SHH STEEL offers NK Rules-compliant NK AH32/DH32/EH36 steel plates. Nippon Kaiji Kyokai Rules for Steel Ships cover survey, construction, materials, and welding for safe shipbuilding. Certified quality, competitive prices, customizable. Trust SHH STEEL!

Close view of NK KF550 hull structural steel plate, ClassNK (NK) rules

NK KF550 Shipbuilding Steel Plate

NK KF550 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 550 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KE550 marine steel plate per ClassNK (NK) rules at SHH STEEL warehouse

NK KE550 Shipbuilding Steel Plate

NK KE550 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 550 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KD550 shipbuilding steel plate to ClassNK (NK) rules, stacked hull plates

NK KD550 Shipbuilding Steel Plate

NK KD550 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 550 N/mm², Charpy −20 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KA500 shipbuilding steel plate to ClassNK (NK) rules, stacked hull plates

NK KA500 Shipbuilding Steel Plate

NK KA500 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 500 N/mm², Charpy 0 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
Close view of NK KF460 hull structural steel plate, ClassNK (NK) rules

NK KF460 Shipbuilding Steel Plate

NK KF460 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 460 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KE460 marine steel plate per ClassNK (NK) rules at SHH STEEL warehouse

NK KE460 Shipbuilding Steel Plate

NK KE460 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 460 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
Close view of NK KD460 hull structural steel plate, ClassNK (NK) rules

NK KD460 Shipbuilding Steel Plate

NK KD460 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 460 N/mm², Charpy −20 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KA460 shipbuilding steel plate to ClassNK (NK) rules, stacked hull plates

NK KA460 Shipbuilding Steel Plate

NK KA460 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 460 N/mm², Charpy 0 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
Close view of NK KF420 hull structural steel plate, ClassNK (NK) rules

NK KF420 Shipbuilding Steel Plate

NK KF420 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 420 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KE420 marine steel plate per ClassNK (NK) rules at SHH STEEL warehouse

NK KE420 Shipbuilding Steel Plate

NK KE420 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 420 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
NK KD420 shipbuilding steel plate to ClassNK (NK) rules, stacked hull plates

NK KD420 Shipbuilding Steel Plate

NK KD420 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 420 N/mm², Charpy −20 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More
Close view of NK KA420 hull structural steel plate, ClassNK (NK) rules

NK KA420 Shipbuilding Steel Plate

NK KA420 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 420 N/mm², Charpy 0 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
View More

Shipbuilding Steel Plates

SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.

Shipbuilding Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X