EN 10025-2 S275JR IPE and IPN Steel I Beams

EN 10025-2 S275JR IPE and IPN steel I-beams are non-alloy sections (1.0044) with 275 MPa yield up to 16 mm and 27 J at +20 °C, between S235 and S355. Tables cover IPE and IPN 80–600 to EN 10365. IPE uses EN 10034; IPN uses EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.
Keywords
EN 10025-2 S275JR I Beam, S275JR IPE, S275JR IPN, EN 10365 IPE 80–600, EN 10365 IPN 80–600
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of EN 10025-2 S275JR IPE and IPN Steel I Beams
Chemical Composition
Carbon Equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source EN 10025-2 S275JR IPE and IPN Steel I Beams from SHH STEEL
FAQ
Conclusion

What are EN 10025-2 S275JR IPE and IPN Steel I Beams?

EN 10025-2 S275JR occupies the band between S235JR and S355JR. The steel number is 1.0044. The 275 MPa yield applies in the thinnest tabulated thickness band, and JR still means 27 J at +20 °C, not a colder test. It is a genuine mid-class grade, not a relabelled S235 certificate and not a discounted S355. If a design actually needs 355 MPa, this is the wrong page.

This article is written for rolled IPE and IPN I-sections, not for EN 10025-2 S275JR steel plate and not for EN 10025-2 S275JR H-beam. The H-beam page covers HEA and HEB for the same grade. IPE remains a parallel-flange I-beam; IPN remains the taper-flange companion in EN 10365, now tabulated here in full from IPN 80 to IPN 600. Long-product tensile and impact tests are normally longitudinal unless the order says otherwise.

Buyers sometimes land on S275JR after a drawing calls for “S275 I-beam” without a series. That is not enough. The order should say IPE or IPN, the EN 10365 designation, and the JR quality letters. A similar depth in S235JR, in an HEA, or in an American S shape does not make the pieces interchangeable.

Material, Dimensions and Tolerances for EN 10025-2 S275JR IPE and IPN I-Beams

Keep the material standard, the shape standard and the tolerance standard separate on an EN 10025-2 S275JR order:

  • EN 10025-2:2019 (or the edition named on the order) for S275JR ladle analysis, carbon equivalent and tensile properties of long products.
  • EN 10365 for IPE and IPN dimensions. The tables below are reference values, not a rolling programme.
  • EN 10034 for IPE tolerances and EN 10024 for IPN tolerances. Name an EN 10163-3 surface class if the finish matters.

S275JR can be certified on other section families, and an IPE can be certified to another grade, when the documents actually say so. Do not assume that “S275 beam” means an IPE, and do not step a depth from the S235JR table and call it S275JR.

EN 10025-2 S275JR IPE and IPN Sizes: EN 10365 Reference Tables

For EN 10025-2 S275JR the shape catalogue is the same EN 10365 pair used on the S235JR and S355JR I-beam pages: IPE 80–600 (18 sizes) and IPN 80–600 (21 sizes). The material grade changes the chemistry and the yield band, not the millimetre designation. These are reference dimensions and theoretical masses, not a claim that every row is produced in S275JR.

Because S275JR often arrives as a “step up” from S235JR on the same IPE size, check the flange thickness against the 275/265 MPa bands. IPE 500 stays at 16.0 mm; IPE 600 and IPN 300 do not. IPN 280, 320, 380 and 600 are footnoted in the source programme for agreement on tonnage and delivery.

IPE series

Parallel-flange I-beams, 18 sizes from IPE 80 to IPE 600, under EN 10365:2017.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) r (mm) A (cm²) Mass (kg/m)
IPE 80 80.0 46.0 3.8 5.2 5 7.6 6.0
IPE 100 100.0 55.0 4.1 5.7 7 10.3 8.1
IPE 120 120.0 64.0 4.4 6.3 7 13.2 10.4
IPE 140 140.0 73.0 4.7 6.9 7 16.4 12.9
IPE 160 160.0 82.0 5.0 7.4 9 20.1 15.8
IPE 180 180.0 91.0 5.3 8.0 9 23.9 18.8
IPE 200 200.0 100.0 5.6 8.5 12 28.5 22.4
IPE 220 220.0 110.0 5.9 9.2 12 33.4 26.2
IPE 240 240.0 120.0 6.2 9.8 15 39.1 30.7
IPE 270 270.0 135.0 6.6 10.2 15 45.9 36.1
IPE 300 300.0 150.0 7.1 10.7 15 53.8 42.2
IPE 330 330.0 160.0 7.5 11.5 18 62.6 49.1
IPE 360 360.0 170.0 8.0 12.7 18 72.7 57.1
IPE 400 400.0 180.0 8.6 13.5 21 84.5 66.3
IPE 450 450.0 190.0 9.4 14.6 21 98.8 77.6
IPE 500 500.0 200.0 10.2 16.0 21 115.5 90.7
IPE 550 550.0 210.0 11.1 17.2 24 134.4 106
IPE 600 600.0 220.0 12.0 19.0 24 156.0 122

