EN 10025-2 S355JR IPE and IPN Steel I Beams
What are EN 10025-2 S355JR IPE and IPN Steel I Beams?
EN 10025-2 S355JR is the usual 355 MPa European I-beam enquiry: steel number 1.0045, 355 MPa minimum yield up to 16 mm, and 27 J at +20 °C. The yield number is not a toughness grade. JR does not become J2 because the beam is deep, and a 355 MPa yield does not excuse a missing impact temperature on the order. This is also not a weathering steel and not a pressure-vessel material.
The listing is for IPE and IPN I-sections. EN 10025-2 S355JR steel plate is a different product form, with its own long-product versus flat-product columns. EN 10025-2 S355JR H-beam covers HEA and HEB for the same grade; that live H-beam page still also lists IPE, which this article takes as the I-beam subject together with IPN. Carbon-equivalent figures for S355JR sit in the chemical-composition section of this page, not in a separate tab, because that is how the verified sister tables were published.
Most S355JR I-beam orders are for IPE. IPN still appears on older European details and should be ordered by its own EN 10365 designation. IPE 300 and IPN 300 are not interchangeable, even though both are 355 MPa in this grade when the flange stays in the same thickness band.
Material, Dimensions and Tolerances for EN 10025-2 S355JR IPE and IPN I-Beams
Write EN 10025-2 S355JR, EN 10365, and the correct tolerance standard as three separate calls on the order:
- EN 10025-2 for the S355JR long-product chemistry, carbon equivalent and tensile properties. This article follows EN 10025-2:2019; the named edition governs.
- EN 10365 for IPE and IPN dimensions. The tables are reference dimensions, not a rolling list for a particular mill.
- EN 10034 for IPE and EN 10024 for IPN. EN 10163-3 is the usual surface-condition reference for sections if a class is to be named.
Do not treat “S355 I-beam” as complete. The quality letters, the series and the designation still have to appear. An HEA, a W-shape or a Q355B I-beam of similar depth is a different product.
EN 10025-2 S355JR IPE and IPN Sizes: EN 10365 Reference Tables
The EN 10025-2 S355JR size tables are the full standard IPE series (18 sizes, IPE 80–600) and the full standard IPN series (21 sizes, IPN 80–600) from EN 10365:2017. They are published here as reference dimensions and theoretical masses. They are not a rolling list, and they are not a promise that every designation is produced in S355JR. Mid-range IPE 200–450 is the usual enquiry core.
Watch the 16 mm yield step on this grade: IPE 500 has a 16.0 mm flange and remains at 355 MPa; IPE 600 (19.0 mm) and IPN 300 (16.2 mm) drop to 345 MPa. IPN 280, 320, 380 and 600 carry the source-programme footnote on agreement for tonnage and delivery.
IPE series
Parallel-flange I-beams, 18 sizes from IPE 80 to IPE 600, under EN 10365:2017.
Swipe horizontally to view all dimensions.
IPN series
Taper-flange I-beams (14% flange slope), 21 sizes from IPN 80 to IPN 600, under EN 10365:2017. Rows marked * are listed in the source programme with the footnote that minimum tonnage and delivery conditions are upon agreement (IPN 280, IPN 320, IPN 380 and IPN 600).
Swipe horizontally to view all dimensions.
HEA and HEB remain on EN 10025-2 S355JR H-beam. American S shapes are on the ASTM A36 S Shape I Beams page. The kg/m figures are theoretical catalogue masses; settlement should follow the contract.
EN 10025-2 S355JR Chemical Composition (Ladle Analysis)
The figures below are ladle-analysis (heat-analysis) maxima for S355JR long products, as published in manufacturer section programmes against EN 10025-2:2019. They are limits, not typical ladle results. Product analysis may differ from ladle analysis by the deviations permitted in the ordered edition of the standard. Do not apply the flat-product table for this grade to IPE or IPN I-beams without checking the long-product columns; phosphorus and sulphur maxima, in particular, are not always the same in the two product forms. The same caution applies when reading S355JR plate data beside this page.
