ASTM A265 SA516 Gr.70 + Inconel 600 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Inconel 600 clad plate bonds nickel-chromium-iron alloy 600 (UNS N06600) to a carbon steel pressure vessel base. Alloy 600 resists hot caustic with oxidizing impurities, chloride stress corrosion cracking and high-temperature oxidation. SHH STEEL produces it by explosion bonding, with 140 MPa shear and UT when ordered.
Keywords
Inconel 600 clad plate, alloy 600 clad steel plate, ASTM A265 600, SA516 Gr.70 + N06600, nickel chromium clad plate
Equivalent Grades:
ASME SA-265, JIS G3602, NB/T 47002.2; 600 = N06600 / 2.4816 / NS3102
Share:
General Description
Material Specification
Base and Cladding Materials
Bonding Methods
Chemical Composition
Mechanical Properties
Heat Treatment
Tolerances
Available Sizes
Weldability
Applications
Testing and Certification
Equivalent Material Grade
Why choose Us
FAQ
Conclusion

What is ASTM A265 SA516 Gr.70 + Inconel 600 nickel alloy clad plate?

ASTM A265 SA516 Gr.70 + Inconel 600 nickel alloy clad plate is a composite plate in which alloy 600 (UNS N06600, widely known as Inconel 600), a nickel-chromium-iron alloy, is metallurgically bonded to an SA516 Grade 70 carbon steel base. The carbon steel carries pressure and structural loads; the nickel alloy face resists the corrosive medium. It is ordered to ASTM A265, or the identical ASME SA-265, the specification for nickel and nickel-base alloy-clad steel plate.

Fabricators write it as SA516 Gr.70 + N06600, SA516 Gr.70 + Inconel 600 or SA516 Gr.70 + alloy 600. Alloy 600 is nickel with about 15 % chromium and 8 % iron. Chromium adds resistance to oxidizing conditions and sulfur that pure nickel lacks, while the high nickel keeps it immune to chloride stress corrosion cracking and resistant to caustic.

In clad plate form alloy 600 is used in two main ways: in caustic and alkali equipment where the stream carries oxidizing species or sulfur compounds, and in vessels that run hot, where its oxidation resistance and stable structure matter.

SHH STEEL can produce Inconel 600 clad plate by explosion bonding, the usual route for nickel alloy claddings, and certifies each plate to the A265 tests on the order. Other nickel alloy claddings are listed under nickel alloy clad plates.

ASTM A265 / ASME SA-265 requirements for Inconel 600 clad plate

ASTM A265 covers plate of a carbon or low-alloy steel base with nickel or a nickel-base alloy integrally and continuously bonded to one or both faces. It is written mainly for pressure vessels but may be used in other structural applications where corrosion resistance is needed. ASME publishes it as SA-265, identical with ASTM A265-12(2019).

Item Requirement for SA516 Gr.70 + Inconel 600
Cladding B168 / SB-168 UNS N06600 (alloy 600)
Other permitted claddings Alloys of B127, B162, B168, B333, B409, B424, B443, B463, B575, B582, B625, or others agreed
Base steel SA516 Grade 70; the standard allows pressure vessel or general structural steels (A20/A20M or A6/A6M)
Product size “Plate” means 3/16 in (4.8 mm) and over in thickness and over 10 in (254 mm) wide
Bond strength 140 MPa (20 000 psi) minimum shear, or three bond bend tests, when the purchaser requires them
Bond integrity Visual below 10 mm total; ultrasonic to A578/A578M procedures at 10 mm and over; Class 1, 3 or 5
Clad surface As-rolled, blasted (descaled and pickled) or 100 % conditioned, unless otherwise specified
Marking Per A20 or A6 for the base, plus the alloy designation and the specification number

A complete order line reads: “Clad plate to ASME SA-265, cladding SB-168 UNS N06600, annealed, 3 mm minimum; base SA-516 Grade 70, 25 mm minimum; Class 1 bond quality, 100 % UT (S12); shear test required; simulated PWHT per S3.” Give the design temperature and medium, so the cladding thickness and base steel can be checked.

