ASTM A269 TP317 Stainless Steel Tube
What is ASTM A269 TP317 Stainless Steel Tube
ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP317 is the higher-molybdenum austenitic in that Table 1 family, listed as UNS S31700, with carbon ≤0.08%, chromium 18.0–20.0%, nickel 11.0–15.0%, and molybdenum 3.0–4.0%. Buyers step from TP316 to A269 TP317 when the material list wants more Mo for tougher chloride or chemical service without jumping yet to a 6Mo super-austenitic. The shop name “317 tube” still needs ASTM A269 on the purchase order so nominal-wall rules, hardness, flaring or flange tests, and marking apply to tubing — not to an A213 boiler-tube or A312 pipe text.
SHH STEEL can produce and supply ASTM A269 TP317 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 mill test certificates reporting Table 1 ladle chemistry and Table 2 hardness. Typical sizes run about 6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare sisters on the A269/A269M hub alongside A269 TP316L, A269 TP316, and copper-bearing A269 UNS S31730. Keep the enquiry on a nominal-wall basis.
If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP317, SA213 TP317, A312 TP317 and SA312 TP317 and match the product standard to the drawing.
Chemical Composition of A269 TP317
Table 1 melting analysis is mandatory for every TP317 heat under A269. Product analysis applies when ordered through A1016/A1016M and A480 Table A1.1. SHH STEEL reports measured ladle (and product, when ordered) values without advertising unpublished tighter catalogue windows as if they were ASTM limits.
Public A269 Table 1 excerpts for TP317 / UNS S31700 are reproduced below (ASTM abstract cross-checked with the tubingchina A269 PDF). Values are maxima unless a range is shown. Confirm the purchased A269/A269M edition before treating any secondary catalogue as the acceptance text.
Melting analysis (heat / ladle analysis) — Table 1
| Element | TP317 (UNS S31700) melting analysis |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 18.0 – 20.0 |
| Nickel (Ni) | 11.0 – 15.0 |
| Molybdenum (Mo) | 3.0 – 4.0 |
| Nitrogen (N) | … (no requirement) |
Source: ASTM A269/A269M Table 1 for TP317 / UNS S31700 (public excerpts). Molybdenum at 3.0–4.0% is the deliberate step above TP316’s 2–3% band; chromium sits in an 18–20% window rather than 316’s 16–18%. Carbon ≤0.08% is the non-L ceiling, so as-welded sensitization risk sits above a low-carbon sister when one is ordered. When copper-bearing high-N chemistry is required instead, open A269 UNS S31730 rather than stretching TP317.
Mechanical Properties of A269 TP317
A269 does not publish a tensile/yield/elongation acceptance table for TP317. Lot acceptance uses Table 2 hardness, flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not import A213 tensile floors onto an A269 TP317 certificate unless the purchase order adds them as project extras.
| Property | TP317 requirement (A269 Table 2) |
|---|---|
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Tensile / yield / elongation | Not specified as an A269 acceptance table for this grade |
Source: ASTM A269/A269M Table 2 for TP317 / UNS S31700 (public PDF excerpt). Hardness ceiling matches the familiar annealed austenitic band used for TP316 under the same table; confirm thin-wall superficial Rockwell alternatives in the purchased edition’s hardness clause before writing them into a quality plan.
Seamless and Welded Tube
TP317 under A269 may be seamless or welded, hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded as the process route on the product.
Seamless TP317 is flare-tested on a lot basis; welded TP317 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydro or NDE test per length. SHH STEEL can produce and supply both seamless and welded A269 TP317 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.
