EN 10025-2 S235JR IPE and IPN Steel I Beams

EN 10025-2 S235JR IPE and IPN steel I-beams are non-alloy sections (1.0038) with 235 MPa yield up to 16 mm and 27 J at +20 °C. This page tabulates IPE 80–600 and IPN 80–600 to EN 10365. IPE tolerances follow EN 10034; IPN tolerances follow EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.
Keywords
EN 10025-2 S235JR I Beam, S235JR IPE, S235JR IPN, EN 10365 IPE 80–600, EN 10365 IPN 80–600
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of EN 10025-2 S235JR IPE and IPN Steel I Beams
Chemical Composition
Carbon Equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source EN 10025-2 S235JR IPE and IPN Steel I Beams from SHH STEEL
FAQ
Conclusion

What are EN 10025-2 S235JR IPE and IPN Steel I Beams?

EN 10025-2 S235JR IPE and IPN steel I-beams start from the 235 MPa structural class, not from a “European I-beam” as a generic product. The steel number is 1.0038. S marks a structural steel, 235 is the minimum yield in the thinnest tabulated thickness band, and JR requires 27 J Charpy V-notch energy at +20 °C. That quality is accepted for many workshops and ordinary frames; it is not a stand-in for a 0 °C or −20 °C test, and it is not a 355 MPa grade.

The rolled I-section is a different product form from EN 10025-2 S235JR steel plate. Sampling and elongation rules for plate should not be read across onto these I-beams. HEA and HEB for the same grade belong on the EN 10025-2 S235JR H-beam page; those H-sections are not republished here. The live H-beam page still also lists IPE; this article is the I-beam listing, with both the parallel-flange IPE series and the taper-flange IPN series tabulated to EN 10365.

The pages sit under I Beams and IPE Beams. IPE 300 and IPN 300 share a 300 mm depth and little else: the flange width, thickness and mass are different, and IPN has a 14% inner flange slope. American Standard S shapes, GB/T 706 taper-flange I-beams and W-shapes are other families again. If an enquiry only says “S235 I-beam,” the quality letters and the series still have to be named.

Material, Dimensions and Tolerances for EN 10025-2 S235JR IPE and IPN I-Beams

A complete EN 10025-2 S235JR I-beam order has to keep three documents distinct:

  • EN 10025-2 is the material standard. The ladle-analysis, carbon-equivalent and tensile values on this page are those for S235JR long products in EN 10025-2:2019. The edition on the order governs acceptance.
  • EN 10365 is the dimensional standard for both IPE and IPN. The two tables below are reference dimensions and theoretical masses for the standard series, not a mill rolling list.
  • EN 10034 sets shape and mass tolerances for IPE. EN 10024 sets the corresponding tolerances for IPN taper-flange I-sections. Surface condition for sections is commonly specified to EN 10163-3; name the class if a tighter finish is required.

A mill may certify S235JR on a different series, or roll an IPE and certify another grade, if that combination is documented. Do not treat “S235JR I-beam” as if it automatically meant IPE 300, and do not treat an HE 300 A, an S12 or a Chinese I of similar depth as the same section.

EN 10025-2 S235JR IPE and IPN Sizes: EN 10365 Reference Tables

Two EN 10365 series are tabulated for EN 10025-2 S235JR. The first is IPE, the parallel-flange I-beam, 18 sizes from IPE 80 to IPE 600. The second is IPN, the older taper-flange I-beam with a 14% flange slope, 21 sizes from IPN 80 to IPN 600. The figures are reference dimensions and theoretical masses for identification and estimating, not a rolling list, and not a claim that every row is produced in S235JR. Dimensional acceptance follows the editions of EN 10365 and of the matching tolerance standard named on the order.

Read the two tables as separate series. IPE 300 is not IPN 300, and neither is an HE 300 A. Mid-range IPE 200 to IPE 400 are the usual enquiry core; the lightest IPE 80–120 rows and the deepest IPE 550–600 rows should be confirmed size by size. The same caution applies at the ends of the IPN range, and four IPN rows carry a source-programme footnote on agreement for tonnage and delivery.