SA516 Gr.70 base and Inconel 600 cladding

A265 certifies each layer to its own specification: the cladding to ASTM B168 and the base to ASTM A516 / ASME SA-516. The pairing puts an expensive corrosion alloy only on the wetted face.

Why Inconel 600 is chosen

Alloy 600 contains at least 72.0 % nickel (with cobalt), 14.0 to 17.0 % chromium and 6.0 to 10.0 % iron, with carbon up to 0.15 %, manganese up to 1.00 %, silicon up to 0.50 %, copper up to 0.50 % and sulfur up to 0.015 %. Annealed plate is strong for a corrosion alloy, with at least 550 MPa tensile and 240 MPa yield.

It resists caustic soda well and better than nickel when oxidizing species or sulfur are present, and it is practically immune to chloride stress corrosion cracking. It is not a strong-acid alloy: for reducing or mixed acids, molybdenum-bearing alloys such as C-276 or C-22 are used.

SA516 Grade 70 base steel

ASME SA516 Grade 70 is the usual base: a carbon-manganese vessel plate with 485 to 620 MPa tensile and 260 MPa minimum yield, available normalized and impact tested. Outside ASME work it is bought as ASTM A516 Grade 70. For high-temperature hydrogen or creep service, a Cr-Mo base such as ASTM A387 Grade 11 Class 2 can replace it.

Alloy 600 compared with other nickel alloy claddings

Cladding Key alloying, % Typical reason to choose it
Alloy 600 (N06600) Ni 72 min, Cr 14–17, Fe 6–10 Hot caustic with oxidizers or sulfur; high temperature
Nickel 201 (N02201) Ni 99.0 min, C 0.02 max Clean hot caustic
Alloy 625 (N06625) Cr 20–23, Mo 8–10 Chloride pitting, seawater, FGD
Alloy 825 (N08825) Ni 38–46, Cr 19.5–23.5, Mo 2.5–3.5 Sulfuric and phosphoric acid

How Inconel 600 clad plate is made

Explosion bonding is the main manufacturing route for nickel alloy clad plate, because it joins alloys of very different strength and melting behaviour without melting either one. Roll bonding is also possible for some nickel alloys and plate sizes, and weld overlay is the alternative for shapes that cannot be clad as plate.

Explosion bonding

The Inconel 600 sheet is positioned above the SA516 plate with a controlled gap and covered with explosive. The detonation accelerates the cladding onto the base at an oblique angle; surface oxides are jetted away and the metals bond in the solid state with a wavy interface. There is no dilution, so the cladding chemistry at the surface is exactly that of the sheet. A265 permits the cladding to be made from several sheets welded together for plates wider than the available alloy sheet, with that welding qualified to ASME Section IX.

Clad plate or weld overlay?

Alloy 600 type overlay with ERNiCr-3 is common on nozzles, but iron dilution changes the surface chemistry. A clad plate gives undiluted B168 alloy over the whole face.

Chemical composition of Inconel 600 cladding and SA516 Gr.70 base

The chemical composition is certified layer by layer by the clad plate manufacturer: the cladding to ASTM B168 and the base to SA-516.

Inconel 600 cladding (UNS N06600), heat analysis

Element Inconel 600 (UNS N06600), % (ASTM B168)
Nickel (Ni), incl. cobalt 72.0 min
Chromium (Cr) 14.0 – 17.0
Iron (Fe) 6.0 – 10.0
Carbon (C) 0.15 max
Manganese (Mn) 1.00 max
Silicon (Si) 0.50 max
Copper (Cu) 0.50 max
Sulfur (S) 0.015 max

These are the B168 limits for UNS N06600. Product analysis, when required, is made to ASTM B880 tolerances.

Product analysis of the cladding is made only when the purchaser asks for it, and the results must meet the cladding specification. For wet chemical analysis A265 asks the laboratory to discard all base metal plus 40 % of the cladding thickness from the bonded side, up to 1.6 mm, so that iron from the steel does not distort the result; spectrometric samples are taken on the centre line of the cladding.

