GB/T 14976 06Cr13 Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 06Cr13 Seamless Stainless Steel Pipe

GB/T 14976 06Cr13 seamless stainless steel pipe (405-lean / UNS S11306-class, S11306), ferritic, Table 2 cast analysis, Rm min 370 MPa / Rp0.2 min 180 MPa, annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr13 (S11306 / 405-lean / UNS S11306-class — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr13 Seamless Stainless Steel Pipe

GB/T 14976-2025 is the Chinese national standard for seamless stainless steel pipes for fluid transport — replacing the 2012 edition and folding in prior LNG and oxygen-line tube GBs. Grade 06Cr13 (unified number S11306) sits in the ferritic set of Table 1. GB/T 14976 06Cr13 is the Chinese 12Cr ferritic seamless fluid mark — and in 2025 it is explicitly ferritic, so do not copy old martensitic footnotes blindly.

SHH STEEL can produce and supply GB/T 14976 06Cr13 as seamless W-C or W-H pipe across the enquiry OD×wall band, heat-treated per Table 1, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and Table 3 tensile results. Duty focus: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Shop language may still say “405-lean pipe,” yet that commercial alias does not select Chinese cast limits, W-C/W-H symbols, or hydrostatic rules. The purchase order has to name GB/T 14976 and 06Cr13 so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care.

Scope discipline: 06Cr13 is seamless fluid-transport pipe under GB/T 14976, not a boiler tube under GB/T 13296 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 06Cr13Al, 12Cr13, 10Cr15, 10Cr17. Role reminder: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Inside this GB/T 14976 series, compare GB/T 14976 06Cr13Al, GB/T 14976 12Cr13, GB/T 14976 10Cr15, GB/T 14976 10Cr17. Hub: GB/T 14976.

When 06Cr13 pipe sits beside plate on the same BOM, link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 713.7 S11306 so purchasing does not treat one product form as the other. Flat Chinese grades in-family are indexed at GB/T 4237. Quote 06Cr13 pipe and plate under separate line items.

Chemical Composition of GB/T 14976 06Cr13

Cast analysis for GB/T 14976 06Cr13 follows Table 2. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤1.00, P ≤0.035, S ≤0.030, Ni ≤0.60, Cr 11.50–13.50. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 405-lean / UNS S11306-class; unified number S11306. Corrosion thread: basic chromium passive film for mild water and organic fluids; not for strong chlorides or reducing acids.

Chemical limits for 06Cr13 under GB/T 14976-2025 appear in the table underneath. Source priority is the 2025 Table 2 extract. If your client specification cites a 2012 footnote, send it before the heat is melted — phosphorus and several grade rows changed. Duty thread: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Grade C Si Mn P S Ni Cr
06Cr13 ≤0.08 ≤1.00 ≤1.00 ≤0.035 ≤0.030 ≤0.60 11.50–13.50

Mechanical Properties of GB/T 14976 06Cr13

Ambient tensile floors for 06Cr13 come from GB/T 14976 Table 3: Rm min 370 MPa, Rp0.2 min 180 MPa, elongation longitudinal min 22% / transverse min 20%. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr13 370 180 22 20

Ambient values from GB/T 14976-2025 Table 3 for 06Cr13. Heat treatment (Table 1): 800–900 °C slow cool or 750 °C air cool. Density 7.75 kg/dm³. Delivery: annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr13

Seamless is not optional wording for 06Cr13: clause 6.2 limits manufacture to W-C or W-H seamless routes. Pick W-C when OD precision and surface finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 14976 line item. Seamless W-C and W-H options remain available for 06Cr13; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Weld-shop note tied to 06Cr13: 410/405-class practice; low heat input; consider PWHT when the duty file demands it.

Ferritic heats follow Table 1 anneal bands with air or slow cool as listed — not austenitic solution practice. Do not copy 06Cr19Ni10 furnace charts onto ferritic marks. Heat-treatment reference for 06Cr13: 800–900 °C slow cool or 750 °C air cool. Pickling follows unless bright heat treatment or overall machining leaves a scale-free surface. Duty thread: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 06Cr13: W-H or W-C; anneal 800–900 °C slow cool or 750 °C air cool per Table 1.

Dimensions and Tolerances for GB/T 14976 06Cr13

SHH STEEL aligns nominal OD (or ID), wall, length tolerance, and precision class (PA ordinary / PC higher) for 06Cr13 before the mill slot is locked. Dimensions follow GB/T 17395 unless otherwise agreed. Size hint: W-H or W-C; anneal 800–900 °C slow cool or 750 °C air cool per Table 1. Tolerance class (PA/PC) follows the precision ordered for 06Cr13, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 06Cr13 caution visible here: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against GB/T 2102 so pickled finishes are not iron-stained in transit. Duty thread: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Equivalent Grades for GB/T 14976 06Cr13

Identity first: GB/T 14976 06Cr13 is the HX/pipe grade for this page. 405-lean / UNS S11306-class helps buyers who think in AISI/UNS labels. Role: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition). Foreign product standards remain separate documents.

System Designation Notes
GB/T 14976 06Cr13 Governing pipe grade for this page
Commercial / UNS (body only) 405-lean / UNS S11306-class Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 06Cr13, move to a sister rather than stretching the alias: GB/T 14976 06Cr13Al, GB/T 14976 12Cr13, GB/T 14976 10Cr15, GB/T 14976 10Cr17. Apps context: low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs. Full list under GB/T 14976. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (06Cr13).

Heat Treatment and Delivery Condition for GB/T 14976 06Cr13

06Cr13 is delivered annealed under GB/T 14976. Table 1 reference: 800–900 °C slow cool or 750 °C air cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 410/405-class practice; low heat input; consider PWHT when the duty file demands it. Recorded furnace charts for 06Cr13 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for 06Cr13 remains W-H or W-C; anneal 800–900 °C slow cool or 750 °C air cool per Table 1.

