing acids; do not market as a universal chloride upgrade over 317L.

Surface Finishes for GB/T 14976 06Cr18Ni12Mo2Cu2

Typical GB/T 14976 supply for 06Cr18Ni12Mo2Cu2 is a clean pickle after the required heat treatment, with bright anneal reserved for scale-free OD/ID appearance and ground/polished finishes reserved for written roughness targets. Use case colour: sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry. Free-iron control starts at the finishing bay, not at commissioning.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Do not polish over unresolved defects on 06Cr18Ni12Mo2Cu2; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GB/T 14976 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 06Cr18Ni12Mo2Cu2.

Inspection and Testing for GB/T 14976 06Cr18Ni12Mo2Cu2

Inspection for GB/T 14976 06Cr18Ni12Mo2Cu2 covers cast analysis, tensile tests, hydrostatic test (or replacing UT/ET), dimensions, appearance, and flattening/bend/flare when ordered. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 06Cr18Ni12Mo2Cu2 unless the mark is one of the four carbon-floor exemptions. Documents follow GB/T 2102 / purchaser-specified EN 10204 styles.

Marking includes 06Cr18Ni12Mo2Cu2, manufacturer, and other mandatory GB/T 2102 data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry. Non-conforming 06Cr18Ni12Mo2Cu2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Corrosion framing beside 06Cr18Ni12Mo2Cu2: Cu + Mo target reducing acids; do not market as a universal chloride upgrade over 317L.

Packaging and Shipping for GB/T 14976 06Cr18Ni12Mo2Cu2

Packaging for 06Cr18Ni12Mo2Cu2 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 06Cr18Ni12Mo2Cu2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 06Cr18Ni12Mo2Cu2: Cu-bearing austenitic fillers; heat-input discipline on standard-carbon heats.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate. Desiccant and wrap choices for 06Cr18Ni12Mo2Cu2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 06Cr18Ni12Mo2Cu2 stays sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry.

Shipping documents list GB/T 14976, 06Cr18Ni12Mo2Cu2, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy. Claims handling for 06Cr18Ni12Mo2Cu2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 06Cr18Ni12Mo2Cu2 stays sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 06Cr18Ni12Mo2Cu2 with the seamless route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless capacity covering W-C and W-H for this mark. Duty focus: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy.

Technical sales can map 06Cr18Ni12Mo2Cu2 against sisters 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3, 015Cr21Ni26Mo5Cu2 and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 06Cr18Ni12Mo2Cu2, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr18Ni12Mo2Cu2 to that written scope.

Supply Capability

SHH STEEL can produce and supply GB/T 14976 06Cr18Ni12Mo2Cu2 across enquiry-oriented OD × wall bands, in seamless W-C or W-H routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr18Ni12Mo2Cu2 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr18Ni12Mo2Cu2 (S31688)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

SHH STEEL can produce and supply GB/T 14976 06Cr18Ni12Mo2Cu2. Stock / Available sizes: enquiry band typically aligns with GB/T 17395 OD×wall practice, with PA or PC precision as ordered. For 06Cr18Ni12Mo2Cu2, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: W-H for heavier acid-line walls; W-C when ID finish matters.

Cut lengths, bevels, special NDT, IGC, and Annex A/B extras add lead time — call them early. Sisters often quoted alongside: 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3, 015Cr21Ni26Mo5Cu2. Email the size list to start. SHH STEEL can produce trial lengths of 06Cr18Ni12Mo2Cu2 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr18Ni12Mo2Cu2 seamless stainless steel pipe used for?
GB/T 14976 06Cr18Ni12Mo2Cu2 is seamless stainless pipe for fluid transport — sulphuric-lean process headers, fertiliser fluid lines, and Chinese acid-service BOMs that call Cu-bearing 316-class chemistry. Role summary: standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy. It is a Chinese product standard grade (S31688), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr18Ni12Mo2Cu2 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr18Ni12Mo2Cu2 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr18Ni12Mo2Cu2?
06Cr18Ni12Mo2Cu2 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr18Ni12Mo2Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr18Ni12Mo2Cu2 compare with sister grades 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3?
06Cr18Ni12Mo2Cu2 is filed as austenitic. Typical sisters on the same RFQ are 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3. Design caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr18Ni12Mo2Cu2?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316Cu-class / UNS S31688 the same as ordering 06Cr18Ni12Mo2Cu2?
No. 316Cu-class / UNS S31688 is a commercial / UNS cross-walk for body text (unified S31688). The purchase order should lock GB/T 14976 and 06Cr18Ni12Mo2Cu2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr18Ni12Mo2Cu2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr18Ni12Mo2Cu2 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-H for heavier acid-line walls; W-C when ID finish matters. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr18Ni12Mo2Cu2 be welded on site?
Shop guidance: Cu-bearing austenitic fillers; heat-input discipline on standard-carbon heats. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr18Ni12Mo2Cu2?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: prefer the low-carbon sister 022Cr18Ni14Mo2Cu2 when as-welded corrosive joints dominate Sister pointers: 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr18Ni12Mo2Cu2 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr18Ni12Mo2Cu2 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr18Ni12Mo2Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr18Ni12Mo2Cu2?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr18Ni12Mo2Cu2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr18Ni12Mo2Cu2 is seamless stainless steel pipe for fluid transport — standard-carbon Mo-Cu austenitic seamless pipe for reducing-acid fluid transport where a Cu lever is written into the alloy. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr18Ni14Mo2Cu2, 06Cr17Ni12Mo2, 06Cr19Ni13Mo3. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X