EN 10297-2 1.4006 Seamless Stainless Steel Tube
What is EN 10297-2 1.4006 Seamless Stainless Steel Tube
If the purchase file still names only a commercial alias such as 410 without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4006 (X12Cr13) selects seamless tube for mechanical and general engineering. EN 10297-2 lists only one martensitic number — 1.4006 / X12Cr13 — so “410 QT seamless tube” under this standard must name the QT level on the purchase order. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Mill path for 1.4006: mechanical seamless OD with QT delivery; confirm hardenability through wall on heavier gauges. SHH STEEL can produce and supply EN 10297-2 1.4006 seamless stainless steel tube — hot-finished or cold-finished on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, hydrostatic, eddy current, ultrasonic, and related NDT Options). Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
On the shop floor people still say “410 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4006, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts. Typical duties include pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named. Design caution: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
Do not treat an EN 10297-2 1.4006 MTC as automatic clearance for pressure equipment — Part 5 of EN 10216 is the pressure seamless home. Likewise, welded pressure tube lives under EN 10217-7, which is a different product form and test regime. Match the product standard to the duty before dual-marking talk begins. Role reminder for 1.4006: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Inside this seamless general-purpose series, compare EN 10297-2 1.4002, EN 10297-2 1.4016. Hub: EN 10297-2.
Chemical Composition of EN 10297-2 1.4006
Cast window focus for 1.4006: Cast analysis for EN 10297-2 1.4006 follows the X12Cr13 limits published for this standard’s corrosion- or heat-resisting tables. Key windows on a typical certificate include C 0.08–0.15, Cr 11.5–13.5, Mo ≤0.75, Si ≤1.00, S ≤0.015. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 410 is body text only. Corrosion thread: martensitic chromium resistance for mild atmospheres; not selected for chloride process duty.
For 1.4006 / X12Cr13, the following chem table is the public EN 10297-2 window SHH STEEL uses at enquiry. Product-analysis Options, when taken, apply the standard’s permitted deviations rather than inventing tighter shop limits. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
| Steel | C | Si | Mn | P | S | Cr | Mo |
|---|---|---|---|---|---|---|---|
| 1.4006 / X12Cr13 | 0.08–0.15 | ≤1.00 | ≤1.50 | ≤0.040 | ≤0.015 | 11.5–13.5 | ≤0.75 |
Mechanical Properties of EN 10297-2 1.4006
Ambient floors focus for 1.4006: Ambient mechanical properties for EN 10297-2 1.4006 follow Tables 6–9 by family. For this grade the delivery-condition floors to watch are: +QT 550: Rp0.2 min 400 MPa, Rm min 550 MPa, A long. min 15%; +QT 650: Rp0.2 min 450 MPa, Rm min 650 MPa, A long. min 12%. Intergranular corrosion resistance per EN ISO 3651-2 is tabulated where applicable — see the IGC column on the mechanical table below. Family: martensitic corrosion-resisting. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +QT 550 | 400 | 410 | 550 min | 15 | 15 | No |
| +QT 650 | 450 | 460 | 650 min | 12 | 12 | No |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4006 / X12Cr13. Guideline solution/anneal band (Annex B): 950–1010 °C harden + temper; cooling: oil or air quench then temper.
Seamless Tube Manufacture for EN 10297-2 1.4006
Seamless route narrative for 1.4006: Seamless 1.4006 / X12Cr13 is manufactured by hot working a pierced hollow and finishing hot or cold before quench-and-temper. Martensitic product is not ordered as soft austenitic stock. Annex A process-route symbols for seamless 1.4006 include HFD (hot finished, heat treated, descaled), CFD (cold finished, heat treated, descaled), CFA (cold finished bright annealed), CFG (ground), and CFP (polished). Combinations may be agreed at enquiry. Weld thread: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows.
Delivery on EN 10297-2 Table 6 is quenched and tempered: order +QT 550 or +QT 650 explicitly for 1.4006. Annex B hardens around 950–1010 °C with oil or air quench, then temper to the ordered QT level — soft annealed stock is not a Table 6 substitute. Mechanical floors differ between QT levels, so the delivery condition belongs in marking and on the MTC. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4006. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4006: mechanical seamless OD with QT delivery; confirm hardenability through wall on heavier gauges. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
Dimensions and Tolerances for EN 10297-2 1.4006
Dimensional order line for 1.4006: Dimensional orders for 1.4006 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Mechanical seamless od with qt delivery; confirm hardenability through wall on heavier gauges. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4006: mechanical seamless OD with QT delivery; confirm hardenability through wall on heavier gauges. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Equivalent Grades for EN 10297-2 1.4006
Equivalence talk for 1.4006 starts with X12Cr13: 1.4006 / X12Cr13 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 410 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4002, 1.4016. Hook for buyers still using only the 410 alias: lock EN 10297-2 1.4006 on the order line. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
Heat Treatment and Delivery Condition for EN 10297-2 1.4006
Delivery on EN 10297-2 Table 6 is quenched and tempered: order +QT 550 or +QT 650 explicitly for 1.4006. Annex B hardens around 950–1010 °C with oil or air quench, then temper to the ordered QT level — soft annealed stock is not a Table 6 substitute. Weld thread: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows.
