Product Showcase
EN 10025-2 Steel Structural Profiles
-
EN 10025-2 S355J2 IPE and IPN Steel I Beams
EN 10025-2 S355J2 IPE and IPN steel I-beams are fully killed non-alloy sections (1.0577) with 355 MPa yield up to 16 mm and 27 J at −20 °C. IPE and IPN follow EN 10365 (80–600). IPE tolerances are EN 10034; IPN tolerances are EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.View More -
EN 10025-2 S355JR IPE and IPN Steel I Beams
EN 10025-2 S355JR IPE and IPN steel I-beams are non-alloy sections (1.0045) with 355 MPa yield up to 16 mm and 27 J at +20 °C. Size tables cover IPE 80–600 and IPN 80–600 to EN 10365. IPE tolerances are EN 10034; IPN tolerances are EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.View More -
EN 10025-2 S275JR IPE and IPN Steel I Beams
EN 10025-2 S275JR IPE and IPN steel I-beams are non-alloy sections (1.0044) with 275 MPa yield up to 16 mm and 27 J at +20 °C, between S235 and S355. Tables cover IPE and IPN 80–600 to EN 10365. IPE uses EN 10034; IPN uses EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.View More -
EN 10025-2 S235JR IPE and IPN Steel I Beams
EN 10025-2 S235JR IPE and IPN steel I-beams are non-alloy sections (1.0038) with 235 MPa yield up to 16 mm and 27 J at +20 °C. This page tabulates IPE 80–600 and IPN 80–600 to EN 10365. IPE tolerances follow EN 10034; IPN tolerances follow EN 10024. SHH STEEL reviews grade, size and certificate requirements before quoting.View More
I Beams and IPE Beams
SHH STEEL supplies hot-rolled I Beams for buildings, frames, and general structural use. Material is specified to the project standard—for example GB/T 700 or GB/T 1591 grades furnished to GB/T 706 I-beam dimensions, or EN 10025-2 grades furnished to IPE or IPN series when so ordered. Dimensional series are stated separately and may include GB/T 706 I-beams (for example 20a, 32c or 63c); EN 10365 IPE; taper-flange IPN or ASTM A6 S shapes; and British universal beams (UB). These I-shaped sections are not H Beams or Wide Flange Beams (W, HEA, HEB, HEM, HW, HM, HN, or JIS H-sections) by depth or mass alone. Sizes and certificates are confirmed per inquiry.
This range covers I Beams and IPE Beams. Buyers also search these sections as I Beam, I-Beam, or Steel I Beams. Typical series are GB/T 706 taper-flange I-beams; EN 10365 IPE (parallel flange) and IPN (taper flange); ASTM A6 S shapes (American Standard Beams); British universal beams (UB); and JIS I-sections. These I-shaped sections are not H Beams or Wide Flange Beams (W, HEA, HEB, HEM, HW, HM, HN, or JIS H-sections) by depth or mass alone. Sizes and certificates are confirmed per inquiry.
I Beams and IPE Beams
X