ASTM A269 UNS S35030 Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 UNS S35030 Stainless Steel Tube

ASTM A269 UNS S35030 nominal-wall seamless and welded austenitic tubing, heat-treated per Table 2 where verified (hardness confirm purchased edition (not verified in public -15 Table 2 excerpt)). SHH STEEL can produce and supply with EN 10204 3.1 MTCs.
Grade
UNS S35030
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 UNS S35030 Stainless Steel Tube

ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. UNS S35030 is a heat-resistant austenitic with molybdenum, copper, and niobium listed in A269 Table 1 block 2 — ordered by UNS for specialty elevated-temperature and chemical tubing when that UNS is named. Name ASTM A269 and UNS S35030 on the purchase order so nominal-wall rules, heat treatment, and hardness apply to tubing — not to an A213 or A312 product text.

SHH STEEL can produce and supply ASTM A269 UNS S35030 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates reporting Table 1 chemistry and Table 2 hardness where verified. Typical sizes ~6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Browse the A269/A269M hub. Keep the wall basis nominal.

Chemical Composition of A269 UNS S35030

Heat analysis under A269 Table 1 is mandatory for every UNS S35030 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.

ASTM A269/A269M-24 store Table 1 excerpt for UNS S35030 — heat-resistant austenitic with Mo, Cu, and Cb.

Melting analysis (heat / ladle analysis) — Table 1

Element UNS S35030 melting analysis
Carbon (C) 0.05 – 0.10
Manganese (Mn) ≤ 1.50
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.015
Silicon (Si) 0.50 – 2.0
Chromium (Cr) 18.5 – 22.5
Nickel (Ni) 22.5 – 27.5
Molybdenum (Mo) 6.0 – 7.0
Nitrogen (N) 0.05 – 0.15
Copper (Cu) 2.5 – 3.5
Columbium (Cb) 0.25 – 0.75

Source: ASTM A269/A269M-24 store Table 1 for UNS S35030. Mo 6–7%, Cu 2.5–3.5%, Cb 0.25–0.75% must appear on the MTC. UNCERTAIN: Table 2 HT/hardness for S35030 not verified in the public -15 PDF Table 2 block — confirm purchased -24/-25 edition.

Mechanical Properties of A269 UNS S35030

ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for UNS S35030. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.

Property UNS S35030 requirement (A269 Table 2)
Hardness, max confirm purchased edition (not verified in public -15 Table 2 excerpt)
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for UNS S35030 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.

Seamless and Welded Tube

Under A269, UNS S35030 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.

Seamless UNS S35030 takes a lot-basis flaring test; welded UNS S35030 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 UNS S35030 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.

Dimensions and Tolerances

Order A269 UNS S35030 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for UNS S35030, say so on the enquiry so SHH STEEL does not build the wrong wall basis.

Equivalent Grades

UNS S35030 is ordered under A269 as listed in Table 1. Related forms may appear under A213/A312/A240 by the same UNS with different wall bases and mechanical tables.

Reference Designation Note
ASTM A269 UNS S35030 This product standard
UNS S35030 Chemistry identity
Other ASTM forms Same UNS where listed Confirm product form before substituting

Compare A269 UNS S35045 for Al-Ti heat-resistant chemistry.

Heat Treatment and Delivery Condition

All A269 UNS S35030 tube is furnished solution heat-treated. Table 2 sets austenitizing at confirm purchased edition (not verified in public -15 Table 2 excerpt), followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”

Item UNS S35030 (A269 Table 2)
Austenitizing temperature confirm purchased edition (not verified in public -15 Table 2 excerpt)
Cooling Water quench or rapid cool
Hardness after heat treatment, max confirm purchased edition (not verified in public -15 Table 2 excerpt)
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for UNS S35030 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.

Corrosion Resistance

Mo plus Cu and Cb with elevated Ni support specialty heat-resistant and chemical duties when S35030 is specified. A269 publishes no PREN — do not invent one. Confirm Table 2 heat treatment and hardness in the purchased edition.

Compare A269 UNS S35045 when Al-Ti heat-resistant chemistry is named instead.

Applications of A269 UNS S35030 Tube

A269 UNS S35030 appears on specialty specs that explicitly call S35030. SHH STEEL can produce and supply that product and will confirm Table 2 digits against the ordered edition on the enquiry.

Not boiler tube or pipe unless those standards separately list the UNS.

Weldability

Specialty austenitics need filler matched after review. Mill autogenous A269 welds are solution-treated with the tube; shop welds are not.

SHH STEEL supplies the mill product and MTC with Mo, Cu, and Cb reported — and will not invent hardness from a sister grade.

Surface Finishes

Pickled and bright-annealed finishes cover most A269 UNS S35030 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.

Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 UNS S35030 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.

Inspection and Testing

Lot testing for A269 UNS S35030 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.

Packaging and Shipping

Export and domestic packs for A269 UNS S35030 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Stencil and tags typically carry ASTM A269, UNS S35030, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 UNS S35030 as seamless or welded tubing with Table 1 chemistry and EN 10204 3.1 documentation, stating Table 2 hardness only from the ordered edition.

If Al-Ti heat-resistant chemistry is named, we also quote A269 UNS S35045.

Supply Capability

SHH STEEL can produce and supply ASTM A269 UNS S35030 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.

Item SHH STEEL capability
Standard ASTM A269 / A269M
Grade UNS S35030
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated (confirm purchased edition (not verified in public -15 Table 2 excerpt)); pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument / hydraulic; often BA
12.7 / 15.9 / 19.1 / 25.4 / 31.8 1.0 / 1.2 / 1.5 / 2.0 / 2.5 Inch OD process and utility
38.1 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Utility and light process
88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Enquiry tip — Compare A269 UNS S35045 for Al-Ti heat-resistant chemistry.

FAQ

What is ASTM A269 UNS S35030 stainless steel tube used for?
A269 UNS S35030 is nominal-wall seamless or welded austenitic tubing for general corrosion-resisting and low- or high-temperature service where this UNS chemistry is specified. It is not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis and tests match.
Does ASTM A269 UNS S35030 include welded tube?
Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What hardness limit applies to A269 UNS S35030?
Where verified, Table 2 lists confirm purchased edition (not verified in public -15 Table 2 excerpt) after the required solution treatment. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 or A312 unless the purchase order adds them.
Is A269 UNS S35030 nominal wall or minimum wall?
Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall practice applies. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What size range can SHH STEEL produce for UNS S35030?
SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 UNS S35030, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Which tests are mandatory on A269 UNS S35030 tube?
Hardness to Table 2 where required; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What certificate does SHH STEEL provide for UNS S35030?
EN 10204 3.1 MTCs report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2 where verified, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, UNS S35030, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
How should I enquire for A269 UNS S35030 with SHH STEEL?
List ASTM A269, grade UNS S35030, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Add the service medium if alloy selection is still open. SHH STEEL can produce and supply to that enquiry. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Why is hardness listed as confirm purchased edition?
S35030 chemistry appears in the A269-24 store Table 1 excerpt, but the public -15 PDF Table 2 block available to the writer did not clearly list this UNS. Hardness must not be invented from a sister grade. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
S35030 vs S35045 under A269?
S35030 includes Mo, Cu, and Cb with a different Ni/Cr window; S35045 emphasizes Al and Ti with higher Ni/Cr and no Mo requirement in the public excerpt. Choose the UNS the drawing names. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.

Conclusion

ASTM A269 UNS S35030 belongs in the A269 nominal-wall tubing family when this chemistry is named for general-service lines. SHH STEEL can produce and supply seamless and welded A269 UNS S35030, heat-treated and tested per the ordered edition, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X