ASTM A36 S Shape I Beams

ASTM A36 S shape I-beams are carbon structural American Standard Beams to ASTM A36/A36M, with 36 ksi [250 MPa] minimum yield and 58–80 ksi tensile strength. The table lists 28 ASTM A6/A6M S designations from S24×121 to S3×5.7. This page is not the A36 wide-flange W-shape listing. SHH STEEL reviews grade, designation and certificate requirements before quoting.
Keywords
ASTM A36 S Shape I Beam, A36 American Standard Beam, A36 S-shape, ASTM A6 S24×121, ASTM A6 S3×5.7
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of ASTM A36 S Shape I Beams
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source ASTM A36 S Shape I Beams from SHH STEEL
FAQ
Conclusion

What are ASTM A36 S Shape I Beams?

ASTM A36 S shape I-beams are rolled American Standard Beams (S shapes) whose material conforms to ASTM A36/A36M and whose dimensions, shape and tolerances conform to ASTM A6/A6M. A36 is a carbon structural steel with a minimum yield point of 36 ksi [250 MPa] and a tensile-strength range of 58–80 ksi [400–550 MPa] for ordinary thicknesses. The designation “S” is the American Standard beam series. S shapes have tapered inner flange surfaces and a different width and mass from a W-shape of similar nominal depth. An S12 is not a W12, and it is not an IPE 300 or a GB I-beam by depth alone.

This page covers the rolled S shape, not plate and not a wide-flange beam. The same specification in plate form is listed separately as ASTM A36 steel plate. The live wide-flange listing is ASTM A36 Wide Flange Beam. Plate chemistry is split by thickness and width, plate elongation rules differ, and the 32 ksi [220 MPa] yield reduction applies only to plates over 8 in [200 mm] thick. The plate page and the W-shape page are not substitute data sheets for S shapes.

These beams are filed under I Beams and IPE Beams in the steel structural profiles category. Sister American pages include ASTM A36 Wide Flange Beam under H Beams and Wide Flange Beams, and ASME SA-36 Wide Flange H Beam when an ASME SA-36/SA-36M certificate is required for a W-shape. European IPE and IPN sections, for example EN 10025-2 S235JR IPE and IPN Steel I Beams, and GB/T 706 Q235B I-beam use different designation systems.

A36 S shapes are used in frames, stringers, walkways and fabrication where an American Standard Beam and a 36 ksi carbon steel are specified and an impact test is not a default requirement. They are not a 50 ksi grade, not a weathering steel, and not a pressure-vessel or nuclear safety material. If the enquiry only says “A36 I-beam” or “A36 beam,” the shape series (S or W), the A6 designation, and any supplementary tests still need to be confirmed.

Material, Dimensions and Tolerances for ASTM A36 S Shapes

Two documents should appear, separately, on the purchase order and on the mill test report:

  • ASTM A36/A36M is the material specification for carbon structural steel. This article uses the chemistry and tensile values published in ASTM A36/A36M-19, the current edition used here. The edition named on the order governs acceptance. Inch-pound and SI values are both official; each system is used as published, not as a converted equivalent mixed into the other.
  • ASTM A6/A6M is the general-requirements standard for rolled structural steel bars, plates, shapes and sheet piling. For S shapes it sets the designation system, dimensional and camber tolerances, marking, and the heat-analysis and tension-test rules that A36 refers to. A36 does not itself contain the S-shape size tables.

A mill may also certify A36 on a W-shape, channel or angle, or roll an S shape to a different material specification, if that combination is in its programme and is fully documented. Do not treat “A36 beam” as if it automatically meant a W12×50 or an S12×31.8, and do not substitute EN 10025-2 S235JR IPE and IPN Steel I Beams or GB/T 706 Q235B I-beam by matching a nominal 12 in or 300 mm depth.

ASTM A36 S Shape Sizes: American Standard Beams (ASTM A6/A6M)

The tables list the 28 standard ASTM A6/A6M S-shape reference dimensions, from S24×121 to S3×5.7: designation, actual depth, flange width, web thickness and flange thickness in inch and millimetre units, mass in lb/ft and kg/m, and the companion SI designation from the same AISC Manual, 15th Edition, shape file already used for the live A36 W-shape tables. They are reference dimensions for identification and estimating, not a rolling list, and not a claim of guaranteed availability or that every S shape is produced in A36. Dimensional acceptance follows the edition of ASTM A6/A6M named on the order.

A designation such as S12×31.8 is a series call: the first number is the nominal depth in inches and the second is the nominal mass in pounds per foot. The actual depth of some rows is slightly above the nominal inch figure (for example S24×121 is 24.5 in deep). That is normal. Root radius is omitted because a single fillet radius is not published as a delivery dimension for these shapes, and a radius is not invented here. The deepest flange in this standard S series is 1.09 in (S24×121 and S24×106), which is below the 3 in [75 mm] flange-thickness notes that apply to some wide-flange shapes.