Dimensions and Tolerances
Order A269 TP317 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M, while thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.
| OD group (A269 Table 4) | Outside diameter tolerance | Wall thickness tolerance |
|---|---|---|
| Up to ½ in. [13 mm] | ±0.005 in. [0.13 mm] | ±15% |
| ½ to 1½ in. [13–38 mm], excl. | ±0.005 in. [0.13 mm] | ±10% |
| 1½ to 3½ in. [38–89 mm], excl. | ±0.010 in. [0.25 mm] | ±10% |
| 3½ to 5½ in. [89–140 mm], excl. | ±0.015 in. [0.38 mm] | ±10% |
| 5½ to 8 in. [140–203 mm], excl. | ±0.030 in. [0.76 mm] | ±10% |
Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language, say so on the enquiry so SHH STEEL does not build the wrong wall basis for a tubing order.
Equivalent Grades
TP317 / UNS S31700 is the ASTM tubing designation for the 3–4% Mo austenitic above the TP316 Mo band. Related product forms may appear under A213 and A312 where those standards list TP317; plate cousins sit under A240 Type 317 where listed. European Mo-rich austenitic designations are commercial cousins only after a chemistry and product-form check against the purchased A269 edition.
| Reference | Designation | Note |
|---|---|---|
| ASTM A269 | TP317 / UNS S31700 | This product standard (nominal-wall tube) |
| UNS | S31700 | Chemistry identity |
| ASTM A213 / A312 | TP317 (where listed) | Different product form / mechanical tables |
| ASTM A240 | Type 317 / S31700 (where listed) | Plate / sheet cousin |
Inside A269, compare A269 TP316 when 2–3% Mo is enough, A269 UNS S31730 when Cu + high N is specified, or a 6Mo grade when seawater-level chlorides demand it.
Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP317, SA213 TP317, A312 TP317 and SA312 TP317. Confirm the product form before treating any of those pages as acceptance text for an A269 order.
Heat Treatment and Delivery Condition
All A269 TP317 tube is furnished solution heat-treated. Table 2 requires a minimum austenitizing temperature of 1900 °F [1040 °C], followed by water quench or other rapid cooling, and seamless tube may be quenched immediately after hot forming while still at or above that temperature. Ordered final anneals below 1900 °F, when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”
| Item | TP317 (A269 Table 2) |
|---|---|
| Austenitizing temperature, min | 1900 °F [1040 °C] |
| Cooling | Water quench or rapid cool |
| Hardness after heat treatment, max | 192 HBW / 200 HV or 90 HRB |
| Delivery condition | Solution heat-treated; pickled or bright-annealed by agreement |
Source: ASTM A269/A269M §6 and Table 2 for TP317. Bright-annealed or pickled surfaces are finish choices on top of the mandatory solution treatment. SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.
Corrosion Resistance
Molybdenum at 3–4% is why TP317 sits above TP316 for many chloride and chemical duties that still do not justify a 6Mo alloy. Chromium at 18–20% supports the passive film; the extra Mo helps in localised-attack regimes where 2–3% Mo is marginal. Carbon up to 0.08% means HAZ sensitization remains a design input for as-welded corrosive fabrications — if low carbon is mandatory, ask whether a low-carbon 317-family listing is on the purchase order or step to another L-grade Mo tube under A269.
A269 publishes no PREN or CPT table for S31700 — do not invent one from marketing sheets. Match the medium honestly: many chemical and chloride-bearing utilities suit TP317; seawater splash zones and aggressive chlorides often need A269 UNS S31254 or similar.
Applications of A269 TP317 Tube
A269 TP317 appears on chemical process transfer tubing, chloride-aware instrument lines that outgrew TP316, pulp and paper related utilities where Mo-rich austenitic is specified, and heat-transfer coils written to A269 rather than A213 when 3–4% Mo is on the material list. Cold-finished bright-annealed tube dominates skid work; pickled welded tube covers larger utility runs.
It is the wrong first choice for Code boiler tube (use A213), for pipe headers (use A312), and for seawater-level chlorides that need 6Mo. SHH STEEL can produce and supply A269 TP317 across the general-service band above and will say when S31730 or a 6Mo grade is the safer metallurgical fit.
When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP317, SA213 TP317, A312 TP317 and SA312 TP317 instead of stretching an A269 tubing page into the wrong product form.