Fabrication HT reminder for 1.4006 (+QT 550 / +QT 650): Hot-working temperature bands in Annex B for X12Cr13 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4006 should match +QT 550 / +QT 650. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Corrosion Resistance of EN 10297-2 1.4006
Corrosion behaviour of EN 10297-2 1.4006 tracks its martensitic balance: martensitic chromium resistance for mild atmospheres; not selected for chloride process duty. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock Corrosion thread: martensitic chromium resistance for mild atmospheres; not selected for chloride process duty.
SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4006. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Family filing for 1.4006 is martensitic corrosion-resisting. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
Applications of EN 10297-2 1.4006 Tube
Applications of EN 10297-2 1.4006 tube centre on mechanical and general engineering rather than PED pressure shells: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named. Role summary: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
Skip 1.4006 when the specification locks a different family — for example forcing ferritic 1.4006 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4002, 1.4016. Primary application sketch: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Weldability of EN 10297-2 1.4006
1.4006 / X12Cr13 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4006: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
Surface Finishes for EN 10297-2 1.4006
Finish selection for 1.4006 on Annex A: For 1.4006, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 410, but the finish symbol still belongs on the EN 10297-2 line. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
Transit protection for 1.4006 is sized to the Annex A finish: heavier wrap for CFA/CFG/CFP, standard export wrap for HFD/CFD. Open-deck ocean exposure without wrap is refused on bright tube. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Inspection and Testing for EN 10297-2 1.4006
Inspection lot framing for 1.4006 in martensitic corrosion-resisting: SHH STEEL EN 10204 3.1 documents for 1.4006 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4006 heat identity intact from cast through bundle tag. Weld thread: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows.
Purchasers who need witness points on 1.4006 should say so at enquiry. Routine mill inspection still records cast chemistry, tensile results, delivery condition, and dimensions; witness adds scheduling, not a different chemistry table. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
Packaging and Shipping for EN 10297-2 1.4006
Dispatch note for 1.4006 (410 body alias only): SHH STEEL ships EN 10297-2 1.4006 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Marking and identity for 1.4006: When cut lengths and special ends are part of the 1.4006 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4006 follows the Annex A symbol on the order. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
Ocean containers loaded with 1.4006 use desiccant and sealed wrap when the route or season warrants it. Inland deliveries may omit container desiccant but never omit end caps on precision OD. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
Why Choose SHH STEEL
Why 1.4006 with SHH STEEL — role: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts. SHH STEEL can produce and supply EN 10297-2 1.4006 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “410 tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Grade advice stays practical for 1.4006. If the duty needs a sister chemistry, we point to 1.4002, 1.4016. Design caution for this number: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock Technical clarification on QT level, cold- versus hot-finished rows, or duplex thin-wall footnotes happens before acknowledgement. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock.
Supply Capability
For 1.4006, SHH STEEL can produce and supply seamless tube in the X12Cr13 analysis with the Annex A finish you name. Lead time tracks hollow stock and heat-treatment slots; Stock / Available sizes below helps size the first RFQ. Use thread: pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4006 / X12Cr13 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +QT 550 / +QT 650 |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Available sizes for 1.4006 follow seamless general-purpose practice: mechanical seamless OD with QT delivery; confirm hardenability through wall on heavier gauges. Dual size lists against sister grades are welcome on one enquiry sheet. Duty thread: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
Dual documentation talk for 1.4006 versus 1.4002, 1.4016 is fine at enquiry — each steel number still needs its own cast compliance. SHH STEEL can produce and supply staged deliveries by size priority. Weld thread: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows.
FAQ
-
What is EN 10297-2 1.4006 seamless stainless steel tube used for?
- EN 10297-2 1.4006 (X12Cr13) is seamless tube for mechanical and general engineering — pump shafts sleeves, wear-resistant mechanical liners, hydraulic components, and general engineering where 410 QT properties are named. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts.
-
Is EN 10297-2 1.4006 the same as EN 10216-5 1.4006?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4006 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4006 / X12Cr13?
- Delivery framing for 1.4006 is +QT 550 / +QT 650 under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 950–1010 °C harden + temper with oil or air quench then temper cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4006?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4006 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4006 compare with sister grades 1.4002, 1.4016?
- 1.4006 / X12Cr13 is filed as martensitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4002, 1.4016. Design caution: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4006 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: preheat/interpass and post-weld temper aligned with QT condition; hydrogen control matters; soft annealed delivery is outside the Table 6 QT rows. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4006?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4006?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4006 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: mechanical seamless OD with QT delivery; confirm hardenability through wall on heavier gauges. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 410 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 410 in body text and BOM notes, but lock EN 10297-2 and 1.4006 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4006?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what martensitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: order +QT 550 or +QT 650 explicitly — the two tempered levels have different Rp/Rm/A floors; do not treat as soft annealed ferritic stock Sister pointers: 1.4002, 1.4016. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4006 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4006 is filed as martensitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4006 (X12Cr13) is seamless stainless tube for mechanical and general engineering — the only martensitic grade in EN 10297-2 — quenched-and-tempered 13%Cr seamless tube for strength-led mechanical parts. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4002, 1.4016. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.