Close view of NK Grade D hull structural steel plate, ClassNK (NK) rules

NK Grade D Shipbuilding Steel Plate

NK Grade D (KD) mild hull structural steel plate to ClassNK Rules Part K, yield 235 N/mm², Charpy at −20 °C. Supplied by SHH STEEL from NK-approved Chinese mills, from stock or mill-rolled, with cutting, dual-class and 3.2 inspection.
Keywords
NK Grade D steel plate, KD steel plate, ClassNK KD hull plate, NK D shipbuilding steel, Nippon Kaiji Kyokai Grade D, mild hull structural steel
Equivalent Grades:
DNV VL D; LR Grade D; BV Grade D; CCS Grade D; KR Grade D; ABS D; RINA Grade D; ASTM A131 Grade D; GB 712 Grade D
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

NK Grade D (KD) shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

Part K names the −20 °C mild hull steel KD, and buyers write NK Grade D. It must be killed, and above 25 mm it must also be fine-grain treated. Yield (235 N/mm²) and tensile (400–520 N/mm²) match KA and KB, so you pay for toughness, not strength. ClassNK plan approval uses it for bilge, sheer and stringer strakes of mild-steel designs.

Equivalent grades: ASTM A131 Grade D · ABS D · DNV NV D · LR Grade D · BV Grade D · CCS Grade D · KR RD · RINA Grade D · GB 712 Grade D.

The ClassNK mild-steel series runs KA/KB (no test or 0 °C), then KD (−20 °C), then KE (−40 °C). KD is the usual answer for thick secondary strakes. Never use KB in place of it.

Plates are made at a steelworks that holds ClassNK manufacturing approval for KD. They are tested in front of, or under the scheme of, an NK surveyor and stamped with the NK mark and the grade. SHH STEEL buys KD from Chinese mills with that approval. We hold common sizes in stock and roll the rest to order, with the NK survey booked at the mill.

NK Grade D / KD: key data

ItemNK Grade D (KD)
Governing rulesClassNK Rules for the Survey and Construction of Steel Ships, Part K (Materials), rolled steel for hull; aligned with IACS UR W11 Grade D (Part K chapter/table numbers not quoted — UNCERTAIN)
Trade name vs NK nameNK Grade D = KD
Strength classmild (normal strength), ReH ≥ 235 N/mm²
Deoxidationkilled ≤25 mm; killed and fine grain >25 mm
Grain refinementrequired
Delivery conditionAR / CR / N / TM per the UR W11 supply table for the ordered thickness; write it on the order
Charpy VCVN at −20 °C; fine grain above 25 mm
Thickness rangeplates up to 100 mm under UR W11 scope; above that by agreement with ClassNK
ToleranceIACS UR W13 minus tolerance as applied by ClassNK (confirm class on order — UNCERTAIN)
Documentsmill inspection certificate carrying the NK surveyor’s stamp or endorsement; EN 10204 3.1/3.2 on request

Available sizes. Chinese plate mills roll KD from about 5 mm up to 100 mm or more, in widths from 1500 to about 3500 mm and lengths up to about 18 m. Most trade is 6–30 mm thick and 2000–2500 mm wide. Thin gauges cut from coil need the coil line to be NK-approved as well.

KD chemical composition — heat and product analysis

ElementHeat (ladle) analysis, %Product (check) analysis, %Remark
C0.21 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateplate
Mn0.60 min.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Si0.10–0.35 (min. waived if Al sol. ≥0.015 %)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
P0.035 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
S0.035 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Al (acid-soluble)0.015 min. where Al is the grain refinernumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatefine-grain practice
Nb / V / Timay replace Al as grain refiner; report if addednumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cu0.35 max. (residual)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateresidual limit, UR W11 note
Cr0.30 max. (residual)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateresidual
Ni0.40 max. (residual)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateresidual
Mo0.08 max. (residual)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateresidual
Nnot specifiednumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatereport if required by purchaser
C + Mn/60.40 max.not applicable (calculated from heat analysis)calculated from heat analysis

Product (check) analysis column: ClassNK Part K specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

The ladle limits are the IACS UR W11 values, which ClassNK applies in Part K. We have not checked them against a current Part K edition (UNCERTAIN), and we do not quote Part K table numbers. The residual limits for Cu, Cr, Ni and Mo come from the UR W11 notes. The mill reports them as measured. KD drops the Mn floor to 0.60 % but adds a 0.10–0.35 % Si window (the minimum is waived when acid-soluble Al ≥ 0.015 %). Grain-refining elements are needed above 25 mm.

