ASTM A992 Steel Structural Profiles

SHH STEEL supplies ASTM A992 high-strength low-alloy steel beams, the usual specification for wide-flange W-shapes in building frames. Common designations include W8, W10, W12, W14, W16, and W18 (for example W12×26, W14×22, or W16×26). Other dimensional series are supplied only when specified and certified, and are not treated as equivalent W-shapes. Dual certification (for example with A572 Grade 50) is provided only when it is stated on the mill certificate. Sizes and certificates are confirmed per inquiry.

ASTM A992 Wide Flange H Beam | ASTM A992 Wide Flange H Beams - SHH STEEL

ASTM A992 Wide Flange H Beam

ASTM A992 steel beam is a rolled structural W-shape to ASTM A992/A992M, with a 50–65 ksi [345–450 MPa] yield window, 65 ksi [450 MPa] minimum tensile strength and a reported carbon-equivalent cap. Dimensions follow ASTM A6/A6M, not HE or HW series. SHH STEEL reviews grade, size, CE and certificate requirements before quoting.
View More

ASTM A992 Steel Structural Profiles

H Beams and Wide Flange Beams HH STEEL supplies hot-rolled steel beam profiles

H Beams and Wide Flange Beams

SHH STEEL supplies hot-rolled steel beam profiles for buildings, bridges, and industrial frames. Material is specified to the project standard—for example ASTM A36, A572, A992, or A709; ASME SA-36 or SA-992; EN 10025-2; GB/T 11263 with GB/T 700 or GB/T 1591 grades; JIS G 3101; ISO 630-1; or GOST practice. Dimensional series are ordered separately and may include ASTM A6 W, S, and HP shapes; EN 10365 HEA, HEB, HEM, and IPE; BS 4-1 UB and UC; GB/T 11263 HW, HM, and HN (and split T); and JIS G 3192 H-sections and I-beams, with designations such as H 300×300×10×15. HW, HM, and HN are GB/T 11263 series names, not JIS nomenclature. A grade such as ASTM A36 can be furnished in EN-series dimensions when so specified and certified; W, HEA, and metric H-sections are not equivalent by nominal depth. Available sizes and certificates are confirmed with each inquiry. This range covers H Beams and Wide Flange Beams. Buyers also search these sections as H Beam, H-Beam, or Steel H Beams; the usual US name is Wide Flange Beam (W shape). Typical series on these pages are ASTM A6 W shapes, EN 10365 HEA, HEB and HEM, GB/T 11263 HW, HM and HN, and JIS G 3192 H-sections. I Beams are a different product family and are listed separately.