ASTM A269 TP347H Stainless Steel Tube
What is ASTM A269 TP347H Stainless Steel Tube
ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. TP347H is the controlled-carbon niobium-stabilized H-grade — ordered when elevated-temperature H-grade practice plus Nb stabilization are named on a general-service tubing enquiry. Jack-approved extra grade: this designation was not verified in the public A269 Table 1 excerpt used for the core queue — chemistry and heat-treatment digits below are cross-checked from A213/A312 sister text and labelled honestly. Name ASTM A269 and TP347H / UNS S34709 on the purchase order only when the purchaser’s edition lists this grade; otherwise order under A213 or A312.
SHH STEEL can produce and supply ASTM A269 TP347H stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates reporting chemistry and hardness against the ordered edition. Typical sizes ~6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Browse the A269/A269M hub. Keep the wall basis nominal.
If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP347H, SA213 TP347H, A312 TP347H and SA312 TP347H and match the product standard to the drawing.
Chemical Composition of A269 TP347H
Heat analysis under A269 Table 1 is mandatory for every TP347H heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.
Cross-checked from ASTM A213 TP347H / UNS S34709 sister text — not verified in the public A269 Table 1 excerpt.
Melting analysis (heat / ladle analysis) — Table 1
| Element | TP347H / UNS S34709 melting analysis |
|---|---|
| Carbon (C) | 0.04 – 0.10 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 17.0 – 19.0 |
| Nickel (Ni) | 9.0 – 13.0 |
| Niobium (Nb / Cb) | ≥ 8 × C, ≤ 1.10 |
Source: A213 TP347H sister chemistry (C 0.04–0.10%, Nb ≥8×C ≤1.10%). Jack-approved A269 extra — confirm the purchased A269 edition lists TP347H. Note A213 finish-route anneal temperatures differ from the common 1900 °F row.
Mechanical Properties of A269 TP347H
ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for TP347H. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.
| Property | TP347H requirement (A269 Table 2) |
|---|---|
| Hardness, max | 192 HBW / 200 HV or 90 HRB (A213 sister — A269 Table 2 not verified) |
| Tensile / yield / elongation | Not specified as an A269 acceptance table for this grade |
Source: ASTM A269/A269M Table 2 for TP347H (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.
Seamless and Welded Tube
Under A269, TP347H tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.
Seamless TP347H takes a lot-basis flaring test; welded TP347H takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 TP347H against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.
Dimensions and Tolerances
Order A269 TP347H by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.
| OD group (A269 Table 4) | Outside diameter tolerance | Wall thickness tolerance |
|---|---|---|
| Up to ½ in. [13 mm] | ±0.005 in. [0.13 mm] | ±15% |
| ½ to 1½ in. [13–38 mm], excl. | ±0.005 in. [0.13 mm] | ±10% |
| 1½ to 3½ in. [38–89 mm], excl. | ±0.010 in. [0.25 mm] | ±10% |
| 3½ to 5½ in. [89–140 mm], excl. | ±0.015 in. [0.38 mm] | ±10% |
| 5½ to 8 in. [140–203 mm], excl. | ±0.030 in. [0.76 mm] | ±10% |
Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for TP347H, say so on the enquiry so SHH STEEL does not build the wrong wall basis.
Equivalent Grades
TP347H / UNS S34709 is offered here as a Jack-approved A269 extra. Related forms appear under A213/A312/A240 by the same UNS with different wall bases and mechanical tables — confirm the product standard before substituting.
| Reference | Designation | Note |
|---|---|---|
| ASTM A269 | TP347H / UNS S34709 | Extra grade — confirm listing in purchased edition |
| UNS | S34709 | Chemistry identity |
| ASTM A213 / A312 | Same grade / UNS where listed | Sister product forms; not A269 tubing |
Compare A269 TP347 and A269 TP321H.
Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP347H, SA213 TP347H, A312 TP347H and SA312 TP347H. Confirm the product form before treating any of those pages as acceptance text for an A269 order.
Heat Treatment and Delivery Condition
All A269 TP347H tube is furnished solution heat-treated. Table 2 sets austenitizing at cold-worked ≥2000 °F [1090 °C] / hot-rolled ≥1925 °F [1050 °C] (A213 sister — A269 Table 2 not verified), followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”
| Item | TP347H (A269 Table 2) |
|---|---|
| Austenitizing temperature | cold-worked ≥2000 °F [1090 °C] / hot-rolled ≥1925 °F [1050 °C] (A213 sister — A269 Table 2 not verified) |
| Cooling | Water quench or rapid cool |
| Hardness after heat treatment, max | 192 HBW / 200 HV or 90 HRB (A213 sister — A269 Table 2 not verified) |
| Delivery condition | Solution heat-treated; pickled or bright-annealed by agreement |
Source: ASTM A269/A269M §6 and Table 2 for TP347H (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.
Corrosion Resistance
Controlled carbon with niobium stabilization targets elevated-temperature service where Nb (Cb) is preferred over titanium. A269 publishes no PREN — do not invent one. Compare TP347 when H-grade carbon is not required, or TP321H when Ti stabilization is named.