Cooling type matters — austenitics need rapid cool after solution treatment; ferritic/martensitic anneal practice follows the air or slow-cool notes in Table 1. Duty thread: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition). Density 7.75 kg/dm³ for weight calcs.

Corrosion Resistance of GB/T 14976 06Cr13

Corrosion behaviour of GB/T 14976 06Cr13 tracks its ferritic balance: basic chromium passive film for mild water and organic fluids; not for strong chlorides or reducing acids. IGC clause 7.5 targets austenitic marks; for ferritic 06Cr13, corrosion testing follows the duty file rather than automatic method E. Design caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 06Cr13 is filed as ferritic. Caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care.

Applications of GB/T 14976 06Cr13 Seamless Pipe

Applications of GB/T 14976 06Cr13 seamless pipe centre on low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs. Role summary: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition). When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs. Duty thread: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Weldability of GB/T 14976 06Cr13

06Cr13 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 410/405-class practice; low heat input; consider PWHT when the duty file demands it. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 06Cr13 should use the same product form and wall class as production, including the seamless finish that will ship. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — ferritic — not a single shop habit. Caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care.

Surface Finishes for GB/T 14976 06Cr13

Surface supply for 06Cr13 should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless pipe, so finish is part of performance, not only appearance. Application framing: low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs. Ambiguous “bright pipe” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Annealed and pickled Standard pipe mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; inspect before polish on ferritic stock
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

OD stencil ink on 06Cr13 should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care. Close bundles only after free-iron and burn marks are cleared.

Inspection and Testing for GB/T 14976 06Cr13

Inspection for GB/T 14976 06Cr13 covers cast analysis, tensile tests, hydrostatic test (or replacing UT/ET), dimensions, appearance, and flattening/bend/flare when ordered. IGC clause 7.5 targets austenitic marks; for ferritic 06Cr13, corrosion testing follows the duty file rather than automatic method E. Documents follow GB/T 2102 / purchaser-specified EN 10204 styles. Sampling plans for 06Cr13 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for 06Cr13 stays low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs.

Marking includes 06Cr13, manufacturer, and other mandatory GB/T 2102 data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs. Non-conforming 06Cr13 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr13: 410/405-class practice; low heat input; consider PWHT when the duty file demands it.

Packaging and Shipping for GB/T 14976 06Cr13

Packaging for 06Cr13 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 06Cr13 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 06Cr13 duty: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care. Desiccant and wrap choices for 06Cr13 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 06Cr13 remains W-H or W-C; anneal 800–900 °C slow cool or 750 °C air cool per Table 1.

Shipping documents list GB/T 14976, 06Cr13, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition). Claims handling for 06Cr13 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 06Cr13: 410/405-class practice; low heat input; consider PWHT when the duty file demands it.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 06Cr13 with the seamless route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless capacity covering W-C and W-H for this mark. Duty focus: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition).

Technical sales can map 06Cr13 against sisters 06Cr13Al, 12Cr13, 10Cr15, 10Cr17 and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 06Cr13, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr13 to that written scope.

Supply Capability

SHH STEEL can produce and supply GB/T 14976 06Cr13 across enquiry-oriented OD × wall bands, in seamless W-C or W-H routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr13 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr13 (S11306)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

SHH STEEL can produce and supply GB/T 14976 06Cr13. Stock / Available sizes: enquiry band typically aligns with GB/T 17395 OD×wall practice, with PA or PC precision as ordered. For 06Cr13, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: W-H or W-C; anneal 800–900 °C slow cool or 750 °C air cool per Table 1.

Cut lengths, bevels, special NDT, IGC, and Annex A/B extras add lead time — call them early. Sisters often quoted alongside: 06Cr13Al, 12Cr13, 10Cr15, 10Cr17. Email the size list to start. SHH STEEL can produce trial lengths of 06Cr13 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr13 seamless stainless steel pipe used for?
GB/T 14976 06Cr13 is seamless stainless pipe for fluid transport — low-pressure water lines, mildly corrosive process drains, and utility fluid piping on Chinese ferritic specs. Role summary: 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition). It is a Chinese product standard grade (S11306), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr13 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr13 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr13?
06Cr13 is delivered annealed under GB/T 14976. Table 1 reference: 800–900 °C slow cool or 750 °C air cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr13 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr13 compare with sister grades 06Cr13Al, 12Cr13, 10Cr15?
06Cr13 is filed as ferritic. Typical sisters on the same RFQ are 06Cr13Al, 12Cr13, 10Cr15. Design caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr13?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 405-lean / UNS S11306-class the same as ordering 06Cr13?
No. 405-lean / UNS S11306-class is a commercial / UNS cross-walk for body text (unified S11306). The purchase order should lock GB/T 14976 and 06Cr13 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr13?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr13 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-H or W-C; anneal 800–900 °C slow cool or 750 °C air cool per Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr13 be welded on site?
Shop guidance: 410/405-class practice; low heat input; consider PWHT when the duty file demands it. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr13?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: 2025 edition files 06Cr13 as ferritic (not martensitic as in older lists) — update old dual-cert habits; weld toughness and grain growth need procedure care Sister pointers: 06Cr13Al, 12Cr13, 10Cr15. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr13 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr13 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr13 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr13?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr13 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr13 is seamless stainless steel pipe for fluid transport — 12% Cr ferritic seamless pipe for mild aqueous fluid service where austenitic cost is not justified (reclassified ferritic in the 2025 edition). SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr13Al, 12Cr13, 10Cr15. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X