EN 10297-2 1.4845 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4845 Seamless Stainless Steel Tube

EN 10297-2 1.4845 / X8CrNi25-21 seamless stainless general-purpose tube (310S), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm min 500 MPa, A long. min 33%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4845 / X8CrNi25-21 (310S — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4845 Seamless Stainless Steel Tube

If the purchase file still names only a commercial alias such as 310S without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4845 (X8CrNi25-21) selects seamless tube for mechanical and general engineering. EN 10297-2 1.4845 is heat-resisting 310S-class seamless tube — confirm the buyer does not actually need corrosion-resisting 1.4335. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Mill path for 1.4845: heat-service seamless OD. SHH STEEL can produce and supply EN 10297-2 1.4845 seamless stainless steel tube — hot-finished or cold-finished on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, hydrostatic, eddy current, ultrasonic, and related NDT Options). Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

On the shop floor people still say “310S tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4845, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class. Typical duties include furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service. Design caution: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Do not treat an EN 10297-2 1.4845 MTC as automatic clearance for pressure equipment — Part 5 of EN 10216 is the pressure seamless home. Likewise, welded pressure tube lives under EN 10217-7, which is a different product form and test regime. Match the product standard to the duty before dual-marking talk begins. Role reminder for 1.4845: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Inside this seamless general-purpose series, compare EN 10297-2 1.4833, EN 10297-2 1.4335, EN 10297-2 1.4876. Hub: EN 10297-2. Related pressure seamless chemistry page: EN 10216-5 1.4335.

Chemical Composition of EN 10297-2 1.4845

Cast window focus for 1.4845: Every 1.4845 heat under EN 10297-2 must meet the cast (ladle) analysis for X8CrNi25-21 in the austenitic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 310S is body text only. Corrosion thread: high Cr-Ni for oxidising heat; carburising atmospheres need separate evaluation.

Use the table as a working cast-analysis checklist for 1.4845 (X8CrNi25-21). It mirrors public BSSA EN 10297-2 figures for buyer convenience; contractual acceptance still cites the edition named on the purchase order. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Steel C Si Mn P S Cr Ni N
1.4845 / X8CrNi25-21 ≤0.10 ≤1.50 ≤2.00 ≤0.045 ≤0.015 24.0–26.0 19.0–22.0 ≤0.11

Mechanical Properties of EN 10297-2 1.4845

Ambient floors focus for 1.4845: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4845 order. General-purpose Table values for this number read: Rp0.2 min 210 MPa, Rp1.0 min 250 MPa, Rm min 500 MPa, longitudinal elongation min 33%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic heat-resisting. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 210 250 500 min 33 35 –

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4845 / X8CrNi25-21. Guideline solution/anneal band (Annex B): 1050–1150 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4845

Seamless route narrative for 1.4845: EN 10297-2 does not offer a welded route for 1.4845. Tube in X8CrNi25-21 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. For 1.4845, SHH STEEL aligns the Annex A symbol to the duty: descaled HFD/CFD for general mechanical tube, CFA for cleaner bright OD, and CFG/CFP when a measured roughness target is part of the order text. Weld thread: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool.

For austenitic 1.4845, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4845 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1050–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4845. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4845: heat-service seamless OD. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

Dimensions and Tolerances for EN 10297-2 1.4845

Dimensional order line for 1.4845: Order EN 10297-2 1.4845 by outside diameter D and wall thickness T for steel name X8CrNi25-21. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Heat-service seamless od. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4845: heat-service seamless OD. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Equivalent Grades for EN 10297-2 1.4845

Equivalence talk for 1.4845 starts with X8CrNi25-21: 1.4845 / X8CrNi25-21 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 310S appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4833, 1.4335, 1.4876. Hook for buyers still using only the 310S alias: lock EN 10297-2 1.4845 on the order line. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Heat Treatment and Delivery Condition for EN 10297-2 1.4845

Austenitic 1.4845 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1050–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool.

