NK KE550 marine steel plate per ClassNK (NK) rules at SHH STEEL warehouse

NK KE550 Shipbuilding Steel Plate

NK KE550 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 550 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
Keywords
NK KE550 steel plate, ClassNK KE550, KE550 extra high strength hull steel, NK EH550 plate, Nippon Kaiji Kyokai KE550, UR W16 marine plate
Equivalent Grades:
DNV VL E550; LR EH55; BV E550; CCS EH550; KR RE56; ABS EH55; RINA per rules; GB 712 EH550
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

NK KE550 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

NK KE550 combines 550 N/mm² yield with −40 °C Charpy toughness. ClassNK names its extra-high-strength steels with the K prefix, the toughness letter and the yield in N/mm²: KA, KD, KE or KF followed by 550. The 550 level is a quenched-and-tempered or advanced TMCP level for jack-up legs, cranes and highly loaded offshore members. It follows IACS UR W16: ReH ≥ 550 N/mm², Rm 670–835 N/mm², A ≥ 16 %.

Equivalent grades: ASTM A131 (no direct grade at this strength) · ABS EH55 / EQ56 · DNV NV E550 · LR EH55 · BV E550 · CCS EH550 · KR RE56 · RINA E550 · GB 712 Grade EH550.

KE550 is made TMCP or quenched and tempered at a mill whose NK approval covers this exact grade and thickness range. It is rolled to order rather than held in stock. SHH STEEL places the order at an NK-approved Chinese mill and arranges the NK survey, with dual class and 3.2 inspection on request.

KE550 key data

ItemNK KE550
Governing rulesClassNK Rules Part K, extra-high-strength rolled steel; IACS UR W16 (Part K numbering UNCERTAIN)
DesignationKE550: K + toughness letter E + yield 550 N/mm²
StrengthReH ≥ 550, Rm 670–835 N/mm², A ≥ 16 %
Charpy V−40 °C; avg. ≥ 55 J L / 37 J T (UR W16-aligned; confirm)
Delivery conditionTM or QT within approved thickness (N only if specially approved)
Steelmakingkilled, fine-grain; vacuum degassing typical
UTusually ordered for this class — agree standard and level
ToleranceIACS UR W13 (confirm class)
DocumentsNK-endorsed certificate incl. Ceq / CET / Pcm; EN 10204 3.2 on request

The maximum thickness depends on the mill’s approval. TM KE550 is often approved to about 50–80 mm and QT thicker, but treat the approval sheet as the limit (UNCERTAIN).

KE550 chemical composition — full alloy list

ElementHeat (ladle) analysis, %Product (check) analysis, %Remark
C0.21 max. (often 0.14–0.20 by route/condition; TM/QT may tighten)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Mn1.70 max. (typically 1.00–1.70; QT route may differ)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Si0.55 max. (QT may allow up to ~0.80 — confirm on mill approval)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
P0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
S0.025 max. (some EQ-style routes tighter — confirm)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Al0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control unless other N-binders)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificategrain refiner / N binder
Nb0.05 max. (when used; combined microalloy caps apply)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
V0.10 max. (when used; combined caps apply)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ti0.05 max. (when used; combined caps apply)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cu0.50 max. (route-dependent; often ≤0.35 in practice)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cr0.20–0.25 max. (route-dependent)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ni2.00 max. or per mill approval (often lower on AH/DH routes)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatetoughness
Mo0.08–0.50 (route-dependent; QT may allow higher)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatehardenability (QT)
B0.005 max. (when intentionally added)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatehardenability (QT)
N0.015 max. (tighter control when Al is the sole N-binder)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Nb+V+TiNb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approvalnot applicable (calculated from heat analysis)combined
Ceq / CET / PcmCeq / CET / Pcm maxima by category and condition on mill approval — report on certificatenot applicable (calculated from heat analysis)calculated

Product (check) analysis column: ClassNK Part K specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

These rows give the UR W16 envelope. ClassNK fixes the exact limits for each mill at approval, so the approval sheet and the order govern (UNCERTAIN vs Part K text). At 550, QT with Ni–Cr–Mo and sometimes B is the norm. Every intentionally added element must appear on the certificate, along with Ceq, CET or Pcm.

KE550 tensile and impact requirements

PropertyValue
ReH (or Rp0.2)550 N/mm² min.
Rm670–835 N/mm²
A16 % min. (transverse)
Charpy−40 °C, ≥ 55 J L / 37 J T

Tests are taken per heat-treatment batch or rolled length, as the approval requires. Thick plate may need extra mid-thickness tests. Results are as per standard and mill certificate.

KE550: toughness and delivery condition

Charpy specimens are usually taken at quarter thickness and tested at −40 °C. Delivery is TM or QT. The choice changes the mill, price and welding behaviour, so state it on the order. At this toughness level, many owners also ask for CTOD or brittle-crack-arrest data. Those are separate requirements (UNCERTAIN), so specify them.

Thickness tolerance and surface quality

Minus tolerance follows UR W13. Plus tolerance and flatness follow the agreed standard. QT plate is flatter than heavy TM plate but harder to straighten, so agree the flatness class at enquiry.

