EN 10297-2 1.4307 Seamless Stainless Steel Tube

EN 10297-2 1.4307 / X2CrNi18-9 seamless stainless general-purpose tube (304L), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 180 MPa, Rm min 460 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4307 / X2CrNi18-9 (304L — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4307 Seamless Stainless Steel Tube

EN 10297-2:2005 (BS EN 10297-2:2005) is the European product standard for seamless circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10216-5, and not for welded general-purpose tube under EN 10296-2. Steel number 1.4307 is listed as X2CrNi18-9 in the austenitic corrosion-resisting set. Buyers who want “304L seamless tube” for mechanical and general engineering under a European product standard are usually looking for EN 10297-2 1.4307 — not a PED Part 5 pressure page by default. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Mill path for 1.4307: instrumentation through mid-process seamless OD, CFD/CFA common for precision. SHH STEEL can produce and supply X2CrNi18-9 under EN 10297-2 1.4307 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

On the shop floor people still say “304L tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4307, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo. Typical duties include food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L. Design caution: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4307: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Inside this seamless general-purpose series, compare EN 10297-2 1.4301, EN 10297-2 1.4306, EN 10297-2 1.4311, EN 10297-2 1.4404. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4307. ASTM/ASME related product pages (not interchangeable by default): A269 TP304L, A213 TP304L, A312 TP304L.

Chemical Composition of EN 10297-2 1.4307

Cast window focus for 1.4307: Every 1.4307 heat under EN 10297-2 must meet the cast (ladle) analysis for X2CrNi18-9 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 304L is body text only. Corrosion thread: low-C chromium-nickel passive film for aqueous and mild chemical media; pitting still tracks Mo-free balance.

Cast chemistry for seamless 1.4307 must land inside X2CrNi18-9 limits. The table is transcribed from public BSSA EN 10297-2 data for quick comparison with sister grades; always re-check the paid standard when a dispute arises. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Steel C Si Mn P S Cr Ni N
1.4307 / X2CrNi18-9 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 17.5–19.5 8.0–10.5 ≤0.11

Mechanical Properties of EN 10297-2 1.4307

Ambient floors focus for 1.4307: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4307 order. General-purpose Table values for this number read: Rp0.2 min 180 MPa, Rp1.0 min 215 MPa, Rm min 460 MPa, longitudinal elongation min 40%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 180 215 460 min 40 35 Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4307 / X2CrNi18-9. Guideline solution/anneal band (Annex B): 1000–1100 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4307

Seamless route narrative for 1.4307: EN 10297-2 does not offer a welded route for 1.4307. Tube in X2CrNi18-9 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Order EN 10297-2 1.4307 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints.

For austenitic 1.4307, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4307 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1000–1100 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4307. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4307: instrumentation through mid-process seamless OD, CFD/CFA common for precision. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Dimensions and Tolerances for EN 10297-2 1.4307

Dimensional order line for 1.4307: Dimensional orders for 1.4307 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Instrumentation through mid-process seamless od, cfd/cfa common for precision. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Length supply for 1.4307 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4307: instrumentation through mid-process seamless OD, CFD/CFA common for precision. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Equivalent Grades for EN 10297-2 1.4307

Equivalence talk for 1.4307 starts with X2CrNi18-9: 1.4307 / X2CrNi18-9 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 304L appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4301, 1.4306, 1.4311, 1.4404. Hook for buyers still using only the 304L alias: lock EN 10297-2 1.4307 on the order line. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

Heat Treatment and Delivery Condition for EN 10297-2 1.4307

Austenitic 1.4307 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1000–1100 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints.

Fabrication HT reminder for 1.4307 (+AT): Hot-working temperature bands in Annex B for X2CrNi18-9 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4307 should match +AT. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Corrosion Resistance of EN 10297-2 1.4307

Corrosion behaviour of EN 10297-2 1.4307 tracks its austenitic corrosion-resisting balance: low-C chromium-nickel passive film for aqueous and mild chemical media; pitting still tracks Mo-free balance. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up Corrosion thread: low-C chromium-nickel passive film for aqueous and mild chemical media; pitting still tracks Mo-free balance.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4307 is filed as austenitic corrosion-resisting — pick tests that match that filing. Family filing for 1.4307 is austenitic corrosion-resisting. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