| Element | Maximum, ladle analysis (mass %) | Notes |
|---|---|---|
| C | 0.24 | Same 0.24% maximum is published for the ≤16 mm, >16–40 mm and >40 mm columns. For nominal thickness >100 mm the carbon content is subject to agreement in the cited programmes. |
| Si | 0.55 | A lower silicon range, typically 0.14–0.25% with phosphorus limited to 0.035%, may be agreed when a defined hot-dip galvanizing category is required. |
| Mn | 1.60 | — |
| P | 0.040 | Long-product maximum in the 2019 section programmes cited for this article. Some mill declarations or flat-product tables use a tighter 0.035% maximum; the certificate must be read against the ordered edition and product form. |
| S | 0.040 | Same comment as phosphorus. The 0.040% figure is the long-product JR maximum in those programmes, not a typical sulphur level. |
| N | 0.012 | The nitrogen maximum does not apply if total aluminium is at least 0.020%, or if sufficient other nitrogen-binding elements are present and are stated on the inspection document. |
| Cu | 0.55 | — |
Carbon equivalent is calculated as CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. Special options for S275 and S355 in clause 7.2.5 of EN 10025-2:2019 can adjust the applicable limit and should be reviewed when they are invoked. Published maxima for S355JR in the section programmes used here are:
| Nominal thickness (mm) | CEV maximum, ladle analysis (%) |
|---|---|
| ≤ 30 | 0.45 |
| > 30 and ≤ 40 | 0.47 |
| > 40, in the documented range through 140–150 mm | 0.47 |
One manufacturer programme prints the third CEV band to 140 mm; a sections declaration of performance for the same grade prints 0.47% through 150 mm. For any flange or web thicker than that documented range, the CEV limit should be agreed against the ordered edition. These CEV figures describe weldability in the sense of the material standard; they are not a welding procedure.
If other alloying elements are added, they are to be reported on the inspection document. The table above does not invent limits for niobium, vanadium or titanium for S355JR; where a programme lists optional micro-alloying maxima, those values belong on the certificate when they are used, not as a default chemistry for this grade.
EN 10025-2 S355JR Mechanical Properties: Yield, Tensile and Impact
Mechanical properties of S355JR are thickness-dependent. The values below are minimums or ranges for long products as published in manufacturer section programmes against EN 10025-2:2019. Yield is the upper yield strength ReH. Elongation A is for a proportional gauge length L0 = 5.65√S0. For long products the standard generally specifies longitudinal test pieces unless the order states otherwise. These figures should not be mixed with the transverse elongation values used for wide flat products of the same grade.
| Nominal thickness t (mm) | Minimum yield ReH (MPa) | Tensile strength Rm (MPa) | Minimum elongation A (%) |
|---|---|---|---|
| t ≤ 16 | 355 | 470–630 | 22 |
| 16 < t ≤ 40 | 345 | 470–630 | 22 |
| 40 < t ≤ 63 | 335 | 470–630 | 21 |
| 63 < t ≤ 80 | 325 | 470–630 | 20 |
| 80 < t ≤ 100 | 315 | 470–630 | 20 |
| 100 < t ≤ 150 | 295 | 450–600 | 18 |
In the table, the 470–630 MPa tensile range applies for 3 mm ≤ t ≤ 100 mm, and the 22% elongation value applies for 3 mm ≤ t ≤ 40 mm, as in the section programmes cited for EN 10025-2:2019.
For H-beams and IPE sections, the governing thickness for these bands is the relevant product thickness defined in EN 10025-2, commonly the flange thickness for the tensile and impact tests on sections. A HE 200 B flange is 15 mm, so it falls in the 355 MPa yield and 22% elongation band; a HE 600 B flange is 30 mm, so the minimum yield is 345 MPa. Always apply the band that matches the actual governing thickness of the ordered size, not the 355 MPa headline value.
The JR quality requires a minimum Charpy V-notch absorbed energy of 27 J at +20 °C, in the longitudinal direction. For sections with a nominal thickness greater than 100 mm, the cited section programmes state that the impact values shall be agreed. If the design specification needs 27 J at 0 °C or at −20 °C, the grade to nominate is S355J0 or S355J2, not S355JR. The strength table above is shared by those qualities; the impact temperature is not.
The mechanical table used here stops at 150 mm, which covers the flange thicknesses of the standard HE A, HE B and IPE series tabulated on this page. Thicker specials, if ever required, must be agreed to the ordered edition and are not given invented values here.
Apply the band that matches the governing thickness, usually the flange. An IPE 500 flange is 16.0 mm, so it remains in the 355 MPa band. An IPE 600 flange is 19.0 mm, so the minimum yield is 345 MPa, not 355 MPa. An IPN 300 flange is 16.2 mm, so the minimum yield is 345 MPa, not 355 MPa. An IPE 500 flange is 16.0 mm and remains in the 355 MPa band; an IPE 600 flange is 19.0 mm and uses the 345 MPa band.
Delivery, Inspection and Identification of EN 10025-2 S355JR IPE and IPN I-Beams
S355JR IPE and IPN sections are commonly delivered in the as-rolled condition of EN 10025-2 unless the order names a different delivery condition. The inspection document should identify the grade, the steel number 1.0045, the dimensional standard, the designation (for example IPE 300), and the ordered edition. Marking should follow the ordered product standards so the piece can be matched to the certificate.
An ordinary works certificate that only says “S355JR beam” without the series, the dimensional standard or the quality letters is not a complete identification. If a specific inspection document type is required (for example EN 10204 3.1), name it on the order. This page does not invent test frequencies or document types beyond those rules.
Weldability and Surface Condition of EN 10025-2 S355JR IPE and IPN I-Beams
The carbon-equivalent limits in this article describe weldability in the sense of EN 10025-2. They are not a welding procedure. Procedure qualification, consumables, preheat and hydrogen control remain the fabricator’s responsibility for the thickness, joint and service actually used. S355JR is a JR or J2 quality as named; a +20 °C Charpy requirement does not by itself define heat-affected-zone toughness after welding.
Surface condition for sections is commonly specified to EN 10163-3. If a class or a special surface requirement matters for painting, galvanizing or fatigue, it should be named on the order. Do not assume that an IPE and an IPN of similar depth will present the same flange taper or the same detailing at the root.
Shape Tolerances for EN 10025-2 S355JR IPE and IPN I-Beams (EN 10034 and EN 10024)
For EN 10025-2 S355JR I-beams, IPE tolerances are EN 10034 and IPN tolerances are EN 10024. Those tables are not reproduced here. The material standard does not set the shape allowances. The edition on the order is the one that applies.
A delivered IPE 400 should come out close to 400 × 180 × 8.6 × 13.5 mm within EN 10034. A delivered IPN 400 should come out close to 400 × 155 × 14.4 × 21.6 mm within EN 10024. The two 400 mm designations are not interchangeable, and the IPN flange taper affects fitting.
Theoretical and weighed mass must not be mixed informally. The contract should state the settlement basis.
Applications and Service Limits for EN 10025-2 S355JR IPE and IPN Steel I Beams
EN 10025-2 S355JR IPE is the workhorse parallel-flange I-beam for European frames, floors and general structures where 355 MPa and a +20 °C impact test are the specified combination. IPN is used when a taper-flange I is actually drawn. Neither series is an H-beam, and JR is the wrong quality if the specification names a sub-zero test.
If the project needs 27 J at −20 °C, use EN 10025-2 S355J2 IPE and IPN Steel I Beams. Lower yield classes are EN 10025-2 S275JR IPE and IPN Steel I Beams and EN 10025-2 S235JR IPE and IPN Steel I Beams. This page is not a span table and not a fire or corrosion design guide.
EN 10025-2 S355JR IPE and IPN Compared with S355J2, S235JR and A36
EN 10025-2 S355JR and EN 10025-2 S355J2 IPE and IPN Steel I Beams share the 355 MPa class and the same IPE and IPN series, but J2 moves the 27 J test to −20 °C and tightens phosphorus and sulphur. An S355JR certificate does not satisfy a J2 line unless the order is changed. EN 10025-2 S235JR IPE and IPN Steel I Beams and EN 10025-2 S275JR IPE and IPN Steel I Beams are lower yield classes, not automatic substitutes.
EN 10025-2 S355JR H-beam is the H-section listing. ASTM A36 S Shape I Beams and ASTM A36 wide-flange beams use ASTM A6 designations. Dual certification is possible only when the delivered piece meets every requirement of each named standard.