IPN series

Taper-flange I-beams (14% flange slope), 21 sizes from IPN 80 to IPN 600, under EN 10365:2017. Rows marked * are listed in the source programme with the footnote that minimum tonnage and delivery conditions are upon agreement (IPN 280, IPN 320, IPN 380 and IPN 600).

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) r1 (mm) r2 (mm) A (cm²) Mass (kg/m)
IPN 80 80.0 42.0 3.9 5.9 3.9 2.3 7.6 5.9
IPN 100 100.0 50.0 4.5 6.8 4.5 2.7 10.6 8.3
IPN 120 120.0 58.0 5.1 7.7 5.1 3.1 14.2 11.1
IPN 140 140.0 66.0 5.7 8.6 5.7 3.4 18.2 14.3
IPN 160 160.0 74.0 6.3 9.5 6.3 3.8 22.8 17.9
IPN 180 180.0 82.0 6.9 10.4 6.9 4.1 27.9 21.9
IPN 200 200.0 90.0 7.5 11.3 7.5 4.5 33.4 26.2
IPN 220 220.0 98.0 8.1 12.2 8.1 4.9 39.5 31.1
IPN 240 240.0 106.0 8.7 13.1 8.7 5.2 46.1 36.2
IPN 260 260.0 113.0 9.4 14.1 9.4 5.6 53.3 41.9
IPN 280* 280.0 119.0 10.1 15.2 10.1 6.1 61.0 47.9
IPN 300 300.0 125.0 10.8 16.2 10.8 6.5 69.0 54.2
IPN 320* 320.0 131.0 11.5 17.3 11.5 6.9 77.7 61.0
IPN 340 340.0 137.0 12.2 18.3 12.2 7.3 86.7 68.0
IPN 360 360.0 143.0 13.0 19.5 13.0 7.8 97.0 76.1
IPN 380* 380.0 149.0 13.7 20.5 13.7 8.2 107.0 84.0
IPN 400 400.0 155.0 14.4 21.6 14.4 8.6 117.7 92.4
IPN 450 450.0 170.0 16.2 24.3 16.2 9.7 146.9 115
IPN 500 500.0 185.0 18.0 27.0 18.0 10.8 179.4 141
IPN 550 550.0 200.0 19.0 30.0 19.0 11.9 212.0 166
IPN 600* 600.0 215.0 21.6 32.4 21.6 13.0 253.7 199

HEA and HEB sizes stay on the EN 10025-2 S275JR H-beam page. IPE 300 is 150 mm wide; IPN 300 is 125 mm wide. Settlement of mass should follow the contract. These rows are not W-shapes, S shapes or GB/T 706 I-beams of a similar depth.

EN 10025-2 S275JR Chemical Composition (Ladle Analysis)

The figures below are ladle-analysis maxima for S275JR long products in EN 10025-2:2019. They are limits, not typical heat results. Carbon is higher than in S235JR, and manganese is limited to 1.50% rather than 1.40%. There is still no general silicon maximum unless a galvanizing agreement is written into the order.

Element Ladle analysis, max (mass %) Notes for S275JR long products
C, t ≤ 16 mm 0.21 —
C, 16 mm < t ≤ 40 mm 0.21 —
C, t > 40 mm 0.22 For nominal thickness greater than 100 mm, carbon is subject to agreement.
Si No general maximum By agreement, silicon may be set at 0.14–0.25% and phosphorus at ≤0.035% for hot-dip galvanizing category B.
Mn 1.50 Higher than the S235JR maximum of 1.40%.
P 0.040 See the galvanizing agreement above. Do not paste a flat-product 0.035% default onto a beam order unless that is what was agreed.
S 0.040 —
N 0.012 The nitrogen maximum does not apply if total aluminium is at least 0.020%, or if sufficient other nitrogen-binding elements are present and reported.
Cu 0.55 —
Other added elements As reported If other elements are added, they shall be mentioned on the inspection document.