Theoretical mass is the tabulated reference value. Settlement should follow the contract — tabulated theoretical mass or weighed mass — and the ordered A6 edition for mass tolerance. These S-shape rows are not interchangeable with W-shapes, with HW, HM or HN, or with IPE, IPN or GB/T 706 I-beams of a similar nominal depth.

S24 to S15

The deeper American Standard S shapes, from S24×121 to S15×42.9. 13 designations in this group.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m) SI designation
S24×121 24.5 8.05 0.8 1.09 622 204 20.3 27.7 121 180 S610×180
S24×106 24.5 7.87 0.62 1.09 622 200 15.7 27.7 106 158 S610×158
S24×100 24 7.25 0.745 0.87 610 184 18.9 22.1 100 149 S610×149
S24×90 24 7.13 0.625 0.87 610 181 15.9 22.1 90 134 S610×134
S24×80 24 7 0.5 0.87 610 178 12.7 22.1 80 119 S610×119
S20×96 20.3 7.2 0.8 0.92 516 183 20.3 23.4 96 143 S510×143
S20×86 20.3 7.06 0.66 0.92 516 179 16.8 23.4 86 128 S510×128
S20×75 20 6.39 0.635 0.795 508 162 16.1 20.2 75 112 S510×112
S20×66 20 6.26 0.505 0.795 508 159 12.8 20.2 66 98.2 S510×98.2
S18×70 18 6.25 0.711 0.691 457 159 18.1 17.6 70 104 S460×104
S18×54.7 18 6 0.461 0.691 457 152 11.7 17.6 54.7 81.4 S460×81.4
S15×50 15 5.64 0.55 0.622 381 143 14 15.8 50 74 S380×74
S15×42.9 15 5.5 0.411 0.622 381 140 10.4 15.8 42.9 64 S380×64

S12 to S3

The mid-range and smaller S shapes, from S12×50 to S3×5.7. 15 designations in this group.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m) SI designation
S12×50 12 5.48 0.687 0.659 305 139 17.4 16.7 50 74 S310×74
S12×40.8 12 5.25 0.462 0.659 305 133 11.7 16.7 40.8 60.7 S310×60.7
S12×35 12 5.08 0.428 0.544 305 129 10.9 13.8 35 52 S310×52
S12×31.8 12 5 0.35 0.544 305 127 8.89 13.8 31.8 47.3 S310×47.3
S10×35 10 4.94 0.594 0.491 254 125 15.1 12.5 35 52 S250×52
S10×25.4 10 4.66 0.311 0.491 254 118 7.9 12.5 25.4 37.8 S250×37.8
S8×23 8 4.17 0.441 0.425 203 106 11.2 10.8 23 34 S200×34
S8×18.4 8 4 0.271 0.425 203 102 6.88 10.8 18.4 27.4 S200×27.4
S6×17.25 6 3.57 0.465 0.359 152 90.7 11.8 9.12 17.25 25.7 S150×25.7
S6×12.5 6 3.33 0.232 0.359 152 84.6 5.89 9.12 12.5 18.6 S150×18.6
S5×10 5 3 0.214 0.326 127 76.2 5.44 8.28 10 15 S130×15
S4×9.5 4 2.8 0.326 0.293 102 71.1 8.28 7.44 9.5 14.1 S100×14.1
S4×7.7 4 2.66 0.193 0.293 102 67.6 4.9 7.44 7.7 11.5 S100×11.5
S3×7.5 3 2.51 0.349 0.26 76.2 63.8 8.86 6.6 7.5 11.2 S75×11.2
S3×5.7 3 2.33 0.17 0.26 76.2 59.2 4.32 6.6 5.7 8.5 S75×8.5

Wide-flange W-shape dimensions belong on the ASTM A36 Wide Flange Beam page, not in this table. Chinese HW/HM/HN sizes belong to GB/T 11263. European IPE sizes are listed on the EN 10025-2 S235JR IPE and IPN Steel I Beams page for that material system, not as A36 S dimensions.

ASTM A36 Chemical Composition for Shapes (Heat Analysis)

The figures below are the heat-analysis limits for shapes in ASTM A36/A36M-19 Table 3, “All” thicknesses. They are not the plate columns of the same table, which split carbon, manganese and silicon by thickness and width. Where the table shows no manganese requirement, manganese still has to be determined and reported on the heat analysis under ASTM A6/A6M.

Element Shapes, all thicknesses (unless noted) Notes
Carbon, max, % 0.26 Do not apply the thickness-split plate columns of Table 3 to W-shapes.
Manganese, % No requirement The heat analysis for manganese shall be determined and reported under ASTM A6/A6M. For shapes with flange thickness over 3 in [75 mm], manganese shall be 0.85–1.35%.
Phosphorus, max, % 0.04 —
Sulfur, max, % 0.05 —
Silicon, % 0.40 max For shapes with flange thickness over 3 in [75 mm], silicon shall be 0.15–0.40%.
Copper, min, % 0.20 when specified Applies only when copper steel is specified on the order.

