ASTM A269 TP XM-15 Stainless Steel Tube
What is ASTM A269 TP XM-15 Stainless Steel Tube
ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP XM-15 / UNS S38100 is a high-silicon, high-nickel austenitic in Table 1, with Si 1.50–2.50%, Ni 17.5–18.5%, Cr 17.0–19.0%, and C ≤0.08%. Buyers specify A269 TP XM-15 when the material list wants elevated silicon for oxidizing acid or related specialty service that commodity 18-8 does not target. Name ASTM A269 on the purchase order so nominal-wall rules and hardness apply to tubing.
SHH STEEL can produce and supply ASTM A269 TP XM-15 stainless steel tube as seamless and welded product, solution annealed, with EN 10204 3.1 certificates. Typical sizes ~6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Browse the A269/A269M hub and compare high-Si A269 UNS S30600 when even higher silicon is specified. Keep the wall basis nominal.
If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP XM-15 and SA213 TP XM-15 and match the product standard to the drawing.
Chemical Composition of A269 TP XM-15
Heat analysis under A269 Table 1 is mandatory for every TP XM-15 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.
Public A269 Table 1 excerpts for TP XM-15 / UNS S38100 (ASTM abstract + tubingchina A269 PDF). Elevated silicon with high nickel defines this grade.
Melting analysis (heat / ladle analysis) — Table 1
| Element | TP XM-15 / UNS S38100 melting analysis |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.030 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | 1.50 – 2.50 |
| Chromium (Cr) | 17.0 – 19.0 |
| Nickel (Ni) | 17.5 – 18.5 |
| Molybdenum (Mo) | … (no requirement) |
| Nitrogen (N) | … (no requirement) |
Source: ASTM A269/A269M Table 1 for TP XM-15 / UNS S38100. Silicon 1.50–2.50% is the signature versus commodity 304/316 (Si ≤1.00%). Nickel 17.5–18.5% is also high. Phosphorus is tighter at ≤0.030%. No Mo requirement.
Mechanical Properties of A269 TP XM-15
ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for TP XM-15. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.
| Property | TP XM-15 requirement (A269 Table 2) |
|---|---|
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Tensile / yield / elongation | Not specified as an A269 acceptance table for this grade |
Source: ASTM A269/A269M Table 2 for TP XM-15 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.
Seamless and Welded Tube
Under A269, TP XM-15 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.
Seamless TP XM-15 takes a lot-basis flaring test; welded TP XM-15 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 TP XM-15 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.
Dimensions and Tolerances
Order A269 TP XM-15 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.
| OD group (A269 Table 4) | Outside diameter tolerance | Wall thickness tolerance |
|---|---|---|
| Up to ½ in. [13 mm] | ±0.005 in. [0.13 mm] | ±15% |
| ½ to 1½ in. [13–38 mm], excl. | ±0.005 in. [0.13 mm] | ±10% |
| 1½ to 3½ in. [38–89 mm], excl. | ±0.010 in. [0.25 mm] | ±10% |
| 3½ to 5½ in. [89–140 mm], excl. | ±0.015 in. [0.38 mm] | ±10% |
| 5½ to 8 in. [140–203 mm], excl. | ±0.030 in. [0.76 mm] | ±10% |
Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for TP XM-15, say so on the enquiry so SHH STEEL does not build the wrong wall basis.
Equivalent Grades
TP XM-15 / UNS S38100 is the ASTM tubing designation for this high-Si austenitic. Related forms may appear under other ASTM standards by the same UNS.
| Reference | Designation | Note |
|---|---|---|
| ASTM A269 | TP XM-15 / UNS S38100 | This product standard |
| UNS | S38100 | Chemistry identity |
| ASTM A269 sister | UNS S30600 | Higher Si (~3.7–4.3%) acid-service austenitic |
Step to A269 UNS S30600 when the list wants the higher-silicon S30600 chemistry.
Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP XM-15 and SA213 TP XM-15. Confirm the product form before treating any of those pages as acceptance text for an A269 order.
Heat Treatment and Delivery Condition
All A269 TP XM-15 tube is furnished solution heat-treated. Table 2 sets austenitizing at ≥1900 °F [1040 °C], followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”
| Item | TP XM-15 (A269 Table 2) |
|---|---|
| Austenitizing temperature | ≥1900 °F [1040 °C] |
| Cooling | Water quench or rapid cool |
| Hardness after heat treatment, max | 192 HBW / 200 HV or 90 HRB |
| Delivery condition | Solution heat-treated; pickled or bright-annealed by agreement |
Source: ASTM A269/A269M §6 and Table 2 for TP XM-15 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.
Corrosion Resistance
Elevated silicon is aimed at certain oxidizing acid and specialty environments where Si-bearing austenitics outperform commodity 304/316 — medium-specific, not a universal upgrade. There is no molybdenum for severe chlorides. A269 publishes no PREN for S38100 — do not invent one.
