EN 10028-6 P460QL2 quenched and tempered special low-temperature pressure vessel steel plate, −60 °C, 1.8864, SHH STEEL

EN 10028-6 P460QL2 Steel Plate | P460QL2 QT -60°C Vessel Plate supplier

EN 10028-6 P460QL2 is European QT fine-grain low-temperature vessel plate, steel number 1.8882. Yield is 460 MPa at ≤50 mm. Impact is −60 °C. SHH STEEL supplies P460QL2 worldwide as a global steel mill sourcing partner.
Keywords
EN 10028-6 P460QL2, P460QL2, P460QL2 steel plate, 1.8882, P460QL2 QT -60°C, P460QL2 equivalent, P460QL2 supplier
Equivalent Grades:
EN 10028-6 P460QL2 / ASTM A517 Gr / GB Q460E (struct near) — Material Specification: EN 10028-6 — Delivery: Quenched + Tempered (QT); -60℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
QT -60°C 460 MPa Pressure-Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-6 P460QL2 Steel?

P460QL2 is the −60 °C quenched-and-tempered quality in the P460 family of EN 10028-6. Buyers search EN 10028-6 P460QL2, P460QL2 steel plate, 1.8882, P460QL2 QT -60°C vessel plate and P460QL2 supplier. QL2 is colder than QL1. This page is not P460Q. Q is room-temperature QT. This page is not P460QH. QH is elevated-temperature QT. This page is not P460QL1. QL1 is −40 °C. This page is not EN 10028-3 P460NL2. NL2 is normalized −50 °C. This page is not EN 10028-5 P460ML2. ML2 is TMCP −50 °C. This page is not P355QL2. P355QL2 is a 355 MPa step.

Yield is 460 MPa at ≤50 mm. Tensile is 570–720 MPa. Steel number is 1.8882. Delivery is QT (Q). Charpy is specified at −60 °C when the order follows QL2. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-6, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

If a drawing says P460QL1, we will not ship P460QL2 and call colder automatically better without the buyer writing the name. If a drawing says −60 °C, we will not ship QL1 and call minus forty close. Dual marking with Q460DR steel plate is possible only when both books are fully met.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-6 P460QL2 Confirmed
Steel number 1.8882 Confirmed
Product specification EN 10028-6 + EN 10028-1 Applied
Steel type Weldable fine-grain QT, −60 °C Confirmed
Usual delivery Q quenched and tempered Confirmed
Yield idea 460 MPa at ≤50 mm Confirmed
Tensile 570–720 MPa at ≤50 mm Confirmed
Impact idea −60 °C Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and carbon steel plates. Chinese low-temperature 460 comparisons belong on GB/T 713.3. Normalized sisters belong on EN 10028-3. TMCP sisters belong on EN 10028-5. Structural QT belongs on EN 10025-6.

Chemical Composition

Cast analysis follows EN 10028-6. Product analysis follows EN 10028-1 when ordered.

Cast Analysis and Product Analysis — EN 10028-6 P460QL2 (1.8882)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.60 0.65
Manganese (Mn) 1.10 – 1.70 1.05 – 1.80
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.010 0.013
Aluminum total (Al), min 0.020 0.015
Nitrogen (N), max 0.015 0.017
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.30 0.35
Molybdenum (Mo), max 0.10 0.12
Nickel (Ni), max 0.80 0.85
Niobium (Nb), max 0.05 0.06
Titanium (Ti), max 0.05 0.06
Vanadium (V), max 0.08 0.10

Phosphorus and sulfur stay tight because QL2 is a colder toughness quality than P460Q. 460 MPa still comes from quench and temper plus micro-alloying, not from extra carbon. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search P460QL2 mechanical properties, P460QL2 impact and P460QL2 -60°C. Yield still falls with thickness. Impact is the QL2 item.

Tensile and Yield — EN 10028-6 P460QL2

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 50 460 570 – 720
50 – 100 440 570 – 720
100 – 150 400 540 – 710
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 17% min on thinner plate. Charpy for QL2 is −60 °C. Energy is commonly 27 J average when the order follows the book. Location and orientation must be written. Do not assume QL1 −40 °C is enough for a QL2 drawing.