Product (check) analysis has no numeric tolerance in UR W11. If your yard or owner wants check analysis, agree the tolerance at enquiry and write it on the order.

KD tensile requirements

PropertyValue
Yield strength ReH235 N/mm² min.
Tensile strength Rm400–520 N/mm²
Elongation A (5.65√S0)22 % min.
Charpy temperature−20 °C

On the flat 200 mm gauge-length test piece, minimum elongation depends on thickness:

t (mm)≤55–1010–1515–2020–2525–3030–4040–50
A200 min. %1416171819202122

KA, KB, KD and KE all share this tensile band. The mill takes one tensile test per batch, with extra tests for large batches or wide thickness spreads, following the UR W11 batch rules.

KD: Charpy V-notch and delivery condition

KD is tested at −20 °C. Batch size depends on delivery condition. Above 25 mm the plate must also be fine-grain killed.

ThicknessAvg. longitudinal (J)Avg. transverse (J)
≤ 50 mm2720
50–70 mm3424
70–100 mm4127

These are average energies for three full-size specimens. One single value may fall below the average if it is at least 70 % of it. Longitudinal specimens are normal unless transverse are ordered. Over 100 mm, agree the requirements with ClassNK.

Thickness tolerance and surface quality

ClassNK uses the IACS UR W13 thickness tolerances for hull plate, which limit the minus side (commonly 0.3 mm — confirm on the order). The plus side, flatness, width and length follow the agreed standard, for example JIS G3193, EN 10029 or GB/T 709. For Japanese-designed ships ordered in Asia, mills often quote the JIS dimension tables, so state which one applies.

Surface defects may be removed by grinding, provided the remaining thickness stays inside the minus tolerance. If you shot-blast and prime at the yard, say so on the order so the plates are not oiled.

KD stock and lead time

Thickness (mm)Width (mm)Length (mm)ConditionApprox. qty
61800 / 20006000–12000AR / CR / N / TM100+ t
820006000–12000AR / CR / N / TM150+ t
102000 / 22006000–12000AR / CR / N / TM200+ t
122000 / 25006000–12000AR / CR / N / TM200+ t
162200 / 25006000–12000AR / CR / N / TM150+ t
2025006000–12000AR / CR / N / TM120+ t
2525006000–12000AR / CR / N / TM100+ t
302200 / 25006000–12000AR / CR / N / TM80+ t
4022006000–12000AR / CR / N / TM50+ t
5022006000–12000AR / CR / N / TM30+ t

Stock quantities change every week, so confirm before you book. Plates are sold as KD with the NK stamp and endorsed certificate. Sizes not in stock are rolled in about 3–5 weeks including survey.

Packing: bundled by size with steel strapping, painted with grade and heat number, shipped in containers (≤11.8 m) or break bulk.

NK Grade D (KD) compared with other societies and standards

Society / standardGradeNote
ClassNKNK Grade D / KDthis page
DNVDNV VL DUR W11 mild steel
LRLR Grade DUR W11 mild steel
BVBV Grade DUR W11 mild steel
CCSCCS Grade DUR W11 mild steel
KRKR Grade DUR W11 mild steel
ABSABS DUR W11 mild steel
RINARINA Grade DUR W11 (no product page yet)
ASTM A131ASTM A131/A131M Grade Dproduct standard; no class stamp
GB 712GB 712 Grade DChinese product standard; no class stamp
JIS G3106SM400A / SM400Bwelded structural steel, not hull steel

All of these follow the same IACS chemistry and tensile limits, so one heat can be certified to several societies if their surveyors attend together. On paper, though, only the NK stamp satisfies ClassNK, so a GB 712 or A131 mill sheet on its own is not acceptable.

Choosing between KA, KB, KD and KE

KD costs more than KB but less than KE, and covers most thick mild-steel strakes in temperate service. ClassNK’s material-grade table picks the letter from the member’s category (secondary, primary, special) and its thickness. That table, not the buyer, decides whether a strake is KD. Mild steel stops at 235 N/mm². If the design needs more, look at NK A32/AH32 to F40/FH40 under NK Steel Plates.

Compared with JIS G3106 SM400 or ASTM A36, KD has similar strength. It differs in the C + Mn/6 cap, the surveyed tests and the NK stamp, which a classed hull requires. Typical NK use: bilge and sheer strakes, stringer plates and thick longitudinal bulkhead plating in mild-steel designs that need −20 °C.

