ASTM A269 UNS S35045 Stainless Steel Tube
What is ASTM A269 UNS S35045 Stainless Steel Tube
ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. UNS S35045 is a heat-resistant high-nickel chromium austenitic under A269 with aluminum and titanium additions for elevated-temperature general-service tubing — not a 6Mo chloride grade. Name ASTM A269 and UNS S35045 on the purchase order so nominal-wall rules, heat treatment, and hardness apply to tubing — not to an A213 or A312 product text.
SHH STEEL can produce and supply ASTM A269 UNS S35045 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates reporting Table 1 chemistry and Table 2 hardness where verified. Typical sizes ~6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Browse the A269/A269M hub. Keep the wall basis nominal.
If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 UNS S35045, SA213 UNS S35045, A312 UNS S35045 and SA312 UNS S35045 and match the product standard to the drawing.
Chemical Composition of A269 UNS S35045
Heat analysis under A269 Table 1 is mandatory for every UNS S35045 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.
Public A269 Table 1 for UNS S35045 — heat-resistant Fe-Ni-Cr austenitic with Al and Ti.
Melting analysis (heat / ladle analysis) — Table 1
| Element | UNS S35045 melting analysis |
|---|---|
| Carbon (C) | 0.06 – 0.10 |
| Manganese (Mn) | ≤ 1.50 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.015 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 25.0 – 29.0 |
| Nickel (Ni) | 32.0 – 37.0 |
| Aluminum (Al) | 0.15 – 0.60 |
| Titanium (Ti) | 0.15 – 0.60 |
| Copper (Cu) | ≤ 0.75 |
Source: ASTM A269/A269M Table 1 for UNS S35045. High Ni/Cr with Al and Ti ranges define heat-resistant intent. Table 2: ≥2000 °F [1095 °C]; hardness 192 HBW / 200 HV or 90 HRB. Mo is not a Table 1 requirement for this UNS in the public excerpt.
Mechanical Properties of A269 UNS S35045
ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for UNS S35045. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.
| Property | UNS S35045 requirement (A269 Table 2) |
|---|---|
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Tensile / yield / elongation | Not specified as an A269 acceptance table for this grade |
Source: ASTM A269/A269M Table 2 for UNS S35045 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.
Seamless and Welded Tube
Under A269, UNS S35045 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.
Seamless UNS S35045 takes a lot-basis flaring test; welded UNS S35045 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 UNS S35045 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.
Dimensions and Tolerances
Order A269 UNS S35045 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.
| OD group (A269 Table 4) | Outside diameter tolerance | Wall thickness tolerance |
|---|---|---|
| Up to ½ in. [13 mm] | ±0.005 in. [0.13 mm] | ±15% |
| ½ to 1½ in. [13–38 mm], excl. | ±0.005 in. [0.13 mm] | ±10% |
| 1½ to 3½ in. [38–89 mm], excl. | ±0.010 in. [0.25 mm] | ±10% |
| 3½ to 5½ in. [89–140 mm], excl. | ±0.015 in. [0.38 mm] | ±10% |
| 5½ to 8 in. [140–203 mm], excl. | ±0.030 in. [0.76 mm] | ±10% |
Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for UNS S35045, say so on the enquiry so SHH STEEL does not build the wrong wall basis.
Equivalent Grades
UNS S35045 is ordered under A269 as listed in Table 1. Related forms may appear under A213/A312/A240 by the same UNS with different wall bases and mechanical tables.
| Reference | Designation | Note |
|---|---|---|
| ASTM A269 | UNS S35045 | This product standard |
| UNS | S35045 | Chemistry identity |
| Other ASTM forms | Same UNS where listed | Confirm product form before substituting |
Compare A269 UNS S35030 when that related heat-resistant UNS is specified.
Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 UNS S35045, SA213 UNS S35045, A312 UNS S35045 and SA312 UNS S35045. Confirm the product form before treating any of those pages as acceptance text for an A269 order.
Heat Treatment and Delivery Condition
All A269 UNS S35045 tube is furnished solution heat-treated. Table 2 sets austenitizing at ≥2000 °F [1095 °C], followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”
| Item | UNS S35045 (A269 Table 2) |
|---|---|
| Austenitizing temperature | ≥2000 °F [1095 °C] |
| Cooling | Water quench or rapid cool |
| Hardness after heat treatment, max | 192 HBW / 200 HV or 90 HRB |
| Delivery condition | Solution heat-treated; pickled or bright-annealed by agreement |
Source: ASTM A269/A269M §6 and Table 2 for UNS S35045 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.
Corrosion Resistance
High Ni/Cr with Al/Ti support oxidation and heat-resistant behaviour in elevated-temperature general service. It is not selected primarily for seawater chloride pitting. A269 publishes no PREN — do not invent one.