Match the medium to the list that named XM-15; for concentrated nitric/related high-Si duties, also compare S30600 under A269.
Applications of A269 TP XM-15 Tube
A269 TP XM-15 appears on specialty chemical and process tubing specs that explicitly call S38100 / XM-15 for high-silicon austenitic service. SHH STEEL can produce and supply that product and will redirect when S30600 or a Mo grade better matches the medium.
It is not boiler tube (A213) or pipe (A312) unless those standards separately list the UNS.
When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP XM-15 and SA213 TP XM-15 instead of stretching an A269 tubing page into the wrong product form.
Weldability
High-silicon austenitics need filler and procedure matched to the alloy — do not assume generic 308 filler without review. Mill autogenous A269 welds are solution-treated with the tube; shop welds are not.
SHH STEEL supplies the mill product and MTC with silicon reported in the 1.50–2.50% band.
Surface Finishes
Pickled and bright-annealed finishes cover most A269 TP XM-15 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.
Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP XM-15 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.
Inspection and Testing
Lot testing for A269 TP XM-15 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including silicon and nickel, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.
Packaging and Shipping
Export and domestic packs for A269 TP XM-15 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.
Stencil and tags typically carry ASTM A269, TP XM-15 / S38100, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.
Why Choose SHH STEEL
SHH STEEL can produce and supply ASTM A269 TP XM-15 as solution-treated seamless or welded tubing with Table 1 high-Si chemistry, Table 2 hardness, and EN 10204 3.1 documentation. We will not relabel 304 as XM-15.
If higher silicon is required, we point to A269 UNS S30600.
Supply Capability
SHH STEEL can produce and supply ASTM A269 TP XM-15 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.
| Item | SHH STEEL capability |
|---|---|
| Standard | ASTM A269 / A269M |
| Grade | TP XM-15 / UNS S38100 |
| Product form | Seamless and welded tube (no filler metal for welded), hot- or cold-finished |
| Delivery condition | Solution heat-treated (≥1900 °F [1040 °C]); pickled or bright-annealed |
| Typical size band | ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement) |
| Testing | Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.
| OD (mm) | Typical nominal walls (mm) | Notes |
|---|---|---|
| 6 / 8 / 10 / 12 / 14 | 0.5 / 0.8 / 1.0 / 1.2 / 1.5 | Instrument / hydraulic; often BA |
| 12.7 / 15.9 / 19.1 / 25.4 / 31.8 | 1.0 / 1.2 / 1.5 / 2.0 / 2.5 | Inch OD process and utility |
| 38.1 / 48.3 / 60.3 / 76.1 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Utility and light process |
| 88.9 / 114.3 / 141.3 / 168.3 | 2.0 / 3.0 / 4.0 / 6.0 / 8.0 | Larger process tube; lock seamless vs welded |
Parallel quotes against A269 UNS S30600 keep silicon level visible.
FAQ
-
What is ASTM A269 TP XM-15 used for?
- A269 TP XM-15 / UNS S38100 is nominal-wall seamless or welded austenitic tubing for general corrosion-resisting and low- or high-temperature service where this chemistry is specified. It is not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis and tests match.
-
Does A269 TP XM-15 include welded tube?
- Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What hardness limit applies to A269 TP XM-15?
- Table 2 caps TP XM-15 at 192 HBW / 200 HV or 90 HRB after the required solution heat treatment. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 or A312 unless the purchase order adds them.
-
Is A269 TP XM-15 nominal wall or minimum wall?
- Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall practice applies. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What size range can SHH STEEL produce for TP XM-15?
- SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP XM-15, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Which tests are mandatory on A269 TP XM-15?
- Hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What certificate does SHH STEEL provide?
- EN 10204 3.1 MTCs report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, TP XM-15 / S38100, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
How should I enquire for A269 TP XM-15?
- List ASTM A269, grade TP XM-15 / UNS S38100, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Why is silicon higher than in TP304?
- Table 1 sets Si 1.50–2.50% for TP XM-15 versus ≤1.00% for TP304 — that elevated silicon is the grade’s defining feature for specialty oxidizing-acid related service. Nickel is also higher (17.5–18.5%). Do not treat XM-15 as a polish or finish name on 304.
-
XM-15 vs UNS S30600 under A269?
- S30600 carries still higher silicon (about 3.7–4.3%) with different Ni/Cr and very low carbon. Choose based on the UNS the drawing names. Both are specialty high-Si austenitics, not interchangeable stamps. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Is XM-15 a molybdenum grade?
- No. Table 1 shows no Mo requirement for TP XM-15. For chloride pitting that needs Mo, open TP316L or a 6Mo A269 grade. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Conclusion
ASTM A269 TP XM-15 / UNS S38100 is the high-silicon austenitic inside the A269 nominal-wall tubing family when S38100 is named for specialty Si-bearing service. SHH STEEL can produce and supply seamless and welded A269 TP XM-15, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.