Close view of NK D36 DH36 hull structural steel plate, ClassNK (NK) rules

NK D36/DH36 Shipbuilding Steel Plate

NK D36/DH36 (KD36) high-tensile hull structural steel plate to ClassNK Part K: ReH 355 N/mm², Rm 490–630 N/mm², Charpy −20 °C. From NK-approved Chinese mills via SHH STEEL, from stock or mill-rolled, with cutting, dual-class and 3.2 inspection.
Keywords
NK D36/DH36 steel plate, KD36 steel plate, ClassNK KD36, NK DH36 shipbuilding plate, NK D36 marine steel, Nippon Kaiji Kyokai DH36, high tensile hull steel
Equivalent Grades:
DNV VL D36; LR DH36; BV DH36; CCS D36/DH36; KR RD36; ABS DH36; RINA DH36; ASTM A131 DH36; GB 712 DH36
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

NK D36/DH36 (KD36) shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

NK D36/DH36 moves the 36 level down to −20 °C. ClassNK writes it KD36, and the trade uses both D36 and DH36. Level 36 is the workhorse of Japanese shipbuilding; most hull girder plating on modern NK-classed bulkers and tankers is a 36 grade. It gives ReH ≥ 355 N/mm², Rm 490–630 N/mm² and A ≥ 21 %. The title uses the dual trade name (D36/DH36) because Japanese and Chinese buyers search for both forms, but the plate itself is stamped KD36.

Equivalent grades: ASTM A131 Grade DH36 · ABS DH36 · DNV NV D36 · LR DH36 · BV DH36 · CCS D36 / DH36 · KR RD36 · RINA DH36 · GB 712 Grade DH36.

In the ClassNK series the letter sets the test temperature (KA 0 °C, KD −20 °C, KE −40 °C, KF −60 °C) and the number sets the yield (32 → 315, 36 → 355, 40 → 390 N/mm²). KD36 is the D letter at level 36. Typical NK uses: thicker deck, bottom and sheer strakes and hatch side coamings needing −20 °C.

SHH STEEL sources KD36 from Chinese mills that hold NK approval for high-tensile hull steel, with the NK survey at the mill. Stock is held in the common 36-level sizes and other sizes are rolled to order.

KD36 (D36/DH36) key data

ItemNK D36/DH36 / KD36
Governing rulesClassNK Rules for the Survey and Construction of Steel Ships, Part K; IACS UR W11 high-tensile grade DH36 (Part K numbering UNCERTAIN)
NamesNK designation KD36; trade dual D36/DH36; IACS DH36
StrengthReH ≥ 355 N/mm², Rm 490–630 N/mm², A ≥ 21 %
Charpy V−20 °C
Steelmakingkilled, fine-grain treated (Al, Nb, V or Ti)
Delivery conditionAR / CR / N / TM as permitted by thickness and grain refiner (QT where approved)
TMCP carbon equivalentCeq ≤ 0.38 % (t ≤ 50 mm), ≤ 0.40 % (50–100 mm), indicative UR W11 practice — confirm at mill approval
Thicknessup to 100 mm (UR W11 scope); beyond by agreement with ClassNK
ToleranceIACS UR W13 as applied by ClassNK (UNCERTAIN class)
DocumentsNK-endorsed mill certificate; EN 10204 3.1/3.2

Commonly traded KD36 runs 8–60 mm thick in 2000–3000 mm widths. Heavier plate depends on the mill’s NK approval range for the delivery condition.

KD36 chemical composition — heat and product analysis

ElementHeat (ladle) analysis, %Product (check) analysis, %Remark
C0.18 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateAH/DH/EH column
Mn0.90–1.60 (AH ≤12.5 mm may be 0.70 min.)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Si0.10–0.50numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
P0.035 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
S0.035 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Al (acid-soluble)0.015 min. acid-soluble (or total Al per UR W11 fine-grain practice)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificategrain refiner
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificategrain refiner / strengthening
V0.05–0.10 when used singlynumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ti0.02 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cu0.35 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ni0.40 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Mo0.08 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
N—numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateno cap in A/D/E column
Nb+V+Ti0.12 max. (combined, when used together)not applicable (calculated from heat analysis)combined microalloy cap
Ceq (TM plate)0.38 / 0.40 max. (calculated)not applicable (calculated from heat analysis)for t ≤ 50 / 50–100 mm