IPE series

Parallel-flange I-beams, 18 sizes from IPE 80 to IPE 600, under EN 10365:2017.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) r (mm) A (cm²) Mass (kg/m)
IPE 80 80.0 46.0 3.8 5.2 5 7.6 6.0
IPE 100 100.0 55.0 4.1 5.7 7 10.3 8.1
IPE 120 120.0 64.0 4.4 6.3 7 13.2 10.4
IPE 140 140.0 73.0 4.7 6.9 7 16.4 12.9
IPE 160 160.0 82.0 5.0 7.4 9 20.1 15.8
IPE 180 180.0 91.0 5.3 8.0 9 23.9 18.8
IPE 200 200.0 100.0 5.6 8.5 12 28.5 22.4
IPE 220 220.0 110.0 5.9 9.2 12 33.4 26.2
IPE 240 240.0 120.0 6.2 9.8 15 39.1 30.7
IPE 270 270.0 135.0 6.6 10.2 15 45.9 36.1
IPE 300 300.0 150.0 7.1 10.7 15 53.8 42.2
IPE 330 330.0 160.0 7.5 11.5 18 62.6 49.1
IPE 360 360.0 170.0 8.0 12.7 18 72.7 57.1
IPE 400 400.0 180.0 8.6 13.5 21 84.5 66.3
IPE 450 450.0 190.0 9.4 14.6 21 98.8 77.6
IPE 500 500.0 200.0 10.2 16.0 21 115.5 90.7
IPE 550 550.0 210.0 11.1 17.2 24 134.4 106
IPE 600 600.0 220.0 12.0 19.0 24 156.0 122

IPN series

Taper-flange I-beams (14% flange slope), 21 sizes from IPN 80 to IPN 600, under EN 10365:2017. Rows marked * are listed in the source programme with the footnote that minimum tonnage and delivery conditions are upon agreement (IPN 280, IPN 320, IPN 380 and IPN 600).

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) r1 (mm) r2 (mm) A (cm²) Mass (kg/m)
IPN 80 80.0 42.0 3.9 5.9 3.9 2.3 7.6 5.9
IPN 100 100.0 50.0 4.5 6.8 4.5 2.7 10.6 8.3
IPN 120 120.0 58.0 5.1 7.7 5.1 3.1 14.2 11.1
IPN 140 140.0 66.0 5.7 8.6 5.7 3.4 18.2 14.3
IPN 160 160.0 74.0 6.3 9.5 6.3 3.8 22.8 17.9
IPN 180 180.0 82.0 6.9 10.4 6.9 4.1 27.9 21.9
IPN 200 200.0 90.0 7.5 11.3 7.5 4.5 33.4 26.2
IPN 220 220.0 98.0 8.1 12.2 8.1 4.9 39.5 31.1
IPN 240 240.0 106.0 8.7 13.1 8.7 5.2 46.1 36.2
IPN 260 260.0 113.0 9.4 14.1 9.4 5.6 53.3 41.9
IPN 280* 280.0 119.0 10.1 15.2 10.1 6.1 61.0 47.9
IPN 300 300.0 125.0 10.8 16.2 10.8 6.5 69.0 54.2
IPN 320* 320.0 131.0 11.5 17.3 11.5 6.9 77.7 61.0
IPN 340 340.0 137.0 12.2 18.3 12.2 7.3 86.7 68.0
IPN 360 360.0 143.0 13.0 19.5 13.0 7.8 97.0 76.1
IPN 380* 380.0 149.0 13.7 20.5 13.7 8.2 107.0 84.0
IPN 400 400.0 155.0 14.4 21.6 14.4 8.6 117.7 92.4
IPN 450 450.0 170.0 16.2 24.3 16.2 9.7 146.9 115
IPN 500 500.0 185.0 18.0 27.0 18.0 10.8 179.4 141
IPN 550 550.0 200.0 19.0 30.0 19.0 11.9 212.0 166
IPN 600* 600.0 215.0 21.6 32.4 21.6 13.0 253.7 199

Chinese HW, HM and HN names belong to GB/T 11263 practice, not to these rows. American Standard S shapes are listed on the ASTM A36 S Shape I Beams page, and HEA or HEB dimensions belong on the EN 10025-2 S235JR H-beam page. The kg/m column is a theoretical catalogue mass. Settlement should follow the contract — theoretical mass or weighed mass.

EN 10025-2 S235JR Chemical Composition (Ladle Analysis)

The figures below are ladle-analysis maxima for S235JR long products in EN 10025-2:2019. They are limits, not typical heat results. Do not mix them with unofficial tables that borrow plate phosphorus figures or that give S235JR a silicon maximum it does not generally have.

Element Ladle analysis, max (mass %) Notes for S235JR long products
C, t ≤ 16 mm 0.17 —
C, 16 mm < t ≤ 40 mm 0.17 —
C, t > 40 mm 0.20 For nominal thickness greater than 100 mm, carbon is subject to agreement.
Si No general maximum A dash in the source table. By agreement, silicon may be set at 0.14–0.25% and phosphorus at ≤0.035% for hot-dip galvanizing category B.
Mn 1.40 —
P 0.040 See the galvanizing agreement above. Do not paste a flat-product 0.035% default onto a beam order unless that is what was agreed.
S 0.040 —
N 0.012 The nitrogen maximum does not apply if total aluminium is at least 0.020%, or if sufficient other nitrogen-binding elements are present and reported.
Cu 0.55 —
Other added elements As reported If other elements are added, they shall be mentioned on the inspection document.