SA516 Grade 70 base steel

Element SA516 Gr.70 heat analysis, % SA516 Gr.70 product analysis, %
Carbon (C), 12.5 mm and under 0.27 max 0.27 max
Carbon (C), over 12.5 to 50 mm 0.28 max 0.28 max
Carbon (C), over 50 to 100 mm 0.30 max 0.30 max
Carbon (C), over 100 mm 0.31 max 0.31 max
Manganese (Mn) 0.85 – 1.20 0.79 – 1.30
Phosphorus (P) 0.025 max 0.025 max
Sulfur (S) 0.025 max 0.025 max
Silicon (Si) 0.15 – 0.40 0.13 – 0.45
Iron (Fe) Balance Balance

Carbon, phosphorus and sulfur limits apply to heat and product analysis alike. For each 0.01 % carbon below the maximum, the manganese maximum may rise by 0.06 %, up to 1.50 % by heat analysis and 1.60 % by product analysis.

Mechanical properties and bond strength

A265 tests the tensile properties, the bond strength and the bond integrity of the plate in its delivered condition.

Tensile test

Condition Tensile test Acceptance
Composite 38 mm and under, base minimum tensile 485 MPa or less and minimum yield 275 MPa or less Full-thickness composite specimen Base minimum up to base maximum plus 35 MPa
Composite over 38 mm, or stronger base Base steel only All base steel tensile requirements
Cladding for corrosion allowance only Cladding need not be included All base steel tensile requirements

Properties of the two layers

Property Inconel 600 cladding (ASTM B168) SA516 Gr.70 base
Tensile strength 550 MPa (80 ksi) min (hot-rolled, annealed plate) 485 – 620 MPa
Yield strength (0.2 % offset) 240 MPa (35 ksi) min 260 MPa min
Elongation 30 % min 21 % min in 50 mm; 17 % min in 200 mm
Hardness Not specified for acceptance in B168 Not specified

Alloy 600 is stronger in tension than SA516 Gr.70. When a full-thickness composite test applies, the A265 rule sets the range from both layers, and alloy 600 raises the upper limit slightly.

Shear and bend tests

When required, the minimum shear strength between cladding and base is 20 000 psi (140 MPa), with at least 1.9 mm of cladding on the specimen and one test per plate as rolled. As an alternative, three bond bend tests through 180° with the cladding in compression are made; at least two must show no more than 50 % separation on either edge.

Ultrasonic bond quality

Class Largest single unbonded area Total unbonded area
Class 1 25 mm (1 in) longest dimension 1 % of clad surface
Class 3 75 mm (3 in) longest dimension 3 % of clad surface
Class 5 58 cm² (9 in²) 5 % of clad surface

The class must be listed on the order; when none is given, plates may be supplied as Class 5. Scanning extent is the manufacturer’s choice unless 100 % coverage, Supplementary Requirement S12, is ordered. Vessels for hot caustic and high-temperature service are normally ordered Class 1 with 100 % coverage.

Heat treatment of Inconel 600 clad plate

A265 does not impose a single heat treatment. Unless the cladding or base specification requires a specific treatment, or the purchaser and manufacturer agree otherwise, the clad plate is furnished in a condition appropriate for the cladding alloy, the base metal, or both.

Alloy 600 clad plate is supplied as-clad and flattened, or stress relieved by agreement, with the alloy sheet annealed before bonding. It tolerates SA516 stress relief and PWHT without harm.

In some caustic services, long exposure in the as-welded or sensitized condition can lead to intergranular attack; follow the licensor’s or the end user’s heat treatment rules where they exist. Keep sulfur-bearing contamination away before any heating.

If the vessel will be post-weld heat treated, order Supplementary Requirement S3 so the test coupons see a simulated PWHT, and state temperature, holding time and number of cycles.

Thickness tolerances and surface finish

Cladding, base and total thickness may each be ordered as minimum or nominal values.