Do not quote 460 MPa yield on a 120 mm plate. Do not treat −60 °C as permission to stamp Q460DR steel plate or EN 10028-3 P460NL2 without checking both books.

Material Comparison

Grade Book What buyers search Swap?
EN 10028-6 P460Q EN 10028-6 P460Q steel plate No
EN 10028-6 P460QH EN 10028-6 P460QH steel plate No
EN 10028-6 P460QL1 EN 10028-6 P460QL1 steel plate No
EN 10028-6 P460QL2 EN 10028-6 P460QL2 steel plate This page
EN 10028-3 P460NL2 EN 10028-3 P460NL2 No
EN 10028-5 P460ML2 EN 10028-5 P460ML2 No
Q460DR steel plate GB/T 713.3 Q460DR No auto swap
15MnNiNbDR steel plate GB/T 713.3 15MnNiNbDR No
SA517 Grade F SA-517 SA517 Gr.F No auto swap

Equivalent Material Grades

Designation Standard / region Notes
EN 10028-6 P460QL2 / 1.8882 EN 10028-6 Name on this page
P460QL1 / 1.8881 EN 10028-6 −40 °C QT sister
P460Q / 1.8879 EN 10028-6 Room-temp QT sister
P460QH / 1.8880 EN 10028-6 Elevated-temp QT sister
EN 10028-3 P460NL2 EN 10028-3 Normalized −50 °C sister
EN 10028-5 P460ML2 EN 10028-5 TMCP −50 °C sister
Q460DR steel plate GB/T 713.3 Chinese low-temp 460
15MnNiNbDR steel plate GB/T 713.3 Chinese −50 °C Nb
SA517 Grade F SA-517 ASME QT vessel

QT -60°C 460 MPa Pressure-Vessel Service

Buyers pick P460QL2 when a PED file wants 460 MPa QT plate and Charpy at −60 °C. Search phrases such as P460QL2 -60°C, P460QL2 QT and 1.8882 steel plate all point here.

It is not a substitute for 09MnNiDR steel plate. That grade is −70 °C nickel steel. It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni. It is not LNG inner-tank plate. That work belongs on 06Ni9DR steel plate. An ASME QT file should name SA-517 with a written −60 °C extra. Dual marking is possible only when both books are met.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

P460QL2 is killed QT fine-grain C-Mn vessel plate at 570–720 MPa tensile. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. Consumables must keep toughness at −60 °C, not only at −40 °C. A P460QL1 procedure is the previous family. A carbon procedure written for SA516 Grade 70 may be light on strength. Preheat and interpass must stay inside the qualified window so the QT structure is not damaged. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is quenched and tempered EN 10028-6 P460QL2 (Q). This is not +N from EN 10028-3 and not M from EN 10028-5.

If the vessel will see PWHT, say so. Impact after simulated PWHT is worth naming on a −60 °C 460 MPa QT file. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-6 P460QL2; 1.8882; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; Q / QT; Charpy at −60 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for P460QL2 QT -60°C vessel plate:

  • Thickness: commonly 8 mm – 150 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Normalized low-temp 460 plate belongs on EN 10028-3 P460NL2. TMCP low-temp 460 plate belongs on EN 10028-5 P460ML2.

Tolerances

Dimensional limits for EN 10028-6 P460QL2 follow EN 10028-1 and EN 10029 unless the purchase order names another table. Class A is the usual mill default for P460QL2 QT -60°C vessel plate. Class B, Class C or Class D is supplied only when written. Do not apply ASTM A36 structural tolerances to a PED −60 °C QT plate without writing them.

Typical thickness tolerance idea for P460QL2 (EN 10029 Class A, reference)

Nominal thickness (mm) Class A minus (mm) Class A plus (mm)
8 – 15 −0.5 +0.9
15 – 25 −0.6 +1.0
25 – 40 −0.7 +1.1
40 – 80 −0.8 +1.2
80 – 150 −1.0 +1.4

Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless the mill quote names a tighter extra. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows EN 10029 Class N unless Class S is written. Edge condition is mill edge or cut edge as ordered. If the vessel calculation used minimum thickness after corrosion, write the allowed minus on the RFQ. SHH STEEL will not assume Class B or a zero-minus extra on P460QL2 unless the order says so.