EN 10025-2 S235JR Carbon Equivalent

The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S235JR long products are:

Nominal thickness (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.35
30 < t ≤ 40 0.35
40 < t ≤ 140 0.38

The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S275 and S355; those conditions are not applied to S235JR on this page.

EN 10025-2 S235JR Mechanical Properties: Yield, Tensile and Impact

Tensile properties of S235JR are thickness-dependent. The values below are from EN 10025-2:2019 for long products, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are given here. Plate elongation and sampling are covered on S235JR steel plate, not by this table.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 235 360–510 26
16 < t ≤ 40 225 360–510 26
40 < t ≤ 63 215 360–510 25
63 < t ≤ 80 215 360–510 24
80 < t ≤ 100 215 360–510 24
100 < t ≤ 150 195 350–500 22

Quality JR requires a Charpy V-notch absorbed energy of 27 J at +20 °C. For long products the test is normally longitudinal unless the order specifies otherwise. If the project needs 27 J at 0 °C or at −20 °C, the grade to nominate is S235J0 or S235J2, not S235JR.

Apply the band that matches the governing thickness, usually the flange. An IPE 500 flange is 16.0 mm, so it remains in the 235 MPa band. An IPE 600 flange is 19.0 mm, so the minimum yield is 225 MPa, not 235 MPa. An IPN 300 flange is 16.2 mm, so the minimum yield is 225 MPa, not 235 MPa. An IPE 500 flange is 16.0 mm and remains in the 235 MPa band; an IPE 600 flange is 19.0 mm and uses the 225 MPa band.

Delivery, Inspection and Identification of EN 10025-2 S235JR IPE and IPN I-Beams

S235JR IPE and IPN sections are commonly delivered in the as-rolled condition of EN 10025-2 unless the order names a different delivery condition. The inspection document should identify the grade, the steel number 1.0038, the dimensional standard, the designation (for example IPE 300), and the ordered edition. Marking should follow the ordered product standards so the piece can be matched to the certificate.

An ordinary works certificate that only says “S235JR beam” without the series, the dimensional standard or the quality letters is not a complete identification. If a specific inspection document type is required (for example EN 10204 3.1), name it on the order. This page does not invent test frequencies or document types beyond those rules.

Weldability and Surface Condition of EN 10025-2 S235JR IPE and IPN I-Beams

The carbon-equivalent limits in this article describe weldability in the sense of EN 10025-2. They are not a welding procedure. Procedure qualification, consumables, preheat and hydrogen control remain the fabricator’s responsibility for the thickness, joint and service actually used. S235JR is a JR or J2 quality as named; a +20 °C Charpy requirement does not by itself define heat-affected-zone toughness after welding.

Surface condition for sections is commonly specified to EN 10163-3. If a class or a special surface requirement matters for painting, galvanizing or fatigue, it should be named on the order. Do not assume that an IPE and an IPN of similar depth will present the same flange taper or the same detailing at the root.

Shape Tolerances for EN 10025-2 S235JR IPE and IPN I-Beams (EN 10034 and EN 10024)

IPE and IPN do not share a tolerance standard. Dimensional and mass tolerances for the IPE series are those of EN 10034; for the IPN series they are those of EN 10024. Neither table is reproduced here. Acceptance is against the edition named on the order. EN 10025-2 does not set these shape tolerances.

The size tables above are nominal reference dimensions. A delivered IPE 300 will measure close to 300 × 150 × 7.1 × 10.7 mm within EN 10034, not as a set of exact advertised millimetres. A delivered IPN 300 will measure close to 300 × 125 × 10.8 × 16.2 mm within EN 10024. Out-of-square and web off-centre matter for end-plate connections, and the tapered IPN flange changes how a plate sits.

The kg/m columns are theoretical catalogue masses. Weighed mass may sit above or below those figures and still be within tolerance. Settlement should follow the contract, not an informal mix of theoretical and weighed mass.

Applications and Service Limits for EN 10025-2 S235JR IPE and IPN Steel I Beams

EN 10025-2 S235JR IPE sections are the everyday European I-beam for floors, roofs, light frames and fabrication where a 235 MPa class and a +20 °C impact quality are actually specified. IPN is still named on some older details and on enquiries that want the taper-flange I. This is not a 355 MPa grade, not a weathering steel, and not a pressure-vessel or nuclear safety material.

This page is not a design guide and does not give span tables. If the project needs 27 J at 0 °C or at −20 °C, nominate S235J0 or S235J2. If it needs the 355 MPa class, use EN 10025-2 S355JR IPE and IPN Steel I Beams. If it needs an H-section, use the H-beam page for this grade, not an IPE depth as a shorthand for HEA.

