EN 10217-7 1.4410 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4410 Welded Stainless Steel Tube

EN 10217-7 1.4410 / X2CrNiMoN25-7-4 welded stainless pressure tube (2507 / S32750), austenitic-ferritic (duplex), cast analysis per EN table, ambient Rp0.2 min 550 MPa, Rm 800–1000, solution annealed 1040–1120 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4410 / X2CrNiMoN25-7-4 (2507 / S32750 — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~12–219 mm OD × 1.0–12.7 mm wall within duplex characterisation (~30 mm wall band unless agreed); other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4410 Welded Stainless Steel Tube

EN 10217-7 covers welded stainless pressure tube only — seamless twins live under EN 10216-5. For welded product, steel number 1.4410 (X2CrNiMoN25-7-4) sits in the austenitic-ferritic (duplex) grade tables and is the designation that belongs on the MTC when the commercial conversation still says 2507 / S32750. Specifying EN 10217-7, 1.4410, test category, and delivery-condition / options on the purchase order is what makes cast chemistry, weld-seam manufacture, heat treatment, mechanical floors, leak-tightness, and marking line up. Engineering role: super duplex 2507 welded pressure tube for severe chloride and high-strength PED service.

SHH STEEL can produce and supply EN 10217-7 1.4410 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover specialty welded sizes; confirm OD×wall and delivery condition early. Browse the series hub at EN 10217-7.

2507 / S32750 welded pressure under EN is 1.4410 — SHH STEEL will not “make it work” with a 2205 procedure on a 1.4410 seam. Typical welded pressure duties include offshore seawater, high-pressure chloride process lines, and chemical PED systems that outgrow 2205. Design caution: super duplex fabrication is unforgiving on heat input and intermetallics — wrong procedures destroy corrosion resistance even if tensile numbers look fine Commercially the grade is often called 2507 / S32750; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4410 / X2CrNiMoN25-7-4 on the MTC. Sister numbers on this hub include EN 10217-7 1.4462, EN 10217-7 1.4501, EN 10217-7 1.4547.4462, 1.4501, 1.4547.

Do not mix product forms: EN 10217-7 1.4410 is welded tube; seamless pressure tube is EN 10216-5. EN ISO 1127 guides preferred sizes. Longitudinal arc/laser routes in Table 1 are the manufacture story — spiral is not treated as a standard Part 7 route on this page. Live seamless sister: EN 10216-5 1.4410. Related live ASTM/ASME anchors: A789 S32750.

Chemical Composition of EN 10217-7 1.4410

For X2CrNiMoN25-7-4 ordered as EN 10217-7 1.4410, cast (ladle) analysis is mandatory against the grade table. Option 6 covers product analysis deviations. SHH STEEL reports the cast that was melted and will not present unpublished tighter ranges as if they were Part 7 limits.

Composition limits shown for 1.4410 follow BSSA’s EN 10217-7 chemical article with public standard cross-check. Ranges beat single maxima where printed. Use the purchased 2021 edition as the contractual text.

Element 1.4410 cast analysis (mass %)
Carbon (C) ≤0.030
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.035
Sulfur (S) ≤0.015
Nitrogen (N) 0.20–0.35
Chromium (Cr) 24.0–26.0
Nickel (Ni) 6.0–8.0
Molybdenum (Mo) 3.00–4.50

Cast limits tabulated for 1.4410 follow BSSA’s EN 10217-7 chemical publication with a public Part 7 cross-check. For this austenitic-ferritic (duplex) X2CrNiMoN25-7-4 entry, intentional addition of unlisted elements needs purchaser agreement; finishing additions remain under scrap controls that protect corrosion and toughness.

Mechanical Properties of EN 10217-7 1.4410

Solution-annealed duplex 1.4410 follows the Part 7 austenitic-ferritic ambient mechanical table for X2CrNiMoN25-7-4, characterised through walls near 30 mm unless Options say otherwise. Proof stress is Rp0.2 only. Impact energies become certified results only when the corresponding Options are ordered.