These limits are heat analysis. Product analysis, when required, follows the permitted variations in ASTM A6/A6M. Unofficial tables that copy a plate carbon of 0.25% or a plate phosphorus of 0.030% into an S-shape enquiry are using the wrong column.

The standard S series tabulated on this page has a maximum flange thickness of 1.09 in, so the over-3 in wide-flange notes in the A36 shapes column do not apply to these 28 designations.

ASTM A36 S Shape Mechanical Properties: Yield, Tensile and Elongation

The tensile requirements below are from ASTM A36/A36M-19 Table 2. The shapes elongation column is used here, not the plates-and-bars column (which has a 23% minimum in 2 in). Tension-test orientation follows ASTM A6/A6M.

Property Requirement Notes for shapes
Tensile strength 58–80 ksi [400–550 MPa] For wide-flange shapes with flange thickness over 3 in [75 mm], the 80 ksi [550 MPa] maximum does not apply. The standard S series on this page does not reach that flange thickness.
Yield point, min 36 ksi [250 MPa] The 32 ksi [220 MPa] reduction is for plates over 8 in [200 mm] thick only. It does not apply to shapes.
Elongation in 8 in [200 mm], min 20% Shapes column of Table 2.
Elongation in 2 in [50 mm], min 21% For wide-flange shapes with flange thickness over 3 in [75 mm], the minimum in 2 in is 19%. The standard S series on this page does not reach that flange thickness.
Charpy V-notch Not required unless specified Order ASTM A6/A6M supplementary requirement S5, or S30 for the alternate core location on structural shapes, if an impact test is needed.

The 36 ksi [250 MPa] yield point applies to shapes at all listed thicknesses. Do not carry the plate-only 32 ksi reduction onto a W-shape certificate. Likewise, the ordinary 80 ksi tensile maximum is waived only for wide-flange shapes with flange thickness over 3 in [75 mm]; most catalogue W-shapes have thinner flanges than that, so the 58–80 ksi range still applies.

A36 does not specify a default Charpy test. If the project needs an impact value, the order should add S5 or, for the alternate core location on structural shapes, S30, and should state the test temperature and the absorbed-energy criterion. Those supplements are not implied by the grade name.

Delivery, Inspection and Identification of ASTM A36 S Shapes

A36 S shapes are commonly delivered in the as-rolled condition unless the order names a different condition. The mill test report should identify ASTM A36/A36M (or the edition on the order), the S designation, and the heat. Marking should follow ASTM A6/A6M so the piece can be matched to the certificate.

An ordinary A36 certificate for a W-shape, a plate or a channel is not an S-shape certificate for the designation on this page. If ASTM A6/A6M supplementary requirements (for example S5 impact testing) are needed, name them on the order. An ASME SA-36/SA-36M mark is a different certificate path; it is not implied by an A36 S-shape order.

Weldability and Surface Condition of ASTM A36 S Shapes

A36 is a readily welded carbon structural steel in ordinary thicknesses, but this page is not a welding procedure. Procedure qualification, consumables and preheat remain the fabricator’s responsibility for the thickness and joint actually used. A Charpy test is not required by A36 unless it is specified.

S shapes have tapered inner flange surfaces. Connection details, cope geometry and fitting to a flat plate are not the same as for a parallel-flange W-shape of similar depth. Surface condition and any special finish for painting or galvanizing should be named on the order when they matter.

ASTM A6/A6M Shape Tolerances and Theoretical Mass for ASTM A36 S Shapes

Dimensional, straightness, camber, sweep, out-of-square and mass tolerances for these S shapes are those of ASTM A6/A6M, not of ASTM A36/A36M. This article does not reproduce the A6 tolerance tables; acceptance is against the edition named on the order.

The size tables above are nominal S-shape reference dimensions. A delivered S12×31.8 will measure close to the tabulated depth, width and thicknesses within the tolerances of the ordered ASTM A6/A6M edition, not as a set of exact advertised inches. Flange out-of-square and web off-centre matter for connections.

The lb/ft and kg/m columns are published theoretical masses. Weighed mass may sit above or below those figures and still be within the A6 mass tolerance. Settlement should follow the contract.

Applications and Service Limits for ASTM A36 S Shape I Beams

A36 S shapes are used as beams, stringers, small frames and miscellaneous members where an American Standard Beam is specified. They are not a substitute for a W-shape column or girder of similar nominal depth, and they are not a 50 ksi, weathering, or pressure-vessel product.

This page is not a design guide and does not give span tables. If the project actually needs a W-shape, an IPE, a GB/T 706 I-beam, or an SA-36 certificate, nominate that product instead of stretching this listing.