EN 10025-2 S275JR Carbon Equivalent

The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S275JR long products are:

Nominal thickness (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.40
30 < t ≤ 40 0.40
40 < t ≤ 140 0.42

The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S275 and S355. If that clause is to be used, it should be named on the order; this page does not invent a raised CEV figure from it.

EN 10025-2 S275JR Mechanical Properties: Yield, Tensile and Impact

Tensile properties of S275JR are thickness-dependent. The values below are from EN 10025-2:2019 for long products, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are given here. Plate elongation and sampling are covered on S275JR steel plate, not by this table.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 275 410–560 23
16 < t ≤ 40 265 410–560 23
40 < t ≤ 63 255 410–560 22
63 < t ≤ 80 245 410–560 21
80 < t ≤ 100 235 410–560 21
100 < t ≤ 150 225 400–540 19

Quality JR requires 27 J at +20 °C. For long products the Charpy test is normally longitudinal unless the order specifies otherwise. If the project needs 27 J at 0 °C or at −20 °C, the grade to nominate is S275J0 or S275J2, not S275JR.

Use the flange, or the specimen-preparation thickness required by the standard, when selecting the band. HE 240 A, with a 12 mm flange, remains at 275 MPa. HE 300 B, with a 19 mm flange, is 265 MPa.

Apply the band that matches the governing thickness, usually the flange. An IPE 500 flange is 16.0 mm, so it remains in the 275 MPa band. An IPE 600 flange is 19.0 mm, so the minimum yield is 265 MPa, not 275 MPa. An IPN 300 flange is 16.2 mm, so the minimum yield is 265 MPa, not 275 MPa. An IPE 500 flange is 16.0 mm and remains in the 275 MPa band; an IPE 600 flange is 19.0 mm and uses the 265 MPa band.

Delivery, Inspection and Identification of EN 10025-2 S275JR IPE and IPN I-Beams

S275JR IPE and IPN sections are commonly delivered in the as-rolled condition of EN 10025-2 unless the order names a different delivery condition. The inspection document should identify the grade, the steel number 1.0044, the dimensional standard, the designation (for example IPE 300), and the ordered edition. Marking should follow the ordered product standards so the piece can be matched to the certificate.

An ordinary works certificate that only says “S275JR beam” without the series, the dimensional standard or the quality letters is not a complete identification. If a specific inspection document type is required (for example EN 10204 3.1), name it on the order. This page does not invent test frequencies or document types beyond those rules.

Weldability and Surface Condition of EN 10025-2 S275JR IPE and IPN I-Beams

The carbon-equivalent limits in this article describe weldability in the sense of EN 10025-2. They are not a welding procedure. Procedure qualification, consumables, preheat and hydrogen control remain the fabricator’s responsibility for the thickness, joint and service actually used. S275JR is a JR or J2 quality as named; a +20 °C Charpy requirement does not by itself define heat-affected-zone toughness after welding.

Surface condition for sections is commonly specified to EN 10163-3. If a class or a special surface requirement matters for painting, galvanizing or fatigue, it should be named on the order. Do not assume that an IPE and an IPN of similar depth will present the same flange taper or the same detailing at the root.

Shape Tolerances for EN 10025-2 S275JR IPE and IPN I-Beams (EN 10034 and EN 10024)

On EN 10025-2 S275JR I-beams, IPE is accepted to EN 10034 and IPN to EN 10024. The material standard does not replace those shape standards, and the millimetre tolerance tables are not copied here. The ordered edition governs.

Use the tabulated reference dimensions as a starting point, not as exact advertised millimetres. IPE 300 and IPN 300 will each come out close to their own EN 10365 row, within their own tolerance standard. The tapered IPN flange is the one that usually surprises a detailer who has only drawn IPE end plates.

Theoretical mass and weighed mass are different settlement bases. The contract should pick one.

Applications and Service Limits for EN 10025-2 S275JR IPE and IPN Steel I Beams

EN 10025-2 S275JR IPE and IPN sections are used where a designer wants more yield than S235JR and does not need the S355 class or a colder impact quality. They turn up in frames, platforms and general fabrication. They are not a weathering grade and not a pressure-vessel material, and JR does not imply a 0 °C test.

If the calculation is actually written for 355 MPa, use EN 10025-2 S355JR IPE and IPN Steel I Beams. If +20 °C is not acceptable, nominate S275J0 or S275J2. H-sections for this grade are on the EN 10025-2 S275JR H-beam page.