BSSA’s EN 10217-7 ambient mechanical article is the public crib behind the 1.4410 table. Annealing bands for X2CrNiMoN25-7-4 are cross-checked from public EN stainless documents and marked UNCERTAIN vs paid Part 7:2021 footnotes. SHH STEEL refuses to blend ASTM or seamless-only tensile floors into this welded certificate.

Property 1.4410 ambient (solution annealed +AT)
Rp0.2 min (MPa) 550
Rp1.0 min (MPa) — (duplex tables use Rp0.2)
Rm (MPa) 800–1000
A min % long / trans 20 / 20
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1040–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 40 at -40 °C (Option to verify)

Citation for 1.4410 / X2CrNiMoN25-7-4: BSSA mechanical properties to BS EN 10217-7 (ambient) plus public EN annealing bands flagged UNCERTAIN vs paid Part 7 footnotes. Impact lines are characterisation until Options convert them to tested results.

Welded Tube Manufacture for EN 10217-7 1.4410

The weld seam on EN 10217-7 1.4410 is longitudinal, not spiral. Arc or laser welding joins the formed edges of X2CrNiMoN25-7-4 strip or plate under one of the Table 1 manufacturing routes, with subsequent outside grind or bead work when that path is selected. Continuous strip forming dominates everyday OD; plate routes cover larger diameters and thicker walls. Welds that only joined coil ends before forming must not remain in the finished tube. Specify EN 10216-5 when the line needs seamless pressure stainless instead of this welded Part 7 product.

On duplex 1.4410, mill weld procedure and any cold work on WCA/WCR routes (commonly OD ≤ 168.3 mm) must protect the austenite–ferrite balance that underwrites chloride SCC resistance for X2CrNiMoN25-7-4. Table 2 symbols separate starting flat-product path and surface: W1/W1A/W1R from hot-rolled, W2/W2A/W2R from cold-rolled, WCA/WCR for cold-finished recrystallized-weld routes, WG/WP when ground or polished scope is agreed. Option 5 locks the symbol; otherwise the manufacturer chooses. SHH STEEL can produce and supply 1.4410 on the common heat-treated descaled and cold-finished routes when the enquiry names the symbol and any bead-work suffix. Shop note from this grade: super-duplex fillers; tight heat-input; often mandatory ferrite and corrosion tests on WPS/PQR

A complete 1.4410 order names the test category up front. TC2 is the heavier seam-NDT path; TC1 is lighter but still includes full leak-tightness unless Option 15 constrains the method. SHH STEEL’s documentation for X2CrNiMoN25-7-4 cites the Table 1 route and Table 2 symbol used on the shipment.

Dimensions and Tolerances for EN 10217-7 1.4410

For X2CrNiMoN25-7-4 welded pressure tube as 1.4410, the purchase order states outside diameter and wall. Preferred dimensions track EN ISO 1127; mass calculations use stainless densities. Tolerance language is EN 10217-7 / EN ISO 1127, with Option 20 for D4. Keep ovality and eccentricity inside their parent tolerances; watch radial offset at the seam.

When lengths must be exact, call Option 19; when ends need bevels on wall ≥ 3.2 mm, call Option 18. Instrumentation and hygienic OD on 1.4410 often prefer cold-finished WCA/WCR. Size, tolerance, and delivery-condition symbol are aligned by SHH STEEL before the forming/weld slot is booked.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

Measured OD × wall for 1.4410 appear on the EN 10204 document against the class you ordered. Straightness and ends for X2CrNiMoN25-7-4 track Part 7; if Option 20 D4 is named, the finishing route must be capable of holding it. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4410 / X2CrNiMoN25-7-4 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4410

Under Part 7 the correct welded designation is 1.4410 (X2CrNiMoN25-7-4). The alias 2507 / S32750 helps humans talk, not mills accept. ASTM/ASME equivalents are live cross-links for comparison; seamless EN 10216-5 is the product-form sister when a weld seam is forbidden.