Fabrication HT reminder for 1.4845 (+AT): For 1.4845, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Delivery framing on the certificate for 1.4845 should match +AT. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Corrosion Resistance of EN 10297-2 1.4845

Corrosion behaviour of EN 10297-2 1.4845 tracks its austenitic heat-resisting balance: high Cr-Ni for oxidising heat; carburising atmospheres need separate evaluation. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows Corrosion thread: high Cr-Ni for oxidising heat; carburising atmospheres need separate evaluation.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4833, 1.4335, 1.4876 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4845 is austenitic heat-resisting. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Applications of EN 10297-2 1.4845 Tube

Applications of EN 10297-2 1.4845 tube centre on mechanical and general engineering rather than PED pressure shells: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service. Role summary: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

Typical BOM language pairs EN 10297-2 1.4845 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “310S” substitutions do not creep in. Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Weldability of EN 10297-2 1.4845

1.4845 / X8CrNi25-21 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows Filler/shop note for 1.4845: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Surface Finishes for EN 10297-2 1.4845

Finish selection for 1.4845 on Annex A: For 1.4845, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 310S, but the finish symbol still belongs on the EN 10297-2 line. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

If 1.4845 will sit in a humid warehouse before use, ask for sealed wrap and humidity indicators on the packing list. Carbon-steel dunnage never contacts the stainless OD — timber or plastic separators are the default. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Inspection and Testing for EN 10297-2 1.4845

Inspection lot framing for 1.4845 in austenitic heat-resisting: NDT intensity on 1.4845 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4845 heat identity intact from cast through bundle tag. Weld thread: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool.

For 1.4845, dimensional inspection covers OD, wall, length, and agreed out-of-roundness/eccentricity. IGC and NDT Options appear as separate certificate lines. Correlation numbers link pieces to the EN 10204 3.1 file without opening every crate. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

Packaging and Shipping for EN 10297-2 1.4845

Dispatch note for 1.4845 (310S body alias only): SHH STEEL ships EN 10297-2 1.4845 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Marking and identity for 1.4845: For 1.4845, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4845 follows the Annex A symbol on the order. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

SHH STEEL closes the packing note for 1.4845 only after caps, wrap, and tags match the Annex A finish and the cut-length list. Shortages or mixed walls are corrected in the warehouse — not discovered at the jobsite. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10297-2 1.4845 seamless stainless steel tube. Why 1.4845 with SHH STEEL — role: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class. Choose SHH STEEL for EN 10297-2 1.4845 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

Grade advice stays practical for 1.4845. If the duty needs a sister chemistry, we point to 1.4833, 1.4335, 1.4876. Design caution for this number: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows Mill slots are planned against the Annex A symbol you order — bright and polished finishes are not assumed. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows.

Supply Capability

SHH STEEL can produce and supply EN 10297-2 1.4845. EN 10297-2 1.4845 supply from SHH STEEL covers hot- and cold-finished seamless routes for X8CrNi25-21. We can produce and supply to the mechanical floors of the ordered delivery condition. The Stock / Available sizes section is the enquiry checklist. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4845 / X8CrNi25-21
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

For 1.4845, treat the size table as an RFQ aid. Context: heat-service seamless OD. Confirm tolerance class and Annex A symbol so CFD/CFA slots are not confused with HFD on the acknowledgement. Duty thread: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.

For 1.4845, ask early about cut-to-length packages and NDT Options. Peer mill size charts are indicative only. SHH STEEL can produce and supply the ordered Annex A finish once the acknowledgement locks OD × wall. Sisters often discussed: 1.4833, 1.4335, 1.4876. Weld thread: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool.

FAQ

What is EN 10297-2 1.4845 seamless stainless steel tube used for?
EN 10297-2 1.4845 (X8CrNi25-21) is seamless tube for mechanical and general engineering — furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class.
Is EN 10297-2 1.4845 the same as EN 10216-5 1.4845?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4845 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4845 / X8CrNi25-21?
Delivery framing for 1.4845 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1050–1150 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4845?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4845 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4845 compare with sister grades 1.4833, 1.4335, 1.4876?
1.4845 / X8CrNi25-21 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4833, 1.4335, 1.4876. Design caution: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4845 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: 310-class fillers; high solution-anneal band; watch sigma risk on slow cool. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4845?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4845?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4845 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: heat-service seamless OD. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 310S belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 310S in body text and BOM notes, but lock EN 10297-2 and 1.4845 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4845?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: distinguish from corrosion-resisting 1.4335 (low-C 25-21) — different tables and Si/C windows Sister pointers: 1.4833, 1.4335, 1.4876. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4845 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4845 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4845 (X8CrNi25-21) is seamless stainless tube for mechanical and general engineering — 25Cr-20Ni austenitic heat-resisting seamless tube (310S-class) for higher oxidation resistance than 309-class. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4833, 1.4335, 1.4876. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *