EN 10025-2 S355J2 IPE and IPN Steel I Beams

EN 10025-2 S355J2 IPE and IPN steel I-beams are fully killed non-alloy sections (1.0577) with 355 MPa yield up to 16 mm and 27 J at −20 °C. IPE and IPN follow EN 10365 (80–600). IPE tolerances are EN 10034; IPN tolerances are EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.
Keywords
EN 10025-2 S355J2 I Beam, S355J2 IPE, S355J2 IPN, EN 10365 IPE 80–600, EN 10365 IPN 80–600
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of EN 10025-2 S355J2 IPE and IPN Steel I Beams
Chemical Composition
Carbon Equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source EN 10025-2 S355J2 IPE and IPN Steel I Beams from SHH STEEL
FAQ
Conclusion

What are EN 10025-2 S355J2 IPE and IPN Steel I Beams?

EN 10025-2 S355J2 is the fully killed 355 MPa quality with a 27 J Charpy requirement at −20 °C and the steel number 1.0577. The J2 letters are the reason for this page. A 355 MPa yield, a deep IPE, or a low ambient temperature on site does not turn an S355JR certificate into S355J2. Phosphorus and sulphur are also tighter than on the JR quality. The steel is killed; that fact belongs on the documents, not as an informal assumption.

The product form here is the I-section, IPE and IPN, not EN 10025-2 S355J2 steel plate and not EN 10025-2 S355J2 H-beam. IPE and IPN dimensions follow EN 10365 and are both tabulated below. Use this page when the specification actually names J2 or a −20 °C test on an I-beam; use the H-beam page when the section is HEA or HEB.

Because J2 is often specified late, after a size has already been picked as IPE 300 or IPN 300, confirm that the flange thickness still supports the 355 MPa band and that the quality letters on the certificate match the order. The two 300 mm designations remain different shapes.

Material, Dimensions and Tolerances for EN 10025-2 S355J2 IPE and IPN I-Beams

An EN 10025-2 S355J2 I-beam order should state the quality letters as clearly as the designation:

  • EN 10025-2 for S355J2 long-product chemistry, carbon equivalent and tensile properties, from EN 10025-2:2019 unless another edition is named.
  • EN 10365 for IPE and IPN reference dimensions.
  • EN 10034 for IPE tolerances and EN 10024 for IPN tolerances, with EN 10163-3 if a surface class is required.

A works certificate that only says “S355 I-beam” is not a J2 identification. Do not accept an S355JR document against a J2 line, and do not treat an HEA of similar depth as the I-beam that was ordered.

EN 10025-2 S355J2 IPE and IPN Sizes: EN 10365 Reference Tables

EN 10025-2 S355J2 uses the same EN 10365 IPE 80–600 and IPN 80–600 series as the JR quality. The difference is the material, not the millimetre designation. The tables are reference dimensions and theoretical masses, not a rolling list, and not a claim that every size is produced in S355J2. Confirm deeper and heavier rows, and the four footnoted IPN sizes, size by size.

The 16 mm yield step still applies: IPE 500 remains in the 355 MPa band; IPE 600 and IPN 300, with flanges above 16 mm, use 345 MPa. That check matters just as much on a J2 order as on a JR order.

IPE series

Parallel-flange I-beams, 18 sizes from IPE 80 to IPE 600, under EN 10365:2017.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) r (mm) A (cm²) Mass (kg/m)
IPE 80 80.0 46.0 3.8 5.2 5 7.6 6.0
IPE 100 100.0 55.0 4.1 5.7 7 10.3 8.1
IPE 120 120.0 64.0 4.4 6.3 7 13.2 10.4
IPE 140 140.0 73.0 4.7 6.9 7 16.4 12.9
IPE 160 160.0 82.0 5.0 7.4 9 20.1 15.8
IPE 180 180.0 91.0 5.3 8.0 9 23.9 18.8
IPE 200 200.0 100.0 5.6 8.5 12 28.5 22.4
IPE 220 220.0 110.0 5.9 9.2 12 33.4 26.2
IPE 240 240.0 120.0 6.2 9.8 15 39.1 30.7
IPE 270 270.0 135.0 6.6 10.2 15 45.9 36.1
IPE 300 300.0 150.0 7.1 10.7 15 53.8 42.2
IPE 330 330.0 160.0 7.5 11.5 18 62.6 49.1
IPE 360 360.0 170.0 8.0 12.7 18 72.7 57.1
IPE 400 400.0 180.0 8.6 13.5 21 84.5 66.3
IPE 450 450.0 190.0 9.4 14.6 21 98.8 77.6
IPE 500 500.0 200.0 10.2 16.0 21 115.5 90.7
IPE 550 550.0 210.0 11.1 17.2 24 134.4 106
IPE 600 600.0 220.0 12.0 19.0 24 156.0 122

IPN series

Taper-flange I-beams (14% flange slope), 21 sizes from IPN 80 to IPN 600, under EN 10365:2017. Rows marked * are listed in the source programme with the footnote that minimum tonnage and delivery conditions are upon agreement (IPN 280, IPN 320, IPN 380 and IPN 600).

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) r1 (mm) r2 (mm) A (cm²) Mass (kg/m)
IPN 80 80.0 42.0 3.9 5.9 3.9 2.3 7.6 5.9
IPN 100 100.0 50.0 4.5 6.8 4.5 2.7 10.6 8.3
IPN 120 120.0 58.0 5.1 7.7 5.1 3.1 14.2 11.1
IPN 140 140.0 66.0 5.7 8.6 5.7 3.4 18.2 14.3
IPN 160 160.0 74.0 6.3 9.5 6.3 3.8 22.8 17.9
IPN 180 180.0 82.0 6.9 10.4 6.9 4.1 27.9 21.9
IPN 200 200.0 90.0 7.5 11.3 7.5 4.5 33.4 26.2
IPN 220 220.0 98.0 8.1 12.2 8.1 4.9 39.5 31.1
IPN 240 240.0 106.0 8.7 13.1 8.7 5.2 46.1 36.2
IPN 260 260.0 113.0 9.4 14.1 9.4 5.6 53.3 41.9
IPN 280* 280.0 119.0 10.1 15.2 10.1 6.1 61.0 47.9
IPN 300 300.0 125.0 10.8 16.2 10.8 6.5 69.0 54.2
IPN 320* 320.0 131.0 11.5 17.3 11.5 6.9 77.7 61.0
IPN 340 340.0 137.0 12.2 18.3 12.2 7.3 86.7 68.0
IPN 360 360.0 143.0 13.0 19.5 13.0 7.8 97.0 76.1
IPN 380* 380.0 149.0 13.7 20.5 13.7 8.2 107.0 84.0
IPN 400 400.0 155.0 14.4 21.6 14.4 8.6 117.7 92.4
IPN 450 450.0 170.0 16.2 24.3 16.2 9.7 146.9 115
IPN 500 500.0 185.0 18.0 27.0 18.0 10.8 179.4 141
IPN 550 550.0 200.0 19.0 30.0 19.0 11.9 212.0 166
IPN 600* 600.0 215.0 21.6 32.4 21.6 13.0 253.7 199

H-section sizes for this grade are on EN 10025-2 S355J2 H-beam. IPE and IPN rows are not W-shapes or Q355 families by depth. Mass settlement should follow the contract.

EN 10025-2 S355J2 Chemical Composition (Ladle Analysis)

The figures below are ladle-analysis maxima for S355J2 long products in EN 10025-2:2019. In addition to the tighter phosphorus and sulphur, J2 is defined as a fully killed steel with nitrogen-binding elements sufficient to bind the available nitrogen. That deoxidation practice, not a tabulated nitrogen maximum, is what belongs on the inspection document.

Element Ladle analysis, max (mass %) Notes for S355J2 long products
C, t ≤ 16 mm 0.20 Tighter than the S355JR carbon table, which allows 0.24%.
C, 16 mm < t ≤ 30 mm 0.20 —
C, t > 30 mm 0.22 This 0.22% maximum applies from above 30 mm, including the remainder of the 16–40 mm band and thicknesses above 40 mm. For nominal thickness greater than 100 mm, carbon is subject to agreement.
Si 0.55 —
Mn 1.60 —
P 0.030 Tighter than both JR (0.040%) and J0 (0.035%).
S 0.030 Tighter than both JR and J0.
N No tabulated maximum S355J2 is supplied as a fully killed steel with nitrogen-binding elements in amounts sufficient to bind the available nitrogen, for example a minimum of 0.020% total aluminium. If other nitrogen-binding elements are used, they shall be reported on the inspection document.
Cu 0.55 This copper maximum does not make the grade a weathering steel.
Other added elements As reported If other elements are added, they shall be mentioned on the inspection document.

EN 10025-2 S355J2 Carbon Equivalent

The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S355J2 long products are:

Nominal thickness (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.45
30 < t ≤ 40 0.47
40 < t ≤ 140 0.47

The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S355. If that clause is to be used, it should be named on the order; this page does not invent a raised CEV figure from it.

EN 10025-2 S355J2 Mechanical Properties: Yield, Tensile and Impact

Tensile properties of S355J2 follow the S355 long-product table in EN 10025-2:2019, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are given here. Plate sampling is covered on S355J2 steel plate, not by this table.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 355 470–630 22
16 < t ≤ 40 345 470–630 22
40 < t ≤ 63 335 470–630 21
63 < t ≤ 80 325 470–630 20
80 < t ≤ 100 315 470–630 20
100 < t ≤ 150 295 450–600 18

The J2 quality requires 27 J at −20 °C. For long products the Charpy test is normally longitudinal unless the order specifies otherwise. That energy and temperature should not be confused with S355K2, which is also tested at −20 °C but at 40 J, or with S355J0 at 0 °C. A JR or J0 certificate does not demonstrate the J2 test.

HE 160 A, with a 9 mm flange, remains at 355 MPa. HE 300 B, with a 19 mm flange, is 345 MPa.

Apply the band that matches the governing thickness, usually the flange. An IPE 500 flange is 16.0 mm, so it remains in the 355 MPa band. An IPE 600 flange is 19.0 mm, so the minimum yield is 345 MPa, not 355 MPa. An IPN 300 flange is 16.2 mm, so the minimum yield is 345 MPa, not 355 MPa. An IPE 500 flange is 16.0 mm and remains in the 355 MPa band; an IPE 600 flange is 19.0 mm and uses the 345 MPa band.

Delivery, Inspection and Identification of EN 10025-2 S355J2 IPE and IPN I-Beams

S355J2 IPE and IPN sections are commonly delivered in the as-rolled condition of EN 10025-2 unless the order names a different delivery condition. The inspection document should identify the grade, the steel number 1.0577, the dimensional standard, the designation (for example IPE 300), and the ordered edition. Marking should follow the ordered product standards so the piece can be matched to the certificate.

An ordinary works certificate that only says “S355J2 beam” without the series, the dimensional standard or the quality letters is not a complete identification. If a specific inspection document type is required (for example EN 10204 3.1), name it on the order. This page does not invent test frequencies or document types beyond those rules.

Weldability and Surface Condition of EN 10025-2 S355J2 IPE and IPN I-Beams

The carbon-equivalent limits in this article describe weldability in the sense of EN 10025-2. They are not a welding procedure. Procedure qualification, consumables, preheat and hydrogen control remain the fabricator’s responsibility for the thickness, joint and service actually used. S355J2 is a JR or J2 quality as named; a −20 °C Charpy requirement does not by itself define heat-affected-zone toughness after welding.

Surface condition for sections is commonly specified to EN 10163-3. If a class or a special surface requirement matters for painting, galvanizing or fatigue, it should be named on the order. Do not assume that an IPE and an IPN of similar depth will present the same flange taper or the same detailing at the root.

Shape Tolerances for EN 10025-2 S355J2 IPE and IPN I-Beams (EN 10034 and EN 10024)

EN 10025-2 S355J2 does not change the shape-tolerance standard. IPE is still EN 10034 and IPN is still EN 10024. Those allowances are not printed here; the ordered edition applies.

Reference dimensions remain the EN 10365 rows. IPE 300 and IPN 300 must each be checked against their own depth, width and thicknesses. The J2 quality does not make those two sections the same, and it does not tighten or loosen the shape tolerances on its own.

State whether settlement is on theoretical or weighed mass.

Applications and Service Limits for EN 10025-2 S355J2 IPE and IPN Steel I Beams

EN 10025-2 S355J2 IPE and IPN sections are used where a 355 MPa I-beam and a −20 °C impact test are both required — typically in colder service, in specifications that name J2, or where the JR quality has already been rejected. They are not a weathering steel and not a nuclear or pressure-vessel default material.

If the specification only requires +20 °C, EN 10025-2 S355JR IPE and IPN Steel I Beams is the matching quality. If the section is an H-beam, use EN 10025-2 S355J2 H-beam. This page does not give span or toughness-design tables.

EN 10025-2 S355J2 IPE and IPN Compared with S355JR, Q355B and A572 Grade 50

The closest European comparison is EN 10025-2 S355JR IPE and IPN Steel I Beams: same yield class and the same IPE and IPN series, different impact temperature and a tighter phosphorus and sulphur table. S355J0 is the 0 °C quality and is a third designation. Q355 families and ASTM A572 Grade 50 can sit in a similar yield band, but they use different chemistry, impact and shape rules.

EN 10025-2 S355J2 H-beam is the H-section listing for this grade. Dual certification is possible only when the delivered piece meets every requirement of each named standard, including the J2 test when J2 is required.

Near-Equivalents for EN 10025-2 S355J2 IPE and IPN Steel I Beams: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to S355J2 H-beam Caution
S355JR / S355J0 EN 10025-2 Same 355 MPa yield class and the same usual HEA, HEB and IPE series, tested at +20 °C and 0 °C respectively. Neither JR nor J0 demonstrates a −20 °C test, and both have looser phosphorus and sulphur than J2. J2 is also a fully killed grade.
S355K2 EN 10025-2 The same −20 °C test temperature, but with a 40 J impact requirement rather than 27 J. K2 is a different quality letter. Do not treat a J2 certificate as if it included the K2 energy value.
S355J2W / S355J2WP EN 10025-5 Weathering grades that share a similar quality letter and test temperature. They are a different standard. They are not S355J2 under EN 10025-2.
Q355D GB/T 1591; dimensions GB/T 11263 A Chinese 355 MPa grade tested at −20 °C, often compared in export enquiries. Q355D has its own impact energy (34 J longitudinal) and the HW/HM/HN shape system. It is not an automatic substitute.
ASTM A572 Grade 50 ASTM A572/A572M; dimensions ASTM A6 A 50 ksi [345 MPa] comparison, usually as W-shapes. A572 Grade 50 has no default −20 °C impact test. The shape systems differ.

Sister beam pages in this series (S235JR, S275JR, S355J0) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page for the +20 °C quality in this yield class.

Sourcing EN 10025-2 S355J2 IPE and IPN Steel I Beams from SHH STEEL

SHH STEEL reviews EN 10025-2 S355J2 IPE and IPN enquiries for the quality letters as well as for the designation and the edition. An S355JR document is not accepted as a silent substitute, and an HEA of similar depth is not treated as the I-beam on the order.

Send the IPE or IPN list, the required inspection document, and a note that J2 or −20 °C is required. Images on this page stay empty; photographs can be provided with a quotation when they are available.

S355J2 IPE and IPN Steel I Beam FAQs

Is an IPE of a given depth the same as the IPN of that depth?
No. Both series are tabulated on this page to EN 10365, but they are different sections. IPE 300 is 300 × 150 × 7.1 × 10.7 mm (42.2 kg/m). IPN 300 is 300 × 125 × 10.8 × 16.2 mm (54.2 kg/m), with tapered inner flange faces. Do not order one designation and expect the other.
Is an IPE beam the same as an H-beam of similar depth?
No. IPE is a parallel-flange I-section. HEA and HEB are H-sections with a different width, thickness and mass at a similar nominal depth. The S355J2 H-beam page covers HEA and HEB. An IPE 300 is not an HE 300 A or an HE 300 B.
Which thickness sets the S355J2 yield on these I-beams?
Apply the band that matches the governing thickness, usually the flange. IPE 500 has a 16.0 mm flange and remains in the 355 MPa band. IPE 600 has a 19.0 mm flange, so the minimum yield is 345 MPa, not 355 MPa. Those flange thicknesses are the tabulated EN 10365 reference values on this page.
Does a S355J2 certificate automatically include a lower-temperature impact test?
No. Quality letters matter. S355J2 carries 27 J at −20 °C. If the project needs a different test temperature, nominate the matching quality (for this class, S355JR or S355J0) instead of assuming it from the yield number or the IPE size.
Can I use a Chinese I-beam or an American S shape as a substitute for IPE?
Not by matching a nominal depth or a similar mass. GB/T 706 taper-flange I-beams and ASTM A6 S shapes are different series, with different designation systems, dimensions and tolerances. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Request a Quotation for EN 10025-2 S355J2 IPE and IPN Steel I Beams

EN 10025-2 S355J2 IPE and IPN steel I-beams are a fully killed non-alloy structural sections (1.0577) with 355 MPa minimum yield up to 16 mm and 27 J impact at −20 °C. Nominate the IPE or IPN size to EN 10365 (the tables cover IPE 80–600 and IPN 80–600) and the material to EN 10025-2:2019 (or the edition on the order). Both the IPE 80–600 and IPN 80–600 tables are reference dimensions, not rolling lists. The IPE table is a set of reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X