When dual marking is requested, each standard’s mechanical and test regime still has to be satisfied on its own terms — an ASTM alias of 2507 / S32750 does not waive EN 10217-7 tensile, leak-tightness, or TC1/TC2 rules for 1.4410 / X2CrNiMoN25-7-4. Keep the welded versus seamless product-form split explicit on the purchase order and on the MTC.

Reference Designation Note
EN 10217-7 1.4410 / X2CrNiMoN25-7-4 This product standard (welded pressure tube)
EN steel name X2CrNiMoN25-7-4 EN 10027-1 designation used in body and marking
Commercial alias (body only) 2507 / S32750 Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4410 Related live page — different product form (seamless)
A789 S32750 A789 S32750 Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4462, EN 10217-7 1.4501, EN 10217-7 1.4547. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4410. Live cross-standard anchors: A789 S32750.

Heat Treatment and Delivery Condition for EN 10217-7 1.4410

Heat treatment on 1.4410 is not a separate afterthought — it is built into many Table 2 delivery symbols (W1A, W2A, WCA, WCR, W1R/W2R among them). The mechanical tables for X2CrNiMoN25-7-4 assume solution-annealed (+AT) material after uniform heating and rapid cool. For X2CrNiMoN25-7-4 under steel number 1.4410, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Annealing temperature listed for 1.4410 / X2CrNiMoN25-7-4 is 1040–1120 °C; cooling water or air. These figures are public EN cross-checks and stay UNCERTAIN until a paid Part 7 footnote is confirmed. Option 5 freezes whether the tube is descaled, bright-annealed, ground, or polished after that heat treatment.

Item 1.4410
Solution annealing band (public) 1040–1120 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

For 1.4410, SHH STEEL treats delivery condition as a certified fact. The EN 10204 document states which Table 2 symbol was applied to X2CrNiMoN25-7-4, what heat treatment that implied, and how the weld seam was left after finishing — especially important when WCA/WCR recrystallized-weld routes were ordered.

Corrosion Resistance of EN 10217-7 1.4410

Choose 1.4410 (X2CrNiMoN25-7-4) when welded PED tubing must carry this corrosion story: high Cr-Mo-N duplex for very high pitting resistance and chloride SCC performance in seawater-class media. Delivery-condition IGC resistance is characterised to EN ISO 3651-2 methods in the Part 7 tables, but a tested IGC result still requires Option 13 on the order.

Sensitisation limits associated with IGC guidance are time-and-temperature metallurgy notes for X2CrNiMoN25-7-4. They do not replace PED joint design or justify skipping Option 13 when a tested IGC result is required on 1.4410. Use EN 10217-7 1.4462, EN 10217-7 1.4501, EN 10217-7 1.4547 if the alloy family is wrong.

Applications of EN 10217-7 1.4410 Tube

Applications for steel number 1.4410 / X2CrNiMoN25-7-4 cluster around welded PED service that tolerates a mill seam: offshore seawater, high-pressure chloride process lines, and chemical PED systems that outgrow 2205. Delivery condition and test category on the order decide how that tube is finished and inspected before it reaches the spool.

Skip 1.4410 when the specification locks seamless product (EN 10216-5 — see EN 10216-5 1.4410), when ASTM A269/A312 text is the only acceptance language, or when corrosion/strength clearly points at another family. SHH STEEL can produce and supply X2CrNiMoN25-7-4 welded tube in the enquiry band and will redirect to a sister or live ASTM/ASME page when that is wiser. Related live pages: A789 S32750.