EN 10025-2 S235JR IPE and IPN Compared with S355JR, Q235B and A36

EN 10025-2 S235JR and EN 10025-2 S355JR IPE and IPN Steel I Beams can share the IPE and IPN series, but they are different yield classes with different chemistry and carbon-equivalent tables. An enquiry that only says “European I-beam” is incomplete. S235J0 and S235J2 keep the 235 MPa class and move the 27 J test to 0 °C and −20 °C, with tighter phosphorus and sulphur.

The H-section companion is EN 10025-2 S235JR H-beam. That is a different product form. GB/T 706 Q235B I-beam is a near-equivalent in yield class under a different dimensional standard. ASTM A36 S Shape I Beams are a 36 ksi grade on American Standard S shapes to ASTM A6, not an IPE or IPN substitute by depth. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Near-Equivalents for EN 10025-2 S235JR IPE and IPN Steel I Beams: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to S235JR H-beam Caution
S235J0 / S235J2 EN 10025-2 Same 235 MPa yield class. J0 is tested at 0 °C and J2 at −20 °C, both at 27 J. J0 and J2 also use tighter phosphorus and sulphur. They are not interchangeable with JR on a +20 °C specification.
Q235B GB/T 700; dimensions GB/T 11263 A 235 MPa Chinese carbon steel with a 27 J impact requirement at +20 °C. Different chemistry table and the HW/HM/HN shape system, not HEA/HEB/IPE.
ASTM A36 ASTM A36/A36M; dimensions ASTM A6 A general structural carbon steel, often compared in export enquiries. Yield class is 36 ksi [250 MPa], not 235 MPa, and the shape system is W, not HEA/HEB/IPE.
SS400 JIS G 3101; dimensions often JIS G 3192 A general-structural carbon steel used on Japanese and Taiwanese projects. SS400 has its own tensile window and no JR/J0/J2 impact ladder.

Sister beam pages in this series (S275JR, Q235B, A36, SS400) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page for the 355 MPa European comparison.

Sourcing EN 10025-2 S235JR IPE and IPN Steel I Beams from SHH STEEL

SHH STEEL reviews enquiries for EN 10025-2 S235JR IPE and IPN sections against a named size list and a named edition. The grade letters, the steel number 1.0038, the IPE or IPN designation, and the certificate type are checked before a quotation is prepared. An HEA, a W-shape, an S shape or a GB I-beam of similar depth is not treated as the same item, and an IPE row is not used to fill a missing IPN designation.

Send the designation list, the EN 10025-2 edition, the inspection document type, any impact or surface-class options, and delivery notes. Images on this page stay empty; photographs can be provided with a quotation when they are available.

S235JR IPE and IPN Steel I Beam FAQs

Is an IPE of a given depth the same as the IPN of that depth?
No. Both series are tabulated on this page to EN 10365, but they are different sections. IPE 300 is 300 × 150 × 7.1 × 10.7 mm (42.2 kg/m). IPN 300 is 300 × 125 × 10.8 × 16.2 mm (54.2 kg/m), with tapered inner flange faces. Do not order one designation and expect the other.
Is an IPE beam the same as an H-beam of similar depth?
No. IPE is a parallel-flange I-section. HEA and HEB are H-sections with a different width, thickness and mass at a similar nominal depth. The S235JR H-beam page covers HEA and HEB. An IPE 300 is not an HE 300 A or an HE 300 B.
Which thickness sets the S235JR yield on these I-beams?
Apply the band that matches the governing thickness, usually the flange. IPE 500 has a 16.0 mm flange and remains in the 235 MPa band. IPE 600 has a 19.0 mm flange, so the minimum yield is 225 MPa, not 235 MPa. Those flange thicknesses are the tabulated EN 10365 reference values on this page.
Does a S235JR certificate automatically include a lower-temperature impact test?
No. Quality letters matter. S235JR carries 27 J at +20 °C. If the project needs a different test temperature, nominate the matching quality (for this class, S235J0 or S235J2) instead of assuming it from the yield number or the IPE size.
Can I use a Chinese I-beam or an American S shape as a substitute for IPE?
Not by matching a nominal depth or a similar mass. GB/T 706 taper-flange I-beams and ASTM A6 S shapes are different series, with different designation systems, dimensions and tolerances. Dual certification is possible only when the delivered piece meets every requirement of each named standard.

Request a Quotation for EN 10025-2 S235JR IPE and IPN Steel I Beams

EN 10025-2 S235JR IPE and IPN steel I-beams are a non-alloy structural sections (1.0038) with 235 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Nominate the IPE or IPN size to EN 10365 (the tables cover IPE 80–600 and IPN 80–600) and the material to EN 10025-2:2019 (or the edition on the order). Both the IPE 80–600 and IPN 80–600 tables are reference dimensions, not rolling lists. The IPE table is a set of reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X