EN 10025-2 S275JR IPE and IPN Compared with S235JR, S355JR and A36

EN 10025-2 S275JR sits between EN 10025-2 S235JR IPE and IPN Steel I Beams and EN 10025-2 S355JR IPE and IPN Steel I Beams. The three grades can be ordered on the same IPE or IPN designation, but the certificates are not interchangeable. S275J0 and S275J2 keep the 275 MPa class and move the impact test.

EN 10025-2 S275JR H-beam is the H-section listing, not a second name for IPE. ASTM A36 S Shape I Beams and ASTM A36 wide-flange beams belong to ASTM A6. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Near-Equivalents for EN 10025-2 S275JR IPE and IPN Steel I Beams: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to S275JR H-beam Caution
S275J0 / S275J2 EN 10025-2 Same 275 MPa yield class. J0 is tested at 0 °C and J2 at −20 °C, both at 27 J. J0 and J2 also use tighter phosphorus and sulphur, and J2 is a fully killed grade. They are not interchangeable with JR on a +20 °C specification.
S235JR / S355JR EN 10025-2 Lower and higher yield classes in the same standard and usually the same HEA, HEB and IPE series. S235JR is a 235 MPa grade; S355JR is a 355 MPa grade with a different chemistry and CEV table. The quality letters are not a substitute for choosing the yield class.
ASTM A36 ASTM A36/A36M; dimensions ASTM A6 A general structural carbon steel sometimes compared in mixed-origin packages. A36 is a 36 ksi [250 MPa] grade on W-shapes, below the S275 yield class, and is not an automatic substitute.
Q235B / Q355B GB/T 700 or GB/T 1591; dimensions GB/T 11263 Chinese general-structural grades that bracket the 275 MPa class. Neither is a 275 MPa grade, and both use HW/HM/HN, not HEA/HEB/IPE.

Sister beam pages in this series (S235JR, S355J0, S355J2) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page for the 355 MPa JR comparison. The S235JR steel plate page is a plate data sheet, not an S235JR beam page.

Sourcing EN 10025-2 S275JR IPE and IPN Steel I Beams from SHH STEEL

Enquiries for EN 10025-2 S275JR IPE and IPN should name the series, the designation and the edition. SHH STEEL checks those points, the steel number 1.0044, and the certificate type before quoting, and does not treat an S235JR piece or an HEA of similar depth as the same item.

Send the size list, the inspection document type and any impact option. Images on this page stay empty; photographs can be provided with a quotation when they are available.

S275JR IPE and IPN Steel I Beam FAQs

Is an IPE of a given depth the same as the IPN of that depth?
No. Both series are tabulated on this page to EN 10365, but they are different sections. IPE 300 is 300 × 150 × 7.1 × 10.7 mm (42.2 kg/m). IPN 300 is 300 × 125 × 10.8 × 16.2 mm (54.2 kg/m), with tapered inner flange faces. Do not order one designation and expect the other.
Is an IPE beam the same as an H-beam of similar depth?
No. IPE is a parallel-flange I-section. HEA and HEB are H-sections with a different width, thickness and mass at a similar nominal depth. The S275JR H-beam page covers HEA and HEB. An IPE 300 is not an HE 300 A or an HE 300 B.
Which thickness sets the S275JR yield on these I-beams?
Apply the band that matches the governing thickness, usually the flange. IPE 500 has a 16.0 mm flange and remains in the 275 MPa band. IPE 600 has a 19.0 mm flange, so the minimum yield is 265 MPa, not 275 MPa. Those flange thicknesses are the tabulated EN 10365 reference values on this page.
Does a S275JR certificate automatically include a lower-temperature impact test?
No. Quality letters matter. S275JR carries 27 J at +20 °C. If the project needs a different test temperature, nominate the matching quality (for this class, S275J0 or S275J2) instead of assuming it from the yield number or the IPE size.
Can I use a Chinese I-beam or an American S shape as a substitute for IPE?
Not by matching a nominal depth or a similar mass. GB/T 706 taper-flange I-beams and ASTM A6 S shapes are different series, with different designation systems, dimensions and tolerances. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Request a Quotation for EN 10025-2 S275JR IPE and IPN Steel I Beams

EN 10025-2 S275JR IPE and IPN steel I-beams are a non-alloy structural sections (1.0044) with 275 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Nominate the IPE or IPN size to EN 10365 (the tables cover IPE 80–600 and IPN 80–600) and the material to EN 10025-2:2019 (or the edition on the order). Both the IPE 80–600 and IPN 80–600 tables are reference dimensions, not rolling lists. The IPE table is a set of reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X