KE550 mill-roll supply

Thickness (mm)Width (mm)ConditionTypical lot
122000 / 2500TM / QTper heat / rolling
162200 / 2500TM / QTper heat / rolling
202500TM / QTper heat / rolling
252500TM / QTper heat / rolling
302200 / 2500TM / QTper heat / rolling
402200TM / QTper heat / rolling
502200TM / QTper heat / rolling

KE550 is not held as open stock. These are the sizes we normally quote against mill rolling slots. Lead time is about 6–10 weeks including NK survey (commercial estimate).

Packing: bundled by size with steel strapping, painted with grade and heat number, shipped in containers (≤11.8 m) or break bulk.

NK KE550 compared with other societies

Society / standardGradeNote
ClassNKNK KE550this page
DNVDNV VL E550
LRLR EH55LR numbers by yield/10
BVBV E550no H
CCSCCS EH550
KRKR RE56KR yield-class number
ABSABS EH55 / EQ56ABS commercial / official
RINARINA (per rules)not verified
ASTM A131no equivalentstops at FH40
GB 712GB 712 Grade EH550product standard

All sit in the same UR W16 band. The names differ, and only the NK stamp counts for ClassNK.

Where KE550 sits in the ClassNK extra-high-strength series

The neighbours are KE500 below and KE620 above. Within level 550, the letter sets the test temperature: KA 0 °C, KD −20 °C, KE −40 °C, KF −60 °C. Moving to a different level needs ClassNK plan approval. Typical uses: upper-deck crack-arrest strakes, hatch coamings of large container ships and LNG/LPG carrier structure needing −40 °C, at extra-high strength. See NK Steel Plates and offshore platform steel plates.

Fabricating KE550

Welding needs a procedure qualified on KE550 and approved by ClassNK, with low-hydrogen consumables of matching strength and −40 °C toughness. Heat input must be limited to protect HAZ toughness in QT plate. Preheat is usually needed on thick sections. Do not hot form or stress relieve above the tempering temperature without agreement from the mill and ClassNK.

NK survey, certificates and receiving checks

The certificate gives the full alloy analysis, Ceq/CET/Pcm, tensile results, −40 °C Charpy results, delivery condition, UT result and plate numbers, with the NK endorsement. On receipt, check the KE550 stamp, impact temperature and NK endorsement. Dual class with ABS, DNV, LR or BV and 3.2 witness are available.

Ordering errors seen with KE550

  • Writing AH550 or A550 without ClassNK, so the plate gets the wrong stamp
  • Leaving TM vs QT open
  • No UT requirement
  • Ceq/Pcm not requested
  • Ordering from a mill whose NK approval does not cover the thickness
  • Expecting an ASTM A131 dual certificate

Buying KE550 from China: concerns and answers

ConcernAnswer
Is the NK stamp genuine?Only mills with ClassNK approval for KE550; certificate and stamp traceable to the heat; third-party witness on request
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed orderssizes grouped onto one heat where possible
Delivery visibilityweekly photos from rolling to loading
Ready-to-fit partscutting, bevelling and drilling in our own workshop

Ordering KE550

State NK KE550, TM or QT, sizes and quantities, UT level, dual class, certificate type and port. Send to SHH STEEL.

Sample line: “Plate to ClassNK Rules Part K, grade KE550, QT, 40 × 2500 × 10000 mm, 8 pcs, UT EN 10160 S1E1, NK-endorsed certificate with Pcm, EN 10204 3.2.”

FAQ

What does the name KE550 mean?
K is the ClassNK prefix, E is the toughness letter (−40 °C), and 550 is the minimum yield in N/mm². It is the IACS UR W16 EH550 grade.
Is KE550 available from stock?
Rarely. It is rolled to order at an NK-approved mill, typically in 6–10 weeks including survey.
TM or QT — which should I order?
QT is usual at this level, especially in thick plate. TM is possible in thinner gauges where the approval allows. State it on the order.
What impact energy is required?
Indicatively at least 55 J longitudinal or 37 J transverse average at −40 °C (UR W16-aligned; confirm on the certificate).
Which elements appear on the certificate?
C, Mn, Si, P, S, Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B and N where added, plus Ceq, CET or Pcm.
Can KE550 be dual-certified?
Yes, with ABS, DNV, LR or BV, if all the surveyors attend the same tests.
What welding precautions apply?
Use a ClassNK-approved procedure qualified on this grade, low-hydrogen consumables and controlled heat input. Do not apply post-weld heat above the tempering temperature.
What payment terms do you accept?
T/T with a deposit and the balance after inspection, or L/C at sight.

Conclusion

NK KE550 (KE550) is ClassNK extra-high-strength hull steel under Part K of the Rules for the Survey and Construction of Steel Ships: yield 550 N/mm², tensile 670–835 N/mm², Charpy −40 °C. An NK-classed hull accepts it only with the NK stamp and an endorsed certificate.

SHH STEEL supplies KE550 from NK-approved Chinese mills, with cutting, dual class, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X