ASTM A36 S Shapes Compared with A36 W-Shapes, SA-36 and IPE

The same material specification rolled as a wide-flange beam is ASTM A36 Wide Flange Beam. W and S are different A6 series. A W12×35 and an S12×31.8 are not interchangeable by nominal depth. ASME SA-36 Wide Flange H Beam uses the ASME SA-36/SA-36M certificate path on W-shapes; an ordinary A36 S-shape certificate is not an SA-36 certificate.

EN 10025-2 S235JR IPE and IPN Steel I Beams and GB/T 706 Q235B I-beam can sit in a similar depth band, but they use different designation systems, taper rules and tolerances. A572 Grade 50 and A992 are related higher-strength American grades and are commonly furnished as W-shapes, not as a drop-in S-shape substitute for A36. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Near-Equivalents for ASTM A36 S Shape I Beams: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or a mill certificate. Where a project allows an alternative, the substitution should be written into the order and verified on the test report.

Grade / designation Standard Relationship to A36 S shape I-beams Caution
ASME SA-36 ASME SA-36 (Boiler and Pressure Vessel Code, Section II alignment) Often chemically and mechanically aligned with ASTM A36, and commonly requested together on plate. This page is the ASTM A36 S-shape product. An ASME listing is a separate certification path and is not assumed by ticking this category.
Q235B GB/T 700; dimensions GB/T 11263 A general carbon structural steel often compared in export enquiries. Yield class is 235 MPa, not 250 MPa, with a 27 J impact requirement at +20 °C. HW/HM/HN are not S-shapes.
S235JR EN 10025-2 A 235 MPa European carbon structural grade with a +20 °C impact quality. Different chemistry, impact rules and HEA/HEB/IPE (or UB/UC) shape series. Not an automatic substitute.
ASTM A572 Grade 50 ASTM A572/A572M A 50 ksi (345 MPa) high-strength low-alloy grade often rolled as the same S-shapes. Higher yield class and a different chemistry table. Do not substitute on a contract that names A36.
ASTM A992 ASTM A992/A992M The usual modern grade for US building S-shapes. A992 has its own chemistry, yield and tensile window. It is not a silent upgrade of A36, and A36 is not a silent substitute for A992.

Sister beam pages in this series (A572 Grade 50, A992, Q235B, S235JR) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page when a European 355 MPa comparison is needed.

Sourcing ASTM A36 S Shape I Beams from SHH STEEL

SHH STEEL reviews enquiries for ASTM A36 S shapes against a named A6 designation list and a named edition. We check whether the order is for an S shape or a W-shape, the A36 edition, and the certificate type before quoting. We do not treat a W-shape, an IPE or a GB I-beam of similar depth as the same item, and we do not invent a root radius or an unofficial size.

Send the S designation list, the A36/A36M and A6/A6M editions, any supplementary tests, and delivery notes. Images on this page stay empty; photographs can be provided with a quotation when they are available.

A36 S Shape I Beam FAQs

Is an A36 S shape the same as an A36 wide-flange beam?
No. Both can be certified to ASTM A36/A36M, but S and W are different ASTM A6 series. S shapes are American Standard Beams with tapered inner flange surfaces. A W12 is not an S12. The wide-flange listing is a separate page.
How many S shapes are tabulated here?
Twenty-eight designations, from S24×121 to S3×5.7, taken from the AISC Steel Construction Manual, 15th Edition, Type = S, in both US customary and SI companion designations. The tables are reference dimensions, not a rolling list.
Does the 32 ksi yield reduction for thick A36 plate apply to these S shapes?
No. The 32 ksi [220 MPa] yield reduction applies to plates over 8 in [200 mm] thick. It does not apply to shapes. The S series tabulated here is far below that plate-thickness band.
Is an A36 S-shape certificate the same as ASME SA-36?
No. SA-36/SA-36M is the ASME Boiler and Pressure Vessel Code Section II, Part A listing. An ordinary ASTM A36 certificate is not an SA-36 certificate unless the order and the documents actually carry that mark.
Can I substitute an IPE or a GB/T 706 I-beam for an S shape?
Not by matching a nominal depth or a similar mass. IPE, GB/T 706 I-beams and A6 S shapes are different series, with different flange taper, dimensions and tolerances.

Request a Quotation for ASTM A36 S Shape I Beams

ASTM A36 S shape I-beams are carbon structural American Standard Beams with 36 ksi [250 MPa] minimum yield and 58–80 ksi [400–550 MPa] tensile strength. Nominate the S designation to ASTM A6/A6M and the material to ASTM A36/A36M-19 (or the edition on the order). The tables cover the 28 standard S shapes from S24×121 to S3×5.7 as reference dimensions, not a rolling list. This page is not the A36 wide-flange listing. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X