Near-Equivalents for EN 10025-2 S355JR IPE and IPN Steel I Beams: Not Automatic Substitutes
The comparisons below are near-equivalents used for orientation. They are not a licence to substitute one grade for another on a contract, a drawing, or a mill certificate. Chemistry windows, deoxidation, impact temperature, thickness bands, product form and the dimensional standard all have to be checked. Where a project allows an alternative grade, the substitution should be written into the order and verified on the inspection document.
| Grade / designation | Standard | Relationship to S355JR H-beam | Caution |
|---|---|---|---|
| S355J0 / S355J2 | EN 10025-2 | Same nominal yield class; tighter impact temperature (0 °C or −20 °C). | Not the same quality as JR. Use when the specification requires the lower test temperature. |
| Q355B | GB/T 1591 (material); dimensions often GB/T 11263 | Comparable 355 MPa yield class with an ambient-temperature impact requirement in the B quality. | Different chemistry table, product standard and shape series (HW/HM/HN). Not an automatic substitute. |
| ASTM A572 Grade 50 | ASTM A572; W-shape dimensions ASTM A6 | Comparable 50 ksi (345 MPa) yield class, widely used for welded and bolted frames. | Different chemistry, toughness practice and shape system. Dual certification is possible only when both standards are fully met. |
| ASTM A992 | ASTM A992; W-shape dimensions ASTM A6 | Common US wide-flange grade with a similar yield class and additional constraints used for building frames. | A W-shape grade, not an HEA/HEB equivalent. Do not treat A992 as a drop-in name for S355JR European sections. |
| JIS SM490 or similar 490 MPa class | JIS G 3106 (or related); dimensions JIS G 3192 | Similar strength class in Japanese welded-structure practice; SS400 / JIS G 3101 is a lower general-structural class and is not a match. | Confirm the exact JIS grade letters (A/B/C) and the shape standard. SM490 is not identical to S355JR. |
ISO 630 and other regional structural grades may also be offered as near-equivalents in some markets. They are omitted from the table where a precise, product-form-specific match was not verified for this article. If a buyer’s specification names one of those grades, it should be handled as its own line, not absorbed into S355JR by informal equivalence.
Sourcing EN 10025-2 S355JR IPE and IPN Steel I Beams from SHH STEEL
SHH STEEL reviews EN 10025-2 S355JR IPE and IPN enquiries against the named designation, the steel number 1.0045, and the edition on the order. A JR requirement is not treated as a J2 requirement, and an HEA or W-shape of similar depth is not treated as an IPE.
Send the IPE or IPN list, the inspection document type and any impact or surface options. Images on this page stay empty; photographs can be provided with a quotation when they are available.
S355JR IPE and IPN Steel I Beam FAQs
-
Is an IPE of a given depth the same as the IPN of that depth?
- No. Both series are tabulated on this page to EN 10365, but they are different sections. IPE 300 is 300 × 150 × 7.1 × 10.7 mm (42.2 kg/m). IPN 300 is 300 × 125 × 10.8 × 16.2 mm (54.2 kg/m), with tapered inner flange faces. Do not order one designation and expect the other.
-
Is an IPE beam the same as an H-beam of similar depth?
- No. IPE is a parallel-flange I-section. HEA and HEB are H-sections with a different width, thickness and mass at a similar nominal depth. The S355JR H-beam page covers HEA and HEB. An IPE 300 is not an HE 300 A or an HE 300 B.
-
Which thickness sets the S355JR yield on these I-beams?
- Apply the band that matches the governing thickness, usually the flange. IPE 500 has a 16.0 mm flange and remains in the 355 MPa band. IPE 600 has a 19.0 mm flange, so the minimum yield is 345 MPa, not 355 MPa. Those flange thicknesses are the tabulated EN 10365 reference values on this page.
-
Does a S355JR certificate automatically include a lower-temperature impact test?
- No. Quality letters matter. S355JR carries 27 J at +20 °C. If the project needs a different test temperature, nominate the matching quality (for this class, S355J0 or S355J2) instead of assuming it from the yield number or the IPE size.
-
Can I use a Chinese I-beam or an American S shape as a substitute for IPE?
- Not by matching a nominal depth or a similar mass. GB/T 706 taper-flange I-beams and ASTM A6 S shapes are different series, with different designation systems, dimensions and tolerances. Dual certification is possible only when the delivered piece meets every requirement of each named standard.
Request a Quotation for EN 10025-2 S355JR IPE and IPN Steel I Beams
EN 10025-2 S355JR IPE and IPN steel I-beams are a non-alloy structural sections (1.0045) with 355 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Nominate the IPE or IPN size to EN 10365 (the tables cover IPE 80–600 and IPN 80–600) and the material to EN 10025-2:2019 (or the edition on the order). Both the IPE 80–600 and IPN 80–600 tables are reference dimensions, not rolling lists. The IPE table is a set of reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.