Item ASTM A265 requirement
Ordered to minimum thickness Cladding, base and total not below the ordered minimums
Nominal: base steel or total 0.3 mm under
Nominal: cladding 0.8 mm under
Over-tolerance of the total Greater of 3 mm or 10 % of the ordered total, provided each minimum is met
Width, length, flatness A20/A20M or A6/A6M, as appropriate for the base

Order the alloy 600 cladding as a minimum thickness, usually 2 to 3 mm for shells and more for tube sheets.

Stock sizes and thickness combinations of Inconel 600 clad plate

SA516 Gr.70 + Inconel 600 clad plate is ordered by cladding plus base thickness, width and length. SHH STEEL keeps common sizes in stock or produces them quickly, and any other pair inside the production range can be made to order.

Cladding + base, mm Total, mm Typical use
2 + 12 14 Caustic tanks
3 + 14 17 Vessel shells
3 + 20 23 Pressure vessels
3 + 25 28 Hot service shells
4 + 30 34 Heads
5 + 40 45 Tube sheets
6 + 50 56 Tube sheets
8 + 70 and over 78 and over Heavy sections, explosion bonded
Dimension Production range
Cladding thickness 2 mm to 20 mm (thicker by explosion bonding on request)
Base steel thickness 6 mm to 200 mm
Total thickness 8 mm to 220 mm
Width 1000 mm to 3000 mm; wider by explosion bonding with welded cladding
Length 2000 mm to 12000 mm
Discs and blanks Round tube sheet blanks and head blanks cut to drawing
Location China

For nickel alloys, the cladding is usually 2 to 6 mm because of alloy cost; tube sheets take thicker layers so that tube-to-tubesheet welds stay inside the alloy.

Welding SA516 Gr.70 + Inconel 600 clad plate

Clad joints are welded in two parts: a carbon steel weld for strength, then a nickel alloy overlay that restores the Inconel 600 face. Carbon steel filler must not reach the cladding.

  1. Prepare the joint to the qualified procedure, usually bevelled from the steel side with the cladding cut back from the root.
  2. Weld the SA516 Gr.70 with matching carbon steel filler.
  3. Back-gouge the clad side to sound weld metal.
  4. Overlay the carbon steel weld with ERNiCr-3 (AWS A5.14) or ENiCrFe-3 (AWS A5.11), using enough layers to bring iron dilution at the surface within the limit the service needs.
  5. Clean the finished overlay; nickel alloys are not normally pickled like stainless steel, but heat tint and slag must be removed.

ERNiCr-3 tolerates iron dilution well and is the usual filler for alloy 600 and for nickel alloy to steel joints. Lay two or more layers over the steel weld for a surface close to cladding chemistry.

Procedures and welders are qualified to ASME Section IX, which A265 also requires for welded cladding and for cladding repairs. Repairs are checked by liquid penetrant and reported on the certificate.

Applications of Inconel 600 clad plate

Inconel 600 clad plate is used where caustic or high-temperature service needs more than pure nickel.

  • Caustic evaporators handling liquor with chlorates or other oxidizers.
  • Alumina digesters and Bayer process vessels.
  • Chemical vessels for organic chlorides and fatty acids.
  • Heat treatment and furnace components in clad form.
  • Pulp and paper alkali recovery equipment.
  • Vinyl chloride and chlorinated hydrocarbon processing.

Inconel 600 clad plate vs solid alloy 600

For vessel walls over about 10 mm, clad plate saves most of the alloy, and the steel base welds to carbon steel shells and nozzles with ordinary procedures.

Testing and certification

The A265 certificate reports the chemical analysis of both layers, the Section 7 test results, the bond quality class and any additional tests on the order.

Test or document Basis Frequency / note
Chemical analysis of both layers SA-516 and ASTM B168 Each heat; product analysis (S2) if ordered
Tensile test A265 and the base specification Each plate as rolled
Shear test or three bond bend tests A265 When specified
Ultrasonic bond inspection A578/A578M procedures, Class 1/3/5 10 mm and thicker; 100 % with S12
Charpy V-notch impact Supplementary Requirement S5 When ordered for the base
Simulated PWHT of coupons Supplementary Requirement S3 When the vessel is heat treated
Corrosion test of cladding Agreed method When ordered
Penetrant test of cladding repairs A265 Section 14 Each repair, reported with location and procedure
Mill test certificate EN 10204 3.1; 3.2 with third-party inspection on request Each plate or lot

If your project does not accept weld repairs of the cladding, or wants to approve them first, state that restriction on the order; A265 lists it as a purchaser option.