Applications of A269 TP347H Tube
A269 TP347H (extra) appears on heat-resistant tubing specs that name H-grade 347. SHH STEEL can produce and supply that product against the ordered edition and will redirect to A213 when Code boiler tube is actually required.
Not boiler tube or pipe unless those standards are ordered.
When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP347H, SA213 TP347H, A312 TP347H and SA312 TP347H instead of stretching an A269 tubing page into the wrong product form.
Weldability
Nb-stabilized H-grade austenitics need filler matched after review. Mill autogenous A269 welds are solution-treated with the tube; shop welds are not. Note the higher A213 finish-route anneal for cold-worked product.
SHH STEEL supplies the mill product and MTC with C and Nb reported.
Surface Finishes
Pickled and bright-annealed finishes cover most A269 TP347H orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.
Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP347H when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.
Inspection and Testing
Lot testing for A269 TP347H covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry (A213 sister cross-check; confirm A269 edition), solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.
Packaging and Shipping
Export and domestic packs for A269 TP347H use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.
Stencil and tags typically carry ASTM A269, TP347H, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.
Why Choose SHH STEEL
SHH STEEL can produce and supply ASTM A269 TP347H as solution-treated seamless or welded tubing with H-grade Nb-stabilized chemistry cross-checked from A213 sister text and EN 10204 3.1 documentation against the ordered edition.
If TP347 is enough, we quote that grade on the same size list.
Supply Capability
SHH STEEL can produce and supply ASTM A269 TP347H Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.
| Item | SHH STEEL capability |
|---|---|
| Standard | ASTM A269 / A269M |
| Grade | TP347H / UNS S34709 |
| Product form | Seamless and welded tube (no filler metal for welded), hot- or cold-finished |
| Delivery condition | Solution heat-treated (cold-worked ≥2000 °F [1090 °C] / hot-rolled ≥1925 °F [1050 °C] (A213 sister — A269 Table 2 not verified)); pickled or bright-annealed |
| Typical size band | ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement) |
| Testing | Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.
| OD (mm) | Typical nominal walls (mm) | Notes |
|---|---|---|
| 6 / 8 / 10 / 12 / 14 | 0.5 / 0.8 / 1.0 / 1.2 / 1.5 | Instrument / hydraulic; often BA |
| 12.7 / 15.9 / 19.1 / 25.4 / 31.8 | 1.0 / 1.2 / 1.5 / 2.0 / 2.5 | Inch OD process and utility |
| 38.1 / 48.3 / 60.3 / 76.1 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Utility and light process |
| 88.9 / 114.3 / 141.3 / 168.3 | 2.0 / 3.0 / 4.0 / 6.0 / 8.0 | Larger process tube; lock seamless vs welded |
Enquiry tip — Compare A269 TP347 and A269 TP321H.
FAQ
-
What is ASTM A269 TP347H stainless steel tube used for?
- When the purchaser’s A269 edition lists TP347H, it is nominal-wall seamless or welded austenitic tubing for general corrosion-resisting and low- or high-temperature service. It is not Code boiler tube (A213) and not pipe (A312). This pack is a Jack-approved extra — confirm the grade appears in the ordered A269 edition before treating these digits as acceptance text.
-
Does ASTM A269 TP347H include welded tube?
- Where A269 lists the grade, seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes once the edition and size are named. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What hardness limit applies to A269 TP347H?
- A269 Table 2 was not verified for this extra grade in the public excerpt. Sister A213 text lists 192 HBW / 200 HV or 90 HRB (A213 sister — A269 Table 2 not verified) after solution treatment — treat that as a cross-check only until the purchased A269 edition is confirmed. Do not invent tensile floors.
-
Is A269 TP347H nominal wall or minimum wall?
- A269 is nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Do not assume A213 minimum-wall practice applies to an A269 order. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What size range can SHH STEEL produce for TP347H?
- SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP347H, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation against the ordered edition.
-
Which tests are mandatory on A269 TP347H tube?
- Where A269 lists the grade: hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. Confirm Table 2 digits in the purchased edition for this extra grade. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What certificate does SHH STEEL provide for TP347H?
- EN 10204 3.1 MTCs report ladle chemistry, solution-treatment condition, hardness against the ordered edition, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, TP347H, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
How should I enquire for A269 TP347H with SHH STEEL?
- List ASTM A269 (edition if known), grade TP347H / UNS S34709, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. If the grade is not in your edition, ask for A213 or A312 instead. SHH STEEL can produce and supply to a clear enquiry.
-
Why is TP347H labelled an A269 extra?
- TP347H was not found in the public A269 Table 1 excerpt. Jack approved it as an extra; chemistry and finish-route anneal are cross-checked from A213 sister text and must be confirmed against the purchased A269 edition. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
TP347H vs TP347 under A269?
- TP347H requires C 0.04–0.10% with Nb ≥8×C; verified A269 TP347 allows C ≤0.08% with Nb 10×C min to 1.10% max. Choose the grade the drawing names. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Conclusion
ASTM A269 TP347H / UNS S34709 is offered as a Jack-approved extra for buyers who name this grade on an A269 enquiry. Confirm the purchased edition lists it; otherwise order the A213 or A312 sister. SHH STEEL can produce and supply seamless and welded A269 TP347H against the ordered edition with EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.