ASTM A265/A265M

Product Showcase

ASTM A265/A265M Clad Steel Plates

SHH STEEL offers ASTM A265/A265M (ASME SA-265) nickel alloy clad plates, with Inconel 625, Incoloy 825, Hastelloy C276, Monel 400 or Nickel 200 cladding on SA516 Gr.70 and other pressure vessel steels. ASTM A265 specifies carbon or low-alloy steel base plate integrally bonded to nickel or nickel-base alloy cladding, with shear and ultrasonic bond tests. Certified, customizable. Trust SHH STEEL!

ASTM A265 SA387 Gr.22 Cl.2 + Inconel 625 Nickel Alloy Clad Plate

ASTM A265 SA387 Gr.22 Cl.2 + Inconel 625 clad plate bonds alloy 625 (UNS N06625) to a 2¼Cr-1Mo pressure vessel base for hot, high-pressure hydrogen equipment with corrosive process sides. SHH STEEL produces it by explosion bonding with normalizing and tempering, simulated PWHT, shear and UT tests as ordered.
View More

ASTM A265 SA516 Gr.60 + Monel 400 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.60 + Monel 400 clad plate bonds nickel-copper alloy 400 (UNS N04400) to a lower-carbon SA516 Grade 60 pressure vessel base. It suits HF alkylation, crude overhead and seawater vessels at moderate pressure, with good weld hardness control. SHH STEEL produces it by explosion bonding with shear and UT tests.
View More

ASTM A265 SA516 Gr.70 + Incoloy 800H Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Incoloy 800H clad plate bonds iron-nickel-chromium alloy 800H (UNS N08810) to a carbon steel pressure vessel base. The alloy face resists oxidation, carburization and chloride stress corrosion cracking while the steel carries the load. SHH STEEL produces it by explosion bonding with shear and UT tests.
View More

ASTM A265 SA516 Gr.70 + Alloy 20 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Alloy 20 clad plate bonds niobium-stabilized alloy 20 (UNS N08020) to a carbon steel pressure vessel base. Its nickel, copper and molybdenum resist sulfuric acid and chloride stress corrosion cracking. SHH STEEL produces it by explosion bonding with shear and UT tests as ordered.
View More

ASTM A265 SA516 Gr.70 + Alloy 59 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Alloy 59 clad plate bonds low-carbon nickel-chromium-molybdenum alloy 59 (UNS N06059) to a carbon steel pressure vessel base. With 23 % chromium and 16 % molybdenum it resists oxidizing and reducing acids and severe chlorides. SHH STEEL produces it by explosion bonding with shear and UT tests as ordered.
View More

ASTM A265 SA516 Gr.70 + Hastelloy B-3 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Hastelloy B-3 clad plate bonds nickel-molybdenum alloy B-3 (UNS N10675) to a carbon steel pressure vessel base. With about 28 to 30 % molybdenum it resists hydrochloric acid at all concentrations in reducing conditions. SHH STEEL produces it by explosion bonding with shear and UT tests as ordered.
View More

ASTM A265 SA516 Gr.70 + Hastelloy C22 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Hastelloy C22 clad plate bonds alloy C-22 (UNS N06022) to a carbon steel pressure vessel base. With 22 % chromium and 13 % molybdenum, C-22 resists both oxidizing and reducing acids and severe chloride pitting. SHH STEEL produces it by explosion bonding, with 140 MPa shear and ultrasonic tests when ordered.
View More

ASTM A265 SA516 Gr.70 + Inconel 600 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Inconel 600 clad plate bonds nickel-chromium-iron alloy 600 (UNS N06600) to a carbon steel pressure vessel base. Alloy 600 resists hot caustic with oxidizing impurities, chloride stress corrosion cracking and high-temperature oxidation. SHH STEEL produces it by explosion bonding, with 140 MPa shear and UT when ordered.
View More

ASTM A265 SA516 Gr.70 + Nickel 201 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Nickel 201 clad plate bonds low-carbon pure nickel (UNS N02201) to a carbon steel pressure vessel base. Its 0.02 % carbon limit prevents graphitization, so it is the nickel cladding for caustic service above about 315 °C. SHH STEEL produces it by explosion bonding, with 140 MPa shear and ultrasonic tests when ordered.
View More

ASTM A265 SA516 Gr.70 + Nickel 200 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Nickel 200 clad plate bonds commercially pure nickel (UNS N02200) to a carbon steel pressure vessel base. Pure nickel is the classic material for caustic soda evaporators and concentrators below about 315 °C. SHH STEEL produces it by explosion bonding, with 140 MPa shear and ultrasonic tests when ordered.
View More

ASTM A265 SA516 Gr.70 + Monel 400 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Monel 400 clad plate bonds nickel-copper alloy 400 (UNS N04400) to a carbon steel pressure vessel base. It resists hydrofluoric acid, seawater, brines and crude unit overhead corrosion at a fraction of solid alloy cost. SHH STEEL produces it by explosion bonding, with 140 MPa shear and ultrasonic tests when ordered.
View More

ASTM A265 SA516 Gr.70 + Hastelloy C276 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Hastelloy C276 clad plate bonds alloy C-276 (UNS N10276) to a carbon steel pressure vessel base by explosion bonding. Its 15 to 17 % molybdenum and tungsten resist strong reducing acids, wet chlorine and FGD condensate. SHH STEEL produces it in common thickness pairs, with 140 MPa bond shear and ultrasonic tests when ordered.
View More

Nickel Alloy Clad Plates

SHH STEEL, a top Nickel Alloy Clad Plates exporter, produces and exports nickel alloy clad plates for oil, gas, and power industries. Our plates, with Inconel 625 or Hastelloy C276 cladding (ASTM A265), ensure high-temperature strength and corrosion resistance. We deliver in 15-35 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for Inconel clad plates and custom solutions.

Nickel Alloy Clad Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X