Equivalent standards and grades

Other standards describe the same product with their own test levels; use them to cross-check, not to substitute without review.

Standard Scope Bond shear requirement
ASTM A265 / ASME SA-265 Nickel and nickel-base alloy-clad steel plate 140 MPa min, when specified
JIS G3602 Nickel and nickel alloy clad steels Per JIS G3602
NB/T 47002.2 Clad plate for pressure equipment, nickel-steel Per NB/T 47002.2
Layer ASTM / ASME UNS EN / W.Nr. JIS GB
Cladding B168 / SB-168 UNS N06600 (alloy 600) UNS N06600 2.4816 (NiCr15Fe) NCF600 NS3102
Base A516 / SA-516 Grade 70 K02700 P355GH (approx.) SGV480 (approx.) GB/T 713 Q345R (approx.)

Chinese projects order the same product under NB/T 47002.2 with NS3102 cladding; Japanese projects use JIS G3602 with NCF600. Stainless claddings for milder duty are covered under ASTM A264.

Why order Inconel 600 clad plate from SHH STEEL

SHH STEEL is a clad plate manufacturer in China supplying nickel alloy clad plate to vessel, heat exchanger and FGD fabricators. For alloy 600 orders we confirm the medium and temperature, and whether Nickel 201 or alloy 625 would serve better, before quoting.

  • We check the enquiry against ASTM A265 and flag missing items: cladding specification, bond class, shear test, PWHT simulation.
  • We quote cladding and base thicknesses separately, as minimum or nominal.
  • The nickel alloy sheet and the base plate come with traceable mill certificates; UT maps are supplied when 100 % coverage is ordered.
  • Tube sheet discs and head blanks can be cut to drawing.

FAQ

Where is Inconel 600 clad plate used?
In caustic equipment where oxidizing species or sulfur are present, in alumina and alkali processing, and in vessels that run at high temperature.
Is alloy 600 better than nickel for caustic?
In clean caustic, nickel is equal and cheaper. Alloy 600 is better when the caustic contains oxidizers or sulfur, or at high temperature.
What are the mechanical properties of alloy 600 plate?
B168 hot-rolled annealed plate: 550 MPa minimum tensile, 240 MPa minimum yield and 30 % elongation.
Which filler is used for SA516 Gr.70 + Inconel 600?
Carbon steel filler for the base and ERNiCr-3 or ENiCrFe-3 for the cladding side.
Is ASME SA-265 the same as ASTM A265?
Yes in content. ASME publishes A265 as SA-265 in Section II Part A, identical with ASTM A265-12(2019). Order SA-265 for ASME Code vessels.
What is the HS code for nickel alloy clad plate?
Nickel alloy clad steel plate on a non-alloy steel base, 600 mm or wider, is commonly declared under HS 7210.90, flat-rolled products of iron or non-alloy steel, clad, plated or coated, other. The clad plate HS code depends on the base steel and width: narrower or alloy-steel-base plates fall under other headings, so confirm with your customs broker.
What should I send for a quotation?
ASTM A265 or ASME SA-265, Inconel 600 cladding thickness and specification, base grade and thickness, width, length or drawing, quantity, UT class and coverage, shear or bend test, heat treatment and PWHT simulation, and certificate type.

Request a quotation for ASTM A265 SA516 Gr.70 + Inconel 600 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Inconel 600 nickel alloy clad plate bonds B168 alloy 600 to an SA516 Grade 70 base, with 140 MPa shear when specified and ultrasonic Class 1, 3 or 5. It is the clad plate for hot caustic with oxidizers and for high-temperature process vessels.

Send the thickness pair, plate size or drawing, quantity, tests and certificate type to SHH STEEL, or compare other claddings on our nickel alloy clad plates page. Availability, testing and delivery are confirmed with each quotation.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X