Compare Mo grades when chlorides drive selection, or A269 UNS S35030 when that heat-resistant UNS is named.
Applications of A269 UNS S35045 Tube
A269 UNS S35045 appears on heat-resistant process and utility tubing specs that name S35045. SHH STEEL can produce and supply that product and will redirect when Mo-bearing grades better match corrosive aqueous duty.
Not boiler tube or pipe unless those standards separately list the UNS — A269 remains general-service tubing.
When a sister enquiry is for boiler tube or pipe of the same grade, use A213 UNS S35045, SA213 UNS S35045, A312 UNS S35045 and SA312 UNS S35045 instead of stretching an A269 tubing page into the wrong product form.
Weldability
Heat-resistant austenitics need filler matched after review. Mill autogenous A269 welds are solution-treated with the tube; shop welds are not. Note the ≥2000 °F anneal.
SHH STEEL supplies the mill product and MTC with Ni, Cr, Al, and Ti reported.
Surface Finishes
Pickled and bright-annealed finishes cover most A269 UNS S35045 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.
Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 UNS S35045 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.
Inspection and Testing
Lot testing for A269 UNS S35045 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.
Packaging and Shipping
Export and domestic packs for A269 UNS S35045 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.
Stencil and tags typically carry ASTM A269, UNS S35045, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.
Why Choose SHH STEEL
SHH STEEL can produce and supply ASTM A269 UNS S35045 as solution-treated seamless or welded tubing with Table 1 heat-resistant chemistry, Table 2 hardness, and EN 10204 3.1 documentation.
If aqueous chlorides dominate, we point to Mo-bearing A269 grades instead of stretching a heat-resistant UNS into the wrong duty.
Supply Capability
SHH STEEL can produce and supply ASTM A269 UNS S35045 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.
| Item | SHH STEEL capability |
|---|---|
| Standard | ASTM A269 / A269M |
| Grade | UNS S35045 |
| Product form | Seamless and welded tube (no filler metal for welded), hot- or cold-finished |
| Delivery condition | Solution heat-treated (≥2000 °F [1095 °C]); pickled or bright-annealed |
| Typical size band | ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement) |
| Testing | Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.
| OD (mm) | Typical nominal walls (mm) | Notes |
|---|---|---|
| 6 / 8 / 10 / 12 / 14 | 0.5 / 0.8 / 1.0 / 1.2 / 1.5 | Instrument / hydraulic; often BA |
| 12.7 / 15.9 / 19.1 / 25.4 / 31.8 | 1.0 / 1.2 / 1.5 / 2.0 / 2.5 | Inch OD process and utility |
| 38.1 / 48.3 / 60.3 / 76.1 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Utility and light process |
| 88.9 / 114.3 / 141.3 / 168.3 | 2.0 / 3.0 / 4.0 / 6.0 / 8.0 | Larger process tube; lock seamless vs welded |
Enquiry tip — Compare A269 UNS S35030 when that related heat-resistant UNS is specified.
FAQ
-
What is ASTM A269 UNS S35045 stainless steel tube used for?
- A269 UNS S35045 is nominal-wall seamless or welded austenitic tubing for general corrosion-resisting and low- or high-temperature service where this UNS chemistry is specified. It is not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis and tests match.
-
Does ASTM A269 UNS S35045 include welded tube?
- Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What hardness limit applies to A269 UNS S35045?
- Where verified, Table 2 lists 192 HBW / 200 HV or 90 HRB after the required solution treatment. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 or A312 unless the purchase order adds them. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Is A269 UNS S35045 nominal wall or minimum wall?
- Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall practice applies. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What size range can SHH STEEL produce for UNS S35045?
- SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 UNS S35045, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Which tests are mandatory on A269 UNS S35045 tube?
- Hardness to Table 2 where required; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What certificate does SHH STEEL provide for UNS S35045?
- EN 10204 3.1 MTCs report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2 where verified, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, UNS S35045, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
How should I enquire for A269 UNS S35045 with SHH STEEL?
- List ASTM A269, grade UNS S35045, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Add the service medium if alloy selection is still open. SHH STEEL can produce and supply to that enquiry. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Is S35045 a chloride pitting grade?
- Not primarily. Table 1 chemistry emphasizes high Ni/Cr with Al and Ti for heat-resistant service. For chloride pitting, open Mo-bearing A269 grades such as TP316L or UNS S31254 instead. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Must aluminum and titanium appear on the MTC?
- Yes. Al 0.15–0.60% and Ti 0.15–0.60% are Table 1 ranges for S35045, so ladle analysis should report both with Ni and Cr. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Conclusion
ASTM A269 UNS S35045 belongs in the A269 nominal-wall tubing family when this chemistry is named for general-service lines. SHH STEEL can produce and supply seamless and welded A269 UNS S35045, heat-treated and tested per the ordered edition, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.