Weldability of EN 10217-7 1.4410

Mill welding of EN 10217-7 1.4410 is the longitudinal arc/laser seam on the ordered Table 1 route; field or shop welding is a separate PED joint design. Filler and procedure choices track the austenitic-ferritic (duplex) chemistry of X2CrNiMoN25-7-4. Practical note: super-duplex fillers; tight heat-input; often mandatory ferrite and corrosion tests on WPS/PQR

Shop and field welding decisions on 1.4410 (filler, heat input, PWHT, ferrite targets on duplex) belong to the fabricator’s WPS and the PED file. SHH STEEL’s mill scope for X2CrNiMoN25-7-4 stops at ordered chemistry, longitudinal route, delivery-condition heat treatment, mechanical acceptance, and leak-tightness / NDT as specified.

Surface Finishes for EN 10217-7 1.4410

Delivery-condition symbols double as surface codes on 1.4410. Descaled W1A/W2A, bright-annealed W1R/W2R/WCR, and WG/WP ground or polished map the common finishes for X2CrNiMoN25-7-4. Anything marketed as “hygienic” without a symbol and a measurable note is incomplete order text. Keep carbon-steel strap and rusty fixtures away from the OD — free-iron staining is a stainless-specific failure mode on 2507 / S32750 tube.

Call out interior roughness, electropolish, or protective films explicitly when they matter to the PED spool. SHH STEEL can produce and supply reported descaled, bright-annealed, and polished finishes on 1.4410 / X2CrNiMoN25-7-4 and will not substitute marketing adjectives for measured surface data on 2507 / S32750 welded pressure tube.

Surface and delivery condition are one conversation on Part 7. Changing from W2A to WCR on 1.4410 is a process change for X2CrNiMoN25-7-4, not a sticker change. SHH STEEL plans bright-anneal or polish capacity with the weld slot and documents the symbol that was really applied to this 2507 / S32750 shipment.

Inspection and Testing for EN 10217-7 1.4410

Every 1.4410 length sees leak-tightness testing; chemistry is cast-based; tensile follows TC1 or TC2 sampling; technological tests track diameter and wall. Option 15 can lock hydro versus eddy current. Visual, dimensional, and identification checks apply to X2CrNiMoN25-7-4 as ordered. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4410 purchase order so X2CrNiMoN25-7-4 inspection planning matches the PED file before weld slots are locked.

Choose TC2 when the PED file wants denser seam NDT on 1.4410. Add Option 13 for IGC and the impact Options when verified toughness is required. Certificates from SHH STEEL list cast chemistry, delivery-condition status, ambient tensile, and leak/NDT statements; lead time is not improved by omitting mandatory work.

Impact Options on 1.4410 are the only path to certified joules; characterisation energies in the table are not automatic certificate entries. SHH STEEL runs Charpy work for X2CrNiMoN25-7-4 only when those Options are on the order.

Packaging and Shipping for EN 10217-7 1.4410

Packaging for welded 1.4410 tube is built around surface protection and traceability. Ends are capped, lengths are grouped by OD × wall, and export units take waterproof wrap. Duplex 1.4410 OD that was ordered bright-annealed or polished gets sleeve protection so the W1R/W2R/WCR/WP surface survives handling; descaled W1A/W2A utility tube still needs clean dunnage under the weld seam region. No carbon-steel strap bears on the X2CrNiMoN25-7-4 OD; stainless or padded contact is mandatory so 2507 / S32750 finishes do not arrive with free-iron rust tracks that fail goods-in visual checks.

Expect manufacturer ID, size, EN 10217-7, 1.4410/X2CrNiMoN25-7-4, cast, TC1 or TC2, and inspection correlation on the tube marking set. Option 5 symbols are shown when locked. SHH STEEL checks marking against the order text for every 2507 / S32750 shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4410 / X2CrNiMoN25-7-4 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Crates and bundles for 1.4410 carry IDs that map to MTC heats. Special lengths and bevels are isolated in the pack. SHH STEEL treats the packaging paragraph of the order as production input, not afterthought, for X2CrNiMoN25-7-4. SHH STEEL treats packing and marking for EN 10217-7 1.4410 / X2CrNiMoN25-7-4 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can supply and produce EN 10217-7 1.4410 as ordered welded tube: correct Table 2 condition, ordered test category, and EN 10204 3.1 documents for X2CrNiMoN25-7-4. Generic “2507 / S32750” rack stock is not re-stamped as Part 7, and ASTM or seamless tensile tables are not borrowed onto this certificate.

