EN 10297-2 1.4311 Seamless Stainless Steel Tube

EN 10297-2 1.4311 / X2CrNiN18-10 seamless stainless general-purpose tube (304LN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 270 MPa, Rm min 550 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4311 / X2CrNiN18-10 (304LN — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4311 Seamless Stainless Steel Tube

If the purchase file still names only a commercial alias such as 304LN without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4311 (X2CrNiN18-10) selects seamless tube for mechanical and general engineering. When the stress calculation wants more than 1.4307’s Rp0.2 but the medium is still Mo-free aqueous service, 1.4311 is the EN 10297-2 nitrogen path. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Mill path for 1.4311: same OD×wall conversation as 1.4307 with higher tensile floors on the MTC. SHH STEEL can produce and supply X2CrNiN18-10 under EN 10297-2 1.4311 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

On the shop floor people still say “304LN tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4311, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex. Typical duties include higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors. Design caution: nitrogen raises strength but does not buy Mo-level pitting resistance. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4311: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Inside this seamless general-purpose series, compare EN 10297-2 1.4307, EN 10297-2 1.4301, EN 10297-2 1.4404, EN 10297-2 1.4429. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4311. ASTM/ASME related product pages (not interchangeable by default): A269 TP304L.

Chemical Composition of EN 10297-2 1.4311

Cast window focus for 1.4311: Cast analysis for EN 10297-2 1.4311 follows the X2CrNiN18-10 limits published for this standard’s corrosion- or heat-resisting tables. Key windows on a typical certificate include C ≤0.030, Cr 17.0–19.5, Ni 8.5–11.5, N 0.12–0.22, Si ≤1.00, S ≤0.015. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 304LN is body text only. Corrosion thread: low carbon plus nitrogen; aqueous resistance similar to 304L-family with interstitial strengthening.

Below is the BSSA-sourced EN 10297-2 chemistry window for 1.4311 (X2CrNiN18-10). Maxima apply unless a band is printed. SHH STEEL quotes against this window and reports actual cast values on the EN 10204 document — not a rewritten catalogue paraphrase. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Steel C Si Mn P S Cr Ni N
1.4311 / X2CrNiN18-10 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 17.0–19.5 8.5–11.5 0.12–0.22

Mechanical Properties of EN 10297-2 1.4311

Ambient floors focus for 1.4311: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4311 order. General-purpose Table values for this number read: Rp0.2 min 270 MPa, Rp1.0 min 305 MPa, Rm min 550 MPa, longitudinal elongation min 35%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 270 305 550 min 35 30 Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4311 / X2CrNiN18-10. Guideline solution/anneal band (Annex B): 1000–1080 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4311

Seamless route narrative for 1.4311: EN 10297-2 does not offer a welded route for 1.4311. Tube in X2CrNiN18-10 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. For 1.4311, SHH STEEL aligns the Annex A symbol to the duty: descaled HFD/CFD for general mechanical tube, CFA for cleaner bright OD, and CFG/CFP when a measured roughness target is part of the order text. Weld thread: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement.

For austenitic 1.4311, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4311 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1000–1080 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

When dual documentation against EN 10216-5 is requested for the same 1.4311 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4311: same OD×wall conversation as 1.4307 with higher tensile floors on the MTC. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

Dimensions and Tolerances for EN 10297-2 1.4311

Dimensional order line for 1.4311: SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4311 / X2CrNiN18-10 before rolling or drawing slots are locked. Same od×wall conversation as 1.4307 with higher tensile floors on the mtc. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

For precision mechanical duty on 1.4311, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4311: same OD×wall conversation as 1.4307 with higher tensile floors on the MTC. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Equivalent Grades for EN 10297-2 1.4311

Equivalence talk for 1.4311 starts with X2CrNiN18-10: 1.4311 / X2CrNiN18-10 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 304LN appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4307, 1.4301, 1.4404, 1.4429. Hook for buyers still using only the 304LN alias: lock EN 10297-2 1.4311 on the order line. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

Heat Treatment and Delivery Condition for EN 10297-2 1.4311

Austenitic 1.4311 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1000–1080 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement.

Fabrication HT reminder for 1.4311 (+AT): Hot-working temperature bands in Annex B for X2CrNiN18-10 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4311 should match +AT. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Corrosion Resistance of EN 10297-2 1.4311

Corrosion behaviour of EN 10297-2 1.4311 tracks its austenitic corrosion-resisting balance: low carbon plus nitrogen; aqueous resistance similar to 304L-family with interstitial strengthening. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: nitrogen raises strength but does not buy Mo-level pitting resistance Corrosion thread: low carbon plus nitrogen; aqueous resistance similar to 304L-family with interstitial strengthening.

SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4311. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Family filing for 1.4311 is austenitic corrosion-resisting. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

Applications of EN 10297-2 1.4311 Tube

Applications of EN 10297-2 1.4311 tube centre on mechanical and general engineering rather than PED pressure shells: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors. Role summary: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4307. Primary application sketch: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Weldability of EN 10297-2 1.4311

1.4311 / X2CrNiN18-10 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: nitrogen raises strength but does not buy Mo-level pitting resistance Filler/shop note for 1.4311: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

Surface Finishes for EN 10297-2 1.4311

Finish selection for 1.4311 on Annex A: Interior Ra limits, electropolish, or special protection for X2CrNiN18-10 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4311 when the mill can measure and report the finish. Alias reminder: commercial talk may say 304LN, but the finish symbol still belongs on the EN 10297-2 line. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

Storage guidance for 1.4311: keep bundles off bare concrete in coastal yards, avoid chloride-bearing tarps against CFA OD, and leave end caps fitted until fabrication. Special export crate liners are available when the packing note asks for them. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Inspection and Testing for EN 10297-2 1.4311

Inspection lot framing for 1.4311 in austenitic corrosion-resisting: Specific inspection applies to EN 10297-2 1.4311 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4311 heat identity intact from cast through bundle tag. Weld thread: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement.

Technological tests on 1.4311 follow the order matrix — they are not assumed. IGC, when required, cites EN ISO 3651-2. Stencil or inkjet marking stays light on polished OD so the finish remains acceptable after receipt inspection. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

Packaging and Shipping for EN 10297-2 1.4311

Dispatch note for 1.4311 (304LN body alias only): Export packing for 1.4311 / X2CrNiN18-10 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavy HFD bundles use spacers to stop fretting in transit. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Marking and identity for 1.4311: When cut lengths and special ends are part of the 1.4311 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4311 follows the Annex A symbol on the order. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

Packing lists for 1.4311 map bundle IDs to heats and sizes so receiving inspection can clear documents without unpacking every crate. Damaged wrap discovered at destination is reported with photos before the material is issued to fabrication. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

Why Choose SHH STEEL

Why 1.4311 with SHH STEEL — role: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex. SHH STEEL can produce and supply EN 10297-2 1.4311 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “304LN tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

Grade advice stays practical for 1.4311. If the duty needs a sister chemistry, we point to 1.4307, 1.4301, 1.4404, 1.4429. Design caution for this number: nitrogen raises strength but does not buy Mo-level pitting resistance Quotes state scope boundaries in plain language so purchasing and engineering share the same acceptance standard. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: nitrogen raises strength but does not buy Mo-level pitting resistance.

Supply Capability

Supply capability for EN 10297-2 1.4311 / X2CrNiN18-10 starts with your OD × wall list and delivery-condition choice. SHH STEEL can produce and supply against that list with EN 10204 3.1 documents; the Stock / Available sizes block frames enquiry sizes rather than a public warehouse catalogue. Use thread: higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4311 / X2CrNiN18-10
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Available sizes conversation for 1.4311 starts with your OD × wall matrix. Typical note: same OD×wall conversation as 1.4307 with higher tensile floors on the MTC. Send preferred delivery condition (+A / +AT / +QT as applicable) and any eddy-current or hydrostatic Options with the size list. Duty thread: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.

On 1.4311, Options and sister duals (1.4307, 1.4301, 1.4404, 1.4429) belong on the same enquiry as the size list. SHH STEEL can produce and supply production heats after a short pilot when forming or polish trials are required. Weld thread: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement.

FAQ

What is EN 10297-2 1.4311 seamless stainless steel tube used for?
EN 10297-2 1.4311 (X2CrNiN18-10) is seamless tube for mechanical and general engineering — higher-design-stress mechanical utilities, nitrogen-specified hygienic lines, and wall-thinning projects driven by 304L proof floors. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex.
Is EN 10297-2 1.4311 the same as EN 10216-5 1.4311?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4311 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4311 / X2CrNiN18-10?
Delivery framing for 1.4311 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1000–1080 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4311?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4311 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4311 compare with sister grades 1.4307, 1.4301, 1.4404?
1.4311 / X2CrNiN18-10 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4307, 1.4301, 1.4404. Design caution: nitrogen raises strength but does not buy Mo-level pitting resistance Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4311 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: match nitrogen-bearing or overlying austenitic fillers; avoid procedures that dilute N without agreement. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4311?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4311?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4311 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: same OD×wall conversation as 1.4307 with higher tensile floors on the MTC. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 304LN belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 304LN in body text and BOM notes, but lock EN 10297-2 and 1.4311 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4311?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: nitrogen raises strength but does not buy Mo-level pitting resistance Sister pointers: 1.4307, 1.4301, 1.4404. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4311 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4311 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4311 (X2CrNiN18-10) is seamless stainless tube for mechanical and general engineering — nitrogen-strengthened low-carbon 18-8 seamless tube needing higher proof strength than 1.4307 without jumping to duplex. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4307, 1.4301, 1.4404. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X