Weldability
TP317 welds with the usual austenitic practices — GTAW and GMAW with matching or over-alloyed Mo-bearing fillers when filler is used on fabrication joints. Autogenous A269 welded tube already carries a mill seam that was cold-worked and solution-treated with the tube; cut-length shop welds are a separate fabrication step outside that mill anneal. Standard carbon means as-welded HAZ sensitization remains a live concern in corrosive service without re-annealing.
Filler selection, purge quality, and interpass control stay with the fabricator. SHH STEEL’s A269 scope is the mill tube, chemistry including the 3–4% Mo range, hardness, and the seamless or welded route named on the purchase order.
Surface Finishes
Pickled and bright-annealed finishes cover most A269 TP317 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough.
Write any maximum Ra or scrubbed-ID note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP317 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.
Inspection and Testing
Lot testing for A269 TP317 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including molybdenum, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection are available when named on the order, and we do not skip mandatory tests to shorten lead time.
Packaging and Shipping
Export and domestic packs for A269 TP317 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.
Stencil and tags typically carry ASTM A269, TP317 / S31700, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.
Why Choose SHH STEEL
SHH STEEL can produce and supply ASTM A269 TP317 as solution-treated seamless or welded tubing with Table 1 chemistry — including the 3.0–4.0% molybdenum range — Table 2 hardness, and EN 10204 3.1 documentation. We keep A269 distinct from A213 and A312 on the MTC, we state seamless versus welded honestly, and we will not paste A213 tensile floors onto an A269 shipment to make the certificate look busier.
On grade selection we stay practical. If 2–3% Mo is enough, we point to A269 TP316 / A269 TP316L; if chlorides outgrow 3–4% Mo, we point to a 6Mo A269 grade rather than stretching TP317 past its envelope.
Supply Capability
SHH STEEL can produce and supply ASTM A269 TP317 stainless steel tube against the edition, process route, and finish named on your enquiry. The capability table and Stock / Available sizes enquiry map below are what buyers use to frame a first-pass size list for higher-Mo process duty.
| Item | SHH STEEL capability for TP317 |
|---|---|
| Standard | ASTM A269 / A269M |
| Grade | TP317 / UNS S31700 |
| Product form | Seamless and welded tube (no filler metal for welded), hot- or cold-finished |
| Delivery condition | Solution heat-treated ≥1900 °F [1040 °C]; pickled or bright-annealed |
| Typical size band | ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement) |
| Testing | Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range for A269 TP317 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats and finishing slots; send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production or partner stock.
| OD (mm) | Typical nominal walls (mm) | Notes |
|---|---|---|
| 6 / 8 / 10 / 12 / 14 | 0.5 / 0.8 / 1.0 / 1.2 / 1.5 | Instrument / hydraulic; often BA |
| 12.7 / 15.9 / 19.1 / 25.4 / 31.8 | 1.0 / 1.2 / 1.5 / 2.0 / 2.5 | Inch OD process and utility |
| 38.1 / 48.3 / 60.3 / 76.1 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Higher-Mo process vs TP316 |
| 88.9 / 114.3 / 141.3 / 168.3 | 2.0 / 3.0 / 4.0 / 6.0 / 8.0 | Larger process tube; lock seamless vs welded |
Parallel quotes against A269 TP316 and A269 UNS S31254 on the same size list keep Mo cost and corrosion margin visible in one enquiry.
FAQ
-
What is ASTM A269 TP317 stainless steel tube used for?
- A269 TP317 is the higher-molybdenum nominal-wall tubing grade for chemical process transfer, chloride-aware instrumentation that outgrew TP316, and related general-service duties where 3–4% Mo is on the material list. It covers seamless and welded tubing under ASTM A269 — not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis, hardness, and tests match the tubing product standard.
-
TP316 vs TP317 under A269 — which should I buy?
- Buy TP316 when 2.00–3.00% molybdenum is enough for the chloride or chemical duty. Buy TP317 when the material list wants 3.0–4.0% Mo and a higher chromium band (18–20% vs 16–18%). They are separate A269 grades with different Table 1 chemistry; do not treat “316/317 tube” as one interchangeable stamp on the MTC.