Product (check) analysis column: ClassNK Part K specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

The ladle values follow IACS UR W11 for high-tensile hull steel, which ClassNK adopts in Part K (not checked against a Part K edition — UNCERTAIN). Many mills melt KD and KE grades from the same heat, then sort plates by Charpy results. The certificate must show the grade actually certified. For TMCP plate, ask for Ceq (and Pcm if your welding procedure uses it) on the certificate. Product analysis tolerances are agreed case by case.

KD36 tensile requirements

PropertyValue
ReH355 N/mm² min.
Rm490–630 N/mm²
A (5.65√S0)21 % min.
Charpy temperature−20 °C

Flat 200 mm test pieces: minimum elongation by thickness

t (mm)≤55–1010–1515–2020–2525–3030–4040–50
A200 min. %1315161718192021

KA36, KD36, KE36 and KF36 share these values. Only the Charpy temperature and, for KF, the chemistry differ.

KD36: Charpy at −20 °C and delivery condition

ThicknessAvg. long. (J)Avg. trans. (J)
≤ 50 mm3424
50–70 mm4127
70–100 mm5034

Required energy rises with thickness. A 70 mm KD36 plate must reach 50 J longitudinal at −20 °C, against 34 J for plate up to 50 mm. The delivery condition (AR, CR, N or TM) affects batch size and test frequency. Most Chinese mills now supply TM plate for this grade, which also helps Ceq.

Thickness tolerance and surface quality

Minus tolerance follows IACS UR W13 as ClassNK applies it. Plus tolerance, flatness and dimensions follow the agreed standard (JIS G3193, EN 10029 or GB/T 709). Weight-optimised high-tensile designs leave less margin, so check thickness at several points on receipt.

KD36 stock and lead time

Thickness (mm)Width (mm)Length (mm)ConditionApprox. qty
61800 / 20006000–12000AR / N / TM100+ t
820006000–12000AR / N / TM150+ t
102000 / 22006000–12000AR / N / TM200+ t
122000 / 25006000–12000AR / N / TM200+ t
162200 / 25006000–12000AR / N / TM150+ t
2025006000–12000AR / N / TM120+ t
2525006000–12000AR / N / TM100+ t
302200 / 25006000–12000AR / N / TM80+ t
4022006000–12000AR / N / TM50+ t
5022006000–12000AR / N / TM30+ t

Stock quantities change every week, so confirm before you book. Plates are sold as KD36 with the NK stamp and endorsed certificate. Sizes not in stock are rolled in about 4–6 weeks including survey.

Packing: bundled by size with steel strapping, painted with grade and heat number, shipped in containers (≤11.8 m) or break bulk.

NK D36/DH36 (KD36) compared with other societies

Society / standardGradeNote
ClassNKNK D36/DH36 / KD36this page
DNVDNV VL D36
LRLR DH36
BVBV DH36
CCSCCS D36 / DH36
KRKR RD36
ABSABS DH36
RINARINA DH36 (designation per RINA rules)no product page yet
ASTM A131ASTM A131/A131M Grade DH36product standard only
GB 712GB 712 Grade DH36product standard only

All share the UR W11 DH36 requirements. Each society accepts only its own stamp, so dual certification must be booked before the plates are tested.

Choosing KD36 within the ClassNK high-tensile series

Read across for toughness (KA36 → KD36 → KE36 → KF36) and down for strength (KD32 → KD36 → KD40). ClassNK’s material-grade table fixes the letter from member category and thickness. The designer fixes the number from the scantlings. Substituting a higher letter of the same number is normally accepted; a lower letter is not.

Above 390 N/mm², ClassNK’s extra-high-strength grades start at KA420 (IACS UR W16). See NK Steel Plates for the full series.