Sister guidance on this hub includes EN 10217-7 LINKPLACE1.4462, EN 10217-7 LINKPLACE1.4501, EN 10217-7 LINKPLACE1.4547. For 1.4410 specifically: super duplex fabrication is unforgiving on heat input and intermetallics — wrong procedures destroy corrosion resistance even if tensile numbers look fine Closing a sale on the wrong chemistry is treated as a failure mode, not a success metric. Live ASTM/ASME anchors: A789 S32750.

Supply Capability

For X2CrNiMoN25-7-4 as EN 10217-7 1.4410, SHH STEEL can produce and supply to the ordered edition and inspection package. Read the capability grid and Stock / Available sizes map as an enquiry aid, not a frozen inventory promise. Specialty welded sizes; confirm od×wall and delivery condition early.

Item SHH STEEL capability for 1.4410
Standard EN 10217-7
Grade 1.4410 / X2CrNiMoN25-7-4
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~12–219 mm OD × 1.0–12.7 mm wall within duplex characterisation (~30 mm wall band unless agreed); other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

No published tonnage claim is made for EN 10217-7 1.4410. The matrix shows enquiry-typical OD × wall bands for X2CrNiMoN25-7-4; live answer needs your size list, test category, and delivery-condition symbol.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Routine extras include Option 19 lengths, Option 18 bevels, Option 13 IGC, and parallel asks on 1.4462, 1.4501, 1.4547. OD × wall examples are not a substitute for the standard. SHH STEEL can produce and supply 1.4410 inside this enquiry framework when materials and weld slots are open.

FAQ

What is EN 10217-7 1.4410 welded stainless steel tube used for?
EN 10217-7 1.4410 (X2CrNiMoN25-7-4) is welded pressure tube for PED-oriented duties that need the austenitic-ferritic (duplex) chemistry story with a longitudinal mill seam. Typical service is offshore seawater, high-pressure chloride process lines, and chemical PED systems that outgrow 2205. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4410 the same as 2507 / S32750 under ASTM A269 or A312?
No. Commercial alias 2507 / S32750 may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A789 S32750.
Does EN 10217-7 1.4410 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4410. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4410?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 550 MPa, Rm 800–1000 MPa, and elongation 20% longitudinal / 20% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4410 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4410 when the enquiry names this steel number or the duty matches super duplex 2507 welded pressure tube for severe chloride and high-strength PED service. Compare EN 10217-7 1.4462, EN 10217-7 1.4501, EN 10217-7 1.4547 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: super duplex fabrication is unforgiving on heat input and intermetallics — wrong procedures destroy corrosion resistance even if tensile numbers look fine
What delivery conditions are available for EN 10217-7 1.4410?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4410?
SHH STEEL can produce and supply EN 10217-7 1.4410 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~12–219 mm OD × 1.0–12.7 mm wall within duplex characterisation (~30 mm wall band unless agreed); other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Specialty welded sizes; confirm od×wall and delivery condition early.
TC1 or TC2 for EN 10217-7 1.4410?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4410?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4410.
What documents come with SHH STEEL EN 10217-7 1.4410?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4410, size, cast, and test category.
How do I enquire for EN 10217-7 1.4410 with SHH STEEL?
Send EN 10217-7, steel number 1.4410 / X2CrNiMoN25-7-4, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4410 (X2CrNiMoN25-7-4) is welded stainless pressure tube for PED-oriented service in the austenitic-ferritic (duplex) family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4410 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X