-
Does ASTM A269 TP317 include welded tube?
- Yes. A269 covers both seamless and welded TP317. Welded tube is made without filler metal, cold-worked, and solution-treated with the tube, then flange- and reverse-flattening-tested on the seam. Site titles omit the word “Welded” by house style, but the purchase order and MTC still state seamless or welded. SHH STEEL can produce and supply both routes.
-
What hardness does A269 require for TP317?
- Table 2 sets a maximum of 192 HBW / 200 HV or 90 HRB after solution treatment at ≥1900 °F [1040 °C]. A269 does not publish a tensile, yield, or elongation acceptance table for TP317, so do not invent 75/30 ksi-style floors from A213 unless the purchase order adds them as extras for the project.
-
Is A269 TP317 a nominal-wall or minimum-wall standard?
- A269 is written on a nominal-wall-thickness basis for general-service tubing. State OD × nominal wall on the enquiry unless you agree a different wall basis with the mill in writing. Table 4 then governs outside-diameter, wall, and cut-length tolerances. Do not assume A213 minimum-wall boiler-tube practice applies to an A269 TP317 order.
-
What size range can SHH STEEL supply for A269 TP317?
- SHH STEEL can produce and supply A269 TP317 in a typical band of about 6–168 mm OD with 0.5–8.0 mm nominal wall, seamless or welded, pickled or bright-annealed, with EN 10204 3.1 mill test certificates. Larger or heavier sizes are quoted by agreement against mill capability — send the OD × wall list for a firm near-term availability answer.
-
When should I choose UNS S31730 or 6Mo instead of TP317?
- Choose UNS S31730 when the material list wants copper (4–5%) plus high nitrogen with a 3–4% Mo austenitic. Choose a 6Mo A269 grade such as UNS S31254 when seawater or aggressive chlorides outgrow the 3–4% Mo band. TP317 remains the straight higher-Mo step above TP316 for many chemical duties under A269.
-
Hydrostatic or NDE testing for A269 TP317?
- Each tube must receive either a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks one method. NDE-tested lengths are marked “NDE” and the certificate states that choice. Hardness and flaring or flange tests remain separate lot requirements beside the hydro/NDE decision.
-
What documents come with SHH STEEL A269 TP317?
- EN 10204 3.1 mill test certificates report ladle chemistry against Table 1 including the 3–4% molybdenum range, solution-treatment condition, hardness against Table 2, and the hydrostatic or NDE statement. Third-party inspection and PMI can be added on the order. Stencil carries ASTM A269, TP317 / S31700, size, heat, and seamless or welded identity.
-
Does TP317 have a low-carbon L grade under A269?
- Standard TP317 in the public A269 Table 1 excerpts is the C ≤0.08% listing (UNS S31700). Low-carbon 317-family chemistries appear as separate grades or supplier listings — for example TP317L is among the extra grades Jack approved for this series but was not found in the public A269 Table 1 excerpt, so confirm against the purchased edition before ordering. Do not assume TP317 automatically means L-grade carbon.
-
How do I enquire for A269 TP317 with SHH STEEL?
- Send ASTM A269, grade TP317 / UNS S31700, seamless or welded preference, OD × nominal-wall list and lengths or coil, finish, and any hydro/NDE lock. Add a short note on the service medium if selection between TP316, TP317, S31730, and 6Mo grades is still open. SHH STEEL can produce and supply to that enquiry.
Conclusion
ASTM A269 TP317 / UNS S31700 is the higher-molybdenum austenitic inside the A269 nominal-wall tubing family when chemical or chloride service needs 3–4% Mo above the TP316 band. SHH STEEL can produce and supply seamless and welded A269 TP317 tube, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send your OD × nominal-wall list and process route. Contact admin@steelspecs.com with the size list and medium notes for a production-backed offer.