Applications of EN 10297-2 1.4307 Tube

Applications of EN 10297-2 1.4307 tube centre on mechanical and general engineering rather than PED pressure shells: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L. Role summary: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Skip 1.4307 when the specification locks a different family — for example forcing ferritic 1.4307 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4301, 1.4306, 1.4311, 1.4404. Primary application sketch: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Weldability of EN 10297-2 1.4307

1.4307 / X2CrNi18-9 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up Filler/shop note for 1.4307: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

Surface Finishes for EN 10297-2 1.4307

Finish selection for 1.4307 on Annex A: Interior Ra limits, electropolish, or special protection for X2CrNi18-9 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4307 when the mill can measure and report the finish. Alias reminder: commercial talk may say 304L, but the finish symbol still belongs on the EN 10297-2 line. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Agree any site-storage constraints for 1.4307 at enquiry. Long inland dwell in winter road-salt regions needs sealed wrap even when ocean freight is not involved. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Inspection and Testing for EN 10297-2 1.4307

Inspection lot framing for 1.4307 in austenitic corrosion-resisting: SHH STEEL EN 10204 3.1 documents for 1.4307 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4307 heat identity intact from cast through bundle tag. Weld thread: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints.

Acceptance marks on 1.4307 reference the inspection lot. If a piece is cut after delivery, retain the marked end or transfer the heat identity under the fabricator’s quality system so traceability survives the saw. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Packaging and Shipping for EN 10297-2 1.4307

Dispatch note for 1.4307 (304L body alias only): SHH STEEL ships EN 10297-2 1.4307 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Marking and identity for 1.4307: For 1.4307, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4307 follows the Annex A symbol on the order. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Project freight for 1.4307 can be staged by installation sequence when the packing list names priority bundles. That staging is agreed before the saw schedule locks. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

Why Choose SHH STEEL

Why 1.4307 with SHH STEEL — role: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo. SHH STEEL can produce and supply EN 10297-2 1.4307 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “304L tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

Grade advice stays practical for 1.4307. If the duty needs a sister chemistry, we point to 1.4301, 1.4306, 1.4311, 1.4404. Design caution for this number: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up Export document packs are assembled to match the heat tags on the bundles you will receive. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up.

Supply Capability

SHH STEEL can produce and supply EN 10297-2 1.4307. SHH STEEL’s EN 10297-2 1.4307 offering is make-to-order seamless tube in X2CrNi18-9. We can produce and supply cut lengths and standard mill lengths. Use the Stock / Available sizes map as a planning aid, then confirm live availability on the quote. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4307 / X2CrNi18-9
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes note for 1.4307: bring the OD × wall list early. Context: instrumentation through mid-process seamless OD, CFD/CFA common for precision. Bright CFA and polished CFP may add finishing lead time versus descaled CFD/HFD. Duty thread: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.

When 1.4307 shares a project with 1.4301, 1.4306, 1.4311, 1.4404, keep separate heat identity tags. SHH STEEL can produce and supply coordinated size lists so fabrication receives matched OD bands without mixed certificates. Weld thread: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints.

FAQ

What is EN 10297-2 1.4307 seamless stainless steel tube used for?
EN 10297-2 1.4307 (X2CrNi18-9) is seamless tube for mechanical and general engineering — food and beverage utilities, pharmaceutical water lines, instrumentation, hydraulic lines, and mechanical process tubing that specifies 304L. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo.
Is EN 10297-2 1.4307 the same as EN 10216-5 1.4307?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4307 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4307 / X2CrNi18-9?
Delivery framing for 1.4307 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1000–1100 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4307?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4307 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4307 compare with sister grades 1.4301, 1.4306, 1.4311?
1.4307 / X2CrNi18-9 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4301, 1.4306, 1.4311. Design caution: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4307 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: 308L-class fillers; mill +AT does not replace fabricator procedures on site joints. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4307?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4307?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4307 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: instrumentation through mid-process seamless OD, CFD/CFA common for precision. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 304L belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 304L in body text and BOM notes, but lock EN 10297-2 and 1.4307 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4307?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: low carbon is not a chloride-SCC cure — move to Mo austenitics or duplex when chlorides and stress stack up Sister pointers: 1.4301, 1.4306, 1.4311. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4307 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4307 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4307 (X2CrNi18-9) is seamless stainless tube for mechanical and general engineering — low-carbon 18-8 austenitic seamless tube for general engineering where as-welded IGC resistance matters more than Mo. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4301, 1.4306, 1.4311. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X