Using KD36 in the yard

Uses: thicker deck, bottom and sheer strakes and hatch side coamings needing −20 °C. Welding: use high-tensile consumables approved by ClassNK for −20 °C toughness (grade 3Y or higher, typical — confirm in the WPS). Preheat and heat input come from the NK-approved procedure and the certificate Ceq. Large-heat-input electrogas or one-side SAW on thick KD36 needs a procedure qualified for that heat input.

Forming: TMCP plate gets part of its strength from controlled rolling. Keep line heating within the mill’s temperature limits, typically below about 650 °C for water cooling (UNCERTAIN, mill-specific).

NK survey, certificates and receiving checks

The certificate lists ladle chemistry including microalloys, Ceq for TM plate, tensile results, Charpy results at −20 °C, delivery condition and plate numbers, with the NK endorsement. We can add EN 10204 3.2 third-party witness, UT to EN 10160 or ASTM A578, Z-direction testing, and dual class with ABS, DNV, LR or BV.

On receipt: check the stamp reads KD36, Charpy results are at −20 °C for the right thickness band, and the NK endorsement is present.

Ordering errors seen with KD36

  • Writing only “AH36” or “A36” without stating ClassNK, so the plate arrives with another society’s stamp
  • Omitting the letter, so toughness is undefined
  • Accepting mild-steel KA–KE certificates against a high-tensile order
  • No Ceq on the certificate for TM plate
  • Substituting KA36 without approval
  • Charpy band for the delivered thickness not checked

Buying KD36 from China: concerns and answers

ConcernAnswer
Is the NK stamp genuine?Only mills with ClassNK approval for KD36; certificate and stamp traceable to the heat; third-party witness on request
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed ordersseveral sizes and NK grades in one container
Delivery visibilityweekly photos from rolling to loading
Ready-to-fit partscutting, bevelling and drilling in our own workshop

Ordering KD36

State: NK D36/DH36 (KD36), delivery condition, sizes and quantities, UT/Z, dual-class, certificate type and port. Send to SHH STEEL.

Sample line: “Hull plate to ClassNK Rules Part K, grade KD36 (NK D36/DH36), TM, 25 × 2500 × 12000 mm, 20 pcs, NK-endorsed certificate with Ceq, EN 10204 3.2, CFR Busan/Imabari.”

FAQ

Why is the plate titled D36/DH36 but stamped KD36?
Buyers search for both A/AH-style names, but ClassNK writes its high-tensile grades with a K prefix. The plate and certificate show KD36, which equals IACS DH36.
What are the strength and toughness of KD36?
ReH ≥ 355 N/mm², Rm 490–620 N/mm², A ≥ 21 %. Charpy at −20 °C, from 34 J (≤50 mm) up to 50 J (70–100 mm) longitudinal average.
Is a TMCP KD36 plate easier to weld?
Usually. TM plate carries a Ceq limit of about 0.38 % (≤50 mm) and 0.40 % (50–100 mm), so it needs less preheat. Your NK-approved procedure still decides.
Can one heat be certified as KD36 and as ABS/DNV/LR/BV DH36?
Yes, if all the surveyors are booked before testing and the plate meets every society’s requirements. It is then stamped with each mark.
Which thicknesses of KD36 do you supply?
Typically 8–60 mm from stock or rolling, up to 100 mm by mill approval. Thicker plate needs a rolling slot.
What changes between KD32, KD36 and KD40?
Only strength: 315, 355 and 390 N/mm² yield. The Charpy temperature stays the same because the letter is the same.
How long is delivery for KD36?
About 7–15 days from stock, and 4–6 weeks for mill rolling plus survey. Confirmed per quote.
What payment terms do you accept?
T/T with the balance after inspection, or L/C at sight. Trial lots are possible.

Conclusion

NK D36/DH36 (KD36) is ClassNK high-tensile hull steel under Part K of the Rules for the Survey and Construction of Steel Ships: yield 355 N/mm², tensile 490–630 N/mm², Charpy −20 °C. An NK-classed hull accepts it only with the NK stamp and an endorsed certificate.

SHH STEEL supplies KD36 from NK-approved Chinese mills, with cutting, dual class, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X