EN 10297-2 1.4563 Seamless Stainless Steel Tube
What is EN 10297-2 1.4563 Seamless Stainless Steel Tube
EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4563 is the austenitic corrosion-resisting grade X1NiCrMoCu31-27-4, commercially discussed as Alloy 28 / N08028. EN 10297-2 1.4563 is the seamless general-purpose home for X1NiCrMoCu31-27-4 — order the steel number when Alloy 28 chemistry is on the list. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Mill path for 1.4563: specialty seamless OD; higher solution-anneal band. SHH STEEL can produce and supply X1NiCrMoCu31-27-4 under EN 10297-2 1.4563 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
On the shop floor people still say “Alloy 28 / N08028 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4563, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service. Typical duties include sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry. Design caution: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4563: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Inside this seamless general-purpose series, compare EN 10297-2 1.4539, EN 10297-2 1.4529, EN 10297-2 1.4547. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4563.
Chemical Composition of EN 10297-2 1.4563
Cast window focus for 1.4563: Buying Alloy 28 / N08028-family seamless tube without locking 1.4563 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X1NiCrMoCu31-27-4; highlight elements for this grade include C ≤0.020, Cr 26.0–28.0, Ni 30.0–32.0, Mo 3.0–4.0, N ≤0.11, Cu 0.70–1.50. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias Alloy 28 / N08028 is body text only. Corrosion thread: high Ni-Cr-Mo-Cu balance for reducing and oxidising acid media within the corrosion-resisting set.
For 1.4563 / X1NiCrMoCu31-27-4, the following chem table is the public EN 10297-2 window SHH STEEL uses at enquiry. Product-analysis Options, when taken, apply the standard’s permitted deviations rather than inventing tighter shop limits. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | Cu | N |
|---|---|---|---|---|---|---|---|---|---|---|
| 1.4563 / X1NiCrMoCu31-27-4 | ≤0.020 | ≤0.70 | ≤2.00 | ≤0.030 | ≤0.010 | 26.0–28.0 | 3.0–4.0 | 30.0–32.0 | 0.70–1.50 | ≤0.11 |
Mechanical Properties of EN 10297-2 1.4563
Ambient floors focus for 1.4563: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4563 order. General-purpose Table values for this number read: Rp0.2 min 215 MPa, Rp1.0 min 245 MPa, Rm min 500 MPa, longitudinal elongation min 40%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 215 | 245 | 500 min | 40 | 35 | Yes |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4563 / X1NiCrMoCu31-27-4. Guideline solution/anneal band (Annex B): 1070–1150 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4563
Seamless route narrative for 1.4563: EN 10297-2 does not offer a welded route for 1.4563. Tube in X1NiCrMoCu31-27-4 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Seamless manufacture for 1.4563 finishes through hot- or cold-finished routes. Pick HFD/CFD for descaled engineering surfaces, CFA for bright anneal, and CFG or CFP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: matching Alloy 28-class fillers; strict cleanliness and heat input.
For austenitic 1.4563, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4563 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1070–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
When dual documentation against EN 10216-5 is requested for the same 1.4563 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4563: specialty seamless OD; higher solution-anneal band. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
Dimensions and Tolerances for EN 10297-2 1.4563
Dimensional order line for 1.4563: Dimensional orders for 1.4563 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Specialty seamless od; higher solution-anneal band. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
For precision mechanical duty on 1.4563, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4563: specialty seamless OD; higher solution-anneal band. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Equivalent Grades for EN 10297-2 1.4563
Equivalence talk for 1.4563 starts with X1NiCrMoCu31-27-4: 1.4563 / X1NiCrMoCu31-27-4 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias Alloy 28 / N08028 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4539, 1.4529, 1.4547. Hook for buyers still using only the Alloy 28 / N08028 alias: lock EN 10297-2 1.4563 on the order line. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
Heat Treatment and Delivery Condition for EN 10297-2 1.4563
Austenitic 1.4563 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1070–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching Alloy 28-class fillers; strict cleanliness and heat input.
Fabrication HT reminder for 1.4563 (+AT): For 1.4563, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Delivery framing on the certificate for 1.4563 should match +AT. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Corrosion Resistance of EN 10297-2 1.4563
Corrosion behaviour of EN 10297-2 1.4563 tracks its austenitic corrosion-resisting balance: high Ni-Cr-Mo-Cu balance for reducing and oxidising acid media within the corrosion-resisting set. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval Corrosion thread: high Ni-Cr-Mo-Cu balance for reducing and oxidising acid media within the corrosion-resisting set.
SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4563. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Family filing for 1.4563 is austenitic corrosion-resisting. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
Applications of EN 10297-2 1.4563 Tube
Applications of EN 10297-2 1.4563 tube centre on mechanical and general engineering rather than PED pressure shells: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry. Role summary: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4539. Primary application sketch: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Weldability of EN 10297-2 1.4563
1.4563 / X1NiCrMoCu31-27-4 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching Alloy 28-class fillers; strict cleanliness and heat input. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching Alloy 28-class fillers; strict cleanliness and heat input.
For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval Filler/shop note for 1.4563: matching Alloy 28-class fillers; strict cleanliness and heat input. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
Surface Finishes for EN 10297-2 1.4563
Finish selection for 1.4563 on Annex A: Surface finish on EN 10297-2 1.4563 is carried by the Annex A symbol: descaled HFD/CFD for general mechanical tube, bright-annealed CFA for cleaner OD appearance, and ground CFG or polished CFP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the stainless surface. Alias reminder: commercial talk may say Alloy 28 / N08028, but the finish symbol still belongs on the EN 10297-2 line. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
Transit protection for 1.4563 is sized to the Annex A finish: heavier wrap for CFA/CFG/CFP, standard export wrap for HFD/CFD. Open-deck ocean exposure without wrap is refused on bright tube. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Inspection and Testing for EN 10297-2 1.4563
Inspection lot framing for 1.4563 in austenitic corrosion-resisting: SHH STEEL EN 10204 3.1 documents for 1.4563 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4563 heat identity intact from cast through bundle tag. Weld thread: matching Alloy 28-class fillers; strict cleanliness and heat input.
Purchasers who need witness points on 1.4563 should say so at enquiry. Routine mill inspection still records cast chemistry, tensile results, delivery condition, and dimensions; witness adds scheduling, not a different chemistry table. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
Packaging and Shipping for EN 10297-2 1.4563
Dispatch note for 1.4563 (Alloy 28 / N08028 body alias only): Finished EN 10297-2 1.4563 (X1NiCrMoCu31-27-4) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Marking and identity for 1.4563: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4563, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4563 follows the Annex A symbol on the order. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
Ocean containers loaded with 1.4563 use desiccant and sealed wrap when the route or season warrants it. Inland deliveries may omit container desiccant but never omit end caps on precision OD. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
Why Choose SHH STEEL
Why 1.4563 with SHH STEEL — role: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service. SHH STEEL can produce and supply EN 10297-2 1.4563 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “Alloy 28 / N08028 tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Grade advice stays practical for 1.4563. If the duty needs a sister chemistry, we point to 1.4539, 1.4529, 1.4547. Design caution for this number: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval Technical clarification on QT level, cold- versus hot-finished rows, or duplex thin-wall footnotes happens before acknowledgement. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval.
Supply Capability
For 1.4563, SHH STEEL can produce and supply seamless tube in the X1NiCrMoCu31-27-4 analysis with the Annex A finish you name. Lead time tracks hollow stock and heat-treatment slots; Stock / Available sizes below helps size the first RFQ. Use thread: sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4563 / X1NiCrMoCu31-27-4 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Available sizes for 1.4563 follow seamless general-purpose practice: specialty seamless OD; higher solution-anneal band. Dual size lists against sister grades are welcome on one enquiry sheet. Duty thread: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
Dual documentation talk for 1.4563 versus 1.4539, 1.4529, 1.4547 is fine at enquiry — each steel number still needs its own cast compliance. SHH STEEL can produce and supply staged deliveries by size priority. Weld thread: matching Alloy 28-class fillers; strict cleanliness and heat input.
FAQ
-
What is EN 10297-2 1.4563 seamless stainless steel tube used for?
- EN 10297-2 1.4563 (X1NiCrMoCu31-27-4) is seamless tube for mechanical and general engineering — sulphuric and phosphoric acid-adjacent mechanical lines, chemical transfer, and fabrications naming N08028-class chemistry. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service.
-
Is EN 10297-2 1.4563 the same as EN 10216-5 1.4563?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4563 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4563 / X1NiCrMoCu31-27-4?
- Delivery framing for 1.4563 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1070–1150 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4563?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4563 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4563 compare with sister grades 1.4539, 1.4529, 1.4547?
- 1.4563 / X1NiCrMoCu31-27-4 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4539, 1.4529, 1.4547. Design caution: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4563 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching Alloy 28-class fillers; strict cleanliness and heat input. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4563?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4563?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4563 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD; higher solution-anneal band. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias Alloy 28 / N08028 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use Alloy 28 / N08028 in body text and BOM notes, but lock EN 10297-2 and 1.4563 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4563?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: specialty alloy cost and weld procedure control — do not substitute from 904L without process approval Sister pointers: 1.4539, 1.4529, 1.4547. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4563 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4563 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4563 (X1NiCrMoCu31-27-4) is seamless stainless tube for mechanical and general engineering — Alloy 28-class high-Ni Cr-Mo-Cu austenitic seamless tube for severe chemical mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4539, 1.4529, 1.4547. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.