Fabrication notes for KD

KD cuts cleanly by gas, plasma or laser without preheat. It welds with consumables approved by ClassNK for mild steel at the right toughness grade (for example grade 1, 2 or 3 for A, D and E respectively, per the shipyard’s qualified procedure). Japanese and Chinese yards weld it with FCAW and one-side SAW on panel lines, under procedures the NK surveyor has approved. Thick or restrained joints may need preheat, which the procedure sets.

Cold bending and line heating are routine. Line heating is used a lot for hull curvature in Japanese practice. For plate ordered for cold flanging, state that quality on the order. For offshore primary steel, see offshore platform steel plates.

NK survey, certificates and receiving checks

The NK surveyor witnesses or audits the tests at the mill and checks the identification. The inspection certificate lists heat number, ladle analysis, tensile results, Charpy results where required, delivery condition and plate numbers, and carries the NK endorsement. On request we add EN 10204 3.2 witness by a third party, ultrasonic testing, or dual certification with ABS, DNV, LR or BV.

At your warehouse: match the stamped KD grade, heat and plate number to the certificate. Check the NK endorsement is present and that Charpy results are at −20 °C where required. Measure thickness at several points against the UR W13 / order tolerance.

Ordering errors seen with KD

  • Plate above 25 mm without fine-grain practice
  • Accepting 0 °C results for a −20 °C order
  • Using KD where yield above 235 N/mm² is needed
  • Leaving the delivery condition off the order
  • No NK endorsement

All of these can be avoided at enquiry stage. Put the full NK grade, delivery condition and certificate type on the order.

Buying KD from China: concerns and answers

ConcernAnswer
Is the NK stamp genuine?Only mills with ClassNK approval for KD; certificate and stamp traceable to the heat; third-party witness on request
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed ordersseveral sizes and NK grades in one container
Delivery visibilityweekly photos from rolling to loading
Ready-to-fit partscutting, bevelling and drilling in our own workshop

Ordering KD

Send SHH STEEL: grade (NK Grade D / KD), sizes and quantity per size, delivery condition, any dual-class or 3.2 requirement, UT or Z needs, surface finish, and destination.

Sample line: “Hull plate to ClassNK Rules Part K, grade KD (NK Grade D), 16 × 2400 × 12000 mm, 40 pcs, NK-endorsed certificate, EN 10204 3.1, FOB Shanghai.”

FAQ

Is NK Grade D the same as ClassNK KD?
Yes. ClassNK Part K designates the grade KD, and the trade usually writes NK Grade D. Put both on the order so the mill and the NK surveyor read the same grade.
What toughness does KD need?
Cvn at −20 °c; fine grain above 25 mm. Average energies are 27/20 J up to 50 mm, 34/24 J at 50–70 mm and 41/27 J at 70–100 mm (longitudinal/transverse).
Can I accept a GB 712 or ASTM A131 certificate for an NK hull?
No. They share the chemistry, but ClassNK accepts only plate from an NK-approved mill with the NK stamp and an endorsed certificate. A heat can be dual-certified if the surveyors attend before testing.
Which sizes of KD are in stock?
Mostly 6–50 mm thick, 2000–2500 mm wide, 6–12 m long. Other sizes are rolled in about 3–5 weeks. Single plates from stock are possible.
Does KD need preheat for welding?
Usually not in normal thicknesses, because C + Mn/6 is capped at 0.40. The shipyard’s NK-approved welding procedure decides. Use ClassNK-approved mild-steel consumables of the right toughness grade.
Can KD replace a tougher NK grade?
Only upwards. KE can replace KD, and KD can replace KB, if properties meet the ordered grade. KD cannot replace a grade with a lower test temperature.
How long is delivery?
About 7–15 days from stock. Mill orders take about 3–5 weeks plus survey and shipping. These are estimates, confirmed per quote.
What payment and inspection options do you offer?
T/T with a deposit and the balance after inspection, or L/C at sight. EN 10204 3.2 witness, UT and dual class with ABS, DNV, LR or BV are available if booked before testing.

Conclusion

NK Grade D (KD) is ClassNK mild hull steel under Part K of the Rules for the Survey and Construction of Steel Ships: yield 235 N/mm², tensile 400–520 N/mm², Charpy −20 °C. An NK-classed hull accepts it only with the NK stamp and an endorsed certificate.

SHH STEEL supplies KD from NK-approved Chinese mills, with cutting, dual class, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X