Supplementary Requirements

Charpy details. Write −60 °C, joules, location and orientation. Do not write “impact as per EN 10028-6” and expect the mill to guess QL2.

Impact after simulated PWHT. When the vessel will be stress-relieved.

Product analysis. Especially P, S, Al, N, Nb and V.

NDE. EN 10160 or ASTM A435 / A578 as named.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
PED high-strength low-temp QT vessels EN 10028-6 P460QL2 shells at −60 °C
Cold-service storage tanks P460QL2 courses
Dual-certified export P460QL2 / Q460DR steel plate when both books fit
Comparison vs TMCP / N P460QL2 next to EN 10028-5 P460ML2

P460QL2 is the plate for a 460 MPa PED file that wants QT and −60 °C. It is the wrong plate for LNG inner tanks. That work belongs on 06Ni9DR steel plate. It is the wrong plate for −40 °C only. That work is P460QL1.

Supply Capability

SHH STEEL sources EN 10028-6 P460QL2 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or QT route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement.

Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard QT about 45–60 days; simulated PWHT / 3.2 about 2 months.

Why Choose SHH STEEL

Experience on this grade is simple: keep the letters after P460. Q, QH, QL1 and QL2 are four different purchase orders. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices P460QL2 from first-line mills, reports 1.8882 chemistry, records QT, prints Charpy at −60 °C when ordered, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. P460QL2 is not P460Q. P460QL2 is not P460QL1. P460QL2 is not EN 10028-5 P460ML2. P460QL2 is not Q345R steel plate. If the drawing says −40 °C, we will not ship QL2 and call colder automatically better without the buyer writing the name.

FAQ

What is P460QL2 steel plate?
P460QL2 is an EN 10028-6 quenched-and-tempered fine-grain pressure-vessel plate, steel number 1.8882. Yield is 460 MPa at ≤50 mm and tensile is 570–720 MPa. QL2 means Charpy at −60 °C on a QT route. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of P460QL2?
Related comparisons are P460NL2, P460ML2, Q460DR and SA-517 Grade F. Dual marking is possible only when both books are fully met.
How is P460QL2 different from P460QL1?
QL1 is −40 °C. QL2 is −60 °C. Same yield step, different impact temperature.
How is P460QL2 different from P460Q?
P460Q is room-temperature QT. P460QL2 is −60 °C QT.
How is P460QL2 different from P460NL2 and P460ML2?
P460NL2 is EN 10028-3 normalized plate. P460ML2 is EN 10028-5 TMCP plate. P460QL2 is EN 10028-6 QT plate. Same cold-service idea, different route and exact impact temperature.
Can SHH STEEL ship P460QL2 to the USA, Europe or the Middle East?
Yes. SHH STEEL quotes FOB Shanghai and CIF to US West, US Gulf, Rotterdam, Jebel Ali, Singapore and other major ports.
What is the delivery time for P460QL2?
Ex-stock about 5–7 days when plate is in yard. Standard QT mill rolling about 45–60 days. Simulated PWHT or 3.2 inspection about 2 months.
Can SHH STEEL issue EN 10204 3.2 for P460QL2?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named on the order.

Conclusion

EN 10028-6 P460QL2 Steel Plate is European quenched-and-tempered fine-grain −60 °C pressure-vessel plate, steel number 1.8882, at the 460 MPa yield step and 570–720 MPa tensile at ≤50 mm. Whether the inquiry says EN 10028-6 P460QL2, 1.8882, P460QL2 QT -60°C Vessel Plate or P460QL2 supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P460QL2 chemistry, recorded QT, Charpy at −60 °C when ordered, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-6 P460QL2 QT -60°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

EN 10028-6 P460QL2 Steel Plate, P460QL2 QT -60°C vessel plate, 1.8882, P460QL2 supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X