EN 10297-2 1.4466 Seamless Stainless Steel Tube
What is EN 10297-2 1.4466 Seamless Stainless Steel Tube
If the purchase file still names only a commercial alias such as 25-22-2 / S31050-class without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4466 (X1CrNiMoN25-22-2) selects seamless tube for mechanical and general engineering. 1.4466 is a specialty austenitic in EN 10297-2 — order it when the chemistry list says 25-22-2, not as a casual upgrade from 1.4404. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Mill path for 1.4466: specialty seamless OD on enquiry; solution anneal band is higher than commodity 316L. SHH STEEL can produce and supply X1CrNiMoN25-22-2 under EN 10297-2 1.4466 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
On the shop floor people still say “25-22-2 / S31050-class tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4466, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service. Typical duties include urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry. Design caution: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
Scope discipline matters: 1.4466 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4466: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Inside this seamless general-purpose series, compare EN 10297-2 1.4335, EN 10297-2 1.4539, EN 10297-2 1.4563. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4466.
Chemical Composition of EN 10297-2 1.4466
Cast window focus for 1.4466: Every 1.4466 heat under EN 10297-2 must meet the cast (ladle) analysis for X1CrNiMoN25-22-2 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 25-22-2 / S31050-class is body text only. Corrosion thread: high Cr-Ni-Mo-N balance for aggressive oxidising and some reducing chemical media within the corrosion-resisting set.
Use the table as a working cast-analysis checklist for 1.4466 (X1CrNiMoN25-22-2). It mirrors public BSSA EN 10297-2 figures for buyer convenience; contractual acceptance still cites the edition named on the purchase order. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| 1.4466 / X1CrNiMoN25-22-2 | ≤0.020 | ≤0.70 | ≤2.00 | ≤0.025 | ≤0.010 | 24.0–26.0 | 2.00–2.50 | 21.0–23.0 | 0.10–0.16 |
Mechanical Properties of EN 10297-2 1.4466
Ambient floors focus for 1.4466: Table mechanical floors for 1.4466 / X1CrNiMoN25-22-2 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 260 MPa, Rp1.0 min 295 MPa, Rm min 540 MPa, longitudinal elongation min 40%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: austenitic corrosion-resisting. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 260 | 295 | 540 min | 40 | 30 | – |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4466 / X1CrNiMoN25-22-2. Guideline solution/anneal band (Annex B): 1070–1150 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4466
Seamless route narrative for 1.4466: EN 10297-2 does not offer a welded route for 1.4466. Tube in X1CrNiMoN25-22-2 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. For 1.4466, SHH STEEL aligns the Annex A symbol to the duty: descaled HFD/CFD for general mechanical tube, CFA for cleaner bright OD, and CFG/CFP when a measured roughness target is part of the order text. Weld thread: matching high-alloy fillers; dilution and interpass control are critical.
For austenitic 1.4466, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4466 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1070–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4466. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4466: specialty seamless OD on enquiry; solution anneal band is higher than commodity 316L. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
Dimensions and Tolerances for EN 10297-2 1.4466
Dimensional order line for 1.4466: Dimensional orders for 1.4466 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Specialty seamless od on enquiry; solution anneal band is higher than commodity 316l. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4466: specialty seamless OD on enquiry; solution anneal band is higher than commodity 316L. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Equivalent Grades for EN 10297-2 1.4466
Equivalence talk for 1.4466 starts with X1CrNiMoN25-22-2: 1.4466 / X1CrNiMoN25-22-2 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 25-22-2 / S31050-class appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4335, 1.4539, 1.4563. Hook for buyers still using only the 25-22-2 / S31050-class alias: lock EN 10297-2 1.4466 on the order line. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
Heat Treatment and Delivery Condition for EN 10297-2 1.4466
Austenitic 1.4466 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1070–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching high-alloy fillers; dilution and interpass control are critical.
Fabrication HT reminder for 1.4466 (+AT): Hot-working temperature bands in Annex B for X1CrNiMoN25-22-2 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4466 should match +AT. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Corrosion Resistance of EN 10297-2 1.4466
Corrosion behaviour of EN 10297-2 1.4466 tracks its austenitic corrosion-resisting balance: high Cr-Ni-Mo-N balance for aggressive oxidising and some reducing chemical media within the corrosion-resisting set. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits Corrosion thread: high Cr-Ni-Mo-N balance for aggressive oxidising and some reducing chemical media within the corrosion-resisting set.
Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4335, 1.4539, 1.4563 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4466 is austenitic corrosion-resisting. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
Applications of EN 10297-2 1.4466 Tube
Applications of EN 10297-2 1.4466 tube centre on mechanical and general engineering rather than PED pressure shells: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry. Role summary: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
Typical BOM language pairs EN 10297-2 1.4466 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “25-22-2 / S31050-class” substitutions do not creep in. Primary application sketch: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Weldability of EN 10297-2 1.4466
1.4466 / X1CrNiMoN25-22-2 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching high-alloy fillers; dilution and interpass control are critical. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching high-alloy fillers; dilution and interpass control are critical.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4466: matching high-alloy fillers; dilution and interpass control are critical. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
Surface Finishes for EN 10297-2 1.4466
Finish selection for 1.4466 on Annex A: For 1.4466, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 25-22-2 / S31050-class, but the finish symbol still belongs on the EN 10297-2 line. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
If 1.4466 will sit in a humid warehouse before use, ask for sealed wrap and humidity indicators on the packing list. Carbon-steel dunnage never contacts the stainless OD — timber or plastic separators are the default. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Inspection and Testing for EN 10297-2 1.4466
Inspection lot framing for 1.4466 in austenitic corrosion-resisting: NDT intensity on 1.4466 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4466 heat identity intact from cast through bundle tag. Weld thread: matching high-alloy fillers; dilution and interpass control are critical.
For 1.4466, dimensional inspection covers OD, wall, length, and agreed out-of-roundness/eccentricity. IGC and NDT Options appear as separate certificate lines. Correlation numbers link pieces to the EN 10204 3.1 file without opening every crate. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
Packaging and Shipping for EN 10297-2 1.4466
Dispatch note for 1.4466 (25-22-2 / S31050-class body alias only): SHH STEEL ships EN 10297-2 1.4466 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Marking and identity for 1.4466: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4466, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4466 follows the Annex A symbol on the order. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
SHH STEEL closes the packing note for 1.4466 only after caps, wrap, and tags match the Annex A finish and the cut-length list. Shortages or mixed walls are corrected in the warehouse — not discovered at the jobsite. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
Why Choose SHH STEEL
Why 1.4466 with SHH STEEL — role: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service. SHH STEEL can produce and supply X1CrNiMoN25-22-2 as EN 10297-2 1.4466 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
Grade advice stays practical for 1.4466. If the duty needs a sister chemistry, we point to 1.4335, 1.4539, 1.4563. Design caution for this number: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits Mill slots are planned against the Annex A symbol you order — bright and polished finishes are not assumed. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4466. EN 10297-2 1.4466 supply from SHH STEEL covers hot- and cold-finished seamless routes for X1CrNiMoN25-22-2. We can produce and supply to the mechanical floors of the ordered delivery condition. The Stock / Available sizes section is the enquiry checklist. Use thread: urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4466 / X1CrNiMoN25-22-2 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
For 1.4466, treat the size table as an RFQ aid. Context: specialty seamless OD on enquiry; solution anneal band is higher than commodity 316L. Confirm tolerance class and Annex A symbol so CFD/CFA slots are not confused with HFD on the acknowledgement. Duty thread: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
For 1.4466, ask early about cut-to-length packages and NDT Options. Peer mill size charts are indicative only. SHH STEEL can produce and supply the ordered Annex A finish once the acknowledgement locks OD × wall. Sisters often discussed: 1.4335, 1.4539, 1.4563. Weld thread: matching high-alloy fillers; dilution and interpass control are critical.
FAQ
-
What is EN 10297-2 1.4466 seamless stainless steel tube used for?
- EN 10297-2 1.4466 (X1CrNiMoN25-22-2) is seamless tube for mechanical and general engineering — urea-adjacent and nitric/chemical process mechanical tubing, high-alloy transfer lines, and duties naming 25-22-2 chemistry. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service.
-
Is EN 10297-2 1.4466 the same as EN 10216-5 1.4466?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4466 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4466 / X1CrNiMoN25-22-2?
- Delivery framing for 1.4466 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1070–1150 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4466?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4466 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4466 compare with sister grades 1.4335, 1.4539, 1.4563?
- 1.4466 / X1CrNiMoN25-22-2 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4335, 1.4539, 1.4563. Design caution: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4466 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching high-alloy fillers; dilution and interpass control are critical. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4466?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4466?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4466 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD on enquiry; solution anneal band is higher than commodity 316L. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 25-22-2 / S31050-class belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 25-22-2 / S31050-class in body text and BOM notes, but lock EN 10297-2 and 1.4466 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4466?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: IGC column in Table 7 is marked “-” for this number — confirm purchaser test Options; do not invent PREN marketing digits Sister pointers: 1.4335, 1.4539, 1.4563. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4466 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4466 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4466 (X1CrNiMoN25-22-2) is seamless stainless tube for mechanical and general engineering — low-C nitrogen-bearing 25Cr-22Ni-2Mo austenitic seamless tube for severe chemical mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4335, 1.4539, 1.4563. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.